Corrosion and Materials Selection

Learn why metals corrode and how polymers and ceramics degrade, and how engineers choose materials that do the job for as long, as cheaply and as cleanly as possible. Use electrode potentials, Faraday's law and oxide growth laws to predict and calculate corrosion; recognize the forms of corrosion and prevent them with material choice, design, inhibitors, coatings and cathodic protection. Then derive performance indices, read Ashby property charts, and weigh cost, life-cycle cost, embodied energy and recycling when selecting a material.

IntermediateLesson 9 of 9 in Materials Science and Engineering Course

What you will learn

  1. Describe the corrosion of metals as linked oxidation and reduction reactions, predict which metal corrodes from electrode potentials, calculate corrosion rates and explain how metals oxidize in hot, dry gases.
    • Describe the corrosion cell and its half-reactions
      Write the anodic and cathodic half-reactions for a metal in water and name the four parts every wet corrosion cell needs.
    • Predict which metal corrodes using electrode potentials
      Use the standard emf series, the Nernst equation and the galvanic series to decide which metal in a couple is oxidized and how strong the driving force is.
    • Calculate corrosion rates and explain polarization and passivity
      Express corrosion rates as penetration rate or current density, convert between them with Faraday's law, and use polarization and passivity to explain why real rates differ from what potentials suggest.
    • Explain oxidation of metals at high temperature
      Describe dry oxidation in hot gases, judge whether an oxide scale protects the metal with the Pilling–Bedworth ratio, and apply linear, parabolic and logarithmic growth laws.
  2. Recognize each form of corrosion from its appearance and conditions, explain why it happens, and prevent it through material choice, the environment, design, coatings and cathodic protection.
    • Recognize uniform, galvanic, crevice and pitting corrosion
      Identify these forms from their appearance and conditions, explain their mechanisms and name the changes that control them.
    • Recognize intergranular attack, selective leaching, erosion–corrosion, stress corrosion and hydrogen embrittlement
      Explain the mechanism, typical alloys and conditions of the forms that act along grain boundaries, on one element of an alloy, under fluid flow or under stress, and how each is controlled.
    • Prevent corrosion through material choice, environment control and design
      Choose materials that suit the environment, change the environment with inhibitors and other measures, and design details that keep water out and avoid harmful metal couples.
    • Protect metals with coatings and cathodic protection
      Explain how barrier, sacrificial and noble coatings work, and how sacrificial-anode and impressed-current cathodic protection keep a structure from corroding.
  3. Explain the physical and chemical ways in which polymers and ceramics deteriorate in service, and choose materials and additives that slow this deterioration.
    • Explain swelling, dissolution and environmental stress cracking of polymers
      Explain how liquids enter and weaken polymers, predict which polymer–liquid pairs are risky, and recognize environmental stress cracking.
    • Explain bond rupture, weathering and the degradation of ceramics
      Explain how radiation, chemical attack and heat break polymer chains, how weathering is slowed with stabilizers, and how ceramics and glasses are attacked.
  4. Translate design requirements into constraints and an objective, derive material performance indices, and use Ashby property charts to screen and rank candidate materials.
    • Translate a design into function, constraints, objective and free variables
      Turn a design brief into the statements that drive materials selection, then screen candidates with limits before ranking them.
    • Derive performance indices for ties, beams, panels and shafts
      Write the objective as an equation, eliminate the free variable with the constraint, and read off the performance index to maximize.
    • Use Ashby property charts to screen and rank materials
      Read logarithmic property charts, draw selection lines for a performance index, and combine limits and indices to arrive at a short list.
  5. Compare materials by cost per function and over a product's whole life, judge the environmental burden across the materials cycle, and design products whose materials can be recovered.
    • Compare materials by cost per unit of function
      Use cost-based performance indices and component cost estimates to compare materials that do the same job.
    • Estimate life-cycle cost, including the cost of corrosion
      Add up the costs of a design over its whole service life, discount future costs, and use the result to judge corrosion-resistant choices.
    • Judge environmental impact across the materials cycle
      Follow a material from extraction to end of life, compare embodied energy, and find the life phase that dominates a product's environmental burden.
    • Design for recycling and explain how each material class is recycled
      Explain how metals, glass, thermoplastics, thermosets, elastomers and composites are recovered, what limits recycling, and how design choices make it easier.

Corrosion and Materials Selection study guide

5 chapters

1

Explain corrosion as an electrochemical process

Corrosion links chemistry to the loss of useful metal. Half-reactions show where atoms dissolve and where electrons are consumed; potentials show the driving force. Rate calculations then connect mass or charge to thickness loss, while polarization and passive films explain why voltage alone cannot predict service life. In hot gases, oxide scales create a different transport barrier whose growth can slow or continue at a steady rate.

1.1 Follow the reactions in a corrosion cell

A metal can lose atoms while looking like a single, continuous piece. Different areas of its surface carry out different reactions. To explain the damage, follow both the electrons in the metal and the ions in the water.

Connect oxidation and reduction

At the anode, metal atoms lose electrons and enter solution:

M→Mn++ne−.

At the cathode, a reduction reaction consumes those electrons. In acid, hydrogen ions can be reduced: 2H++2e−→H2. In neutral or basic aerated water, oxygen is usually reduced: O2+2H2O+4e−→4OH−. In acid, oxygen reduction instead uses hydrogen ions: O2+4H++4e−→2H2O. Dissolved metal ions can also accept electrons, for example Fe3++e−→Fe2+.

The anode and cathode reactions must transfer equal numbers of electrons. If the cathodic reaction slows, the connected anodic reaction must also slow. Oxygen is therefore important in many water systems, but it is not essential to every corrosion reaction: acid can support hydrogen evolution without it.

Trace the four parts

A wet corrosion cell needs an anode, a cathode, an electron-conducting metallic path, and an ion-conducting electrolyte. Electrons travel through the metal from anode to cathode. Ions move in the electrolyte and maintain charge balance. Removing any part stops that cell. Paint can exclude electrolyte; electrical insulation can interrupt a connection between unlike metals.

These parts need not be separate objects. Surface films, grain structure, stress and local composition can create anodic and cathodic regions on one steel plate. Different oxygen supplies also create a concentration cell. Beneath a deposit, oxygen is consumed and poorly replaced; that oxygen-poor region becomes anodic to the exposed surface.

Balance an iron example

For iron in neutral aerated water, write the anode reaction as Fe→Fe2++2e−. Oxygen reduction consumes four electrons, so multiply the iron reaction by two. Adding and canceling electrons gives:

2Fe+O2+2H2O→2Fe2++4OH−.

Iron ions and hydroxide ions form iron(II) hydroxide. Further oxidation produces iron(III)-containing products; rust is a mixture of hydrated oxides and oxyhydroxides. Metal dissolves at the anode, but its solid products may collect elsewhere after ions move through the water. A thick rust deposit need not mark the deepest loss of metal.

For zinc in hydrochloric acid, the two-electron zinc oxidation already balances hydrogen evolution. The net reaction is Zn+2H+→Zn2++H2. Hydrogen bubbles are the visible cathodic product while zinc atoms enter solution.

Key Takeaways

  • Oxidation dissolves metal at the anode; reduction consumes electrons at the cathode.
  • A wet cell requires both a metallic electron path and an electrolyte ion path.
  • Balance electrons before adding half-reactions.
  • An oxygen-poor area can become anodic on a single metal surface.
  • Rust deposits can form away from the site of metal loss.

1.2 Use potentials to predict the reaction

Electrode potentials help identify which half-reaction supplies electrons and which accepts them. Keep the reference conditions attached to the numbers: a standard metal-ion half-cell and an alloy surface in seawater are different systems.

Read reduction potentials

Standard potentials are measured against the standard hydrogen electrode, assigned 0 V. At 25 °C, introductory tables use unit ion activity, commonly approximated by a 1 M solution. A more positive reduction potential means a stronger tendency for the reduction as written. In a connected metal couple under standard conditions, the more negative metal is oxidized.

Useful approximate values in volts are Mg −2.37, Al −1.66, Zn −0.76, Fe²⁺/Fe −0.44, Ni −0.25, Sn −0.14, Pb −0.13, H⁺/H₂ 0, Cu +0.34, Ag +0.80 and Au +1.50. The gold value refers to the Au³⁺/Au couple. Always retain the ion identity when a metal has several oxidation states.

Calculate the spontaneous cell voltage by subtracting the anode reduction potential from the cathode reduction potential:

ΔV∘=Vcathode∘−Vanode∘.

For iron and copper, iron is the anode and ΔV∘=0.34−(−0.44)=0.78 V. For zinc and copper it is 1.10 V. Doubling a half-reaction to balance electrons does not double its potential. Voltage is energy per charge, not the total energy of the reacting batch.

Allow for concentration

For a cell in which metal 1 is oxidized and metal 2 is reduced, both exchanging the same number of electrons, the 25 °C Nernst expression is:

ΔV=(V2∘−V1∘)−0.0592nlog⁡[M1n+][M2n+].

Use a base-10 logarithm. With Fe²⁺ at 0.10 M and Cu²⁺ at 0.0010 M, the ratio is 100. Its logarithm is 2 and the correction is 0.0592(2)/2=0.0592 V. The voltage falls from 0.78 V to about 0.72 V, remaining positive for iron oxidation. Reversing the concentration ratio changes the sign of the correction. At other temperatures replace 0.0592 V with 2.303RT/F using temperature in kelvin.

Choose the series for the environment

A galvanic series ranks actual metals and alloys by measured potential in a named environment. In seawater, magnesium and zinc are active; steel lies below copper alloys; passive stainless steels, titanium and noble metals lie toward the noble end. Stainless steel and nickel have separate active and passive positions because their surface films change their behavior.

Titanium illustrates why standard potentials alone are inadequate for service selection. Its Ti²⁺/Ti potential is about −1.63 V, yet its protective film places it near the noble end in seawater. Aluminum also has a negative standard potential but can corrode slowly under an intact oxide film. Potential difference indicates driving force; surface films, reaction rates and electrode areas determine how rapidly metal is lost. For an alloy joint, use a galvanic series for its service environment, then check those rate-controlling factors.

Key Takeaways

  • Use cathode minus anode reduction potential for the cell voltage.
  • Potentials stay unchanged when half-reactions are multiplied.
  • The Nernst correction depends on the reaction quotient and temperature.
  • Use an environment-specific galvanic series for alloys in service.
  • Potential difference predicts tendency, while kinetics and films govern rate.

1.3 Calculate metal loss and explain the corrosion rate

A voltage tells you whether a reaction is favored. A corrosion rate tells you how quickly a component loses material. Mass measurements, electric current and surface-film behavior connect these two questions to service life.

Convert mass loss to penetration

For a cleaned coupon, the average corrosion penetration rate is:

CPR=87.6WρAt.

Here mass loss W is in mg, density ρ in g/cm³, total exposed area A in cm², and time t in hours; the result is mm/yr. Include both faces and exposed edges. A 100 cm² steel coupon losing 250 mg in 720 h, at density 7.9 g/cm³, gives 87.6(250)/(7.9×100×720)=0.0385 mm/yr. A year contains 8,760 h for this conversion. In US industrial reports, 1 mil is 0.0254 mm, so this is about 1.5 mils per year.

An average penetration rate describes uniform thinning. A narrow pit can pass through a wall while producing little overall mass loss. Allowable rates therefore depend on the component's required life, thickness and failure mode; about 0.50 mm/yr is only a rough comparison value used for some applications.

Convert current to dissolved mass

Faraday's law relates charge to metal loss:

m=ItMnF,F=96 485 C/mol.

Use amperes and seconds. The molar-mass unit determines the mass unit of the result. For iron dissolving as Fe²⁺, n=2. A pipe area of 5,000 cm² at 2 µA/cm² carries I=0.010 A. Over 3.156×107 s, using 55.85 g/mol, the loss is about 91 g. For uniform iron corrosion, 1 µA/cm² corresponds to about 0.0116 mm/yr. Current density, not total current alone, describes the intensity of loss over an exposed surface.

Find what limits the reactions

Polarization is the potential shift from equilibrium when a net current flows. The shift is the overvoltage, η. Activation polarization reflects a slow reaction step and can follow η=±βlog⁡(i/i0). Concentration polarization reflects limited delivery of reactant, such as oxygen. The limiting current density rises when flow brings oxygen to the surface faster.

At the freely corroding mixed potential, total anodic and cathodic currents balance. On potential–log-current-density axes, their intersection gives the corrosion potential and corrosion current density. Faster oxygen reduction increases corrosion of actively dissolving steel. If the potential moves the metal into a passive region, the response can instead be a low corrosion current.

Recognize the passive region

Passivity comes from a thin, adherent oxide film. Aluminum, titanium and chromium-containing alloys benefit from it. Stainless steel contains at least about 10.5% chromium by mass and forms a chromium-rich film only a few nanometers thick. Its anodic current rises during active dissolution, falls on passivation, stays low in the passive range, and rises again in the transpassive region.

Chlorides can break a passive film locally. Stagnant, oxygen-poor gaps can hinder its repair. Temperature and flow also matter: flow can deliver reactants or strip films. Stainless steel must therefore be matched to the water chemistry and geometry; its low passive current is not a guarantee against local attack.

Key Takeaways

  • The 87.6 penetration-rate constant requires mg, g/cm³, cm² and hours.
  • Faraday calculations use charge in coulombs and the correct electron count.
  • Mass-loss penetration rates average over the exposed area.
  • The mixed-potential current balance determines the freely corroding rate.
  • Activation and reactant transport can each limit current.
  • A passive film lowers current but can fail locally.

1.4 Judge oxide scales and their growth

An oxide scale protects hot metal in dry gas if it stays attached and restricts further reaction.

Compare oxide and metal volumes

Metal oxidation supplies electrons for oxygen reduction. A compact scale restricts ion and electron transport; porous scale admits gas. An interface reaction can also control the rate.

The Pilling–Bedworth ratio compares the volume of oxide formed with the volume of metal consumed. For an oxide of formula MaOb:

P ⁣– ⁣B=AOρMaAMρO.

Here AO is oxide formula mass, AM metal atomic mass, and ρM,ρO their densities; a counts metal atoms in the oxide formula, so Al₂O₃ has a=2.

Magnesium gives 40.30(1.74)/(24.31×3.58)=0.81. Aluminum gives 101.96(2.70)/(2×26.98×3.97)=1.29. Below one, too little oxide volume tends to leave gaps. Between about one and two, a compact protective layer is possible. Well above two, large compressive stress promotes cracking and flaking, called spalling; tungsten has a ratio near 3.4.

A protective scale also needs adhesion, slow transport, a high melting point and low vapor pressure. Thermal-expansion mismatch can crack it on cooling. Molybdenum oxide evaporates at high temperature and gives no lasting barrier.

Recognize three growth laws

Let W be mass gain per unit area and t time.

Growth lawEquationPhysical interpretation
LinearW=K3tConstant rate, possible with porous scale, repeated spalling or interface-reaction control
ParabolicW2=K1t+K2Growth slows as transport through a thickening compact scale becomes harder
LogarithmicW=K4log⁡(K5t+K6)Very thin films, often at relatively low temperatures

The constants apply to the specified temperature and units. Under W2=K1t, a gain of 2.0 mg/cm² at 100 h gives K1=0.040 (mg/cm2)2/h. At 400 h, the gain is 0.040(400)=4.0 mg/cm2. Four times the exposure doubles the gain. Linear growth through the first measurement would instead give 8.0 mg/cm².

Interpret mass gain correctly

Mass gain is added oxygen; oxide stoichiometry gives the metal consumed. Chromium, aluminum and silicon additions form slowly growing Cr₂O₃, Al₂O₃ and SiO₂ scales in heat-resistant steels and nickel-based superalloys.

Key Takeaways

  • The Pilling–Bedworth ratio compares oxide volume with consumed metal volume.
  • A ratio near one to two permits protection but does not establish it.
  • Parabolic growth slows as the compact scale thickens.
  • Linear kinetics can result from porous scale or interface-reaction control.
  • Oxidation mass gain measures oxygen uptake.
2

Identify forms of corrosion and choose ways to prevent them

The location and shape of damage help identify the conditions that caused it. Broad thinning, deep pits, attacked grain boundaries and delayed cracks each point toward a different combination of material, environment and stress. Choosing a remedy starts with that mechanism. Material selection, drainage, controlled water chemistry, coatings and electrochemical protection can then be combined to provide the required service life.

2.1 Identify thinning, galvanic attack, crevices and pits

The shape and location of corrosion damage are clues to its mechanism. Start with the service environment and the geometry of the damaged part, then connect them to the electrochemical cell.

Distinguish widespread and coupled attack

Uniform corrosion thins most of the exposed surface at a similar rate. Bare steel rusting over a broad area is a common example. Its predictable average loss allows inspection, planned replacement and added thickness.

Galvanic corrosion requires unlike potentials, electrical contact and a shared electrolyte. The more active metal becomes the anode and corrodes faster; the more noble surface supports cathodic reactions. A steel fastener in a copper plate is therefore vulnerable in seawater.

Area matters. If cathodic reactant supply controls the total current, a large cathode collects current that must be supplied by the anode. Delivering it through a tiny anode creates high anodic current density. An exposed steel rivet of 1 cm² in 100 cm² of copper has roughly 100 times the anodic current density of an equal-area arrangement under that model. A copper rivet in a broad steel plate spreads the anodic loss over a much larger steel area.

Choose nearby metals in the service galvanic series or insulate them with sleeves, washers and gaskets. If coating only one of the coupled metals, coat the cathode. Coating the anode alone can turn a scratch into a tiny exposed anode beside a large bare cathode. Coating both also reduces the exposed cell area.

Trace a crevice cell

Crevice corrosion occurs under gaskets, deposits or lap joints where liquid enters but is poorly exchanged. Oxygen inside is depleted; the exposed surface remains oxygenated. The gap becomes anodic. Dissolved metal ions accumulate, chloride enters to maintain charge balance, and hydrolysis acidifies the trapped liquid. These changes accelerate dissolution inside the gap.

Continuous welds, sealed joints, nonabsorbent gaskets, clean surfaces and complete drainage remove the geometry or retained liquid that sustains the cell. Replacing a grade without addressing an avoidable water trap can leave the cause in place.

Recognize pits and compare stainless steels

Pitting starts at a local breakdown of a passive film, often in chloride-containing water. Once established, a pit develops an acidic, chloride-rich interior much like a crevice. A small opening can hide deep penetration under corrosion products. Low coupon mass loss can therefore accompany a perforated wall.

For stainless steels, a common comparative composition index is:

PREN=%Cr+3.3%Mo+16%N.

Use mass percentages and the same nitrogen coefficient for all comparisons. Typical compositions give 18.8 for 304, about 26 for 316 and about 35 for duplex 2205. Molybdenum and nitrogen raise this index. Higher PREN indicates better relative pitting resistance within the comparison, but does not specify a safe temperature or guarantee seawater suitability. Type 316 can still pit or suffer crevice attack in seawater. Check the actual grade, chloride level, temperature, flow and joint design before selecting it.

Key Takeaways

  • Galvanic attack needs electrical contact and a shared electrolyte.
  • A small active anode next to a large cathode is a severe geometry.
  • Stagnant crevices become oxygen-poor, acidic anodic regions.
  • Pits can penetrate deeply with very little total mass loss.
  • PREN compares stainless compositions; service suitability needs further checks.
  • Coat the cathode or both metals of a galvanic couple.

2.2 Diagnose attack along grains, in flow and under stress

A component can lose strength without broad visible thinning. Grain-boundary chemistry, selective dissolution, moving liquid and tensile stress each produce characteristic damage and call for different remedies.

Examine boundaries and alloy constituents

Intergranular corrosion follows grain boundaries. In sensitized austenitic stainless steel, exposure around 500–800 °C allows chromium carbides to form there. Nearby metal loses chromium and may no longer remain passive. A band beside a weld can suffer this weld decay. Solution treatment around 1000–1100 °C followed by rapid cooling redissolves carbides. Low-carbon 304L or 316L, at most 0.03% carbon, limits carbide formation; titanium-stabilized 321 and niobium-stabilized 347 tie up carbon with other carbide-forming elements.

Selective leaching removes one alloy constituent. Dezincification removes zinc from susceptible brass and leaves a weak, porous, copper-rich red surface. Lower-zinc or dezincification-resistant brass reduces the risk. In gray cast iron, graphitic corrosion removes iron and leaves a graphite network. The pipe can retain its shape while losing most of its strength.

Look at the flow pattern

Erosion–corrosion combines chemical attack with mechanical film removal. Grooves and rounded channels aligned with flow often appear at elbows, tees, valves and impellers. Turbulence, solids and bubbles aggravate it. Lower velocity, smooth changes of direction, larger-radius bends and resistant materials address the mechanism. Cavitation adds damage from collapsing vapor bubbles near the surface.

Connect cracking to environment and stress
MechanismConditions and cluesUseful controls
Stress corrosion cracking (SCC)Tensile stress plus an alloy-specific environment; cracks with little thinningReduce tensile stress, remove the species, or select a resistant alloy
Hydrogen embrittlementAtomic hydrogen enters a susceptible metal; delayed brittle cracking under tensionControl hydrogen entry, use suitable heat treatment, and apply a specified post-plating bake

SCC can occur below yield stress. Welding or cold working can leave enough residual tension. Brass is susceptible in ammonia-containing environments, austenitic stainless steel in warm chlorides, and carbon steel in hot concentrated caustic solutions. Stress-relief heat treatment lowers residual tension; shot peening places the surface in compression.

Hydrogen can enter during acid pickling, electroplating, welding with moisture, sulfide exposure or excessive cathodic protection. High-strength martensitic steel is particularly sensitive. Baking near 200 °C soon after plating can drive out diffusible hydrogen; the required schedule depends on the part and process.

Use the history to choose the remedy

A cold-worked brass fitting cracking in an ammonia-containing building points to SCC. A gray cast iron main that keeps its shape but cuts easily points to graphitic corrosion. A hardened bolt snapping hours after electroplating points to hydrogen embrittlement. Similar-looking cracks do not justify identical treatments: cathodic protection can suppress SCC in some systems, while excessive polarization can introduce hydrogen into high-strength steel.

Key Takeaways

  • Sensitization depletes chromium beside grain-boundary carbides.
  • Selective leaching can leave a weak part that keeps its shape.
  • Flow-aligned damage suggests erosion–corrosion.
  • SCC needs a susceptible alloy, tensile stress and a matching environment.
  • Atomic hydrogen can cause delayed cracking in high-strength steel.
  • Process and exposure history help distinguish cracking mechanisms.
  • Cathodic overprotection can worsen hydrogen damage.

2.3 Choose material, environment and design controls

Corrosion resistance belongs to a material in an environment. Choosing an alloy, changing a liquid and removing a water trap can all be effective, but they address different causes of damage.

Match the material to the service

Stainless steels generally resist nitric acid well but can be attacked rapidly by hydrochloric acid. Aluminum performs well in neutral water yet dissolves in strong alkalis. Titanium and copper–nickel alloys are useful candidates for seawater equipment; plastics and fiber-reinforced plastics can suit acids that attack metals. Among stainless steels, 316 often improves chloride resistance over 304, but detailed service checks still matter.

Weathering steel forms an adherent rust layer during outdoor wet–dry cycles. Small alloy additions, including copper, chromium and nickel, support that layer. Constant dampness or accumulated chloride prevents it from giving the same benefit. A sheltered pocket that stays wet can therefore undermine a design that performs well on freely draining exposed faces.

Change the reaction conditions

Lower temperature usually slows corrosion. Reducing excessive fluid velocity limits film removal. Deaeration and oxygen scavengers reduce oxygen available for cathodic reduction in boiler water. Raising water pH can reduce steel corrosion in a suitable operating range.

An inhibitor is added at a small controlled concentration to lower the rate. Organic film-formers adsorb on metal; passivating inhibitors such as nitrites or molybdates promote protective films; scavengers remove oxygen. These methods fit contained, recirculating fluids where concentration can be maintained. Dosing open seawater around an entire ship hull is impractical.

Passivating inhibitors require adequate concentration. An incomplete film may leave a few active spots surrounded by a large passive surface, concentrating anodic current and accelerating pitting. Establish and monitor the required dose. Historical chromate inhibitors contain toxic hexavalent chromium and are restricted in many uses; inhibitor selection includes compatibility and exposure controls.

Remove the geometry that sustains attack

Design joints to exclude or release liquid. Prefer sealed or continuous welded joints where suitable, avoid absorbent gaskets, and make tanks drain completely. Keep dissimilar metals electrically isolated. Avoid tiny active fasteners in large noble surfaces, sharp flow changes, stress concentrations and unnecessary residual tension.

Provide room for inspection, cleaning and recoating. A surface that cannot be reached may be cheap to build but expensive to maintain. Replaceable wear or corrosion parts can keep the main structure in service.

Add thickness for predictable uniform loss

A corrosion allowance is added to the structural or pressure-required thickness:

a=(uniform penetration rate)(design life).

At 0.10 mm/yr for 25 years, add 2.5 mm to the thickness needed to carry the load. This calculation assumes uniform loss continues at the adopted rate. Extra thickness does not remove an SCC mechanism or reliably control deep pits. Choose a separate treatment for local or cracking damage. The final choice compares material, design and protection together over the required life: painted steel with cathodic protection may be more economical than a much more resistant alloy.

Key Takeaways

  • Select a material–environment pair, including temperature and exposure conditions.
  • Weathering steel needs wet–dry cycles and performs poorly with persistent dampness or high chlorides.
  • Contained systems allow inhibitor concentration to be controlled.
  • Drainage, electrical isolation and inspection access are design controls.
  • A corrosion allowance covers expected uniform loss.

2.4 Combine coatings and electrochemical protection

A coating reduces contact with the environment. Electrochemical protection changes which reaction the structure supports. Using both can reduce current demand while protecting exposed metal at coating defects.

Separate barrier and metallic coatings

Paints, lacquers and polymer linings act mainly as barriers. Surface cleaning and preparation, often grit blasting, give adhesion; edges and scratches are common starting points for underfilm corrosion. Primers may add inhibiting pigments or zinc dust.

Coating on steelBehavior at a wet scratch
Zinc, more active than steelZinc supplies electrons and is consumed; exposed steel is cathodic
Tin, nickel or chromium, more noble than steelExposed steel becomes a small anode beside a large coated cathode

Hot-dip galvanizing applies zinc near 450 °C. Vitreous enamel fuses a glass layer onto steel. Anodizing thickens aluminum's oxide electrochemically, and phosphate conversion coatings help paint adhere. Their protection mechanisms and damage response differ, so the coating name alone is insufficient.

Supply electrons to the structure

Cathodic protection suppresses metal oxidation by making the structure cathodic. Sacrificial anodes of magnesium, zinc or aluminum alloy corrode to supply electrons. Magnesium gives a large driving voltage useful in high-resistivity soil; zinc and aluminum alloys are widely used in seawater. The anodes need electrical connection and an electrolyte path and must be replaced as they are consumed.

Impressed-current protection uses a DC source. Its negative terminal connects to the structure and its positive terminal to inert or slowly consumed auxiliary anodes in the electrolyte. Adjustable current suits large structures. Reversing the terminals would drive oxidation of the structure.

For a 0.20 A demand lasting one year, ideal magnesium consumption is:

m=0.20(3.156×107)(24.31)2(96 485)≈795 g.

At about 50% current efficiency, approximately 1.6 kg is consumed. Add the planned service-life and utilization margins separately; theoretical mass is not the installed anode size.

Interpret protection and access

A widely used buried or submerged steel criterion is −0.85 V or more negative against a saturated copper/copper-sulfate reference electrode, with protective current applied. Voltage drops outside the steel–electrolyte boundary must be considered. A negative reading containing substantial soil voltage drop does not by itself establish the interface potential.

Driving the potential too negative wastes current, can lift coatings and can introduce hydrogen into high-strength steel. Shielded regions may receive too little current, and surfaces above the electrolyte are not protected. Stray current can attack nearby metal where it leaves that metal.

Anodic protection uses a controller to hold a suitable active–passive metal within its passive potential range, for example in some sulfuric-acid equipment. This is a different operating principle from making the structure cathodic.

Key Takeaways

  • Barrier coatings depend on adhesion and continuity.
  • Zinc protects exposed steel sacrificially; a damaged noble coating can accelerate steel loss.
  • Sacrificial and impressed-current systems both supply electrons to the protected structure.
  • Connect the structure to the negative terminal in impressed-current protection.
  • Correct reference-electrode readings for relevant external voltage drops.
  • Coating defects and shielded regions require different current-access checks.
3

Explain how polymers and ceramics degrade

Polymers and ceramics deteriorate through mechanisms tied to their structures. Liquids can enter polymer chains, while light, heat and reactive chemicals can change the chains themselves. Stress can turn a tolerable exposure into a cracking problem. Ceramics usually resist chemical attack well, yet particular liquids and high-temperature environments can dissolve them. Each case calls for a matching material or environmental control.

3.1 Explain why liquids soften or crack polymers

A polymer can deteriorate without a corrosion cell. Liquids may enter between its chains, dissolve them, or assist cracking under stress. The result depends on both the polymer structure and the contacting liquid.

Follow solvent molecules into the material

During swelling, small liquid molecules diffuse between polymer chains and push them apart. The part grows, softens and loses stiffness and strength. Its glass transition temperature falls as chain movement becomes easier. Dissolution goes further: separate chains disperse into a suitable solvent.

Linear and branched thermoplastics can dissolve. A cross-linked network cannot disperse into individual chains without breaking network bonds, so a thermoset or vulcanized rubber can swell while remaining connected. A change in dimensions is therefore possible even when a material does not dissolve.

Match chemical structure and exposure

“Like dissolves like” is a useful screening guide: similar chemical structure and polarity favor liquid uptake or dissolution. Hydrocarbon rubbers swell strongly in hydrocarbon fuels and mineral oils. Nitrile rubber is often used for fuel hoses and seals because its acrylonitrile-containing structure gives better resistance to those liquids.

Higher crystallinity limits accessible regions for liquid molecules. More cross-linking restricts swelling, and higher molecular weight and lower temperature generally improve resistance within a polymer–solvent comparison. These factors guide a choice, but compatibility data at service conditions decide whether the dimensional change is acceptable.

Polystyrene foam in acetone shrinks dramatically as the solid polymer dissolves and its cellular structure collapses. Vulcanized rubber in a suitable solvent can grow substantially while retaining its network. It may partly recover after the solvent leaves; the swelling during use can still destroy a seal's fit.

Account for moisture conditioning

Polar polyamides, including nylon, absorb water. At saturation, uptake can reach several percent by mass. Water acts as a plasticizer, lowering stiffness and strength while often increasing toughness. A nylon gear tested dry can therefore behave differently after prolonged humid service. Select dimensions and properties for the expected moisture condition, including dimensional tolerances as well as strength.

Recognize environmental stress cracking

Environmental stress cracking (ESC) combines stress with a liquid that may cause little damage to an unstressed specimen. Stressed polyethylene can crack in some detergent solutions. Polycarbonate and acrylic parts can craze or crack in contact with particular oils or solvents. Residual molding stresses count as stress even if the external load is small.

Reduce stress concentrations and residual stress, exclude the liquid, or choose a more resistant grade. Higher-molecular-weight polyethylene can improve ESC resistance. The mechanism resembles metal SCC in its need for stress and a matching environment, but it is not an electrochemical metal-dissolution cell. Cathodic protection does not prevent swelling or ESC. For a plastic container, identify the liquid, concentration, temperature and loading before accepting a chemical-resistance rating.

Key Takeaways

  • Swelling absorbs liquid between chains; dissolution disperses chains into the liquid.
  • Cross-linked networks swell but need bond breaking before they can dissolve.
  • Chemical similarity, crystallinity and temperature affect liquid uptake.
  • Moisture-conditioned nylon properties can differ greatly from dry values.
  • ESC depends on the combination of stress and a particular liquid.

3.2 Explain weathering, bond damage and ceramic attack

Polymer degradation can change the chains themselves. Light, oxygen, water and heat may shorten chains or add cross-links, while ceramics and glass can suffer chemical attack despite their generally strong resistance.

Identify the molecular change

Chain scission breaks backbone bonds and lowers molecular weight. Strength and toughness often fall, and the material may discolor or become brittle. Extra cross-linking can also cause embrittlement by restricting chain movement. Similar surface symptoms can therefore arise from different molecular changes.

A photon's energy increases as wavelength decreases:

Emol=hcNAλ.

At 300 nm the energy is about 399 kJ/mol, compared with roughly 350 kJ/mol for a typical carbon–carbon single bond. At 600 nm it is about 199 kJ/mol. Absorption by the polymer or impurities is necessary for photochemical damage; a photon-energy comparison explains why ultraviolet light is particularly important, but energy alone does not specify a weathering rate.

Connect the chemical agent to the bond

Ozone attacks backbone double bonds in natural rubber and styrene–butadiene rubber. On a stretched part, characteristic cracks run across the stretch direction. Saturated-backbone rubbers such as EPDM and silicone resist this attack.

Hydrolysis uses water to break susceptible bonds, including ester links in PET and PLA and amide links in polyamides. Heat, acids and bases accelerate it. Drying PET before melt processing limits hydrolysis in the hot melt. Thermal degradation can also break chains and release gases; PMMA can depolymerize toward monomer, while overheated PVC releases hydrogen chloride. Strong carbon–fluorine bonds and aromatic backbone structures help PTFE, polyimides and PEEK tolerate higher service temperatures. Thermosets char instead of melting for reuse.

Slow outdoor weathering

Weathering combines ultraviolet light, oxygen, moisture, temperature cycling and pollutants. Yellowing, chalking, loss of gloss and surface cracks are useful clues. Carbon black and UV absorbers reduce light reaching vulnerable bonds. Hindered amine light stabilizers (HALS) capture reactive radicals. Antioxidants slow oxidation during processing and service; an opaque coating can shield the surface.

Biodegradation also needs the appropriate environment. PLA generally needs the heat and moisture of industrial composting for useful breakdown rates. A “biodegradable” label gives no service-life estimate in seawater or cool soil.

Check ceramics and glass against their chemicals

Strong ionic and covalent bonding gives many ceramics good chemical resistance. At high temperature, molten slag or glass can dissolve refractory linings. Silicate glass is attacked by hydrofluoric acid and by hot strong alkaline solutions. Water at a loaded glass crack tip can assist slow crack growth, so failure may occur long after loading without any increase in applied force.

Select a ceramic or polymer for the actual agent and temperature. UV stabilizers address light-driven polymer reactions; they do not stop a solvent from swelling a seal or a molten slag from dissolving a refractory.

Key Takeaways

  • Chain scission lowers molecular weight; added cross-links can also embrittle polymers.
  • Shorter-wavelength photons carry more energy.
  • Ozone attacks susceptible double bonds, while hydrolysis attacks ester and amide links.
  • UV screens, HALS and antioxidants act on different parts of weathering.
  • Biodegradation depends on the disposal environment.
  • Ceramics can dissolve chemically, and moisture can assist loaded glass cracks.
4

Select materials using property charts and performance indices

A design brief becomes a materials decision when its job, limits and priorities are made explicit. Screening removes candidates that fail a requirement; ranking compares the survivors on equal performance. Deriving an index shows how material properties and the dimensions you may change work together. Logarithmic charts make that ranking visible, and grade-specific evidence turns a promising family into a practical shortlist.

4.1 Turn a design brief into a selection problem

A useful materials decision begins with the job the part must do. Separate requirements that every candidate must meet from the quantity you want to improve, then compare materials on that common basis.

Translate the brief

Record four statements:

StatementQuestionExample for a lightweight tie
FunctionWhat does the part do?Carry an axial tensile load
ConstraintsWhat must it achieve?Fixed length, limited extension, outdoor resistance
ObjectiveWhat should be minimized or maximized?Minimize mass
Free variablesWhat may change?Material and cross-sectional area

A required stiffness expresses the extension limit. A maximum permitted mass is a constraint, while “as light as possible” is an objective. A brief may contain several constraints even when ranking uses one objective. If mass and cost both matter, their conflict needs a trade-off decision.

Free variables determine which performance equation applies. If area can change, a lower-modulus material can compensate with a larger section. If the entire geometry is fixed, that compensation is unavailable. Write dimensional limits explicitly before choosing an index.

Screen with pass/fail requirements

Screening rejects materials that fail any constraint. A service temperature of 120 °C requires adequate properties at that temperature, not just a room-temperature melting point. A toughness requirement of 15 MPa·m^1/2 removes materials below that limit. Chemical resistance, electrical insulation and available processing routes can also serve as screening attributes.

A candidate that performs exceptionally well on one property cannot make up for failing a mandatory limit. Check all limits before spending effort on a detailed ranking. A chemically incompatible polymer remains unsuitable even if its low density is attractive.

Rank the survivors

Ranking compares feasible materials by a derived combination of properties, a performance index. For a light stiff tie with free area, the index is E/ρ. It rewards stiffness while penalizing density and arises from meeting the same required stiffness for every candidate. It does not simply choose the highest modulus.

Separating the objective into fixed functional and geometric factors and a material factor can make one index useful across a whole class of designs. The derivation states which loads, dimensions and failure limits are held fixed. Change those conditions and the ranking can change.

Document the short list

The leading candidate still needs grade-specific evidence. Check availability, supplied shapes, manufacturing, joining, corrosion under the actual exposure, damage resistance and experience in similar products. Family-level chart bubbles span ranges; a heat treatment or fiber direction can move the relevant properties substantially.

For the tie, an aluminum alloy might pass the outdoor-resistance screen and have competitive specific stiffness. Documentation must still establish a suitable grade, joint details, section size and fabrication route. A shortlist is the start of that detailed engineering decision, not a complete component design.

Key Takeaways

  • Translation separates function, constraints, objective and free variables.
  • A constraint is mandatory; an objective ranks feasible choices.
  • Screen all mandatory limits before ranking.
  • A performance index depends on loading and available geometric changes.
  • Document grade, processing, joining and service behavior for the short list.

4.2 Derive an index from the objective and constraint

A performance index follows from a physical model. Write the quantity to minimize, use the active constraint to eliminate a free dimension, and collect the material properties that remain.

Derive a light stiff tie

For length L, area A and density ρ, mass is m=ALρ. Axial stiffness is S=EA/L. At the minimum area that meets the stiffness requirement, A=SL/E. Substitution gives:

m=SL2ρE.

With length and required stiffness fixed, minimize ρ/E or maximize M=E/ρ. This is specific stiffness. A strong tie instead requires A=F/σf, producing m=FLρ/σf and the index σf/ρ. For a ductile metal, failure strength in this model normally means the allowable yield-based strength.

Derive a light stiff beam

A square beam has I=b4/12=A2/12. Its bending stiffness is S=C1EI/L3, where the support and loading determine C1; a simply supported beam with a central load has C1=48. Solving for area gives:

A=(12SL3C1E)1/2.

Then m=(12S/C1)1/2L5/2ρ/E1/2. The material index is E1/2/ρ. Modulus enters with a smaller exponent because increasing section size improves the second moment of area strongly.

Compare the appropriate models
Minimum-mass functionIndex to maximize
Stiff tie, area freeE/ρ
Strong tie, area freeσf/ρ
Stiff beam, similar section shape and size freeE1/2/ρ
Strong beam, similar section shape and size freeσf2/3/ρ
Stiff panel, length and width fixed, thickness freeE1/3/ρ
Strong panel under the same geometric freedomσf1/2/ρ
Strong solid shaft, diameter freeτf2/3/ρ

If beam depth is fixed and only width changes, I is proportional to width and the stiffness index becomes E/ρ. The name “beam” alone does not determine the exponent.

Read a ranking as a mass comparison

Using GPa and Mg/m³ consistently, steel with 210 and 7.85 has specific stiffness 26.8; aluminum with 70 and 2.70 has 25.9. They are close for stiff ties. For a 2.0 m tie needing stiffness 5.0×107 N/m, A=SL/E gives 476 mm² of steel or 1429 mm² of aluminum. Multiplying area by length and density gives 7.48 kg and 7.71 kg. The aluminum tie needs more area, so its lower density does not give a mass saving here. Their stiff-beam indices are 1.85 and 3.10, so the aluminum mass for equal bending stiffness is 1.85/3.10=0.60 of the steel mass.

For CFRP at 60 GPa and 1.55 Mg/m³, the beam index is 5.00; spruce along the grain at 10 GPa and 0.45 Mg/m³ gives 7.03. Low density is rewarded strongly, but the required section may be much larger. Screen size, directionality, strength, buckling and damage separately. Use one unit system across all candidates.

Key Takeaways

  • Eliminate the free geometric variable using the binding constraint.
  • Light stiff ties maximize specific stiffness.
  • Light stiff beams with scalable similar sections maximize the square-root modulus index.
  • Panel and shaft indices have their own geometry-dependent exponents.
  • For a shared model, equal-function mass is inversely proportional to the index.
  • Fixed depth can change the beam index.

4.3 Read and use logarithmic property charts

Property charts compare material ranges; constant-index lines rank them under a shared design model.

Read the axes and bubbles

An Ashby chart commonly plots modulus vertically against density horizontally. Each step between decade marks multiplies the value by ten. The halfway position between 10 and 100 GPa is 10×100=31.6 GPa, not 55 GPa.

Material classes occupy envelopes, and individual grade ranges appear as bubbles. Metals typically occupy relatively high stiffness and density; engineering polymers are mostly around 0.2–5 GPa and 1–2 Mg/m³. Elastomers can be near 0.001–0.1 GPa. Foams are light and compliant; woods and composites have strong directional and processing effects. A bubble represents a range, not an exact design value.

Convert an index into a line

Let the mass index be M=Ea/ρ. Rearranging yields log⁡E=(1/a)log⁡ρ+(1/a)log⁡M. Therefore:

IndexSlope on modulus–density log axes
E/ρ1
E1/2/ρ2
E1/3/ρ3

These slopes require modulus vertically and density horizontally. On strength–density axes, the corresponding slopes are 1 for σf/ρ, 1.5 for σf2/3/ρ and 2 for σf1/2/ρ.

Points on one line have equal index. Move it parallel upward or toward lower density to seek better performance; materials above it have a higher index.

Combine screens with ranking

First apply the mandatory property limits. A stiffness screen of E>50 GPa excludes ordinary magnesium alloys near 45 GPa, woods and unreinforced polymers. Steel, aluminum alloys, suitable CFRP and many ceramics remain. A toughness screen may then eliminate brittle ceramics; environmental resistance further narrows the set.

For a stiff-beam comparison, a slope-2 line through steel has index 1.85 in GPa and Mg/m³ units. At aluminum's density of 2.70 Mg/m³, the equal-performance line requires E=(1.85×2.70)2≈25 GPa. Aluminum's 70 GPa is above it, explaining its better mass performance for this beam model.

Finish with actual grade data

Other charts compare strength, toughness, cost per volume and embodied energy. Add chemical-resistance screens, then verify the shortlisted grade, heat treatment, fiber orientation and temperature.

Key Takeaways

  • Log-axis midpoints are geometric means.
  • A bubble shows a property range.
  • The index exponent determines the selection-line slope.
  • Screen mandatory limits and then move a parallel ranking line toward higher index.
  • Chart candidates still need grade-specific documentation.
5

Weigh cost, life cycle and recycling in material choices

Mass, purchase price and environmental impact describe different parts of a material choice. An equal-function comparison reveals how much material and processing each design needs. Life-cycle cost adds the timing of maintenance and replacement, while an eco-audit tracks where energy or emissions arise. Recovery at end of life depends on clean material streams and separable products, so durability and recycling belong in the original design decision.

5.1 Compare the cost of doing the same job

Compare the material quantity and processing needed for the same function, not price per kilogram alone.

Replace mass with material cost

If Cm is price per kilogram, material cost is C=mCm. In a minimum-mass derivation, replacing density by Cmρ gives the corresponding material-cost index:

FunctionIndex for minimum material cost
Stiff tieE/(Cmρ)
Stiff beam with similar scalable sectionsE1/2/(Cmρ)
Strong solid shaftτf2/3/(Cmρ)

These indices rank raw material cost under the original loading and geometry assumptions.

Using illustrative relative prices per kilogram of steel 1, aluminum 3.5, CFRP 50 and spruce 1.5, their stiff-beam cost indices are about 1.85, 0.88, 0.10 and 4.7. Steel beats aluminum and CFRP on raw material cost, even though those candidates can make lighter beams. Spruce's high index is useful only if its required size, directionality and environmental resistance pass the design screens.

Identify a real trade-off

For parts providing the same function, plot cost against mass. A candidate is dominated if another feasible candidate is no heavier and no more expensive, with an improvement in at least one. The Pareto front contains choices for which improving mass requires accepting higher cost, or improving cost requires accepting higher mass.

Choose a point using the product’s value for mass saving: a launch vehicle can justify a greater cost per kilogram saved than a stationary support.

Add manufacturing and batch costs

Component cost includes material, processing, energy, labor, tooling, joining, finishing and quality checks. Machining a titanium part from a large billet may discard much of an expensive input. A suitable near-net-shape route can reduce scrap and machining time.

Tooling is spread across production quantity. A mold costing 50,000 cost units adds 5 per part over 10,000 parts, but only 0.05 over 1,000,000 parts. Fixed tooling and variable costs together determine when molding becomes cheaper than machining.

Simplifying geometry and reducing joints can lower cost without changing material. A corrosion-resistant alloy may remove painting and finishing steps, offsetting a higher purchase price. Treat chart prices as estimates and obtain current supplier and process data before committing to production.

Key Takeaways

  • Compare cost per function using the mass actually required.
  • Material-cost indices replace density with price per kilogram times density.
  • Pareto choices trade mass against cost without being dominated.
  • Processing, tooling, joining and finishing contribute to component cost.
  • Divide fixed tooling cost by the production quantity.

5.2 Compare costs over the service life

Life-cycle cost compares acquisition, maintenance and end of life, including when each payment occurs.

Set the comparison period and boundary

Life-cycle cost (LCC) includes material, fabrication and installation; operation, inspection, maintenance and downtime; and removal or disposal minus residual scrap value. Compare designs that deliver the same function for the same service period. Lost production can cost more than the repair itself.

A 40-year handrail example uses neutral cost units. Painted carbon steel costs 1,000 initially and 400 to repaint in years 8, 16, 24 and 32. Undiscounted cost is 1000+4(400)=2600. A 316 stainless handrail costs 2,200 initially with negligible maintenance in this example. Stainless saves 400 before discounting.

Bring future payments to the present

Discount a cost C paid at the end of year t using annual discount rate r:

PV=C(1+r)t.

Enter 3% as 0.03. Discount each payment for its own year, then add the present values to the initial cost. For the handrail at 3%, the four repaintings total about 917 in present value, so painted steel costs about 1,917. At 5%, its total is about 1,662. Both are below the stainless initial cost in this simplified comparison.

A higher rate lowers distant payments’ present value. Divide by the growth factor; multiplying finds a future equivalent. Initial payments are not discounted.

Test what could change the choice

Maintenance intervals, service life, access cost and downtime can reverse the ranking. Repainting on an easily reached indoor handrail differs from repainting above operating equipment. Include scaffolding or closure costs when they apply, and count a higher scrap value as an end-of-life benefit at its actual date.

A long life can justify durable materials, but a component replaced in a few years for other reasons may gain little from 50-year corrosion resistance. Where failure could harm people or cause a serious release, the design first needs acceptable reliability; a low calculated LCC cannot make an unacceptable failure risk satisfactory.

Corrosion costs are substantial at system level. The 2016 NACE IMPACT study estimated about 2.5 trillion US dollars annually, based on roughly 3.4% of world GDP in 2013, and estimated that existing corrosion-control practices could save 15–35%.

Key Takeaways

  • Compare equal functions over a shared service period.
  • Include downtime, access and end-of-life value where relevant.
  • Discount each future payment by its own date.
  • Higher discount rates reduce the present weight of distant maintenance.
  • Reliability requirements remain constraints on a cost choice.

5.3 Compare environmental burden per useful function

Compare equal-function designs through production, use and end of life: lower mass can require more production energy.

Follow the materials cycle

The cycle runs from extraction through refining or synthesis, material processing, manufacture and use to reuse, remanufacturing, recycling, energy recovery or disposal. Use can require energy, maintenance and replacement. Recycling returns material to processing; reuse preserves the component.

Embodied energy measures energy used to produce material from resources, usually per kilogram. A carbon footprint measures greenhouse-gas emissions as carbon dioxide equivalent. They are related but different quantities: energy sources can have different emissions per unit of energy. Compare candidates using one consistent data source and boundary.

Multiply by the mass needed

Illustrative values are 25 MJ/kg for primary steel, within a common 20–30 range, and 186 MJ/kg for primary aluminum versus 8.3 MJ/kg for remelted scrap aluminum in the cited 2019 industry data. A 10 kg steel beam embodies 250 MJ. An equal-stiffness aluminum beam of 6 kg embodies 1,116 MJ from primary metal, about 870 MJ more, or about 50 MJ using the recycled-metal value.

The correct denominator is a functional unit: a part delivering the same required stiffness and service life. Comparing 1 kg of each material ignores the different quantity required to provide the function. Check that both designs also meet strength, space and durability requirements.

Find the dominant phase

An eco-audit estimates energy or carbon in material production, manufacture, transport, use and end of life. Energy-consuming products often have a large use-phase burden. In such a case a mass saving can repay higher embodied energy through lower operating energy. A stationary beam has no comparable vehicle propulsion saving; its material production and replacement frequency can dominate instead.

For the primary-aluminum beam, lifetime use savings must exceed about 870 MJ just to repay the material-energy difference. Compare that saving with any extra manufacturing or maintenance burden before concluding that the total is lower.

Include durability and recovery

Longer service life spreads production burdens over more years and avoids replacement. Protection also uses resources: sacrificial anodes are consumed and coatings require manufacture and maintenance. A low-mass product that fails early may require several replacements to perform the same lifetime function.

Key Takeaways

  • Follow extraction, manufacture, use and every relevant end-of-life route.
  • Embodied energy and carbon footprint measure different quantities.
  • Compare equal-function designs, including service life.
  • A primary-aluminum mass saving can need substantial use-phase energy savings to repay production energy.
  • An eco-audit identifies the dominant life phase.
  • Durability and protection affect lifetime resource use.

5.4 Design products whose materials can be recovered

Recovery depends on how a product is collected, separated and reprocessed. A material may be technically recyclable yet enter a waste stream that cannot deliver clean feedstock at a useful cost.

Preserve value before remelting

Reuse and remanufacturing keep whole products or components functioning and usually save more manufacturing effort than material recycling. Recycled content describes input to a new product. The end-of-life recycling rate describes the fraction of discarded material actually recovered. A high value for one does not establish the other.

Metals can be remelted repeatedly with controlled composition. Magnetic separation recovers steel; eddy-current equipment separates nonferrous metals. Aluminum remelting at 8.3 GJ/t compared with primary production at 186 GJ/t gives an energy saving of 1−8.3/186=0.955, about 95%.

Contamination limits the value of scrap. Copper and tin are difficult to remove from steelmaking streams, and copper can cause cracking in hot working. Mixed aluminum alloys often become casting alloys that tolerate more silicon and iron. Separating alloy streams preserves options for higher-value reuse.

Match recovery to material structure
MaterialCommon routeMain limitation
GlassCrush into cullet and remeltSort by color and exclude ceramics, stones and incompatible glass
ThermoplasticSort, melt and remoldIncompatible resin mixtures and molecular degradation
Thermoset or vulcanized rubberGrind into filler or use specialist recoveryCross-linked networks do not remelt
Fiber compositeGrind, or recover fibers by thermal or chemical processingSeparating matrix and fibers while preserving useful quality

Resin identification codes are 1 PET, 2 HDPE, 3 PVC, 4 LDPE, 5 PP, 6 PS and 7 other or mixed plastics. They identify resin types; local collection acceptance is a separate question. Moisture-sensitive polymers such as PET and polyamides can undergo hydrolysis during reprocessing, while other polymers may undergo scission, branching or additional cross-linking. Sorting and conditioning help preserve quality.

Chemical recycling can depolymerize suitable polymers toward monomers or use pyrolysis to form oils and gases. It can handle some streams unsuitable for mechanical recycling, but uses more energy than direct remelting. Ground tires become crumb rubber; devulcanization recovers only part of the original properties. Thermoset composite recovery can preserve carbon-fiber length, although cutting and handling may shorten fibers. Glass-fiber composites can enter cement-kiln routes, using resin as fuel and mineral content as feedstock.

Make separation possible

Use fewer compatible materials, mark plastic types and make parts accessible. Screws or snap fits can allow unlike parts to separate; inseparable adhesive joints and multilayer laminates can contaminate a stream. Avoid unnecessary coatings and inserts that reduce scrap value. Where performance permits, a thermoplastic can offer a remelting route unavailable to a thermoset. Design the recovery route alongside the service requirements, then check collection, sorting and markets for the intended destination.

Key Takeaways

  • Reuse and remanufacturing preserve component value before material reprocessing.
  • Recycled content and end-of-life recycling rate describe different flows.
  • Clean, separated alloy streams retain more value.
  • Thermoplastics remelt; cross-linked thermosets and rubbers do not.
  • Glass recycling needs clean, composition-compatible cullet.
  • Composite recovery must manage both matrix and fibers.
  • Accessible, separable joints improve recovery.

Corrosion and Materials Selection examples

5 Walkthroughs

1

From electrode reactions to a metal-loss prediction

17 steps
Build a corrosion cell, calculate its driving voltage and metal loss, then compare growth laws for a hot oxide scale.
  1. 1
    IntroductionFollow matter and charge

    Metal oxidation supplies electrons to a connected reduction reaction. Trace the cell’s paths, then separate its driving voltage from its metal-loss current.

    In dry oxidation, ask whether the growing scale restricts transport.

  2. 2
    ExplanationBuild the complete cell

    A wet cell needs anodic oxidation, cathodic reduction, a metallic electron path and an electrolyte ion path.

    Different areas of one plate can provide the two reactions; electrons travel through metal and ions through liquid.

  3. 3
    ExampleBalance the electron transfer

    Iron releases two electrons per atom: Fe→Fe2++2e−. Oxygen reduction in neutral water consumes four: O2+2H2O+4e−→4OH−.

    Double the iron reaction before adding them. Two iron atoms dissolve for each oxygen molecule reduced, and no electrons remain in the net equation.

  4. 4
    ChallengeCan acid corrosion continue without oxygen?

    A zinc sample is in oxygen-free acid. Can a corrosion cell still operate? Name the cathodic reaction.

    ---reveal---

    Yes. Zinc oxidation supplies electrons to hydrogen-ion reduction: 2H++2e−→H2. The metal path and acid electrolyte connect the reactions. Removing oxygen stops oxygen reduction, but does not remove this alternative cathodic reactant.

  5. 5
    ExampleFind the standard driving voltage

    Take an iron–copper cell under standard conditions. The reduction potentials are −0.44 V for Fe²⁺/Fe and +0.34 V for Cu²⁺/Cu.

    Iron has the more negative value and supplies the oxidation reaction. Subtract its tabulated reduction potential from copper's: ΔV∘=0.34−(−0.44)=0.78 V. Keep both signs when subtracting.

  6. 6
    ExampleApply the concentration correction

    Keep the same cell at 25 °C, but use Fe²⁺ at 0.10 M and Cu²⁺ at 0.0010 M. Both ions exchange two electrons.

    The ratio is 0.10/0.0010=100, whose base-10 logarithm is 2. Thus ΔV=0.78−(0.0592/2)(2)≈0.72 V. The voltage falls but remains positive for iron oxidation.

  7. 7
    ChallengeChoose the right evidence for a seawater joint

    An engineer ranks a titanium–steel seawater joint only with standard metal-ion potentials. What important effect is missing, and which evidence includes it?

    ---reveal---

    The surface films are missing. Passive titanium behaves much more nobly in seawater than its pure-metal standard potential suggests. Use a seawater galvanic series that includes the relevant surface states, then check geometry and reaction rates.

  8. 8
    ExamplePut the coupon data in the right units

    A steel coupon has 100 cm² total exposed area and loses 250 mg in 30 days. Its density is 7.9 g/cm³.

    The constant 87.6 requires hours, so use t=30(24)=720 h. Include all wetted faces in the stated area. The average penetration calculation is CPR=87.6(250)/(7.9×100×720)=0.0385 mm/yr.

  9. 9
    ExampleConvert current density into current

    A steel surface of 5,000 cm² corrodes at 2 µA/cm². Multiply before applying Faraday's law:

    I=(2×10−6)(5000)=0.010 A.

    For one year, use 3.156×107 seconds. Current density describes the rate per area; total current measures charge per second over the complete exposed region.

  10. 10
    ExampleTurn charge into iron loss

    Assume iron dissolves as Fe²⁺, so each mole of iron releases two moles of electrons. With molar mass 55.85 g/mol:

    m=0.010(3.156×107)(55.85)2(96 485)≈91 g.

    The same charge would imply a different mass for a different electron count or molar mass. Those quantities come from the actual dissolution reaction.

  11. 11
    Key InsightWhy voltage and rate can disagree

    A favorable voltage need not produce a large corrosion current. Surface kinetics, reactant delivery and passive films can slow the reactions.

    Local film breakdown can concentrate attack while much of the surface remains resistant.

  12. 12
    ChallengeInterpret faster flow in an active system

    Actively corroding steel is limited by oxygen delivery. Flow increases oxygen transport, and the steel stays active. What happens to its corrosion current?

    ---reveal---

    It increases. Faster cathodic oxygen reduction requires a larger balancing anodic current, which means faster iron dissolution. The result depends on the stated active behavior; a transition into a passive region would require a different reading of the polarization curve.

  13. 13
    ExplanationLook for a protective scale

    A compact oxide can slow transport through the surface layer. A Pilling–Bedworth ratio near one to two permits coverage.

    Adhesion, slow diffusion and resistance to thermal cracking or evaporation are also needed for protection.

  14. 14
    ExampleUse parabolic growth

    For zero-intercept parabolic oxidation, W2=Kt. A gain of 2.0 mg/cm² in 100 h gives K=2.02/100=0.040 in compatible units.

    At 400 h, W=0.040(400)=4.0 mg/cm2. The thickening scale slows further growth. A linear model through the first point would predict 8.0 mg/cm² instead.

  15. 15
    ChallengeDistinguish oxygen uptake from metal consumption

    A dry oxidation test records a 10 mg mass gain with no scale loss. Has exactly 10 mg of metal been consumed? Explain.

    ---reveal---

    No. The gain is oxygen added to the retained specimen. Calculate metal consumption from the oxide formula and molar masses. For example, one mole of a simple MO oxide contains one mole of metal but only one mole of oxygen atoms; these masses are different.

  16. 16
    ChallengeCombine an average rate with a failure clue

    A steel wall shows a low coupon-average corrosion rate but develops a leak at one narrow hole. Why can these observations agree, and what should be measured next?

    ---reveal---

    Localized pitting can remove little total metal while penetrating deeply. Measure pit depth and remaining wall thickness at the damaged sites. An average mass-loss rate spreads the loss over the coupon and cannot describe the maximum local penetration.

  17. 17
    RecapKeep three questions separate

    Identify the oxidation and reduction reactions, use potentials for direction, and use current or mass loss for rate.

    For dry oxidation, establish the scale behavior and growth law before extrapolating exposure time.

2

Diagnose damage and choose a matching control

18 steps
Use location, shape, exposure and process history to distinguish mechanisms, then select design changes, coatings and electrochemical protection.

Save this lesson to follow every Walkthrough step by step.

  1. 1
    IntroductionStart with the evidence of damage
  2. 2
    ExplanationCompare broad thinning with local holes
  3. 3
    ExampleFind the concentrated anode
  4. 4
    ChallengeDecide which coupled surface to coat
  5. 5
    ConnectionSee why a gap becomes aggressive
  6. 6
    ExplanationConnect weld heat to grain boundaries
  7. 7
    ExampleRead flow damage and selective loss
  8. 8
    ChallengeUse the plating history
  9. 9
    Key InsightResidual tension still counts as stress
  10. 10
    ExplanationChoose a compatible material and exposure
  11. 11
    ExampleAdd thickness for uniform loss
  12. 12
    ChallengeExplain an inhibitor failure
  13. 13
    ExplanationCompare two damaged metal coatings
  14. 14
    ExampleTrace an impressed-current connection
  15. 15
    ChallengeCorrect the ideal anode estimate
  16. 16
    TipRead a potential at the right interface
  17. 17
    ChallengeCombine geometry and protection
  18. 18
    RecapMatch the intervention to the cause
3

Explain a nonmetallic part failure

11 steps
Distinguish liquid uptake from bond damage, connect stress to cracking, and choose a control for the actual degradation mechanism.

Save this lesson to follow every Walkthrough step by step.

  1. 1
    IntroductionAsk what changed in the material
  2. 2
    ExplanationSeparate uptake from dissolution
  3. 3
    ExampleCondition a nylon part for service
  4. 4
    ChallengeDiagnose a detergent-exposed corner
  5. 5
    ExampleCompare photon energies
  6. 6
    ExplanationConnect the agent to a vulnerable bond
  7. 7
    Key InsightChoose the additive for its job
  8. 8
    ChallengeExplain delayed failure of glass
  9. 9
    ConnectionCheck the disposal environment too
  10. 10
    ChallengeSeparate two causes of loss of stiffness
  11. 11
    RecapUse structure to explain the symptom
4

Derive and use a lightweight-material ranking

15 steps
Translate a brief, derive tie and beam indices, then screen and rank candidates on logarithmic property axes.

Save this lesson to follow every Walkthrough step by step.

  1. 1
    IntroductionCompare equal jobs
  2. 2
    ExampleTranslate a lightweight tie
  3. 3
    ChallengeSeparate a limit from a priority
  4. 4
    ExampleWrite the tie's two equations
  5. 5
    ExampleEliminate the free area
  6. 6
    ExplanationLet bending change the exponent
  7. 7
    ExampleCompare steel and aluminum beams
  8. 8
    ChallengeChange the free dimension
  9. 9
    ConnectionKeep panel and shaft models distinct
  10. 10
    ExplanationRead ratios on a logarithmic axis
  11. 11
    ExampleTurn the beam index into a line
  12. 12
    ChallengeCheck a chart point against the line
  13. 13
    TipScreen before chasing the highest bubble
  14. 14
    ChallengeCombine screening and ranking
  15. 15
    RecapKeep the model attached to the index
5

Choose between competing lifetime designs

16 steps
Compare equal-function material and component costs, discount maintenance, estimate an energy break-even point and improve recovery.

Save this lesson to follow every Walkthrough step by step.

  1. 1
    IntroductionSet one useful basis for comparison
  2. 2
    ExplanationInclude the mass needed for the job
  3. 3
    ExampleSpread the tooling cost
  4. 4
    ChallengeRemove a dominated candidate
  5. 5
    ExampleList the payments before discounting
  6. 6
    ExampleApply the time value of money
  7. 7
    ChallengeFind a missing lifetime cost
  8. 8
    ExplanationTrack the environmental life phases
  9. 9
    ExampleCalculate the production-energy difference
  10. 10
    ExampleFind the energy break-even point
  11. 11
    ChallengeInclude an extra replacement
  12. 12
    ExplanationPreserve clean material streams
  13. 13
    ConnectionLet structure determine the recovery route
  14. 14
    ChallengeImprove the product's exit route
  15. 15
    ChallengeCombine durability, cost and energy
  16. 16
    RecapChoose the trade-off with evidence

Corrosion and Materials Selection practice questions

50 Practice Questions in 5 sets

Set 1: Connect corrosion mechanisms with material choices10 Practice Questions

Question 1 of 10

A steel structure needs 0.12 A for 2.0 years. Magnesium dissolves as Mg²⁺ with molar mass 24.31 g/mol and current efficiency 50%. Use 3.156 × 10⁷ s/yr and F = 96,485 C/mol. What magnesium consumption is expected before additional utilization margins?
  1. About 0.954 kg
  2. About 1.91 kg
  3. About 0.477 kg
  4. About 3.82 kg
Show answerHide answer
Answer: B
The required charge is 0.12(2)(3.156×107) C, giving about 0.954 kg of theoretical magnesium consumption. Divide by 0.50 current efficiency to obtain about 1.91 kg. Multiplying by efficiency would incorrectly reduce the metal needed despite charge lost to self-corrosion.

Question 2 of 10

A tie has fixed length and required axial stiffness. Its area may change to minimize mass. Which property combination should be maximized?
  1. Eρ
  2. E1/3/ρ
  3. E/ρ
  4. E1/2/ρ
Show answerHide answer
Answer: C
Eliminate area using A=SL/E to obtain m=SL2ρ/E, then maximize E/ρ. The square-root modulus index applies to scalable beams in bending, not this axial stiffness constraint.

Question 3 of 10

What happens to susceptible brass during dezincification?
  1. Zinc dissolves, leaving a weak copper-rich network.
  2. Copper dissolves, leaving a weak zinc-rich network.
  3. Zinc dissolves, leaving a denser copper-rich layer.
  4. Copper and zinc dissolve uniformly at their original ratio.
Show answerHide answer
Answer: A
Dezincification preferentially removes zinc and leaves a porous, weak, copper-rich residue. A red surface can therefore signal damage even if the part keeps its outline. Treating that residue as a dense protective copper layer overlooks the loss of load-bearing material within the original brass.

Question 4 of 10

For Zn oxidation coupled to Cu²⁺ reduction at 25 °C, the standard voltage is 1.10 V. Both ions have charge 2+, with Zn²⁺ at 0.020 M and Cu²⁺ at 0.20 M. What is the cell voltage?
  1. About 1.10 V
  2. About 1.07 V
  3. About 1.13 V
  4. About 1.16 V
Show answerHide answer
Answer: C
The ion ratio is 0.10, so ΔV=1.10−(0.0592/2)(−1)≈1.13 V. Reversing the ratio changes the correction’s sign and gives the incorrect 1.07 V.

Question 5 of 10

What chemical process can shorten PET chains when wet material is heated during reprocessing?
  1. Galvanic coupling
  2. Hydrolysis
  3. Sensitization
  4. Passivation
Show answerHide answer
Answer: B
Water can cleave the ester links in PET through hydrolysis, shortening chains during hot processing. Passivation describes a protective metal surface state and does not explain this molecular change. Drying reduces water available for the chain-breaking reaction in the melt.

Question 6 of 10

Three materials pass a temperature limit. One fails the required chemical-resistance rating but has the highest stiffness-to-density ratio. How should selection proceed?
  1. Rank it first, then average its chemical and stiffness scores
  2. Keep it first because the highest index overrides a single failure
  3. Remove the temperature limit and rank every material together
  4. Reject it, then rank the candidates that pass both limits
Show answerHide answer
Answer: D
Every mandatory requirement must be met, so failure of the chemical-resistance screen removes the candidate. Ranking compares the remaining feasible choices. Averaging a failed constraint with a strong index would silently change the brief from a requirement into a negotiable preference.

Question 7 of 10

A static indoor support has negligible use energy. Two equal-life candidates have identical manufacture, transport and disposal burdens. What evidence most directly compares their remaining energy burden?
  1. Required material mass without production-energy intensity
  2. Required mass times embodied energy per kilogram
  3. Density alone for the two candidate materials
  4. Embodied energy per kilogram without the required material mass
Show answerHide answer
Answer: B
With the other stated burdens equal and use energy negligible, the material-production contribution is the remaining difference. Multiply each design’s required mass by its embodied energy per kilogram. Density alone omits both the mass needed for the function and the energy intensity of producing it.

Question 8 of 10

An outdoor plastic becomes chalky and brittle. The new formulation includes carbon black. What part of the damage process does carbon black mainly reduce?
  1. Ultraviolet light reaching vulnerable material
  2. Water reacting with every ester linkage
  3. All chemical uptake from contacting liquids
  4. Residual tensile stress from the molding process
Show answerHide answer
Answer: A
Carbon black screens ultraviolet radiation and reduces light available to initiate polymer damage. It does not remove molded residual stress or establish chemical compatibility with every liquid. Weathering can involve several agents, so UV screening addresses one important part of the combined exposure.

Question 9 of 10

Iron dissolves as Fe²⁺ at a total corrosion current of 0.0060 A for 48 h. Use 55.85 g/mol and F = 96,485 C/mol. How much iron dissolves?
  1. About 0.150 g
  2. About 0.600 g
  3. About 0.00625 g
  4. About 0.300 g
Show answerHide answer
Answer: D
Faraday’s law gives m=0.0060(172800)(55.85)/(2×96485)≈0.300 g. The divisor is two because iron forms Fe²⁺; omitting it incorrectly doubles the mass.

Question 10 of 10

What glass feedstock is made by crushing sorted recovered glass for remelting?
  1. Clinker
  2. Dross
  3. Slag
  4. Cullet
Show answerHide answer
Answer: D
Crushed recovered glass used in a new glass batch is cullet. Sorting by composition and color and removing contaminants are needed for useful remelting. Slag is associated with high-temperature metallurgical processing and is not the name of this prepared glass feedstock.
Set 2: Apply rates, compatibility and design constraints10 Practice Questions

Save this lesson to see every answer and practice every set.

Question 1 of 10

An oxide has formula M₂O₃, formula mass 150 g/mol and density 5.0 g/cm³. The metal has atomic mass 50 g/mol and density 7.0 g/cm³. What is its Pilling–Bedworth ratio?
  1. 0.476
  2. 1.40
  3. 2.10
  4. 4.20
Show answerHide answer

Save this lesson to see this answer.

Question 2 of 10

A carbon-steel fastener contacts a large copper sheet in salt water. Only one of the two materials can be painted. Which should be painted to reduce the galvanic risk at coating defects?
  1. The copper sheet
  2. The steel face
  3. The steel fastener
  4. Either one equally
Show answerHide answer

Save this lesson to see this answer.

Question 3 of 10

A log E–log ρ chart has a slope-2 selection line through E = 80 GPa, ρ = 4.0 Mg/m³. At ρ = 2.0 Mg/m³, a candidate has E = 30 GPa. How does it compare for the same scalable stiff-beam model?
  1. It beats the line; equal performance there needs 10 GPa
  2. It beats the line; equal performance there needs 20 GPa
  3. It lies on the line; equal performance there needs 30 GPa
  4. It loses to the line; equal performance there needs 40 GPa
Show answerHide answer

Save this lesson to see this answer.

Question 4 of 10

Two feasible designs last 20 years. A costs 900 initially plus 200 maintenance and 300 shutdown cost at years 5, 10 and 15. B costs 2,100 initially with no later costs. Use zero discounting and equal end-of-life value. Which has lower life-cycle cost?
  1. A, by 600 cost units
  2. B, by 300 cost units
  3. A, by 300 cost units
  4. B, by 900 cost units
Show answerHide answer

Save this lesson to see this answer.

Question 5 of 10

On a log chart with E vertical and ρ horizontal, what slope represents constant E¹ᐟ³/ρ?
  1. 2
  2. 1/3
  3. 1
  4. 3
Show answerHide answer

Save this lesson to see this answer.

Question 6 of 10

A steel plate is partly covered by a wet, nonconducting deposit. Oxygen reaches the bare region more readily than the covered region. Where is anodic attack expected, and why?
  1. On both regions equally, since the metal is identical
  2. On the bare region, where oxygen supply is higher
  3. Under the deposit, where oxygen supply is lower
  4. Under the deposit, because electrons flow through it
Show answerHide answer

Save this lesson to see this answer.

Question 7 of 10

A nylon latch meets its stiffness requirement in dry testing. In humid service it becomes larger and deflects too much, without visible cracks. A redesign must keep the same nylon grade. Which evidence is needed to size the new latch?
  1. Moisture-conditioned tensile strength with the original dry modulus
  2. Moisture-conditioned dimensions with the original dry modulus
  3. Dry tensile strength and the original dry dimensions only
  4. Moisture-conditioned modulus and dimensions at service conditions
Show answerHide answer

Save this lesson to see this answer.

Question 8 of 10

A stainless tank has a few deep holes beneath small surface deposits, with very little overall thinning. What form of corrosion does this describe?
  1. Intergranular corrosion
  2. Uniform corrosion
  3. Pitting
  4. Selective leaching
Show answerHide answer

Save this lesson to see this answer.

Question 9 of 10

Light at 320 nm and 640 nm reaches a polymer. What is the photon-energy ratio E₃₂₀/E₆₄₀, and does that ratio alone establish the relative degradation rate?
  1. 2; absorption and a damage pathway still matter
  2. 1/2; absorption and a damage pathway still matter
  3. 2; degradation must proceed twice as fast at 320 nm
  4. 4; degradation must proceed four times as fast at 320 nm
Show answerHide answer

Save this lesson to see this answer.

Question 10 of 10

A dedicated mold costs 36,000 cost units and makes 12,000 parts. What tooling charge should be allocated to each part?
  1. 30 cost units
  2. 3 cost units
  3. 0.333 cost units
  4. 4 cost units
Show answerHide answer

Save this lesson to see this answer.

Set 3: Compare damage, performance and lifetime burdens10 Practice Questions

Save this lesson to see every answer and practice every set.

Question 1 of 10

A maintenance payment of 800 cost units is due in 5 years. At a 4% annual discount rate, what is its present value?
  1. About 658 cost units
  2. About 769 cost units
  3. About 973 cost units
  4. About 640 cost units
Show answerHide answer

Save this lesson to see this answer.

Question 2 of 10

A rubber seal absorbs liquid, grows larger and softens while remaining connected. What process is observed?
  1. Dissolution
  2. Depolymerization
  3. Chain scission
  4. Swelling
Show answerHide answer

Save this lesson to see this answer.

Question 3 of 10

A rectangular beam has fixed length and depth h, but width b may change. Its bending constraint fixes EI; I = bh³/12 and mass is proportional to ρb. Which index minimizes mass?
  1. E1/2/ρ
  2. E2/ρ
  3. E1/3/ρ
  4. E/ρ
Show answerHide answer

Save this lesson to see this answer.

Question 4 of 10

Two steel coupons have the same area and mass-loss penetration rate. One shows uniform thinning and the other has isolated deep pits. A wall-thickness decision uses only that average rate. What additional measurement is most important, and why?
  1. Maximum pit depth, since local penetration can control leakage
  2. Total current alone, since it uniquely locates the deepest pit
  3. Average rust thickness, since deposits mark the deepest loss
  4. Average wall thickness, since it already accounts for all local loss
Show answerHide answer

Save this lesson to see this answer.

Question 5 of 10

A glass component carries a constant tensile load in moist air and fails long after loading. No bulk dissolution or impact is observed. What mechanism best explains delayed failure?
  1. Mechanical overload from an increase in the applied force
  2. Water-assisted growth of an existing stressed crack
  3. Bulk glass dissolution followed by uniform wall thinning
  4. Thermal shock from a rapid change in the applied temperature
Show answerHide answer

Save this lesson to see this answer.

Question 6 of 10

A tie must meet both axial stiffness S and tensile load F at fixed L; area is free. For material P, SL/E = 300 mm² and F/σf = 500 mm², with density 2.0 Mg/m³. For Q the areas are 400 and 250 mm², with density 3.0 Mg/m³. Which is lighter at equal length?
  1. Q, using 400 mm²
  2. P, using 300 mm²
  3. P, using 500 mm²
  4. Q, using 250 mm²
Show answerHide answer

Save this lesson to see this answer.

Question 7 of 10

A welded austenitic stainless vessel develops attack beside grain boundaries in a band near the weld. What microstructural change best explains it?
  1. Chromium enrichment beside grain-boundary carbides
  2. Carbon depletion in grain interiors without chromium loss
  3. Chromium depletion beside grain-boundary carbides
  4. Chromium depletion inside grains but not near boundaries
Show answerHide answer

Save this lesson to see this answer.

Question 8 of 10

A low-alloy weathering-steel enclosure rusts rapidly only in a salt-laden pocket that stays wet. Its open faces cycle wet and dry and remain sound. Which change best addresses the observed difference?
  1. Reduce inspection access to keep the pocket sheltered
  2. Increase humidity around all faces to equalize exposure
  3. Remove the water trap and control chloride retention
  4. Use the same steel with a smaller uniform allowance
Show answerHide answer

Save this lesson to see this answer.

Question 9 of 10

Two materials pass all screens for a stiff beam with similar scalable sections. A has E = 144 GPa, ρ = 4.0 Mg/m³, price 2 cost units/kg. B has E = 81 GPa, ρ = 2.0 Mg/m³, price 4 cost units/kg. Which costs less in raw material for equal stiffness, and why?
  1. A; its beam cost index is 1.50 versus 1.125
  2. B; its beam cost index is 4.50 versus 3.00
  3. B; density alone establishes the required mass ratio
  4. A; price per kilogram alone establishes the ranking
Show answerHide answer

Save this lesson to see this answer.

Question 10 of 10

Standard reduction potentials are −0.76 V for Zn²⁺/Zn and −0.25 V for Ni²⁺/Ni. What is the standard voltage for zinc oxidation coupled to nickel-ion reduction?
  1. 1.01 V
  2. 0.51 V
  3. −1.01 V
  4. −0.51 V
Show answerHide answer

Save this lesson to see this answer.

Set 4: Check assumptions in corrosion and selection models10 Practice Questions

Save this lesson to see every answer and practice every set.

Question 1 of 10

During corrosion, copper ions accept electrons and become copper metal. At which electrode does this reaction occur?
  1. The electrolyte
  2. The anode
  3. The metallic connection
  4. The cathode
Show answerHide answer

Save this lesson to see this answer.

Question 2 of 10

A housing uses a thermoset matrix with long carbon fibers. The recovery goal is to retain fibers for another application. Why is ordinary remelting unsuitable, and what route could recover fibers?
  1. The network melts first; hot filtering always preserves fiber length
  2. The network does not remelt; pyrolysis or solvolysis may recover fibers
  3. The network remelts; slow cooling separates fibers from liquid resin
  4. The network only swells; immersion alone yields clean dry fibers
Show answerHide answer

Save this lesson to see this answer.

Question 3 of 10

A pump cover must tolerate 140 °C, and its mass should be as low as possible. How is the temperature requirement classified?
  1. A free variable
  2. An objective
  3. A constraint
  4. A ranking result
Show answerHide answer

Save this lesson to see this answer.

Question 4 of 10

Three steel-bolt batches receive the same tensile load in dry service. High-strength plated bolts crack hours later; high-strength unplated bolts and lower-strength plated bolts survive. What mechanism and process change best account for this pattern?
  1. Hydrogen embrittlement; limit hydrogen entry and bake promptly after plating
  2. Hydrogen embrittlement; stress-relieve only before the hydrogen-producing plating step
  3. Stress corrosion cracking; exclude chlorides from the already dry service
  4. Stress corrosion cracking; lower residual stress but retain the plating process
Show answerHide answer

Save this lesson to see this answer.

Question 5 of 10

A cross-linked elastomer and an uncross-linked thermoplastic contact a good solvent for their chains. Why may the elastomer stay connected even after large liquid uptake?
  1. Its network links prevent all solvent molecules from entering
  2. Its network links prevent separate chains from dispersing
  3. Its network converts the solvent into a solid surface film
  4. Its chains have no attraction to any solvent molecules
Show answerHide answer

Save this lesson to see this answer.

Question 6 of 10

A pipe requires 4.0 mm of structural wall thickness and must tolerate uniform loss of 0.12 mm/yr for 20 years. What minimum thickness follows from adding that corrosion allowance?
  1. 8.0 mm
  2. 6.4 mm
  3. 4.6 mm
  4. 2.4 mm
Show answerHide answer

Save this lesson to see this answer.

Question 7 of 10

Equal-function components last the same service period. Steel uses 12 kg at 24 MJ/kg; primary aluminum uses 7 kg at 180 MJ/kg. All other non-use energy burdens are equal. What lifetime use-energy saving must aluminum exceed to have the lower total energy?
  1. 972 MJ
  2. 156 MJ
  3. 1,260 MJ
  4. 288 MJ
Show answerHide answer

Save this lesson to see this answer.

Question 8 of 10

For a 10-year service period, design A costs 1,200 initially and 500 at year 5. Design B costs 1,600 initially with no later costs. End-of-life values are equal. At 5% annual discounting, which costs less in present value?
  1. A, by about 8 cost units
  2. B, by about 100 cost units
  3. A, by about 400 cost units
  4. B, by about 108 cost units
Show answerHide answer

Save this lesson to see this answer.

Question 9 of 10

A panel has fixed length and width with thickness free. For equal bending stiffness, compare A: E = 27 GPa, ρ = 1.5 Mg/m³ and B: E = 64 GPa, ρ = 2.4 Mg/m³. Which has lower mass, and what is mA/mB?
  1. B; about 1.20
  2. A; about 0.625
  3. A; about 0.833
  4. B; about 1.48
Show answerHide answer

Save this lesson to see this answer.

Question 10 of 10

A titanium–steel seawater joint is assessed only from pure-metal standard potentials, predicting rapid titanium loss. What evidence best corrects this assessment?
  1. Standard potentials multiplied by electrode areas
  2. Standard potentials with oxidation signs for both metals
  3. Densities and atomic masses of the connected metals
  4. Seawater potentials with the passive surface states
Show answerHide answer

Save this lesson to see this answer.

Set 5: Resolve multistep material and lifetime decisions10 Practice Questions

Save this lesson to see every answer and practice every set.

Question 1 of 10

A square-section beam may change size but not cross-sectional shape. Material A has E = 100 GPa, ρ = 5.0 Mg/m³; B has E = 64 GPa, ρ = 2.0 Mg/m³. What is B’s mass relative to A for the same bending stiffness and length?
  1. 0.625
  2. 2.00
  3. 0.40
  4. 0.50
Show answerHide answer

Save this lesson to see this answer.

Question 2 of 10

A zinc-coated steel panel and a tin-coated steel panel each have a small wet scratch through to steel. Which coating can protect the exposed steel by preferential dissolution?
  1. Zinc
  2. Both equally
  3. Neither coating
  4. Tin
Show answerHide answer

Save this lesson to see this answer.

Question 3 of 10

An engineer is comparing linear and parabolic dry-oxidation models. A test starts at zero mass gain and gives 1.5 mg/cm² after 25 h and 3.0 mg/cm² after 100 h. Using the model that fits both measurements, what gain is predicted at 400 h?
  1. 4.5 mg/cm²
  2. 6.0 mg/cm²
  3. 24.0 mg/cm²
  4. 12.0 mg/cm²
Show answerHide answer

Save this lesson to see this answer.

Question 4 of 10

Two stainless grades contain, in mass percent, X: 20 Cr, 1.5 Mo, 0.10 N; Y: 18 Cr, 2.5 Mo, 0.20 N. A warm chloride crevice is expected. What comparison follows using the PREN convention with nitrogen factor 16?
  1. Y ranks higher; that establishes resistance in the crevice
  2. X ranks higher; the crevice still needs a service check
  3. Y ranks higher; the crevice still needs a service check
  4. X and Y tie; their combined alloy additions are equal
Show answerHide answer

Save this lesson to see this answer.

Question 5 of 10

A coupon loses 180 mg after 15 days. Its density is 8.0 g/cm³ and total exposed area is 60 cm². What average penetration rate does this represent?
  1. About 2.19 mm/yr
  2. About 0.091 mm/yr
  3. About 0.00380 mm/yr
  4. About 0.0456 mm/yr
Show answerHide answer

Save this lesson to see this answer.

Question 6 of 10

A 40 kg product contains 12 kg of recovered feedstock. At end of life, 75% of its mass is collected, and 80% of that collected mass is reprocessed into usable feedstock. What are its recycled content and actual end-of-life recycling rate?
  1. 30% recycled content; 75% end-of-life recycling
  2. 30% recycled content; 60% end-of-life recycling
  3. 30% recycled content; 80% end-of-life recycling
  4. 60% recycled content; 30% end-of-life recycling
Show answerHide answer

Save this lesson to see this answer.

Question 7 of 10

Two feasible beam designs provide identical service. A weighs 9 kg and costs 90 units; B weighs 6 kg and costs 132 units. The project values each kilogram saved at 12 units. Which design is preferred under this valuation, and by how much?
  1. A, by 42 units
  2. B, by 6 units
  3. B, by 36 units
  4. A, by 6 units
Show answerHide answer

Save this lesson to see this answer.

Question 8 of 10

Polyethylene caps crack near tightly molded corners after detergent contact. Unstressed specimens in the same detergent and stressed specimens without detergent remain intact. Which mechanism and redesign best follow from the combined evidence?
  1. Environmental stress cracking; reduce stress and verify a resistant grade
  2. Environmental stress cracking; keep corner stress and rely on unstressed data
  3. Solvent dissolution; keep the grade and choose by unstressed immersion data
  4. Residual-stress cracking alone; keep the detergent and change only the molding
Show answerHide answer

Save this lesson to see this answer.

Question 9 of 10

What value is halfway between 100 and 10,000 on a logarithmic axis?
  1. 5,050
  2. 500
  3. 1,000
  4. 2,000
Show answerHide answer

Save this lesson to see this answer.

Question 10 of 10

A molded part carries resin code 5. The local collection system accepts only codes 1 and 2. What can be concluded about that part?
  1. It is PET, and the stated system accepts that resin
  2. It is HDPE, and the stated system accepts that resin
  3. It is PP, and the stated system accepts that resin
  4. It is PP, and the stated system does not accept that resin
Show answerHide answer

Save this lesson to see this answer.

Stuck on your own question? Homework Help

Key Terms

98 Key Terms, each with its definition

A

Activation polarization
Activation polarization is a potential shift associated with overcoming a slow reaction step at the electrode surface.
A sluggish hydrogen-evolution step can restrict metal dissolution even when the cell voltage is large.
Anode
An anode is an electrode region where oxidation releases electrons.
The iron beneath a damp deposit can be the anode while the exposed surface supports reduction.
Anodic protection
Anodic protection holds an active–passive metal at a potential within its passive range.
A potentiostat can maintain a suitable acid-storage vessel within its stable passive potential range.
Antioxidant
An antioxidant is an additive that slows oxidation reactions.
A hot-service polymer may need oxidation control even where sunlight does not reach the part.
Ashby chart
An Ashby chart plots material property ranges against one another, commonly on logarithmic axes, to support screening and ranking.
A modulus–density chart lets a designer compare polymers, metals, woods and composites in one view.

B

Barrier coating
A barrier coating protects by separating the substrate from its environment.
A poorly bonded paint edge can allow water to spread beneath the coating on a steel panel.
Biodegradation
Biodegradation is breakdown of a material through biological activity under environmental conditions that support the relevant processes.
A PLA package may need industrial composting conditions instead of cool soil for useful breakdown.

C

Carbon footprint
A carbon footprint is the greenhouse-gas emissions associated with a stated product or activity, expressed as carbon dioxide equivalent.
Two energy sources can supply the same heat while contributing different greenhouse-gas emissions.
Cathode
A cathode is an electrode region where reduction consumes electrons.
Hydrogen bubbles form at cathodic sites when hydrogen ions accept electrons from dissolving zinc.
Cathode-to-anode area ratio
The cathode-to-anode area ratio compares exposed electrode areas and helps indicate current concentration on the dissolving metal.
Coating an active surface alone can leave a scratch with a very unfavorable electrode-area ratio.
Cathodic protection
Cathodic protection suppresses oxidation of a metal structure by supplying electrons and making the structure a cathodic surface.
A buried coated pipe can receive protective current at accessible defects in its coating.
Cell potential
A cell potential is the voltage difference between its cathode and anode.
A positive voltage of 1.10 V favors zinc oxidation with copper-ion reduction under standard conditions.
Chain scission
Chain scission breaks polymer backbone bonds and lowers molecular weight.
A weathered plastic bracket can become brittle as ultraviolet-assisted reactions shorten its chains.
Chemical compatibility
Chemical compatibility is a material's ability to retain required properties in contact with a particular substance under specified conditions.
A seal rating must match the liquid composition and service temperature, not just the polymer family.
Chemical recycling
Chemical recycling converts polymer waste into monomers or other chemical feedstocks through processes that alter its molecular structure.
A suitable depolymerization route can recover monomer from a polymer unsuitable for direct remolding.
Concentration polarization
Concentration polarization is a potential shift caused by limited delivery or removal of reacting species at an electrode.
Stirring aerated water can raise the limiting oxygen-reduction current by improving oxygen delivery.
Corrosion
Corrosion is destructive attack of a material by its environment.
A steel tank loses useful wall thickness when its surface reacts with the water it contains.
Corrosion allowance
A corrosion allowance is extra thickness to cover expected uniform loss during service.
A design rate of 0.08 mm/yr over 20 years requires 1.6 mm of extra thickness for uniform loss.
Corrosion inhibitor
A corrosion inhibitor is a controlled additive that lowers the corrosion rate.
A recirculating cooling loop can maintain and monitor inhibitor concentration during operation.
Corrosion penetration rate
A corrosion penetration rate is average thickness loss per unit time, calculated from uniform loss or from mass loss and exposed area.
A coupon result of 0.04 mm/yr must be compared with the wall allowance and required service life.
Cost per function
Cost per function is the expense of delivering a specified amount of useful performance, accounting for the material quantity required.
Comparing equally stiff beams can favor steel even when an aluminum beam has lower mass.
Crevice corrosion
Crevice corrosion is local attack within a stagnant narrow gap where solution chemistry becomes more aggressive than outside.
Salt water trapped beneath a gasket can acidify and attack stainless steel inside the gap.
Cullet
Cullet is crushed glass used as feedstock for making new glass.
A ceramic fragment in a glass-recycling stream can cause a defect in the new glass product.
Current density
Current density is electric current divided by the electrode area carrying it.
The same total current causes faster local metal loss when it passes through a smaller anode.

D

Deaeration
Deaeration is removal of dissolved gases from a liquid.
Removing dissolved oxygen from feedwater can slow steel corrosion before water enters a boiler.
Design constraint
A design constraint is a mandatory requirement every feasible design must meet.
A corrosion-resistance requirement can remove a candidate before its low mass is considered.
Design for disassembly
Design for disassembly makes components accessible and separable so useful parts and clean material streams can be recovered.
Screws joining unlike materials can permit separation that an inseparable adhesive joint would prevent.
Design objective
A design objective is the quantity improved when feasible designs are ranked.
Minimum mass ranks feasible tie materials differently from minimum initial material cost.
Differential aeration cell
A differential aeration cell is a corrosion cell created by unequal oxygen supply, with the oxygen-poor region becoming anodic.
A sheltered wet gap beneath a washer can corrode while the surrounding surface remains aerated.
Discount rate
A discount rate is the annual rate used to convert costs or benefits at different times onto a common present-value basis.
Increasing the rate reduces the present contribution of repainting scheduled far into the future.
Dissolution
Dissolution disperses separate polymer chains into a compatible solvent.
Polystyrene foam collapses as its polymer dissolves into a compatible solvent such as acetone.
Dominated candidate
A dominated candidate is no better than another feasible choice on every objective and is strictly worse on at least one.
A beam that is heavier and more expensive than another feasible beam has no mass–cost advantage.
Downtime cost
Downtime cost is the value lost while equipment or a service is unavailable.
A leaking process line can stop production and make the outage more expensive than the replacement pipe.

E

Eco-audit
An eco-audit is a screening estimate of energy or carbon burdens across life phases that identifies the largest contributions.
A vehicle-component audit may show that use-phase savings repay a higher material-production burden.
Electrolyte
An electrolyte is a medium that carries electric current through moving ions.
Salt water connects the electrode reactions ionically while the metal carries the electrons.
Embodied energy
Embodied energy is the energy required to produce a material or product within a stated system boundary, often reported per kilogram.
Multiplying MJ/kg by the mass of an equal-function component estimates its material-energy burden.
End-of-life recycling rate
An end-of-life recycling rate is the fraction of discarded material that is actually recovered and reprocessed into usable material.
Collection losses lower the recycling rate even when the metal itself remelts without difficulty.
Environmental stress cracking
Environmental stress cracking is crazing or cracking of a polymer when stress acts together with a liquid that promotes the damage.
A detergent-exposed polyethylene part can crack near a stressed molded corner without dissolving.
Erosion–corrosion
Erosion–corrosion is combined chemical attack and mechanical wear by moving fluid that repeatedly damages protective surface films.
Grooves at a pump outlet suggest that turbulence or suspended particles are removing its film.

F

Faraday's law
Faraday's law relates the amount of material transformed at an electrode to the electric charge transferred and the electron count.
An anode-consumption estimate uses current multiplied by time and the metal's electrochemical equivalent.
Free variable
A free variable is a design feature that may change while requirements are met.
If beam depth is fixed but width is free, the stiffness index differs from that of a square section free to scale.
Functional unit
A functional unit is a defined amount of service used as the common basis for comparing the environmental burdens of alternatives.
Two beams must provide the same stiffness and service life before their embodied energies are compared.

G

Galvanic corrosion
Galvanic corrosion is accelerated attack of the more active member of an electrically connected couple in a common electrolyte.
A small steel bolt in a large wet copper sheet can lose metal rapidly at the joint.
Galvanic series
A galvanic series ranks metal and alloy potentials in a specified environment.
The seawater series distinguishes stainless steel in its active state from the same family when passive.
Graphitic corrosion
Graphitic corrosion is selective loss of iron from gray cast iron, leaving a graphite-rich network with very low mechanical strength.
An old water main may retain its outline even though the remaining wall is easily cut.

H

Half-reaction
A half-reaction shows one oxidation or reduction process, including electron transfer.
Doubling the iron oxidation half-reaction balances the four electrons used in oxygen reduction.
Hindered amine light stabilizer
A hindered amine light stabilizer is an additive that captures reactive radicals involved in light-driven polymer degradation.
HALS can complement UV screening in a polymer formulation intended for prolonged outdoor use.
Hydrogen embrittlement
Hydrogen embrittlement is loss of ductility or toughness associated with hydrogen entering a susceptible metal and promoting cracking.
A plated high-strength fastener can fail hours later under tension if diffusible hydrogen remains.
Hydrolysis
Hydrolysis is cleavage of chemical bonds through reaction with water.
Drying PET before melt processing reduces water-driven chain damage at the processing temperature.

I

Impressed-current protection
Impressed-current protection uses an external DC power supply and auxiliary anodes to deliver adjustable cathodic current to a structure.
A pipeline under protection connects to the negative terminal, while ground-bed anodes connect to the positive one.
Intergranular corrosion
Intergranular corrosion is preferential attack at or beside grain boundaries that can weaken a material with little overall metal loss.
Chromium-depleted zones beside boundary carbides can corrode while grain interiors remain passive.

L

Life-cycle cost
Life-cycle cost is the total cost of providing a function over its service life, including acquisition, use, maintenance and end of life.
An inaccessible painted component may cost more to maintain than a higher-priced resistant alloy.
Linear oxidation
Linear oxidation is growth in which mass gain per unit area increases at a constant rate under the specified exposure conditions.
A porous scale can allow continued gas access and produce approximately linear mass gain.
Logarithmic axis
A logarithmic axis places equal numerical ratios at equal distances, making several orders of magnitude readable on one chart.
The midpoint between 10 and 100 GPa is about 31.6 GPa on a logarithmic modulus axis.

M

Materials cycle
The materials cycle follows resources through extraction, processing, manufacture, use and the available end-of-life routes.
Recycling returns recovered metal to processing, while reuse retains a whole component in service.
Materials documentation
Materials documentation checks the practical evidence needed to judge shortlisted grades, processing routes and actual service behavior.
A promising chart candidate still needs joining, supply-form and environmental-resistance checks.
Materials screening
Materials screening removes candidates that fail mandatory property or service limits before the surviving options are ranked.
A maximum-temperature limit eliminates a polymer that softens too much at the required service temperature.
Mechanical recycling
Mechanical recycling recovers material through physical sorting and reprocessing without intentionally returning it to molecular feedstocks.
Clean thermoplastic scrap can be granulated, melted and molded into a new product.
Mixed potential
A mixed potential is the freely corroding electrode potential at which the total anodic and cathodic currents balance.
The intersection of the two polarization curves identifies both corrosion potential and current density.

N

Near-net-shape processing
Near-net-shape processing makes a part close to its final geometry, reducing later machining and the amount of discarded material.
A suitable forging route can reduce costly titanium removal compared with machining from a large billet.
Nernst equation
The Nernst equation relates equilibrium electrode or cell potential to temperature and the activities of reacting species.
Raising the product-to-reactant ion ratio reduces the driving voltage for a metal reaction.
Noble coating
A noble coating is a metallic layer less active than the substrate that protects mainly by remaining intact as a physical barrier.
A scratch through tin can expose a small steel anode beside a much larger cathodic tin surface.
Noble metal behavior
Noble behavior means a relatively positive potential and a lower tendency to supply anodic dissolution current within a given comparison.
Passive titanium lies toward the noble end of a seawater series despite its negative standard potential.

O

Oxide scale
An oxide scale is a solid reaction layer produced when oxygen reacts with a metal surface, commonly during high-temperature exposure.
A furnace alloy relies on a compact attached scale to slow further contact between oxygen and metal.
Oxygen scavenger
An oxygen scavenger is a chemical that removes dissolved oxygen, reducing its availability for cathodic reduction in a water system.
Sodium sulfite treatment can reduce oxygen-driven steel corrosion in suitable boiler-water service.

P

Parabolic oxidation
Parabolic oxidation is scale growth in which squared mass gain per area varies linearly with time, as transport slows through the layer.
Under zero-intercept parabolic growth, a ninefold exposure gives a threefold mass gain.
Pareto front
A Pareto front is the set of feasible choices where improving one objective requires worsening another, so none is dominated.
An aircraft designer chooses among mass–cost compromises according to the value of saving mass.
Passivity
Passivity is a low-reactivity state maintained by a protective surface film.
A chromium-rich film lets stainless steel maintain a low corrosion rate in a compatible environment.
Performance index
A performance index is a combination of material properties derived from a design objective and its constraints for ranking candidates.
A stiffness-limited tie's index follows by eliminating area between the tie's mass and stiffness equations.
Pilling–Bedworth ratio
The Pilling–Bedworth ratio compares the volume of oxide formed with the volume of metal consumed to make that oxide.
Al₂O₃ needs a metal coefficient of two when the oxide and metal molar volumes are compared.
Pitting corrosion
Pitting corrosion is concentrated attack that creates deep local holes in a surface.
A tank wall can leak from one pit even while coupon mass loss suggests only slight average thinning.
Pitting resistance equivalent number
A pitting resistance equivalent number is a composition-based index for comparing relative pitting resistance of stainless steels.
Adding molybdenum raises PREN, but a service-temperature and crevice check is still needed.
Plasticization
Plasticization is increased polymer-chain mobility caused by a small-molecule additive or absorbed liquid, lowering stiffness and glass transition.
Moisture-conditioned nylon can be more flexible and tougher than the same grade tested dry.
Polarization
Polarization is the shift of an electrode's potential from its equilibrium value when a net electrochemical current flows.
A potential–current plot shows how the steel and oxygen reactions respond as their currents change.
Present value
A present value is a future payment expressed as an equivalent amount today.
A repair due in 15 years contributes less than its face amount to a positive-rate present-cost total.
Property envelope
A property envelope is the chart region enclosing the range of values associated with a material class or group of candidates.
The polymer envelope spans grades whose stiffness depends strongly on structure and temperature.

R

Recycled content
Recycled content is the fraction of recovered feedstock used in a new product.
A sheet can contain recycled aluminum even if the finished product is poorly collected at end of life.

S

Sacrificial coating
A sacrificial coating is a metallic layer more active than its substrate, so it corrodes preferentially and can protect exposed defects.
Zinc surrounding a wet scratch supplies electrons that make the exposed steel cathodic.
Second moment of area
The second moment of area describes the distribution of cross-sectional area about a bending axis and controls elastic bending stiffness.
For a square section, increasing area also increases its distance from the bending axis.
Selection line
A selection line joins property combinations with equal performance index and can be shifted in parallel to seek a higher index.
On log modulus versus log density axes, a slope-2 line represents constant square-root modulus divided by density.
Selective leaching
Selective leaching removes one alloy constituent preferentially by dissolution.
Dezincified brass can turn reddish as zinc is removed and a weak copper-rich skeleton remains.
Sensitization
Sensitization is a microstructural change that makes an alloy susceptible to intergranular attack, as chromium carbides deplete nearby steel.
An austenitic stainless weld heat-affected zone can become sensitized after time at elevated temperature.
Spalling
Spalling is cracking and detachment of a surface layer such as oxide scale.
Repeated heating and cooling can detach scale and expose fresh metal to the furnace gas.
Specific stiffness
Specific stiffness is Young’s modulus divided by density.
Steel and aluminum have similar specific stiffness despite their very different moduli and densities.
Specific strength
Specific strength is the relevant failure strength divided by density.
A strong lightweight tie benefits from high allowable strength relative to its material density.
Standard electrode potential
A standard electrode potential is a half-cell reduction voltage relative to the standard hydrogen electrode under standard conditions.
The Fe²⁺/Fe value of about −0.44 V helps predict iron oxidation when coupled to copper.
Standard hydrogen electrode
The standard hydrogen electrode is the reference half-cell assigned zero potential for reporting standard electrode voltages.
Two tabulated metal potentials must use the same reference before their difference is calculated.
Stiffness-limited design
A stiffness-limited design is sized by the deformation or deflection requirement, which determines the minimum dimensions in the model.
A panel can need extra thickness to meet a deflection limit even when its strength is sufficient.
Strength-limited design
A strength-limited design is sized so the stress does not exceed the adopted failure or allowable strength under the specified loading.
The minimum area of a tensile tie follows from its load divided by the allowable strength.
Stress corrosion cracking
Stress corrosion cracking is crack growth caused by tensile stress acting with an environment to which the particular alloy is susceptible.
Residual stress can help warm chloride solution crack an austenitic stainless component below yield.
Subcritical crack growth
Subcritical crack growth is slow extension of a crack under conditions below those needed for immediate unstable fracture.
Moisture at a loaded glass crack tip can let the flaw grow until the part fails under constant load.
Swelling
Swelling is enlargement of a polymer through absorption of a liquid.
A fuel-exposed rubber seal can become oversized and soft even though it remains one connected piece.

T

Tooling cost
Tooling cost is the fixed expense of molds, dies or similar production equipment that is allocated across the parts it makes.
A large production run spreads an injection mold's fixed cost over many more finished housings.

U

Ultraviolet absorber
An ultraviolet absorber is an additive that absorbs damaging UV radiation and reduces the light available to initiate polymer degradation.
An outdoor transparent component may use UV absorbers to extend its useful exposure life.
Uniform corrosion
Uniform corrosion removes thickness at a similar rate over most exposed surfaces.
Measured thinning of a steel wall can be used to plan an inspection interval and corrosion allowance.

W

Weathering
Weathering is outdoor degradation caused by the combined action of light, oxygen, moisture, temperature changes and pollutants.
Yellowing, chalking and surface cracks can appear together on an unstabilized outdoor plastic cover.
Weathering steel
Weathering steel is a low-alloy steel that develops an adherent rust layer under suitable outdoor wet–dry exposure conditions.
A bridge detail that traps salt water may perform poorly even when the open faces weather well.
Weld decay
Weld decay is intergranular corrosion in a sensitized band near a stainless steel weld after exposure to a suitable corrosive environment.
Choosing a low-carbon grade can reduce carbide precipitation in a welded stainless assembly.

About this lesson

By StudeliReport a mistake

Make your own Study Materials

Turn your notes, slides and documents into Study Guides, Practice Questions, Flashcards and 6 more tools.

Get Started