Strengthening Mechanisms and Failure

Learn why metals deform by the motion of dislocations and how engineers make that motion harder: by refining grains, dissolving alloying atoms and cold working, and by annealing to restore ductility. Then analyze how parts fail: ductile and brittle fracture, fracture toughness and the ductile-to-brittle transition, fatigue under fluctuating loads, and creep at high temperature. Worked calculations cover resolved shear stress, the Hall–Petch equation, percent cold work, critical crack size, S–N curves, creep rates and the Larson–Miller parameter.

BeginnerLesson 5 of 9 in Materials Science and Engineering Course

What you will learn

  1. Describe how dislocations move through a crystal, why slip needs far less stress than shearing a whole plane of atoms at once, and calculate the resolved shear stress that starts slip.
    • Describe dislocations and how their motion produces slip
      Identify edge, screw and mixed dislocations by their Burgers vectors, follow how a moving dislocation shifts one part of a crystal over another, and explain strain fields, interactions and dislocation density.
    • Find slip systems and calculate the resolved shear stress
      Name the slip systems of FCC, BCC and HCP metals, apply Schmid's law to a single crystal, and explain how slip and twinning proceed in polycrystalline metals.
  2. Explain and quantify how smaller grains, dissolved alloying atoms and cold work raise the strength of a metal by hindering dislocation motion, and what each method costs.
    • Strengthen a metal by refining its grain size
      Explain why grain boundaries block slip, use the Hall–Petch equation, measure grain size and choose practical ways to make grains finer.
    • Strengthen a metal with solid solutions
      Explain how dissolved substitutional and interstitial atoms strain the lattice and hold back dislocations, and predict how alloying changes strength, ductility and conductivity.
    • Strengthen a metal by cold work
      Calculate percent cold work, explain why tangled dislocations raise strength, and predict how strength, ductility and other properties change as cold work increases.
  3. Explain how recovery, recrystallization and grain growth undo the effects of cold work, and use recrystallization temperature and percent cold work to plan forming routes.
    • Explain recovery, recrystallization and grain growth
      Describe what happens to a cold-worked metal as it is heated, find its recrystallization temperature, and calculate grain growth with time.
    • Choose hot or cold working and plan an annealing route
      Distinguish hot from cold working by the recrystallization temperature, compare their results, and calculate the cold-work and annealing steps that reach a final size with the required properties.
  4. Describe how materials fracture, recognize fracture surfaces, use fracture toughness to judge whether a cracked part is safe, and explain impact testing and the ductile-to-brittle transition.
    • Tell ductile from brittle fracture
      Describe the stages of ductile and brittle fracture, recognize their fracture surfaces, and explain why ductile fracture is preferred in engineering structures.
    • Use fracture toughness to assess a cracked part
      Explain why cracks concentrate stress, apply the fracture-toughness equation to find a critical stress or crack size, and compare materials for designs that tolerate cracks.
    • Interpret impact tests and the ductile-to-brittle transition
      Describe the Charpy and Izod impact tests, read absorbed energy against temperature, and explain which materials have a ductile-to-brittle transition and what shifts it.
  5. Describe fluctuating stresses, read S–N curves, explain how fatigue cracks start and grow, and choose design, surface and environmental measures that extend fatigue life.
    • Describe cyclic stresses and read S–N curves
      Calculate mean stress, stress range, amplitude and stress ratio for a load cycle, and read fatigue life, fatigue limit and fatigue strength from an S–N curve.
    • Explain how fatigue cracks start, grow and leave evidence
      Follow the stages of fatigue failure from crack initiation to final fracture, and read beachmarks and striations on a fracture surface.
    • Extend fatigue life through design, surface and environment
      Explain how mean stress, stress concentrations, surface condition and environment affect fatigue life, and choose measures that extend it.
  6. Read creep curves, calculate how creep rate changes with stress and temperature, estimate rupture life with the Larson–Miller parameter, and explain how alloys are made creep resistant.
    • Describe the creep curve and how stress and temperature affect it
      Read the stages of a creep curve, explain the atomic mechanisms of creep, and calculate how the steady-state creep rate changes with stress and temperature.
    • Estimate creep life and choose creep-resistant alloys
      Use the Larson–Miller parameter to trade temperature against rupture life, and explain which material features resist creep.

Strengthening Mechanisms and Failure study guide

6 chapters

1

How dislocations let metals deform

A metal can change shape permanently without breaking into pieces. The change begins with tiny line defects moving through its crystals, one row of bonds at a time. Following those defects explains both easy slip in pure metals and the obstacles that make alloys stronger. Crystal orientation then connects this atomic picture to a calculation: how much of an applied tensile stress actually drives a particular slip system?

1.1 Dislocations, glide, and permanent shape change

Bending a metal strip leaves a permanent change because parts of its crystals have slipped past one another. Dislocations make this possible at stresses far below those needed to shear an entire atomic plane at once. Bonds near a moving line defect break and re-form; the metal remains continuous.

Recognize the line defect

An edge dislocation is the edge of an extra half-plane of atoms ending inside the crystal. A screw dislocation has a spiral arrangement of atomic planes around its line. The Burgers vector, 𝐛, measures the lattice displacement: a circuit of equal atom-to-atom steps around the defect fails to close by this vector.

CharacterBurgers vector relative to line
EdgePerpendicular
ScrewParallel
MixedBetween these limiting orientations

A curved dislocation can be edge-like at one point and screw-like at another while keeping the same Burgers vector along its length. A dislocation is a distorted region of the lattice, not an open crack.

Follow slip through the crystal

Under shear, an edge dislocation advances as bonds ahead of its extra half-plane rearrange. Repeating this local change carries the defect across the crystal. When it emerges, the two sides have shifted relative to each other by one Burgers vector, leaving a surface step. Moving a wrinkle across a rug illustrates how a local disturbance can produce a much larger overall displacement.

The line and Burgers vector lie in the slip plane. Motion within it is glide. An edge dislocation can move out of that plane by climb, which requires atoms or vacancies to diffuse. Climb therefore matters at high temperatures. A screw dislocation can cross-slip to another plane containing its Burgers vector. Edge and screw lines move in different directions, but both produce slip in the Burgers-vector direction.

Ideal shear-strength estimates are roughly G/30 to G/10, where G is shear modulus. Pure copper or aluminum single crystals can begin slipping near 1 MPa of resolved shear stress. Only bonds around the moving line rearrange at each instant, explaining this large difference.

Why more defects can mean more strength

An edge dislocation compresses the lattice on the extra-half-plane side and stretches it on the opposite side. A screw dislocation creates shear strain. These strain fields store energy, roughly proportional to Gb2 per unit length. Short Burgers vectors cost less energy.

Same-sign edge dislocations on one slip plane repel. Opposite signs attract and can annihilate when they meet. At high densities, dislocations intersect and obstruct one another, so further slip needs more stress.

Dislocation density is total line length divided by volume, with units of inverse square meters. For a density of 1014 m−2 in one cubic centimeter:

L=ρV=1014×10−6=108 m.

That is 100,000 km of line within a tiny volume. Annealed metals commonly have about 1010–1012 m−2; heavy cold work can raise this to 1015–1016 m−2. Dislocations enable slip, but crowding them makes slip harder. Metallic bonding allows easy rearrangement; the directional or ionic bonding of many ceramics strongly resists dislocation motion, so fracture commonly occurs first.

Key Takeaways

  • Slip produces plastic strain through local bond rearrangement around moving dislocations.
  • The Burgers vector is perpendicular to an edge line and parallel to a screw line.
  • Glide stays within a slip plane; climb requires diffusion.
  • Dislocation strain fields interact, and dense dislocations obstruct further slip.
  • Dislocation density measures line length per volume, in inverse square meters.

1.2 Slip systems and the stress that starts slip

A tensile load does not drive every slip system equally. The orientation of the plane and direction determines the shear stress available to move a dislocation. A slip system combines a slip plane with a slip direction lying in that plane.

Compare crystal structures

FCC metals slip on {111}⟨110⟩ systems: four plane orientations with three directions each give 12 systems. Copper, aluminum, and nickel can accommodate extensive deformation and remain ductile at very low temperatures.

BCC metals slip in ⟨111⟩ directions on {110}, {211}, and {321} planes, giving 48 potential systems. Their planes are not truly close-packed. Dislocation motion becomes harder as temperature falls, despite the large system count.

Basal slip in HCP zinc or magnesium uses (0001)⟨112ˉ0⟩: one plane with three directions. A grain needs at least five independent systems to accommodate an arbitrary shape change while fitting its neighbors. Basal slip alone cannot do this, so deformation is restricted.

Resolve tensile stress onto a system

Schmid's law gives the resolved shear stress:

τR=σcos⁡ϕcos⁡λ=mσ.

Here ϕ is the angle between the loading axis and the plane normal, while λ is the angle to the slip direction. The Schmid factor m cannot exceed 0.5. Its maximum occurs when both angles are 45°. In a general three-dimensional orientation, the two angles need not add to 90°.

Slip starts when the resolved stress reaches the critical resolved shear stress, τcrss. Compare all candidate systems; the largest favorable Schmid factor reaches its threshold first:

σy=τcrssmmax.

For a crystal with τcrss=0.80 MPa, ϕ=50∘, and λ=45∘, the factor is about 0.455. At 1.5 MPa tension, resolved shear is about 0.68 MPa, below the threshold. Yield begins at about 0.80/0.455=1.76 MPa. Using the angle to the plane itself would give the wrong projection.

Use crystal directions

In a cubic crystal, (hkl) has normal [hkl]. Find an angle cosine by dividing a dot product by the two direction lengths. For tension along [010], plane (110), and direction [1ˉ11]:

cos⁡ϕ=12,cos⁡λ=13,m=16≈0.408.

The direction lies in the plane because their dot product is zero. If its critical shear stress is 20 MPa, this system begins slipping near 49 MPa tension.

Make neighboring grains fit

A polycrystal contains differently oriented grains. Favorably aligned grains start slipping first, but neighboring grains constrain their shape changes. Several systems must operate, making the polycrystal harder to deform than a favorably oriented single crystal. Slip lines mark surface offsets; heavy rolling elongates grains.

Deformation twinning shears a region into a mirror-related orientation across a twin plane. It is important in BCC and HCP metals under conditions that restrict slip, such as low temperature or rapid loading. Its direct strain is small, but the reorientation can make further slip easier. Annealing twins in FCC brass form during heating, through a different process.

Key Takeaways

  • A slip system combines a plane and a direction within that plane.
  • FCC has 12 easy slip systems; basal HCP slip offers only three.
  • The plane normal, not the plane, defines the Schmid angle.
  • The system with the largest favorable Schmid factor reaches its slip threshold first.
  • Neighbor constraints make polycrystalline deformation require multiple slip systems.
  • Twinning can reorient a region to favor further slip.
2

Three ways to make slip harder

Grain boundaries, dissolved atoms, and other dislocations can all obstruct a moving dislocation. Each obstacle changes the properties of the finished metal, but the trade-offs differ. Grain refinement can improve both strength and toughness; alloying also affects conductivity; cold work changes the shape and stores energy. Calculations of grain size and area reduction help connect a processing choice to a required property.

2.1 Grain boundaries and the Hall–Petch equation

A dislocation reaching a grain boundary encounters a different crystal orientation and a disordered atomic region. Its slip plane does not simply continue into the next grain. Dislocations pile up until the local stress can activate slip across the boundary. High-angle boundaries are stronger obstacles than low-angle ones.

Relate grain diameter to strength

Finer grains provide more boundaries and shorter uninterrupted slip distances. The Hall–Petch equation describes the resulting yield strength:

σy=σ0+kyd−1/2.

The constants belong to the material and its condition. If grain diameter d is in meters, use ky in MPa⋅m1/2. A plot of yield strength against inverse square root of diameter is linear, with slope ky and intercept σ0.

Suppose a steel has σ0=70 MPa and ky=0.74 MPa⋅m1/2. At a 25 μm diameter:

d=25×10−6 m,d−1/2=200 m−1/2. σy=70+0.74(200)=218 MPa.

At 4 μm, the inverse square root is 500, giving 440 MPa. Halving diameter multiplies the grain-size contribution by the square root of two; it neither doubles total strength nor changes the intercept.

Find constants from measurements

Suppose yield strengths are 150 MPa at 100 μm and 250 MPa at 16 μm. Their inverse square roots are 100 and 250 in inverse square-root meters. Calculate the slope before the intercept:

ky=250−150250−100≈0.667 MPa⋅m1/2. σ0=150−ky(100)≈83.3 MPa.

Keeping the unrounded slope gives about 306 MPa at 9 μm. Fitting strength against reciprocal diameter would describe a different, incorrect relationship.

Measure the grain size

For the intercept method, divide total line length on the image by magnification to get actual length, then divide by boundary crossings. Five 50 mm lines at 200× have an actual total length of 1.25 mm. With 100 crossings, the mean intercept is 0.0125 mm, or 12.5 μm.

The ASTM grain size number uses a historical definition:

n100=2G−1.

Here n100 counts grains per square inch on a 100× image. Thus 64 gives G=7. If measured at magnification M, first convert using n100=nM(M/100)2. A larger number means finer grains. ISO 643 instead relates grains per square millimeter at actual size to its index by m=8×2G.

Choose a refining route

Faster solidification, inoculants such as titanium and boron in aluminum, controlled rolling, or cold work followed by recrystallization can produce fine grains. Niobium, vanadium, and titanium additions can form particles that pin boundaries. Long hot holds allow coarsening.

Grain refinement improves both strength and toughness and lowers the transition temperature of ferritic steels. At very small sizes, often a few tens of nanometers, boundary-based deformation can make Hall–Petch predictions fail. In high-temperature creep, boundary sliding and diffusion make coarse grains advantageous instead.

Key Takeaways

  • Grain boundaries interrupt slip and shorten dislocation travel.
  • Hall–Petch strength varies with inverse square root of grain diameter.
  • Match the diameter unit to the Hall–Petch coefficient.
  • Correct image length for magnification before calculating a mean intercept.
  • A larger ASTM grain size number means finer grains.
  • Fine grains improve low-temperature strength and toughness; coarse grains help resist boundary-controlled creep.

2.2 Dissolved atoms as obstacles

Brass gains strength when zinc dissolves in copper. Solid-solution strengthening comes from solute atoms interfering with dislocations, not from the added element being intrinsically stronger.

Distort the host lattice

A substitutional solute replaces a host atom, as zinc or nickel does in copper and magnesium in aluminum. An interstitial solute occupies a gap, as carbon or nitrogen does in iron.

A smaller substitutional atom produces tensile lattice strain; a larger one produces compressive strain. Small atoms favor compressed regions near an edge dislocation, while large atoms favor stretched regions. Partly canceling the dislocation's strain field lowers energy, so pulling it away requires extra stress. Distorted regions also obstruct its passage.

Strengthening generally increases with dissolved concentration and size mismatch. Interstitial carbon and nitrogen strongly distort BCC iron, even at low concentrations. Ferrite dissolves at most about 0.022 wt% carbon at 727 °C.

Compare the properties

Copper and nickel dissolve in all proportions. Adding nickel to copper up to about 50 wt% increases yield and tensile strengths while elongation falls. Copper–nickel piping combines strength with corrosion resistance in seawater.

Solute atoms scatter conduction electrons, reducing electrical and thermal conductivity. This explains why wiring favors nearly pure copper even when a copper alloy would be stronger. Ductility and toughness usually decrease somewhat as solution strengthening increases.

Above a solubility limit, additional element can form a second phase. Its particles are different obstacles from atoms dissolved in the host: total alloying addition is then not the dissolved concentration.

Connect pinning to the yield curve

In low-carbon steel, interstitial carbon and nitrogen gather around dislocations. Stress reaches an upper yield point before enough dislocations break free. It then drops to a lower yield point while Lüders bands of plastic deformation spread at nearly constant stress. The lower point is normally reported as yield strength for this behavior.

Combine strengthening methods

Recrystallization removes cold-work dislocation structures but does not remove strengthening from atoms that remain dissolved. Tungsten and molybdenum in nickel alloys therefore contribute during hot service.

Aluminum–magnesium alloys such as 5083 combine solution strengthening with cold work without a precipitation-hardening treatment. Impurities concentrated at grain boundaries can instead embrittle a metal; their location matters as well as their identity.

Key Takeaways

  • Dissolved substitutional and interstitial atoms hinder slip through lattice distortion.
  • Strengthening depends on dissolved concentration and size mismatch.
  • Solute pinning explains upper and lower yield points in low-carbon steel.
  • Solution strengthening usually trades some ductility and conductivity for strength.
  • Recrystallization removes cold-work strength but retains strengthening from atoms that remain dissolved.

2.3 Cold work, area reduction, and property changes

Drawing wire or rolling sheet below the recrystallization temperature causes strain hardening. Deformation multiplies dislocations; their closer spacing, interacting strain fields, and tangles obstruct further slip.

Calculate area reduction

Percent cold work uses the original and deformed cross-sectional areas:

%CW=A0−AdA0×100.

For a round rod, area is proportional to diameter squared:

%CW=d02−dd2d02×100.

Drawing copper from 15.2 to 12.2 mm gives squared diameters of 231.04 and 148.84 square millimeters. The area fraction removed is 82.20/231.04, giving 35.6% cold work. The diameter decrease is only 19.7%; using it would understate the area reduction.

For rolling at constant width, use thickness reduction: 4 to 3 mm gives 25% cold work. If width changes too, use both dimensions to calculate areas.

Follow strength and ductility

Yield strength, tensile strength, and hardness rise with cold work; elongation at fracture falls. Yield strength rises faster than tensile strength, bringing them closer together. After unloading, reloading in the same direction reaches plastic flow near the previously attained stress.

Elastic modulus stays nearly unchanged because obstructing slip changes yielding, not elastic bond stiffness. Density changes negligibly. Conductivity falls slightly, residual stresses remain, and elongated grains make properties depend on direction.

Read a property window

Suppose a chart reaches the required yield strength of 300 MPa at 25% cold work. Elongation stays at or above the required 10% only up to 40% cold work. The usable window is 25%–40%: the strength curve sets its lower limit and ductility sets its upper limit.

A power law describes part of many true-stress–true-strain curves:

σT=KεTn.

A larger strain-hardening exponent means faster hardening. Typical annealed values are about 0.2 for low-carbon steel and 0.4–0.5 for copper or brass.

Check heat and repeated loading

Recovery and recrystallization remove cold-work strengthening, so a drawn part can soften during hot service or near a weld. Lead at room temperature is already above its recrystallization temperature; deforming it there is hot working.

Repeatedly bending a paper clip both work-hardens the bend and causes low-cycle fatigue. Cyclic plastic strain starts and grows a crack until the remaining section breaks.

Key Takeaways

  • Cold work increases dislocation density and resistance to further slip.
  • Calculate cold work from area reduction, using squared diameters for round rods.
  • Strength and hardness rise while ductility falls; elastic modulus stays nearly constant.
  • Select a cold-work window that meets strength and elongation requirements together.
  • Recovery and recrystallization remove cold-work strengthening.
3

Annealing and forming routes

A cold-worked metal stores energy in its dislocations. Heating gives atoms and defects enough mobility to reduce that stored energy, restoring ductility but reducing strength. The amount of deformation before heating, and the temperature and time of the hold, control the result. Planning a forming route therefore means tracking both dimensions and material condition, especially which reduction remains after the last recrystallization anneal.

3.1 Recovery, new grains, and grain growth

A heavily cold-worked metal has elongated grains, many tangled dislocations, and stored strain energy. Heating enables defects and boundaries to move. Recovery, recrystallization, and grain growth produce different changes, so they must be distinguished when choosing an anneal.

Recovery rearranges defects

During recovery, dislocations glide and climb; opposite signs can annihilate. Others rearrange into lower-energy walls that divide grains into subgrains. Residual stresses decrease and conductivity returns toward its original value. Strength and hardness fall only slightly, so recovery can relieve stress without fully softening the metal.

Recrystallization replaces deformed grains

New grains with low dislocation density form at favorable sites, often old boundaries or heavily deformed regions. They grow into the cold-worked material, driven by the difference in stored energy. The new grains are equiaxed: each grain has roughly equal dimensions in different directions, although different grains need not have equal sizes.

Strength and hardness drop sharply and ductility returns. The metal stays solid, with the same crystal structure and composition. A recrystallization anneal removes the cold-worked condition; recovery alone does not fully reset it.

The recrystallization temperature is conventionally the temperature that completes recrystallization in one hour. It is often around one third to one half of the absolute melting temperature and can approach 0.7 in some alloys. More prior cold work, greater purity, or a longer available annealing time lowers the temperature needed. A small reduction below the critical cold-work amount, often 2%–20%, may not supply enough stored energy to recrystallize.

Judge temperature relative to melting

Ratios require kelvin. Lead melts near 600.7 K, so at 293 K its homologous temperature is about 0.49; it can recrystallize near room temperature. Tungsten melts near 3695 K and needs roughly 1473 K to recrystallize. Working it at 1000 °C, or 1273 K, still counts as cold working.

Grain growth removes boundary area

After recrystallization, a continued hot hold lets larger grains consume smaller ones. Reducing total grain-boundary area lowers energy. A common growth relation is:

dn−d0n=Kt.

For many metals the exponent is near two. The constant increases rapidly with temperature. With initial diameter 20 μm and diameter 40 μm after 30 min:

K=402−20230=40 μm2/min.

At a total elapsed time of 120 min:

d=202+40(120)=5200≈72 μm.

A straight-line diameter extrapolation would give 100 μm and would miss the square-law relation. Use one consistent time origin and the original grain size.

Choose the hold

Across increasing one-hour annealing temperatures, recovery changes strength little, recrystallization causes a sharp fall, and subsequent coarsening causes a slower further fall. To obtain fine recrystallized grains, use sufficient prior cold work and a short hold at the lowest temperature that completes recrystallization. Excess time or temperature promotes growth and reduces Hall–Petch strength. In this process, the important action is the hot hold that rearranges defects and grains; slow cooling alone does not define recrystallization annealing.

Key Takeaways

  • Recovery relieves residual stress with only modest softening.
  • Recrystallization replaces deformed grains with new grains of low dislocation density.
  • Equiaxed describes dimensions within a grain, not equal sizes across all grains.
  • Recrystallization depends on prior cold work, purity, temperature, and time.
  • Grain growth reduces boundary area and generally lowers room-temperature strength.
  • Use kelvin for homologous temperatures and the correct exponent for grain growth.

3.2 Hot working and intermediate anneals

A forming route must reach the final size and leave the required strength and ductility. Full recrystallization resets the cold-worked condition, so only later deformation counts toward retained cold work.

Choose hot or cold working

Hot working occurs above the metal's recrystallization temperature. Recrystallization accompanies or follows deformation, allowing large reductions with relatively low forces and breaking up coarse cast structures. Drawbacks include heating energy, scale, poorer finish, and less accurate dimensions.

Cold working below that temperature gives strain hardening, good finish, and close tolerances. It needs greater force and leaves less ductility for further forming.

Room temperature can be hot working for lead and tin, while 1000 °C can still be cold working for tungsten. Classification depends on the metal.

Check direct drawing

A copper rod starts at 12.0 mm and must finish at 8.0 mm with 20%–30% retained cold work:

%CW=100122−82122≈55.6.

The direct route exceeds the window. Recrystallizing at an intermediate diameter restores ductility and permits a smaller retained final reduction.

Choose 25% for the last pass. Its final area must be 75% of the area at the anneal:

di=df1−%CW/100=80.75≈9.24 mm.

Draw 12.0 → 9.24 mm, recrystallize, then draw 9.24 → 8.0 mm. The first stage gives about 40.7% cold work; the last gives 25%. Retain the unrounded intermediate diameter when checking percentages.

Verify the available sizes

The window endpoints give:

80.80≤di≤80.70,

or about 8.94–9.56 mm. Every diameter in this range lies between the 12 mm starting rod and 8 mm product.

If direct drawing gives less than the minimum required cold work, an intermediate anneal cannot increase it. The process then needs a larger starting section or another route.

Track successive passes

Without recrystallization, compare final area with the original area. Drawing 12 → 10 → 8 mm gives 55.6% total cold work; adding the two pass percentages is incorrect because their starting areas differ. Remaining area fractions multiply.

A recovery anneal relieves stress but does not reset this reference as a full recrystallization anneal does.

Key Takeaways

  • Hot and cold working are defined relative to recrystallization temperature.
  • Calculate direct area reduction before choosing an intermediate anneal.
  • After recrystallization, retained cold work is measured from the annealed section.
  • Successive cold-work percentages do not add; remaining area fractions multiply.
4

Cracks, fracture, and impact behavior

A part can resist yielding yet fail from a sharp crack. Fracture analysis connects the deformation visible on a broken surface to the local stress at a flaw. Crack geometry and fracture toughness then help predict the load or flaw size that triggers rapid failure. Impact tests add another dimension: a metal's behavior under a notch and sudden loading can change sharply with temperature, even when its ordinary tensile strength looks adequate.

4.1 Ductile and brittle fracture surfaces

Ductile and brittle fracture describe the plastic deformation accompanying separation. Temperature, loading rate, and stress state can change which mode occurs in the same metal.

Follow ductile separation

A moderately ductile tensile bar first necks. Microvoids form around inclusions or second-phase particles, then enlarge and join into a crack roughly perpendicular to tension. Further void joining extends it outward. The rim finally shears near 45° to the axis, producing a cup-and-cone surface. Very soft metals can neck almost to a point.

Ductile surfaces often look dull and fibrous. Under an electron microscope, dimples mark the joined voids. Rounded dimples suggest tensile separation; elongated dimples indicate stronger shear involvement.

Trace a brittle crack

Brittle fracture involves little overall plastic deformation and often leaves a flat section perpendicular to tension. Transgranular cleavage crosses grains along crystal planes, leaving facets that can appear sparkling or granular.

Intergranular fracture instead follows weakened grain boundaries, outlining grain shapes on the surface. Impurity segregation or hydrogen can contribute to boundary weakness.

Some steels show V-shaped chevrons whose tips point toward the origin; other surfaces have ridges fanning outward from it. These patterns help locate an initiating weld flaw, inclusion, or sharp corner. The origin can be far from the region that broke last.

Judge stability and warning

Ductile tearing often grows stably: further loading or displacement is needed to continue it. It can later become unstable, depending on geometry and loading. Brittle growth commonly becomes rapid and unstable with little warning.

Engineers favor ductile behavior because plastic deformation absorbs energy and often gives visible warning. High yield strength does not provide the same protection: a sharp crack can trigger fracture before gross yielding, while a notch constrains local plastic flow.

Consider material and conditions

FCC metals are generally ductile. Many ferritic steels are ductile at room temperature but can cleave when cold; conventional polycrystalline tungsten can already be brittle at room temperature. Ceramics and glasses usually show little plasticity at room temperature. Polymers can be ductile or brittle as temperature and loading rate change.

A smooth specimen loaded slowly at room temperature therefore does not establish the behavior of a cold, notched part struck suddenly.

Key Takeaways

  • Ductile and brittle describe plastic deformation before separation.
  • Ductile tensile fracture develops through void formation, growth, and joining.
  • Dimples record microvoid separation; cleavage facets record brittle cracking through grains.
  • Intergranular cracks follow boundaries; chevrons can point toward an origin.
  • Ductile tearing can become unstable, and high strength alone does not ensure toughness.

4.2 Fracture toughness and critical flaw size

A crack concentrates stress near its tip. Longer cracks and sharper tips create larger local stresses, explaining why real brittle materials fail far below an ideal bond-breaking strength. Plastic flow can blunt a tip in a ductile metal, redistributing its stress.

Distinguish two measures

For a sharp elliptical flaw, an approximate concentration is Kt=2a/ρt. The radius ρt measures tip sharpness. An internal crack 4 mm long has half-length 2 mm; a 2 μm tip radius gives Kt=22/0.002≈63. This dimensionless factor compares local and nominal stresses.

The stress intensity factor instead characterizes the near-tip stress field:

K=Yσπa.

Its units are MPam when stress is in MPa and crack size in meters. The geometry factor Y is about 1 for a central through crack in a wide plate, where total length is 2a, and about 1.12 for a small edge crack of depth a.

Compare crack driving force with resistance

Fracture begins when stress intensity reaches the applicable fracture toughness, Kc. Thick specimens constrain the tip into plane strain, producing a lower limiting toughness called KIc. Mode I opens the crack faces in tension. Thin specimens can show higher toughness because constraint is lower.

A necessary thickness check is:

B≥2.5(KIcσy)2.

For toughness 87.4 and yield strength 1420 MPa, the right side is 0.00947 m, or about 9.5 mm. Thickness alone does not validate a test; crack, ligament, geometry, and load-response requirements must also be met.

Calculate a critical size or stress

For a wide plate with KIc=50 MPam, Y=1, and 400 MPa tension:

ac=1π(50400)2≈0.00497 m.

This is half-length, so the critical internal crack is about 9.9 mm long. An inspection threshold must be appreciably smaller.

For a 2 mm edge crack in the same material:

σc=501.12π(0.002)≈563 MPa.

Omitting the edge factor predicts 631 MPa and overestimates the load capacity. Compare the calculated fracture stress with yield strength as a separate check; yielding first requires considering plastic behavior.

Understand toughness and energy

Griffith's brittle-crack balance compares released elastic energy with the energy of new surfaces:

σc=2Eγsπa.

For glass with modulus 69 GPa and surface energy 0.3 J/m², a 1 μm flaw gives about 115 MPa, while a 100 μm flaw gives 11.5 MPa. A hundredfold larger flaw reduces strength tenfold.

Typical plane-strain toughness rises from about 0.7–0.8 in soda-lime glass to 3–5 in alumina, 25–30 in 7075-T651 aluminum, 45–65 in Ti-6Al-4V, and 50 to above 100 in low-alloy steels, in MPa√m. Values depend on condition and orientation. For the same alloy, a stronger condition can have lower toughness: conditions with 50 and 87.4 toughness fracture near 515 and 900 MPa for a 3 mm internal half-crack, even though their yield strengths are 1640 and 1420 MPa. Tensile toughness is stress–strain area, and impact energy is measured in joules; neither substitutes for fracture toughness in a crack calculation.

Key Takeaways

  • Distinguish dimensionless stress concentration from stress intensity in MPa√m.
  • Use half-length for an internal crack and depth for an edge crack.
  • Fracture occurs when the crack driving force reaches the applicable toughness.
  • Check geometry, units, and yield strength when assessing a cracked part.
  • The plane-strain thickness criterion is necessary but not a complete test-validity check.
  • Higher yield strength can come with lower tolerance of sharp cracks.

4.3 Impact energy and the ductile-to-brittle transition

A notch, rapid loading, and low temperature can favor brittle fracture. Impact testing combines these effects in a controlled specimen. Repeating the test at different temperatures shows whether a material changes from high-energy ductile behavior to low-energy brittle behavior.

Measure absorbed impact energy

In the Charpy test, a bar rests horizontally on two supports. A pendulum strikes the side opposite its central notch. A full-size V-notch specimen is 10 mm × 10 mm × 55 mm, with a 2 mm deep, 45° notch. An Izod test instead clamps the specimen upright as a cantilever. ISO 148-1 specifies Charpy testing; ASTM E23 covers notched-bar impact testing, including Charpy and Izod.

The energy absorbed is the pendulum's loss of potential energy:

E=mg(h0−hf).

A 20 kg pendulum dropping from 1.5 m and rising to 0.9 m after fracture loses 20(9.81)(0.6)=117.72 J, about 118 J. A smaller return height means more energy was absorbed. Specimen dimensions and notch geometry must match when comparing results.

Impact energy describes breaking a notched specimen quickly. It cannot be inserted as fracture toughness into an equation for a sharp crack; the quantities have different units and meanings.

Read the transition curve

Many ferritic steels show an S-shaped energy-versus-temperature curve. At high temperatures, the upper shelf has high absorbed energy and largely fibrous fracture. At low temperatures, the lower shelf has low energy and mostly cleavage. Between them is the transition region.

The ductile-to-brittle transition temperature, or DBTT, requires a criterion. It might be the temperature reaching a specified energy or giving 50% fibrous fracture area. These criteria can give different values. Changing specimen size, notch, or loading rate can also change the result.

For example, S355J2 specifies at least 27 J at −20 °C in a Charpy V-notch test. A result of 40 J at −20 °C meets that requirement. A 15 J result at −40 °C gives information about lower-temperature behavior, but service selection there also requires thickness, stress, geometry, loading rate, and applicable design requirements.

Explain which metals change behavior

In BCC metals, the stress needed to move dislocations rises steeply as temperature falls. Cleavage can then become easier than plastic flow. Ferritic steels and some HCP metals show a transition. FCC aluminum, copper, nickel, and austenitic stainless steels remain ductile at very low temperatures, making them useful in cryogenic equipment.

Finer grains, nickel, and manganese lower the transition temperature in steels. More carbon raises it and reduces upper-shelf energy; neutron irradiation can raise it as well. Keeping tensile-service temperatures above the relevant transition with a margin helps avoid brittle failure.

Connect material and structure

Welded Liberty ships in cold seas combined transition-sensitive steel, sharp hatch corners, and a continuous crack path across welded plates. Rounded corners reduced local stress, tougher steel improved low-temperature behavior, and crack-arresting strakes interrupted propagation. The failures show why steel properties, service temperature, and structural detail must be considered together.

Key Takeaways

  • Charpy specimens are simply supported; Izod specimens are clamped.
  • Absorbed energy is the pendulum energy lost during fracture.
  • A DBTT value requires a stated energy or fracture-appearance criterion.
  • Fine grains and nickel can improve low-temperature toughness in ferritic steels.
  • Impact energy, crack toughness, and service suitability answer different questions.
5

Fatigue under repeated loading

A shaft or spring can fail after many load cycles even when each load is below yield. Fatigue analysis tracks the cycle, the time spent starting and growing a crack, and the conditions that accelerate damage. Stress amplitude and mean stress describe different parts of the loading. Surface detail and environment then explain why a polished laboratory specimen and a component in service can have very different lives.

5.1 Stress cycles and S–N curves

Fatigue is damage and eventual failure under fluctuating stress. A part can experience little overall plastic deformation and still develop a crack through repeated local slip. Comparing the peak stress only with yield strength misses this time-dependent accumulation of cyclic damage.

Describe one load cycle

Use positive stress for tension and negative stress for compression. The maximum and minimum define four useful quantities:

σm=σmax+σmin2,σr=σmax−σmin. σa=σr2,R=σminσmax.

Mean stress is the cycle's center; range is its full height; amplitude is half that height. With a maximum of 250 MPa and minimum of −50 MPa, the mean is 100 MPa, range 300 MPa, amplitude 150 MPa, and ratio −0.2. Subtracting a negative minimum increases the range.

A fully reversed cycle has equal tensile and compressive extremes, zero mean, and R=−1. A cycle from zero to a tensile peak has R=0. Repeated cycles can have a nonzero mean, while random loading changes less regularly.

Read a life curve

Fatigue tests cycle specimens at specified amplitudes until failure. An S–N curve plots stress amplitude against cycles to failure, usually with a logarithmic cycle axis. At a chosen amplitude, read across to the curve and then down to obtain fatigue life. To select a stress for a required life, start on the cycle axis and read in the reverse direction.

A curve applies to the stress ratio or mean stress and environment used in its test. An amplitude-based graph must be entered using amplitude, not maximum stress.

For many steels and titanium alloys, a test curve levels off at a fatigue limit. Below that amplitude, failure is not expected in those test conditions. For many steels the limit is about 35%–60% of tensile strength. Aluminum, copper, and magnesium alloy curves keep declining, so quote fatigue strength at a specified life, such as ten million cycles.

For example, a steel test limit of 280 MPa lies above an operating amplitude of 150 MPa. An aluminum fatigue strength of 130 MPa at ten million cycles does not support that same life at 150 MPa; the higher amplitude corresponds to a shorter life on its curve.

Convert cycles into operating time

A rotating shaft in steady bending can give one stress cycle per revolution. At 1800 revolutions per minute:

t=1071800=5555.6 min≈92.6 h.

Ten million cycles can accumulate in less than four days. Always establish the number of stress cycles per revolution before doing this conversion.

Recognize the life regime and scatter

Low-cycle fatigue involves appreciable cyclic plastic strain and relatively few cycles, often below roughly ten thousand to one hundred thousand. Repeatedly bending a paper clip is an example. High-cycle fatigue involves mostly elastic bulk loading and longer lives.

Identically loaded specimens can have widely different lives. A typical S–N curve may represent median behavior, so designing directly to it can leave many parts failing earlier. Reliability-based curves or safety factors address that scatter. Corrosion, rough surfaces, and a higher tensile mean stress can reduce life from a smooth-specimen test result.

Key Takeaways

  • Stress amplitude is half the range; mean stress locates the cycle center.
  • Read an S–N curve with its stated stress measure and test conditions.
  • A fatigue strength must name the cycle count; a fatigue limit is a test-condition threshold.
  • Convert cycles to time using the actual cycle frequency.
  • Mostly elastic loading can still cause fatigue, and fatigue lives scatter.

5.2 How fatigue cracks grow and leave marks

A fatigue break often seems sudden because the final separation is rapid. Before that event, a crack has been developing through repeated loading. Finding its origin and growth region helps explain the failure and choose a useful remedy.

Separate initiation, propagation, and final fracture

Crack initiation commonly occurs at the surface, near a scratch, thread, sharp shoulder, keyway, or concentrated slip band. Internal inclusions and pores can also initiate cracks. The local cyclic strain is greater than the nominal stress alone suggests.

During propagation, the crack first follows a short crystallographic shear path, then generally grows perpendicular to the tensile stress. As load rises, local plastic flow blunts the tip; as load falls, the tip sharpens again. Repeated advance lengthens the crack, which increases the driving stress intensity at a given nominal load.

Final fracture occurs when the crack reaches a critical size at the cycle maximum or the remaining section overloads. Under linear-elastic conditions, compare maximum stress intensity with the applicable toughness:

Kmax=Yσmaxπa,Kmax=Kc at fracture.

Use plane-strain toughness when the relevant constraint conditions apply. A crack can grow under cycling while its maximum stress intensity remains below the value for rapid final fracture.

Account for the total life
Nf=Ni+Np.

The total consists of initiation cycles plus propagation cycles. At low nominal stress, initiation often consumes most of the life. At higher stress, cracks can initiate early, leaving propagation as a large part of the life. A surface treatment that delays initiation and an inspection program that detects growth therefore act at different stages.

Read beachmarks and striations

Beachmarks are curved bands visible without an electron microscope. They record changes or interruptions in loading. Their pattern can locate the origin, like contours showing earlier crack-front positions.

Striations are fine ridges visible under an electron microscope. In the usual striation-forming process, they mark cycle-by-cycle crack advance. Their spacing can increase with stress range. One beachmark may span thousands of striations, so counting beachmarks as individual load cycles would greatly undercount the history.

Continuous, unchanging loading may leave no beachmarks. Their absence alone cannot exclude fatigue. Surface evidence must be interpreted with loading history and the rest of the fracture.

Use the two surface regions

The fatigue-growth region is often relatively smooth and may have rubbed surfaces or visible bands. The final-fracture region is commonly rougher and can itself be ductile or brittle. With comparable geometry, a small final region suggests the crack grew across much of the section under relatively low nominal stress; a large final region suggests a higher load broke a smaller remaining crack-growth section.

A shaft with beachmarks centered at a sharp keyway corner and a small rough region opposite it points to fatigue starting at that corner. A larger corner radius reduces concentration, while surface compression can delay initiation and early growth. Dye penetrant, ultrasonic, or eddy-current inspection can detect cracks before critical size, with method and intervals selected for the component and expected growth.

Key Takeaways

  • Fatigue progresses through initiation, crack growth, and final separation.
  • Total fatigue life includes both initiation and propagation cycles.
  • Beachmarks record load changes; striations show much finer crack advance.
  • A missing beachmark pattern does not exclude fatigue.
  • Use the origin, growth region, and final-fracture region together in a failure analysis.

5.3 Design and surface choices that extend fatigue life

A fatigue-resistant part needs more than an adequate static yield strength. Local stress, surface condition, mean stress, and environment all change the time needed to initiate and grow cracks. Useful improvements act on the cause of cyclic damage.

Reduce local tensile loading

At a fixed amplitude, increasing tensile mean stress generally shortens life. A compressive mean stress helps by reducing crack opening. Tensile residual stresses from welding or grinding can add to the harmful effect even when the externally applied cycle is unchanged.

Section changes concentrate stress. Use generous fillet radii at shoulders, gradual transitions, and holes positioned away from highly stressed regions. A rounded shaft shoulder reduces the local driving stress without requiring a different bulk alloy. Fine grains and fewer inclusions can also improve steel fatigue behavior by limiting slip concentration and crack origins.

Improve the surface

Machining grooves and scratches are small notches. Polishing removes these sites, while careful handling preserves the improved finish. A later scratch can undermine the benefit.

Shot peening plastically indents a surface with small hard particles. The surrounding material restrains the deformed layer, leaving residual compression that opposes applied surface tension. This delays crack initiation and early growth. It changes the near-surface stress state; it does not eliminate the applied load cycle.

Case hardening can produce a hard steel surface with compressive residual stress. In contrast, decarburization, or loss of carbon from the surface during processing, leaves a softer skin and reduces fatigue strength. Surface chemistry and residual stress matter alongside roughness.

Allow thermal expansion

A component that is free to expand develops little stress from uniform heating. Restraining that expansion creates compressive stress during heating; repeated heating and cooling can create a damaging thermal cycle.

For full elastic restraint, the approximate stress magnitude is:

∣σ∣=αE∣ΔT∣.

With steel expansion coefficient 12×10−6 K−1, modulus 200 GPa, and a 100 K temperature change, first convert modulus to 200,000 MPa. Multiplying by the expansion coefficient gives 2.4 MPa/K, then by 100 K gives 240 MPa. Repeated restraint can cause thermal fatigue. Expansion joints, smaller temperature swings, or lower-expansion materials reduce the cause.

Control corrosion fatigue

Corrosion and cyclic stress reinforce each other. Pits concentrate stress and provide crack origins; the environment also accelerates propagation. A steel's fatigue limit measured in benign conditions can disappear in corrosive service.

Protective coatings, resistant alloys, reduced stress, and removal of the corrosive agent address this combination. Polishing alone cannot control a continuing chemical attack, while corrosion protection alone leaves a sharp structural notch unchanged.

Choose measures together

A stronger steel often has a higher fatigue limit in laboratory tests, but a rough finish, tensile residual stress, or seawater can consume that advantage. Compare fatigue data at the actual amplitude and mean stress, then account for geometry, surface, and environment.

Key Takeaways

  • Higher tensile mean and residual stresses generally shorten fatigue life.
  • Rounded transitions and smooth surfaces reduce crack-starting stress concentrations.
  • Shot peening leaves useful surface compression.
  • Constrained temperature cycling can cause fatigue without a changing external force.
  • Corrosion can remove the fatigue limit seen in benign steel tests.
  • Match a remedy to the source of damage: load, geometry, surface, or environment.
6

Creep strain and rupture in hot service

A hot component can slowly change shape under a steady load, even when the stress is below yield. Temperature controls diffusion and dislocation climb, while stress strongly affects the deformation rate. A creep assessment must consider both accumulated strain and the time to rupture. The material's grain structure and stable alloying features matter because strengthening that works during room-temperature forming may disappear during a long hot hold.

6.1 Creep curves, rates, and temperature

Creep is permanent deformation that accumulates with time under sustained stress or load. In metals it becomes important above roughly 0.4 of the absolute melting temperature. Room temperature is already high relative to lead's melting point; polymers can also creep at room temperature.

Read the creep curve

A test holds temperature and load or stress constant and records strain against time. Loading first gives an instantaneous, mostly elastic strain. The subsequent curve has three stages:

StageSlope of strain–time curveMain balance
PrimaryDecreasesHardening initially outweighs recovery
SecondaryNearly constantHardening and recovery balance
TertiaryIncreases toward ruptureCavities, cracks, and section loss accelerate damage

The secondary slope is the steady-state creep rate. In constant-load tests, necking raises true stress as area shrinks, helping accelerate tertiary creep. Rupture lifetime is the elapsed time to separation.

Use absolute temperature

The homologous temperature is T/Tm, with both values in kelvin. Nickel melts near 1728 K, so 0.4 of its melting temperature is about 691 K, or 418 °C. Aluminum melts near 933 K; its corresponding value is 373 K, about 100 °C. A modest Celsius temperature can therefore be significant for a lower-melting metal.

The 0.4 ratio is a useful indicator of when creep becomes important, not a sharp on/off boundary. Time, stress, and the active mechanism also determine how much strain accumulates.

Calculate a stress effect

At fixed temperature, a power-law model gives:

ε˙s=K1σn.

Taking a ratio removes the unknown constant. With stress exponent five, a rise from 50 to 60 MPa multiplies rate by:

ε˙2ε˙1=(6050)5=2.48832.

A starting rate of 10−6 h−1 becomes about 2.5×10−6 h−1. A 20% stress rise produces much more than a 20% rate rise.

Calculate a temperature effect

Including thermal activation gives:

ε˙s=K2σnexp⁡(−QcRT).

Use activation energy in J/mol, R=8.314 J/(mol⋅K), and kelvin. At fixed stress, raising temperature from 900 to 950 K with activation energy 250 kJ/mol multiplies rate by:

exp⁡[2500008.314(1900−1950)]≈5.8.

The exponent is positive for a temperature rise. Keeping energy in kilojoules while using this gas constant would make the increase far too small.

Connect the rate to mechanisms and life

Diffusion creep transports atoms by vacancy diffusion through grains or boundaries and often has stress exponent near one. Dislocation creep combines glide and diffusion-assisted climb and has larger exponents. Grain-boundary sliding contributes at high temperatures.

For a steady-state strain estimate, multiply rate by time. An allowance of 1% over 100,000 h corresponds to 0.01/100000=10−7 h−1. Use the strain as a fraction, and account for primary and tertiary contributions when they matter. Long-life components may be limited by shape change; a short-life hot part may instead be limited by rupture.

Key Takeaways

  • Primary creep slows, secondary creep has a nearly constant rate, and tertiary creep accelerates.
  • Use kelvin for the ratio of service temperature to melting temperature.
  • Creep rate can rise steeply with both stress and temperature.
  • Diffusion enables vacancy transport, climb, and other high-temperature deformation.
  • Accumulated strain and rupture lifetime are separate service limits.

6.2 Larson–Miller life and creep-resistant structures

Long creep lives are estimated from shorter tests by connecting temperature, stress, and rupture time. The Larson–Miller parameter is one widely used way to combine temperature and time. Its use begins with a material's measured master curve at the relevant stress.

Read the parameter correctly
P=T(C+log⁡10tr).

Temperature is in kelvin, rupture time is in hours, and the constant is calibrated for the material and those conventions. A common approximate value for metals is 20. Some plots display the parameter divided by one thousand, so an axis value of 22.0 can mean a full parameter of 22,000.

At one specified stress, the master curve supplies the parameter. Rearranging gives:

log⁡10tr=P/T−C,tr=10P/T−C.

If the curve gives 22,000 at 200 MPa and the constant is 20, operation at 1000 K gives logarithm two and a life of 100 h. At 950 K, the logarithm is approximately 3.158 and life is about 1440 h. A 50 K reduction increases the predicted life more than fourteenfold.

Work backward from required life

For a required 10,000 h at that same stress:

T=PC+log⁡10tr=2200020+4≈917 K.

This is about 644 °C. A lower temperature increases the predicted rupture life. Reading the parameter at a different stress, using Celsius, using natural logarithms, or putting minutes into an hours-based relation changes the prediction incorrectly. Extrapolation depends on the tested material retaining relevant creep behavior over the predicted range.

Choose a structure that survives hot service

High melting temperature keeps service temperature low on the homologous scale, and high modulus helps resist deformation. Refractory metals such as tungsten and molybdenum, nickel-base superalloys, stainless steels, and some ceramics serve in hot applications. Thermal-barrier coatings lower the metal temperature of turbine blades.

Grain boundaries can slide and develop cavities. Coarse grains reduce boundary-controlled creep, reversing the low-temperature grain-refinement benefit. Directionally solidified blades align long grains with the main load and avoid transverse boundaries. Single-crystal blades eliminate grain boundaries entirely.

Keep obstacles stable

Dissolved tungsten and molybdenum in nickel slow dislocation motion and diffusion. Fine, stable second-phase particles such as oxides, carbides, or ordered superalloy precipitates obstruct dislocations. Their benefit requires resistance to coarsening during the hot exposure.

Cold work supplies a dense dislocation structure, but hot service permits recovery and recrystallization, removing that advantage. An alloy selected solely for high room-temperature cold-work strength may therefore soften while creep continues below its yield strength.

Key Takeaways

  • Larson–Miller combines kelvin and base-10 logarithm of rupture time in hours.
  • Read the master curve at the actual stress and restore any axis scale factor.
  • Coarse, aligned, or single-crystal grains resist boundary-controlled creep.
  • Stable solutes and particles retain useful obstacles during hot service.
  • Cold-work strength is lost through recovery and recrystallization at high temperature.

Strengthening Mechanisms and Failure examples

6 Walkthroughs

1

From a line defect to the onset of slip

14 steps
Follow dislocation motion, then resolve an applied load onto competing slip systems.
  1. 1
    IntroductionWhy a crystal can bend

    A copper crystal can deform at stresses far below those needed to shear a whole atomic plane. Moving dislocations make that possible.

    Follow the local bond rearrangement, then use crystal orientation to determine how much of an applied load drives slip.

  2. 2
    AnalogyMove a local disturbance

    Imagine moving a wrinkle across a rug. A small region moves at a time, but the rug ends up displaced.

    A dislocation provides a similar route for crystal slip: only bonds near its line rearrange at each instant. The analogy describes the sequence of motion; in the metal, bonds re-form and the solid remains continuous. Slip does not leave an open gap across the crystal.

  3. 3
    ExplanationIdentify edge and screw character

    An edge dislocation ends an extra half-plane; its Burgers vector is perpendicular to its line. A screw dislocation has a spiral lattice arrangement and a parallel vector.

    A curved line can mix both characters while keeping the same Burgers vector.

  4. 4
    ExplanationSeparate glide from climb

    Glide stays within a slip plane. Edge climb leaves that plane through diffusion of atoms or vacancies, so heating speeds it.

    A screw dislocation can instead cross-slip to another suitable plane containing its Burgers vector.

  5. 5
    ChallengeCheck a motion mechanism

    An edge dislocation is blocked on its slip plane. During a hot hold it moves out of that plane as vacancies diffuse. What motion occurred, and why does heating help?

    ---reveal---

    It climbed. Vacancy diffusion changes the edge of the extra half-plane and allows motion out of the original plane. Heating speeds the diffusion required for this process; ordinary glide remains in-plane.

  6. 6
    ExampleCount line length in a small sample

    A sample has volume 3 mm³ and dislocation density 2×1013 m−2. First convert its volume:

    3 mm3=3×10−9 m3.

    Then multiply density by volume:

    L=(2×1013)(3×10−9)=6×104 m.

    The sample contains 60 km of dislocation line. Density is line length per volume, not the length of a single defect.

  7. 7
    Key InsightWhy extra dislocations strengthen

    Dislocations enable slip, but at high density their strain fields interact and their lines obstruct one another. Deformation creates more such obstacles.

    Same-sign edge defects on one plane repel; opposite signs can attract and annihilate when they meet.

  8. 8
    ExplanationChoose a plane and an in-plane direction

    A slip system contains both a plane and a direction lying within it. FCC metals have 12 easy systems; basal HCP slip provides only three.

    Neighboring grains must stay joined during deformation. At least five independent systems are needed for arbitrary shape change, so the available systems affect polycrystal ductility. BCC has many potential systems, but low temperature makes their motion harder.

  9. 9
    ExplanationProject the tensile stress

    An applied tensile stress drives only part of its magnitude as shear on a selected system:

    τR=mσ,m=cos⁡ϕcos⁡λ.

    Measure the first angle to the plane normal and the second to the slip direction. The largest possible Schmid factor is 0.5. Slip starts when resolved shear reaches the system's critical resolved shear stress.

  10. 10
    ExampleCompare two orientations

    A crystal has two candidate systems with Schmid factors 0.30 and 0.45. Both have critical resolved shear stress 9 MPa.

    The tensile thresholds are:

    σ1=9/0.30=30 MPa, σ2=9/0.45=20 MPa.

    The second system starts first. Its larger factor converts more of the same tensile load into the shear needed for slip.

  11. 11
    ChallengeFind the first active system

    Two systems have factors 0.25 and 0.40 and the same critical shear stress, 8 MPa. At 22 MPa applied tension, which system can slip?

    ---reveal---

    Their resolved stresses are 22(0.25)=5.5 MPa and 22(0.40)=8.8 MPa. Only the second reaches 8 MPa. Its threshold is 20 MPa tension; the first would need 32 MPa.

  12. 12
    ChallengeLink geometry and defect resistance

    Two specimens have the same most favorable Schmid factor, 0.40. Before deformation, critical shear stress is 8 MPa. After a dense dislocation network forms, it is 12 MPa. Predict the change in tensile yield stress and explain its cause.

    ---reveal---

    Yield stress rises from 8/0.40=20 MPa to 12/0.40=30 MPa. Orientation is unchanged; the interacting dislocation network raises resistance to motion. A change in geometric projection is not needed to explain the result.

  13. 13
    ConnectionReorient a constrained grain

    A grain in a polycrystal cannot deform independently of its neighbors. Several slip systems must combine to preserve continuity.

    Twinning adds another possibility: it shears part of the grain into a mirror-related orientation. Although the twin gives limited direct strain, its new orientation can make slip more favorable. This is especially useful where the original slip options are restricted.

  14. 14
    RecapConnect the two requirements

    Slip needs a movable defect and sufficient resolved shear on an available system. Compare the resolved stress with the critical value to predict its onset.

    For a polycrystal, neighboring grains also constrain deformation, so multiple slip systems must accommodate their shape changes.

2

Choose an obstacle to slip

15 steps
Compare grain refinement, dissolved solutes, and cold work using mechanisms and calculations.

Save this lesson to follow every Walkthrough step by step.

  1. 1
    IntroductionOne mechanism, three kinds of obstacle
  2. 2
    ExplanationStop slip at a boundary
  3. 3
    ExampleUse an inverse square root
  4. 4
    ChallengeChange the grain contribution
  5. 5
    ChallengeCorrect a microscope measurement
  6. 6
    ExplanationStrain the lattice with dissolved atoms
  7. 7
    ConnectionExplain a yield-point drop
  8. 8
    ChallengeChoose a conductor alloy
  9. 9
    TipKeep dissolved atoms distinct from particles
  10. 10
    ExampleCalculate a drawing reduction
  11. 11
    ChallengeCheck rolling at constant width
  12. 12
    ExplanationRead two property limits together
  13. 13
    ChallengeCompare a hot hold across mechanisms
  14. 14
    Key InsightChange the grain-size choice in hot service
  15. 15
    RecapChoose for the required properties
3

Plan a drawing route with an anneal

12 steps
Follow defect changes during heating and select an intermediate diameter for a required final cold-work window.

Save this lesson to follow every Walkthrough step by step.

  1. 1
    IntroductionReach size and properties together
  2. 2
    ExplanationRelieve stress before replacing grains
  3. 3
    TipRecognize the grain shape
  4. 4
    ExampleCalculate square-law growth
  5. 5
    ChallengeUse a measured growth constant
  6. 6
    ExplanationClassify the forming temperature
  7. 7
    ExampleCheck the direct reduction
  8. 8
    ExampleSet the last pass
  9. 9
    ChallengeChoose the intermediate size yourself
  10. 10
    Key InsightDo not add pass percentages
  11. 11
    ChallengeDiagnose an annealing substitution
  12. 12
    RecapTrack dimensions and material state
4

Assess a cracked plate and an impact result

16 steps
Read fracture evidence, calculate crack tolerance, and interpret a temperature-dependent impact requirement.

Save this lesson to follow every Walkthrough step by step.

  1. 1
    IntroductionA strong part can still contain a dangerous crack
  2. 2
    ExplanationWatch ductile separation develop
  3. 3
    ExplanationRead a brittle crack path
  4. 4
    ChallengeInterpret two surfaces
  5. 5
    TipUse the right crack dimension
  6. 6
    ExampleBuild an edge-crack calculation
  7. 7
    ExampleCompare intensity with resistance
  8. 8
    ChallengeAccount for an internal crack
  9. 9
    ExplanationKeep thickness validity separate
  10. 10
    Key InsightRelate flaw size to brittle strength
  11. 11
    ExampleUse a pendulum energy loss
  12. 12
    ExplanationChoose a transition criterion
  13. 13
    ChallengeRead an energy requirement
  14. 14
    ChallengeExplain a cold notch failure
  15. 15
    ConnectionChoose a low-temperature improvement
  16. 16
    RecapMatch the evidence to the question
5

Follow a rotating shaft toward fatigue failure

15 steps
Describe a load cycle, interpret fatigue evidence, and select changes that delay crack damage.

Save this lesson to follow every Walkthrough step by step.

  1. 1
    IntroductionRepeated small loads can accumulate damage
  2. 2
    ExampleCalculate center and excursion
  3. 3
    ExplanationRead finite-life data
  4. 4
    ChallengeUse a cycle with a tensile mean
  5. 5
    ExampleConvert a cycle count into time
  6. 6
    ExplanationSeparate the parts of fatigue life
  7. 7
    ExplanationRead bands at two scales
  8. 8
    ChallengeLocate the initiating detail
  9. 9
    ConnectionUse peak loading for the final threshold
  10. 10
    ExplanationReduce the initiation stress
  11. 11
    ExampleCreate a thermal cycle without an actuator
  12. 12
    ChallengeMatch a remedy to thermal fatigue
  13. 13
    ChallengeCombine environment and crack origin
  14. 14
    TipLeave room for life scatter
  15. 15
    RecapBuild the fatigue assessment in order
6

Estimate creep strain and hot-service life

13 steps
Read a creep curve, calculate rate changes, and choose temperature and microstructure for a rupture-life requirement.

Save this lesson to follow every Walkthrough step by step.

  1. 1
    IntroductionSteady load can produce continuing strain
  2. 2
    ExplanationRead three changing slopes
  3. 3
    ExampleCompare temperature on the absolute scale
  4. 4
    ExampleUse a power-law rate ratio
  5. 5
    ChallengeCheck a strain allowance
  6. 6
    ExplanationIncrease rate by thermal activation
  7. 7
    ConnectionConnect movement to the microstructure
  8. 8
    ExplanationRead one point from a master curve
  9. 9
    ExampleTurn a parameter into life
  10. 10
    ChallengeFind a temperature limit
  11. 11
    ExplanationKeep the strengthening features stable
  12. 12
    ChallengeChoose a hot-service redesign
  13. 13
    RecapCheck two service limits

Strengthening Mechanisms and Failure practice questions

50 Practice Questions in 5 sets

Set 1: Forming routes and annealing10 Practice Questions

Question 1 of 10

An anneal recrystallizes a cold-worked solid-solution alloy while its solute remains dissolved. Which strengthening contribution remains?
  1. The full original cold-work dislocation network.
  2. The contribution from dissolved solute atoms.
  3. The strength from elongated cold-worked grains.
  4. The added hardness from unrecovered tangles.
Show answerHide answer
Answer: B
Dissolved atoms remain lattice obstacles after recrystallization. The original cold-work contribution falls because new low-dislocation-density grains replace the deformed structure.

Question 2 of 10

Which annealing process primarily relieves residual stress with only modest loss of strength?
  1. Recrystallization
  2. Grain growth
  3. Hot deformation
  4. Recovery
Show answerHide answer
Answer: D
Recovery rearranges defects and relieves stress with little softening. Recrystallization replaces deformed grains and causes a much sharper strength drop, so it does not match the stated limited change.

Question 3 of 10

A 150× micrograph has test lines totaling 240 mm with 80 grain-boundary crossings. What is the mean intercept length?
  1. 20 μm
  2. 2 μm
  3. 200 μm
  4. 30 μm
Show answerHide answer
Answer: A
The actual line length is 240/150=1.6 mm. Dividing by 80 crossings gives 0.020 mm, or 20 μm. A 30 μm result would use 100× instead of the stated 150×, so it would not correct the image length for the actual magnification.

Question 4 of 10

A plate is rolled from 6 to 4.2 mm thickness without changing its width. What percent cold work does this give?
  1. 18%
  2. 43%
  3. 30%
  4. 51%
Show answerHide answer
Answer: C
At constant width, cross-sectional area scales directly with thickness. The reduction is (6−4.2)/6=0.30, or 30% cold work. Dividing by final thickness gives about 43%, but percent cold work uses the original area, not the area left after deformation.

Question 5 of 10

With grain-growth exponent two, grains start at 12 μm and the growth constant is 16 μm²/min. What diameter is predicted after 40 min?
  1. 25.3 μm
  2. 25.5 μm
  3. 30.5 μm
  4. 28.0 μm
Show answerHide answer
Answer: D
The squared diameter becomes 122+16(40)=784 μm2. Taking its square root gives 28 μm. Omitting the initial squared diameter gives 640≈25.3 μm, which describes only the growth term and loses the contribution from the original grains.

Question 6 of 10

Two successive 30% area reductions are made without a recrystallization anneal. What is the total percent cold work?
  1. 60%
  2. 51%
  3. 49%
  4. 42%
Show answerHide answer
Answer: B
Each pass retains 70% of its starting area, so the final fraction is 0.70×0.70=0.49. The total area removed is 51%. Adding the two 30% reductions gives 60% but ignores that the second pass starts from a smaller area than the first.

Question 7 of 10

After cold drawing, a wire has higher yield strength but almost the same elastic modulus. Why are these results consistent?
  1. Drawing changes elastic bond stiffness while leaving slip resistance unchanged.
  2. Drawing raises both elastic and plastic slopes by the same geometric factor.
  3. Drawing hinders plastic slip while changing elastic bond stiffness very little.
  4. Drawing changes only cross-sectional size while leaving the material condition unchanged.
Show answerHide answer
Answer: C
Cold work multiplies and tangles dislocations, raising the stress needed for further plastic flow. The initial elastic slope depends mainly on atomic bond stiffness and changes little. Treating yield strength and modulus as the same property would incorrectly predict a proportional increase in both.

Question 8 of 10

An 18 mm rod must finish at 12 mm with 30%–40% retained cold work. A full intermediate recrystallization anneal is available. What intermediate diameter range can meet the requirement?
  1. About 14.34–15.49 mm
  2. About 13.15–14.34 mm
  3. About 15.49–16.97 mm
  4. About 12.00–14.34 mm
Show answerHide answer
Answer: A
Direct drawing gives 55.6%, so the final pass must start after an intermediate anneal. The endpoints are 12/0.70 and 12/0.60, or 14.34–15.49 mm, both below 18 mm. Using diameter percentages directly gives a different range because the property window is based on area reduction.

Question 9 of 10

A micrograph at 200× contains 32 grains per square inch of image area. What ASTM grain size number follows from this count?
  1. 6
  2. 8
  3. 7
  4. 9
Show answerHide answer
Answer: B
Convert the count to the 100× reference: 32(200/100)2=128 grains per square inch. Then 128=27, so G−1=7 and G=8. Applying the grain-number equation directly to 32 gives 6 but ignores the squared magnification correction.

Question 10 of 10

A rod can only be reduced from 10 to 9 mm, but the required retained cold work is 25%–35%. A proposed route inserts a recrystallization anneal at an intermediate diameter. Can any such reduction route meet the requirement?
  1. Yes; annealing at 9.5 mm creates 29% retained cold work.
  2. Yes; the two pass percentages can be added to reach 25%.
  3. No; the available total area reduction is only 19%.
  4. No; the available total area reduction is already 36%.
Show answerHide answer
Answer: C
Direct drawing gives 100(1−92/102)=19%, below the minimum. Even the smallest allowed final reduction target, 25%, would need an annealed diameter 9/0.75≈10.39 mm, larger than the starting rod. An anneal can remove retained cold work but cannot create the missing area reduction.
Set 2: Dislocation motion and strengthening10 Practice Questions

Save this lesson to see every answer and practice every set.

Question 1 of 10

What does an increase in ASTM grain size number indicate?
  1. A coarser structure with fewer grains per reference image area.
  2. A finer structure with more grains per reference image area.
  3. A finer structure with less total grain-boundary area per volume.
  4. A coarser structure with shorter dislocation slip distances.
Show answerHide answer

Save this lesson to see this answer.

Question 2 of 10

Why can a dislocation produce permanent slip at a much smaller stress than simultaneous shear of an entire atomic plane?
  1. The defect removes the bonds from the whole slip plane.
  2. The entire plane loses its elastic stiffness during slip.
  3. Only a small region of bonds rearranges as the defect moves.
  4. The defect makes the entire crystal elastically softer.
Show answerHide answer

Save this lesson to see this answer.

Question 3 of 10

A specimen volume is 4 mm³ and its dislocation density is 3×1013 m−2. What total dislocation line length does it contain?
  1. 120 km
  2. 12 km
  3. 1200 km
  4. 12,000 km
Show answerHide answer

Save this lesson to see this answer.

Question 4 of 10

For the same applied tensile stress, which slip system has the largest resolved shear stress?
  1. A system with Schmid factor 0.24
  2. A system with Schmid factor 0.36
  3. A system with Schmid factor 0.12
  4. A system with Schmid factor 0.48
Show answerHide answer

Save this lesson to see this answer.

Question 5 of 10

A single crystal has critical resolved shear stress 15 MPa and largest Schmid factor 0.30. At what tensile stress does slip begin?
  1. 4.5 MPa
  2. 50 MPa
  3. 30 MPa
  4. 45 MPa
Show answerHide answer

Save this lesson to see this answer.

Question 6 of 10

Why does adding dissolved magnesium strengthen an aluminum solid solution?
  1. Solute atoms make the host planes more closely packed.
  2. Solute atoms greatly increase elastic bond stiffness.
  3. Solute atoms remove dislocations during deformation.
  4. Solute lattice distortions hinder dislocation motion.
Show answerHide answer

Save this lesson to see this answer.

Question 7 of 10

A round rod is drawn from 20 to 16 mm diameter without annealing. What is its percent cold work?
  1. 36%
  2. 20%
  3. 25%
  4. 44%
Show answerHide answer

Save this lesson to see this answer.

Question 8 of 10

A property chart meets the minimum yield strength at 22% cold work and retains the minimum elongation up to 37%. What range meets both requirements?
  1. 0%–22%
  2. 37%–59%
  3. 22%–37%
  4. 22%–59%
Show answerHide answer

Save this lesson to see this answer.

Question 9 of 10

A BCC crystal is pulled along [001]. Consider plane (101) and in-plane direction [1 1 −1]. The critical resolved shear stress is 18 MPa. At what tensile stress does this system reach its slip threshold? Use the magnitude of the resolved shear.
  1. About 44 MPa
  2. About 22 MPa
  3. About 31 MPa
  4. About 62 MPa
Show answerHide answer

Save this lesson to see this answer.

Question 10 of 10

A metal yields at 160 MPa with 100 μm grains and 280 MPa with 25 μm grains. Both conditions follow one Hall–Petch line. What yield strength is predicted for 4 μm grains?
  1. 600 MPa
  2. 700 MPa
  3. 800 MPa
  4. 640 MPa
Show answerHide answer

Save this lesson to see this answer.

Set 3: Crack tolerance and impact behavior10 Practice Questions

Save this lesson to see every answer and practice every set.

Question 1 of 10

Two conditions of one alloy have the same crack geometry and size. Their applicable fracture toughness values are 45 and 72 MPa√m. By what factor do their predicted critical stresses differ?
  1. 1.60
  2. 1.26
  3. 2.56
  4. 0.625
Show answerHide answer

Save this lesson to see this answer.

Question 2 of 10

A fracture surface has dimples corresponding to joined cavities. What process produced this surface?
  1. Brittle transgranular cleavage
  2. Brittle grain-boundary separation
  3. Dislocation recovery into subgrains
  4. Ductile microvoid coalescence
Show answerHide answer

Save this lesson to see this answer.

Question 3 of 10

A steel impact curve reports a transition temperature using a 50% fibrous fracture criterion. Why might an energy-based criterion give another temperature?
  1. The fibrous criterion measures yield strength instead of fracture.
  2. The criteria select different points within a transition range.
  3. The energy criterion removes the effect of test temperature.
  4. The criteria must coincide if specimen geometry is unchanged.
Show answerHide answer

Save this lesson to see this answer.

Question 4 of 10

A wide plate has an internal crack 10 mm long and carries 200 MPa tension. With geometry factor 1, what stress intensity results?
  1. About 35.4 MPa√m
  2. About 11.2 MPa√m
  3. About 25.1 MPa√m
  4. About 79.3 MPa√m
Show answerHide answer

Save this lesson to see this answer.

Question 5 of 10

A material has plane-strain toughness 60 MPa√m and yield strength 1200 MPa. What minimum thickness follows from B≥2.5(KIc/σy)2?
  1. 6.25 mm
  2. 2.50 mm
  3. 12.5 mm
  4. 62.5 mm
Show answerHide answer

Save this lesson to see this answer.

Question 6 of 10

A 12 kg pendulum starts at height 1.8 m and rises to 1.1 m after breaking a specimen. With g=9.81 m/s2, what energy was absorbed?
  1. About 129 J
  2. About 212 J
  3. About 82.4 J
  4. About 47.1 J
Show answerHide answer

Save this lesson to see this answer.

Question 7 of 10

Brittle fracture chevrons point toward a weld defect, while the roughest final region lies elsewhere. Where should the initiating flaw investigation begin?
  1. At the roughest region of the fracture surface.
  2. At the weld defect indicated by the chevron tips.
  3. At the region farthest from the chevron tips.
  4. At the grain boundaries along the cleavage path.
Show answerHide answer

Save this lesson to see this answer.

Question 8 of 10

A wide plate with a 2.5 mm edge crack has Y=1.12. Condition A has toughness 42 MPa√m and yield strength 1000 MPa; B has toughness 63 MPa√m and yield strength 800 MPa. Which condition has the greater load capacity before fracture or yielding in this assessment?
  1. A; its 1000 MPa yield strength controls before its crack fractures.
  2. B; its 800 MPa yield strength controls before its crack fractures.
  3. A; predicted fracture occurs near 474 MPa, above B’s fracture stress.
  4. B; predicted fracture occurs near 635 MPa, below its yield strength.
Show answerHide answer

Save this lesson to see this answer.

Question 9 of 10

A thick plate uses an internal-crack assessment with Y=1, toughness 48 MPa√m, and stress 300 MPa. Inspection reliably detects total crack lengths of at least 12 mm. Is that detection threshold below the calculated critical total length?
  1. No; the critical total length is about 8.15 mm.
  2. Yes; the critical total length is about 32.6 mm.
  3. Yes; the critical total length is about 16.3 mm.
  4. No; the critical total length is about 4.07 mm.
Show answerHide answer

Save this lesson to see this answer.

Question 10 of 10

Two steels meet the same yield requirement. At −25 °C, A absorbs 22 J and B absorbs 38 J in matching Charpy tests. The stated requirement is 30 J at −25 °C. A proposal selects A solely because its room-temperature energy is higher. What conclusion follows?
  1. B meets the stated cold-test criterion; room-temperature ranking does not rescue A.
  2. A meets the stated cold-test criterion because its warm-test ranking controls.
  3. Both meet the stated criterion because their yield requirements are identical.
  4. Neither can be compared because energy must first be converted into toughness.
Show answerHide answer

Save this lesson to see this answer.

Set 4: Repeated loads and hot-service damage10 Practice Questions

Save this lesson to see every answer and practice every set.

Question 1 of 10

A load cycle runs from −90 to 150 MPa. What is its stress amplitude?
  1. 120 MPa
  2. 240 MPa
  3. 30 MPa
  4. 150 MPa
Show answerHide answer

Save this lesson to see this answer.

Question 2 of 10

A fracture surface contains microscopic striations inside a much wider beachmark band. What history do these features support?
  1. One load cycle for each beachmark, with many pauses between.
  2. One loading interruption for every microscopic ridge.
  3. Many small cyclic advances within a broader loading-history interval.
  4. Many grain-boundary crossings within one sudden cleavage event.
Show answerHide answer

Save this lesson to see this answer.

Question 3 of 10

At the matching stress ratio, an aluminum alloy has fatigue strength 115 MPa at 2 × 10⁷ cycles on a continuously falling S–N curve. A component operates at 130 MPa amplitude. How does its curve-predicted life compare with 2 × 10⁷ cycles?
  1. It is exactly 2 × 10⁷ cycles.
  2. It is shorter than 2 × 10⁷ cycles.
  3. It is longer than 2 × 10⁷ cycles.
  4. It is unlimited below the tensile yield stress.
Show answerHide answer

Save this lesson to see this answer.

Question 4 of 10

Two otherwise identical polished parts have the same applied cyclic load. One is shot-peened and retains compressive surface residual stress. Why is its fatigue life usually longer?
  1. Surface compression raises the applied cycle’s measured stress amplitude.
  2. Surface compression eliminates all tensile stress throughout the section.
  3. Surface compression replaces the need to check the applied mean stress.
  4. Surface compression opposes tension during initiation and early growth.
Show answerHide answer

Save this lesson to see this answer.

Question 5 of 10

At fixed temperature, an alloy’s creep rate is proportional to stress to the fourth power. Reducing stress from 120 to 90 MPa changes the rate by what factor?
  1. About 0.316
  2. About 0.750
  3. About 0.563
  4. About 3.160
Show answerHide answer

Save this lesson to see this answer.

Question 6 of 10

At the actual operating stress, a master curve gives P=24000 with C=20. What temperature corresponds to a predicted rupture life of 1000 h?
  1. About 1200 K
  2. About 1043 K
  3. About 923 K
  4. About 800 K
Show answerHide answer

Save this lesson to see this answer.

Question 7 of 10

A rotating shaft surface cycles between −70 and 170 MPa once per revolution at 1500 revolutions per minute. Matching S–N data give 9 × 10⁶ cycles at 120 MPa amplitude. What operating time corresponds to that curve point?
  1. 60 h
  2. 150 h
  3. 200 h
  4. 100 h
Show answerHide answer

Save this lesson to see this answer.

Question 8 of 10

A fatigue crack is internal and 6 mm long in a wide plate with Y=1 and applicable toughness 38 MPa√m. The cycle runs from 50 to 350 MPa. Does the maximum-cycle linear-elastic fracture threshold appear reached?
  1. Yes; maximum intensity is about 48.1 MPa√m.
  2. No; maximum intensity is about 14.6 MPa√m.
  3. No; maximum intensity is about 34.0 MPa√m.
  4. Yes; maximum intensity is about 68.0 MPa√m.
Show answerHide answer

Save this lesson to see this answer.

Question 9 of 10

A fully restrained elastic bar repeatedly heats from 300 to 370 K and cools back. Its expansion coefficient is 10 × 10⁻⁶ K⁻¹ and modulus 160 GPa. An otherwise identical installation permits free uniform expansion. What thermal-stress comparison is expected?
  1. The restrained heating stress is about 112 MPa tension; the free case is near zero.
  2. The restrained heating stress is about 112 MPa compression; the free case is near zero.
  3. The restrained heating stress is about 56 MPa compression; the free case is near zero.
  4. Both cases develop about 112 MPa compression during uniform heating.
Show answerHide answer

Save this lesson to see this answer.

Question 10 of 10

A part allows 0.8% secondary creep over 40,000 h. Its current rate is 4 × 10⁻⁷ h⁻¹ at 100 MPa, with stress exponent four. Temperature stays fixed. Approximately what maximum stress meets this secondary-strain allowance?
  1. 71 MPa
  2. 92 MPa
  3. 95 MPa
  4. 84 MPa
Show answerHide answer

Save this lesson to see this answer.

Set 5: Choose and justify a material decision10 Practice Questions

Save this lesson to see every answer and practice every set.

Question 1 of 10

A brittle crack runs along weakened grain boundaries instead of crossing their interiors. What is the fracture path called?
  1. Transgranular cleavage
  2. Intergranular fracture
  3. Microvoid coalescence
  4. Cup-and-cone separation
Show answerHide answer

Save this lesson to see this answer.

Question 2 of 10

At the same stress and Larson–Miller parameter, temperature is reduced while the material constant stays fixed. What happens to the predicted rupture time?
  1. It increases because P/T − C becomes larger.
  2. It decreases because P/T − C becomes larger.
  3. It is unchanged because stress did not change.
  4. It decreases because the melting temperature is unchanged.
Show answerHide answer

Save this lesson to see this answer.

Question 3 of 10

Two cycles have equal amplitude. One is fully reversed and the other is entirely tensile with a positive mean. For the same material and surface, which is generally more damaging in fatigue?
  1. The fully reversed cycle is more damaging.
  2. The cycles must have equal fatigue damage.
  3. The cycle with lower minimum stress is worse.
  4. The tensile-mean cycle is more damaging.
Show answerHide answer

Save this lesson to see this answer.

Question 4 of 10

A fine-grained steel is proposed for a cold structure and a coarse-grained version for a boundary-creep-limited hot part. Why can both selections be sensible?
  1. Fine grains increase low-temperature slip distances; coarse grains reduce boundary-controlled creep.
  2. Fine grains hinder low-temperature slip; coarse grains retain cold-work strength in hot service.
  3. Fine grains hinder low-temperature slip; coarse grains reduce boundary-controlled creep.
  4. Fine grains lower room-temperature yield strength; coarse grains reduce boundary-controlled creep.
Show answerHide answer

Save this lesson to see this answer.

Question 5 of 10

At fixed temperature with growth exponent two, grains grow from 18 to 30 μm in 24 min. What total hold time from the initial 18 μm state gives 42 μm grains?
  1. 60 min
  2. 36 min
  3. 48 min
  4. 72 min
Show answerHide answer

Save this lesson to see this answer.

Question 6 of 10

A 15 mm rod must finish at 9 mm with 25%–30% retained cold work after full recrystallization. A proposal anneals at 11 mm and then draws to 9 mm. What change meets the target?
  1. Keep 11 mm; the final retained cold work is within 25%–30%.
  2. Anneal near 12.0 mm instead; 11 mm leaves too little final cold work.
  3. Use recovery at 11 mm instead; it resets retained cold work to zero.
  4. Anneal near 10.6 mm instead; 11 mm leaves too much final cold work.
Show answerHide answer

Save this lesson to see this answer.

Question 7 of 10

A wide plate has a central crack 12 mm long, Y=1, toughness 55 MPa√m, and yield strength 700 MPa. A proposed static tensile load gives 450 MPa. Which limit has been crossed in the linear-elastic crack assessment?
  1. Neither limit is crossed because the fracture threshold is about 568 MPa.
  2. The fracture threshold, about 401 MPa, is exceeded while nominal stress remains below yield.
  3. Only the yield threshold is crossed because crack fracture occurs above 700 MPa.
  4. Both limits are crossed because nominal stress exceeds 401 MPa and therefore exceeds yield.
Show answerHide answer

Save this lesson to see this answer.

Question 8 of 10

A shaft has a sharp shoulder, tensile surface residual stress, and corrosion pits at its fatigue origin. A redesign keeps the same nominal cycle. Which combination addresses all three identified causes?
  1. A larger fillet radius, surface compression, and higher tensile mean stress.
  2. A smaller fillet radius, surface compression, and corrosion protection.
  3. A larger fillet radius, surface compression, and corrosion protection.
  4. A larger fillet radius, tensile surface stress, and corrosion protection.
Show answerHide answer

Save this lesson to see this answer.

Question 9 of 10

At unchanged stress, an alloy’s creep activation energy is 200 kJ/mol. Temperature rises from 800 to 850 K. Its original rate is 1 × 10⁻⁷ h⁻¹. About how much secondary strain accumulates in 10,000 h at the new temperature? Use R=8.314 J/(mol⋅K).
  1. 0.17%
  2. 0.10%
  3. 5.9%
  4. 0.59%
Show answerHide answer

Save this lesson to see this answer.

Question 10 of 10

At 180 MPa, an alloy master curve shows P/1000=23.5, with C=20. A part must last 20,000 h. What approximate temperature limit follows, and how does a proposed 1000 K compare?
  1. 967 K; 1000 K gives a shorter predicted life than required.
  2. 967 K; 1000 K gives a longer predicted life than required.
  3. 1175 K; 1000 K gives a longer predicted life than required.
  4. 23.5 K; 1000 K gives a shorter predicted life than required.
Show answerHide answer

Save this lesson to see this answer.

Stuck on your own question? Homework Help

Key Terms

88 Key Terms, each with its definition

A

Anisotropy
Anisotropy means that a material property depends on the direction in which it is measured.
A heavily rolled sheet can show different mechanical behavior along and across the rolling direction.
ASTM grain size number
The ASTM grain size number is an index based on grains per square inch at 100× magnification, with larger numbers denoting finer grains.
An image containing more grains in the same reference area corresponds to a larger grain size number.

B

Beachmark
A beachmark is a visible band recording a loading change or interruption during fatigue crack growth.
Curved beachmarks centered on a keyway corner suggest where a shaft’s fatigue crack originated.
Brittle fracture
Brittle fracture is separation with little plastic deformation, often involving rapid crack growth across a relatively flat section.
A cold notched ferritic steel component can fail by cleavage before showing much overall distortion.
Burgers vector
The Burgers vector gives the size and direction of lattice displacement associated with a dislocation.
A Burgers circuit around an edge defect fails to close in a direction perpendicular to the defect line.

C

Charpy test
A Charpy test measures energy absorbed when a swinging pendulum breaks a notched bar resting horizontally on two supports.
Testing the same steel at several temperatures reveals how its absorbed impact energy changes.
Chevron marking
A chevron marking is a V-shaped fracture feature whose tip points toward the crack origin.
An analyst follows chevron tips toward a suspected weld flaw to locate where the brittle crack began.
Cleavage
Cleavage is brittle crack growth through grains along particular crystal planes.
A sparkling steel fracture surface can contain cleavage facets from cracks crossing grain interiors.
Climb
Climb is diffusion-assisted motion of an edge dislocation out of its slip plane.
At high temperature, climb can let a dislocation pass an obstacle that prevents continued glide.
Cold working
Cold working is plastic deformation below the metal’s recrystallization temperature, producing strain hardening and reduced ductility.
Cold rolling can improve sheet finish and dimensional accuracy while increasing the required forming force.
Corrosion fatigue
Corrosion fatigue is fatigue damage accelerated by a corrosive environment through pit formation, crack initiation, and faster crack growth.
A protective coating can help a cyclically loaded steel part by reducing exposure to corrosive liquid.
Crack initiation
Crack initiation is the early formation of a crack at a locally damaged region, often at a surface notch, scratch, inclusion, or slip band.
Removing machining scratches can extend the initiation part of a component’s high-cycle fatigue life.
Crack propagation
Crack propagation is the extension of an existing crack; under fatigue, repeated loading drives progressive advance before final separation.
An inspection program aims to find a propagating crack before it reaches a critical size at peak load.
Creep
Creep is time-dependent permanent deformation under sustained load or stress, especially important at high temperature relative to melting.
A boiler tube can slowly change dimensions during years of service even when its stress is below yield.
Critical crack size
Critical crack size is the flaw dimension at which the applied load produces the fracture condition for the material and geometry.
Inspection aims to detect a crack well before it reaches the critical depth at the operating stress.
Critical resolved shear stress
Critical resolved shear stress is the shear-stress threshold that starts slip on a system at a specified temperature and strain rate.
Slip begins when the resolved stress on the most favorable system reaches its critical value.
Cup-and-cone fracture
A cup-and-cone fracture is a tensile fracture shape with a central void-growth region and an outer shear lip in a ductile round bar.
The outer rim of a broken tensile specimen commonly slopes near 45° to the tensile loading axis.

D

Decarburization
Decarburization is the loss of carbon from a steel surface during processing.
Controlling the heating atmosphere helps preserve the carbon content of a fatigue-critical steel surface.
Deformation twinning
Deformation twinning is a shear process that reorients a crystal region into a mirror-related orientation across a twin plane.
Twinning in an HCP grain can put additional slip directions into a more favorable loading orientation.
Diffusion creep
Diffusion creep is deformation by stress-driven atomic transport through grains or along their boundaries, often with a stress exponent near one.
Fine grains can increase the importance of diffusion and boundary-controlled creep at high temperature.
Directional solidification
Directional solidification is controlled growth of elongated grains along a chosen direction, reducing boundaries transverse to a main load.
Long grains aligned with a turbine blade’s main stress help reduce harmful transverse-boundary deformation.
Dislocation
A dislocation is a line defect in a crystal whose movement allows permanent slip.
A moving dislocation lets a copper crystal deform while only nearby bonds rearrange at each instant.
Dislocation creep
Dislocation creep is high-temperature deformation involving dislocation glide and diffusion-assisted climb past obstacles.
A stress exponent well above one is consistent with a dislocation-controlled creep regime.
Dislocation density
Dislocation density is total dislocation line length per unit volume, measured in inverse square meters.
Drawing a wire multiplies dislocations and raises its dislocation density above the annealed value.
Ductile fracture
Ductile fracture is separation accompanied by substantial plastic deformation, commonly through microvoid formation, growth, and joining.
A necked tensile bar with a cup-and-cone surface shows evidence of considerable plastic deformation.
Ductile-to-brittle transition temperature
The ductile-to-brittle transition temperature is a temperature selected by a stated criterion within a material’s changing fracture behavior.
A laboratory can report the temperature giving 50% fibrous area instead of using a fixed-energy criterion.

E

Edge dislocation
An edge dislocation is the line at the end of an extra atomic half-plane inside a crystal, with its Burgers vector perpendicular to the line.
The lattice is compressed on the extra-half-plane side of an edge dislocation and stretched on the other side.
Equiaxed grain
An equiaxed grain has roughly equal dimensions in different directions.
After recrystallization, an image can show equiaxed grains distributed across a range of diameters.

F

Fatigue
Fatigue is progressive damage under fluctuating stress that can cause failure after repeated cycles, even below the material’s yield strength.
An axle can develop a fatigue crack after many rotations despite having an adequate static yield margin.
Fatigue limit
A fatigue limit is a stress-amplitude threshold below which fatigue failure is not expected under the test conditions that establish it.
A steel fatigue limit measured in a benign environment may not remain valid in corrosive service.
Fatigue strength
Fatigue strength is the cyclic stress amplitude associated with failure at a specified number of cycles under stated test conditions.
An aluminum alloy’s reported fatigue strength needs a cycle count because its S–N curve keeps declining.
Fillet radius
A fillet radius measures the curvature of a rounded transition between intersecting surfaces.
Increasing the shoulder fillet on a shaft can delay fatigue initiation at the change in diameter.
Final-fracture zone
The final-fracture zone is the region that separates rapidly after fatigue growth leaves a critical crack or an overloaded remaining section.
A small rough final zone can accompany a large smooth region grown under relatively low nominal stress.
Fracture toughness
Fracture toughness is resistance to extension of an existing sharp crack, expressed as a critical stress intensity under specified conditions.
A lower-strength alloy condition can tolerate a larger flaw if its fracture toughness is substantially higher.

G

Glide
Glide is dislocation movement within a slip plane that produces permanent shear.
At ordinary forming temperatures, glide carries much of the plastic deformation in a ductile metal.
Grain growth
Grain growth is the increase in average grain size as boundary motion lets larger grains consume smaller ones, reducing total boundary energy.
An unnecessarily long anneal can coarsen the new grains and reduce the strength gained from refinement.
Grain refinement
Grain refinement is the reduction of average grain size, increasing boundary barriers and usually improving low-temperature strength and toughness.
Controlled rolling can produce fine-grained steel with useful strength and low-temperature toughness.
Griffith criterion
The Griffith criterion predicts brittle crack growth when released elastic energy supplies the energy needed to create new fracture surfaces.
A larger surface flaw reduces the tensile stress needed to break glass in the Griffith model.

H

Hall–Petch equation
The Hall–Petch equation relates yield strength to a constant plus a term proportional to the inverse square root of average grain diameter.
A fourfold reduction in grain diameter doubles the grain-size term while leaving the intercept unchanged.
Homologous temperature
Homologous temperature is service temperature divided by melting temperature, both on an absolute scale.
The same Celsius service temperature represents a higher homologous temperature for aluminum than for nickel.
Hot working
Hot working is plastic deformation above the metal’s recrystallization temperature, enabling large reductions without retained strain hardening.
Lead can undergo hot working at room temperature because its recrystallization temperature is low.

I

Inoculant
An inoculant is a material added to a melt to promote grain nucleation during solidification and thereby produce a finer grain structure.
Titanium and boron additions can provide useful grain-refining sites during aluminum alloy solidification.
Intergranular fracture
Intergranular fracture is crack growth along weakened grain boundaries.
Boundary embrittlement can leave a fracture surface that outlines the shapes of individual grains.
Intermediate anneal
An intermediate anneal is a heat treatment between forming stages that can recrystallize the metal and restore ductility for further reduction.
A rod is drawn partway, recrystallized, and then finished with a smaller reduction to retain the required cold work.
Interstitial solute
An interstitial solute is a dissolved atom occupying a gap between host atoms.
Small amounts of dissolved carbon or nitrogen can strongly hinder dislocation motion in ferritic iron.
Izod test
An Izod test measures impact behavior using a notched specimen clamped upright as a cantilever and struck by a pendulum.
The Izod clamp arrangement differs from the two-support geometry used for a Charpy specimen.

L

Larson–Miller parameter
The Larson–Miller parameter combines absolute temperature with the base-10 logarithm of rupture time to correlate creep-rupture data.
A master curve provides the parameter at the selected stress before temperature is converted into predicted life.
Lower shelf
The lower shelf is the low-energy region of an impact-energy curve associated with predominantly brittle fracture at low temperatures.
Cooling transition-sensitive steel toward its lower shelf reduces the energy absorbed during impact.
Lüders band
A Lüders band is a localized band of plastic deformation that spreads through a specimen during discontinuous yielding after solute pinning.
Visible Lüders bands may travel along a steel tensile specimen near its lower yield-point stress.

M

Mean intercept length
Mean intercept length is the actual total test-line length divided by its grain-boundary crossings on a microstructural image.
A metallographer corrects the image line length for magnification before reporting an intercept in micrometers.
Mean stress
Mean stress is the average of the maximum and minimum stresses in a load cycle.
Shifting a stress cycle toward tension raises its mean even if its amplitude stays unchanged.
Microvoid coalescence
Microvoid coalescence is the joining of small cavities into a crack during ductile fracture after the cavities nucleate and enlarge.
Dimples on an electron-microscope image mark the cavities that joined as the metal separated.

P

Percent cold work
Percent cold work is the decrease in cross-sectional area divided by the original area, multiplied by one hundred for deformation below recrystallization.
A rod diameter reduction must be squared before calculating the corresponding percentage of cold work.
Plane strain
Plane strain is a constrained deformation state with negligible strain in one direction, approached near the interior of a thick cracked specimen.
A sufficiently thick toughness specimen restricts crack-tip deformation through its thickness.
Plane-strain fracture toughness
Plane-strain fracture toughness is the limiting opening-mode crack resistance measured under high constraint and predominantly linear-elastic conditions.
A toughness test must meet crack and load-response requirements as well as the necessary thickness check.
Primary creep
Primary creep is the early creep stage in which strain rate decreases as strain hardening initially exceeds the effects of recovery.
The strain–time curve becomes less steep after loading while the metal develops resistance to further creep.

R

Recovery
Recovery is the thermally assisted rearrangement and partial removal of defects in a cold-worked metal, relieving stress with limited softening.
A stress-relief anneal can reduce residual stress while retaining much of the cold-worked metal’s strength.
Recrystallization
Recrystallization is replacement of cold-worked grains by new grains with low dislocation density, restoring ductility while reducing strength.
New grains grow into the deformed regions during a suitable anneal without melting or changing crystal structure.
Recrystallization temperature
The recrystallization temperature is conventionally the temperature that completes recrystallization in one hour for a given prior condition.
More prior cold work can lower the temperature required for a one-hour recrystallization treatment.
Residual stress
Residual stress is internal stress that remains in a body after external loads or the processing conditions that created it have been removed.
Cold forming can leave residual stresses that a later stress-relief anneal reduces through recovery.
Resolved shear stress
Resolved shear stress is the component of an applied stress that drives shear on a particular slip plane in its slip direction.
Two differently oriented grains under the same tensile load can have different resolved shear stresses.
Rupture lifetime
Rupture lifetime is the time to creep separation at a specified stress and temperature.
A component can meet a rupture-life requirement yet still exceed an allowable dimensional creep strain.

S

S–N curve
An S–N curve relates cyclic stress amplitude to cycles to failure for specimens tested under specified loading and environmental conditions.
A designer enters an amplitude-based S–N graph with half the stress range to read an estimated fatigue life.
Scale
Scale is an oxide layer formed on a metal surface during hot processing.
A hot-worked product may need scale removal before its final surface or dimensions are finished.
Schmid factor
The Schmid factor is the product of the cosines of the loading-axis angles to the slip-plane normal and to the slip direction.
A crystal with a smaller favorable Schmid factor needs more tensile stress to reach the same slip threshold.
Screw dislocation
A screw dislocation is a line defect with a spiral arrangement of atomic planes and a Burgers vector parallel to its line.
A screw dislocation can cross-slip onto another suitable plane that contains its Burgers vector.
Secondary creep
Secondary creep is the stage with a nearly constant strain rate as deformation hardening and recovery approximately balance.
The nearly straight middle segment of a creep curve supplies the steady-state rate for a strain estimate.
Shot peening
Shot peening is surface treatment by repeated small particle impacts that create a compressive residual-stress layer and improve fatigue resistance.
Peening a spring can delay surface crack initiation by opposing applied tensile stress near the surface.
Single-crystal blade
A single-crystal blade is a turbine blade formed as one crystal, eliminating grain boundaries that could slide or develop cavities in hot service.
Removing grain boundaries helps a turbine blade resist boundary-controlled high-temperature damage.
Slip band
A slip band is a group of surface slip lines left by repeated dislocation passage.
Fine bands become visible on a polished single-crystal surface after enough plastic deformation.
Slip system
A slip system combines a crystallographic slip plane with a direction lying in that plane.
The FCC family combines close-packed {111} planes with suitable ⟨110⟩ directions within those planes.
Solid-solution strengthening
Solid-solution strengthening is increased resistance to plastic flow caused by dissolved atoms whose lattice distortions impede dislocations.
Dissolved magnesium helps strengthen an aluminum alloy before any extra strength from cold work is considered.
Solubility limit
A solubility limit is the greatest amount that can remain dissolved in a phase at a given temperature.
Adding more alloying element beyond its solubility limit can produce a separate phase in the metal.
Strain field
A strain field is the spatial pattern of elastic lattice distortion around a defect, which stores energy and interacts with other defects.
An alloying atom can lower energy by partially canceling the strain field near an edge dislocation.
Strain hardening
Strain hardening is the increase in flow strength during plastic deformation as dislocations multiply and obstruct further dislocation motion.
A cold-drawn wire needs greater stress for further plastic stretching than it did before drawing.
Strain-hardening exponent
The strain-hardening exponent is the exponent on true plastic strain in a power-law flow curve, describing how rapidly flow stress rises.
A metal with a larger hardening exponent builds flow stress more rapidly as plastic strain increases.
Stress amplitude
Stress amplitude is half the difference between maximum and minimum cyclic stress.
A cycle from −60 to 180 MPa has an amplitude of 120 MPa even though its peak is 180 MPa.
Stress concentration factor
The stress concentration factor is the dimensionless ratio of local peak stress near a flaw or geometric feature to nominal stress.
Increasing a fillet radius can lower the peak stress relative to the nominal stress in a stepped part.
Stress intensity factor
The stress intensity factor quantifies the near-tip stress field of a crack from applied stress, crack size, and geometry.
An engineer converts an edge-crack depth to meters before calculating intensity in MPa√m.
Stress ratio
Stress ratio is the minimum cyclic stress divided by the maximum cyclic stress.
A fully reversed tensile–compressive cycle has a stress ratio of minus one and zero mean stress.
Striation
A striation is a microscopic ridge associated with a small increment of fatigue crack advance.
An electron microscope can reveal many striations inside the much wider spacing of one beachmark.
Subgrain
A subgrain is a region within a grain separated from adjacent regions by low-angle boundaries.
Recovery can organize dislocations into subgrain boundaries before full recrystallization occurs.
Substitutional solute
A substitutional solute is a dissolved atom replacing a host atom at a regular lattice site.
A zinc atom can replace a copper atom in the copper-rich solid solution that makes up brass.

T

Tertiary creep
Tertiary creep is the accelerating stage before rupture, driven by damage such as cavities, cracks, and increasing stress as section area shrinks.
A constant-load specimen can creep faster as necking reduces the area supporting the same applied load.
Thermal fatigue
Thermal fatigue is cyclic damage caused by stresses from repeated temperature changes when thermal expansion or contraction is restrained.
An expansion joint reduces the restraint that would otherwise turn temperature cycling into stress cycling.
Thermal-barrier coating
A thermal-barrier coating is an insulating surface layer that lowers the temperature of the underlying metal during hot service.
A ceramic coating lets a turbine blade’s metal operate cooler than the surrounding hot gas.

U

Upper shelf
The upper shelf is the high-energy region of an impact-energy curve where fracture is largely ductile and changes less with temperature.
A ferritic steel specimen tested on its upper shelf usually shows substantial fibrous fracture area.

Y

Yield point phenomenon
The yield point phenomenon is a tensile response with an upper stress peak followed by a lower yielding level as pinned dislocations break free.
Low-carbon steel can begin yielding with a stress drop while plastic deformation bands spread along it.

About this lesson

By StudeliReport a mistake

Make your own Study Materials

Turn your notes, slides and documents into Study Guides, Practice Questions, Flashcards and 6 more tools.

Get Started