Heat Treatment of Metals: Phase Transformations

Learn how heat treatment controls the structure and properties of metals. Start with how new phases nucleate and grow over time, then follow austenite as it becomes pearlite, bainite or martensite. Use TTT and CCT diagrams to predict microstructures, choose annealing, normalizing, hardening and tempering treatments for steels, and strengthen aluminum and other alloys by precipitation hardening. Finish by classifying steels, cast irons and nonferrous alloys and decoding their designations, including AISI/SAE, UNS, EN and aluminum temper codes.

IntermediateLesson 7 of 9 in Materials Science and Engineering Course

What you will learn

  1. Describe how a new phase nucleates and grows, why the rate of a transformation depends on temperature, and calculate how far a transformation has progressed with the Avrami equation.
    • Explain nucleation and growth of a new phase
      Relate the driving force, the interface energy and diffusion to the critical nucleus size, and explain why new phases usually start at grain boundaries and other defects.
    • Describe transformation progress with the Avrami equation
      Use the S-shaped fraction-transformed curve, the Avrami equation and the reaction rate to calculate how far and how fast a transformation proceeds, and explain why heat treatments produce metastable structures.
  2. Explain how pearlite, bainite, spheroidite and martensite form in iron–carbon alloys, what each looks like, and how its structure controls hardness, strength and ductility.
    • Explain pearlite and proeutectoid phases
      Describe how pearlite and proeutectoid ferrite or cementite form on slow cooling, calculate their fractions with the lever rule, and explain coarse and fine pearlite.
    • Explain bainite and spheroidite
      Describe how bainite forms below the pearlite range and how spheroidite forms on long heating below the eutectoid temperature, and compare their structures and properties.
    • Explain how martensite forms and why it is hard
      Describe the diffusionless martensitic transformation, the structure of martensite and its start and finish temperatures, and explain why its hardness depends mainly on carbon content.
    • Compare the mechanical properties of steel microstructures
      Rank pearlite, bainite, spheroidite, martensite and tempered martensite by hardness, strength and ductility, explain the ranking from their structures, and match a structure to a service need.
  3. Read isothermal transformation (TTT) and continuous cooling transformation (CCT) diagrams, follow heat-treatment paths on them, and predict the resulting microstructures and their fractions.
    • Read an isothermal transformation (TTT) diagram
      Identify the curves, regions and lines of a time–temperature–transformation diagram and explain how composition and alloying change its shape.
    • Follow heat-treatment paths on a TTT diagram
      Trace isothermal and multistep cooling paths, determine which products form and in what fractions, and explain what happens to austenite that has not yet transformed.
    • Use CCT diagrams and critical cooling rates
      Read continuous cooling transformation diagrams with cooling curves, define the critical cooling rate, and predict the microstructure produced by a given cooling rate or position in a part.
  4. Choose and explain annealing, normalizing, hardening and tempering treatments for steels, including their temperatures, cooling methods and the microstructures and properties they produce.
    • Choose an annealing treatment
      Use the critical temperatures to distinguish process annealing, stress relief, full annealing and spheroidizing, and choose the right treatment for a part.
    • Use normalizing to refine the grain structure
      Explain how normalizing refines and evens out the microstructure of steels and compare normalized and fully annealed steels.
    • Harden steel by quenching and judge hardenability
      Explain how austenitizing and quenching produce martensite, distinguish hardness from hardenability, use Jominy end-quench data to compare steels, and reduce distortion and cracking.
    • Temper martensite and use interrupted quenches
      Choose a tempering temperature to balance strength and toughness, avoid the embrittlement ranges, and use martempering and austempering to reduce distortion.
  5. Explain which alloys can be precipitation hardened, carry out the solution treatment, quench and aging steps, and interpret aging curves to choose aging conditions.
    • Identify hardenable alloys and the heat-treatment steps
      Use the phase diagram to decide whether an alloy can be precipitation hardened, and describe the solution treatment, quench and aging steps with their temperatures.
    • Explain the precipitation mechanism and aging curves
      Describe the sequence of precipitates that forms during aging, explain why strength peaks and then falls, and use aging curves to choose an aging temperature and time.
  6. Classify ferrous and nonferrous alloys by composition, structure and use, and decode the common designation systems for steels and aluminum alloys.
    • Classify steels and cast irons
      Distinguish plain-carbon, low-alloy, tool and stainless steels and the main types of cast iron, and relate their composition and structure to typical uses.
    • Read steel designations
      Decode AISI/SAE, UNS and EN steel designations to find the steel family, carbon content and main alloying elements, and compare grades across the systems.
    • Classify nonferrous alloys and read aluminum designations
      Describe the main nonferrous alloy families and their uses, and decode aluminum alloy and temper designations, including the heat-treatable series.

Heat Treatment of Metals study guide

6 chapters

1

How phase transformations proceed over time

Heat treatment changes more than temperature: atoms must find a new arrangement, and that rearrangement takes time. Follow the energy balance that allows a nucleus to survive, then connect atom mobility with growth. Quantify the resulting transformation curve with the Avrami equation and compare half-times at different temperatures. These ideas explain why rapid processing can preserve a structure that an equilibrium diagram would not predict.

1.1 Why new phases need nuclei and time

A new phase needs a way to start and a way to spread. These are nucleation and growth. Their different temperature responses explain why cooling faster can make a finer structure or prevent a diffusion-dependent transformation altogether.

The energy cost of starting

Below an equilibrium transformation temperature, forming the new phase lowers the volume free energy. Write this change per volume as ΔGv<0. Creating the boundary around a new particle costs interface energy, γ per area. For a spherical particle,

ΔG=43πr3ΔGv+4πr2γ.

The positive surface term dominates for a tiny cluster. As the radius grows, the negative volume term eventually wins. The energy curve therefore has a maximum:

r∗=−2γΔGv,ΔG∗=16πγ33(ΔGv)2.

An embryo smaller than the critical radius tends to dissolve. A nucleus larger than it lowers free energy by growing. Crossing the equilibrium temperature alone does not remove this barrier.

Calculate a critical radius

For homogeneous solidification of copper, take the solidification enthalpy change as −1.77 × 10⁹ J/m³, interface energy as 0.177 J/m², melting point as 1085 °C (1358 K), and undercooling as 236 K. First find the volume driving force:

ΔGv=ΔHfΔTTm=(−1.77×109)(236)1358≈−3.08×108 J/m3.

Then r∗=2(0.177)/(3.08×108)≈1.15×10−9 m, or 1.15 nm. Substitution in the barrier formula gives about 9.8 × 10⁻¹⁹ J. A sphere of this radius contains roughly 540 atoms when the copper FCC cell edge is 0.3615 nm and each cell contains four atoms. Halving the undercooling halves the driving-force magnitude, doubles the critical radius, and quadruples the barrier.

Why boundaries are good starting sites

In heterogeneous nucleation, a grain boundary, inclusion, dislocation, or mold wall supplies an existing interface. Less new interface must be created, so the barrier is smaller. In the spherical-cap model,

ΔGhet∗=S(θ)ΔGhom∗,S(θ)=(2+cos⁡θ)(1−cos⁡θ)24.

The factor lies between zero and one; the critical radius stays the same. Ferrite and pearlite commonly begin at austenite grain boundaries. Grain refiners in a casting provide additional starting sites.

Why the fastest transformation occurs in the middle

More undercooling increases the thermodynamic driving force. At the same time, lower temperature slows atom transport: D=D0exp⁡(−Qd/RT), with temperature in kelvin. Near equilibrium, limited nucleation slows the transformation; far below it, limited diffusion slows growth. An intermediate temperature gives the fastest overall reaction and the nose of a TTT curve.

At small undercooling, relatively few nuclei and long diffusion distances produce coarse structures. Greater undercooling gives more nuclei and shorter distances, producing finer structures. Diffusion-dependent transformations include solidification, recrystallization, grain growth, and austenite decomposition. Martensite uses coordinated atom shifts without long-range diffusion, so its kinetics must be treated separately.

Key Takeaways

  • A stable nucleus must exceed the critical radius.
  • The interface costs energy; the new phase supplies a negative volume-energy change.
  • Heterogeneous nucleation lowers the barrier without changing the critical radius in the cap model.
  • Driving force and atom mobility together control transformation speed.
  • Greater undercooling commonly produces a finer diffusion-formed structure.

1.2 Calculate transformation progress

A transformation has a history: little changes at first, conversion accelerates, and then the remaining parent material becomes harder to reach. At a fixed temperature, the fraction transformed forms an S-shaped curve, often plotted against logarithmic time.

Use the Avrami equation
y=1−exp⁡(−ktn).

Here y is the transformed fraction from zero to one, t is elapsed time, and k and n describe this reaction at this temperature. The exponent commonly lies around 1–4. If time is in seconds, the units of k are s−n, making the exponent dimensionless. The curve levels off when growing particles meet and untransformed regions shrink.

Suppose 40% has transformed after 60 s and n=2. Use the fraction 0.40, leaving an untransformed fraction of 0.60:

k=−ln⁡(1−y)tn=−ln⁡0.60602≈1.42×10−4 s−2.

To find the time for a chosen fraction, rearrange:

t=[−ln⁡(1−y)k]1/n.

For 95%, use −ln⁡0.05=ln⁡20. The time is about 145 s. After 120 s, direct substitution gives about 0.87, or 87% transformed. Doubling the time does not simply double the fraction.

Define the transformation rate

The conventional rate is the reciprocal of the half-transformation time:

t0.5=(ln⁡2k)1/n,r=1t0.5.

For the example, the half-time is about 70 s and the rate is about 0.014 s⁻¹. This rate characterizes the whole reaction. It is different from the changing slope of the fraction–time curve.

Measured data can determine both constants. Rearrange into the straight-line form

ln⁡[−ln⁡(1−y)]=ln⁡k+nln⁡t.

The slope is n and the vertical intercept is ln⁡k. Two data points are the minimum for determining two constants; more points help test the fit.

Connect time with temperature

For a diffusion-controlled process such as recrystallization, the rate often follows r=Aexp⁡(−Q/RT). Comparing two temperatures removes the unknown prefactor:

ln⁡(r2/r1)=QR(1T1−1T2).

If the half-time falls from 100 min at 100 °C to 10 min at 130 °C, the rate increases tenfold. Convert to 373.15 and 403.15 K before substituting; with R=8.314 J/(mol·K), the activation energy is about 96 kJ/mol. The corresponding half-time at 115 °C is about 30 min. Using Celsius inside the reciprocal-temperature terms gives the wrong result.

This increasing-rate Arrhenius relation describes a diffusion-controlled regime. Undercooled austenite also faces a nucleation barrier, so its overall rate rises and then falls as cooling proceeds. Real heating and cooling therefore lag the equilibrium diagram: transformations require superheating or undercooling and time. Heat treatment deliberately retains nonequilibrium states, including martensite and supersaturated solutions, because slow room-temperature diffusion prevents rapid relaxation.

Key Takeaways

  • Use fractions, not percentages, in the Avrami equation.
  • The units of k depend on n and the chosen time unit.
  • The conventional rate is the reciprocal half-time.
  • The linearized Avrami plot gives n from slope and ln k from intercept.
  • Arrhenius calculations require kelvin.
  • A phase diagram does not specify how quickly equilibrium is reached.
2

The microstructures that form from austenite

Austenite can form layers, fine particles, or a carbon-trapping distorted lattice. Learn how pearlite, bainite, spheroidite, and martensite develop, and connect their appearance with hardness and ductility. Use the lever rule to distinguish phases from microconstituents, then choose a structure for a cutting edge, a loaded shaft, or a bar that must be machined. Composition and thermal history must be considered together.

2.1 Pearlite and the phase that forms first

Slowly cooled austenite forms ferrite and cementite, but those phases can be arranged in different microconstituents. Distinguishing phase fractions from microconstituent fractions is essential when using the lever rule.

What pearlite contains

At 727 °C, austenite containing 0.76 wt% C undergoes the eutectoid reaction:

γ→α+Fe3C.

Austenite is FCC; ferrite is BCC and holds at most 0.022 wt% C at this temperature. Cementite contains 6.70 wt% C. Austenite can dissolve up to 2.14 wt% C at its maximum solubility. Pearlite is the layered product of the eutectoid reaction. Ferrite and cementite grow together, with carbon moving from the ferrite into the cementite. Pearlite is a microconstituent containing two phases, not a separate phase.

Within eutectoid pearlite, the ferrite fraction is

Wα=6.70−0.766.70−0.022≈0.89.

The balance, about 0.11, is cementite. Ferrite layers are therefore much thicker than cementite layers.

Carbon below the eutectoid composition

In a hypoeutectoid steel, between 0.022 and 0.76 wt% C, ferrite forms before the eutectoid reaction. This proeutectoid ferrite starts at austenite boundaries between A3 and A1. Its low carbon content leaves the remaining austenite richer in carbon. At A1, that remaining austenite reaches the eutectoid composition and becomes pearlite.

For a 0.40 wt% C steel just below A1, use the tie-line ends 0.022 and 0.76 to find microconstituents:

WP=0.40−0.0220.76−0.022≈0.51,Wα,pro=1−WP≈0.49.

To find total cementite, use the phase endpoints instead:

WFe3C=0.40−0.0226.70−0.022≈0.057.

The steel is about 51% pearlite but only 5.7% cementite. Total ferrite includes both proeutectoid ferrite and ferrite inside pearlite.

Carbon above the eutectoid composition

A hypereutectoid steel, above 0.76 and up to 2.14 wt% C, first forms proeutectoid cementite between Acm and A1. For 1.00 wt% C,

WFe3C,pro=1.00−0.766.70−0.76≈0.040.

The remaining 96% becomes pearlite. Slow cooling can form a brittle cementite network along the old grain boundaries. Normalizing or spheroidizing changes this unfavorable arrangement.

Layer spacing changes properties

Just below A1, carbon can diffuse relatively far and coarse pearlite forms. At lower temperatures in the pearlite range, down to about 540 °C, thinner layers form. Fine pearlite has more ferrite–cementite boundary area per volume, obstructs dislocations more strongly, and is harder and stronger but less ductile.

Increasing carbon raises the total cementite fraction. The pearlite fraction rises only up to the eutectoid composition; above it, increasing proeutectoid cementite reduces the pearlite fraction. Faster cooling also reduces the amount of proeutectoid phase and refines pearlite, so equilibrium lever-rule fractions apply to slow cooling, not every heat-treated steel.

Key Takeaways

  • Pearlite contains ferrite and cementite, about 89% and 11% by mass.
  • Proeutectoid ferrite forms below the eutectoid composition; proeutectoid cementite forms above it.
  • Choose lever-rule endpoints for the quantity requested.
  • Fine pearlite is harder than coarse pearlite at the same carbon content.
  • Pearlite reaches its maximum fraction at the eutectoid composition.

2.2 Bainite particles and spheroidite spheres

Ferrite and cementite do not have to form layers. Their shape, size, and placement explain why bainite can be strong while spheroidite is easy to machine, even though both contain the same two phases.

Form bainite from austenite

Bainite forms below the pearlite range and above the martensite start temperature. For the plain eutectoid steel considered here, this is roughly 540–220 °C. The overall reaction involves carbon redistribution and takes time, so a TTT diagram shows start and finish curves. The product is not fine lamellar pearlite.

ProductTypical formation rangeCarbide arrangement
Upper bainiteAbout 300–540 °CParticles between ferrite laths
Lower bainiteBelow about 300 °C, above MsVery fine particles within ferrite plates

Upper bainite often looks feathery in an optical microscope; lower bainite looks dark and needle-like. Resolving the fine carbide arrangement needs an electron microscope. The range boundaries depend on the steel, so use its transformation diagram to identify the product.

The small particle spacing makes bainite stronger and harder than pearlite of the same carbon content while retaining useful ductility. Lower bainite is generally tougher than upper bainite. Austempering produces bainite by avoiding the pearlite nose and holding in the bainite range until transformation is complete.

Follow the parent austenite

Pearlite and bainite compete for the austenite still available. In plain-carbon steel their TTT regions may join around one nose; alloy steels often show separate pearlite and bainite noses. If a hold converts all the austenite to pearlite, later cooling into the bainite range does not create bainite from that pearlite. A new pearlite-to-bainite treatment first needs austenite again.

For example, after a complete pearlite hold, moving the specimen to 400 °C leaves a pearlitic structure. Starting instead with austenite, cooling rapidly to 400 °C, and holding past the bainite finish time produces upper bainite. The starting structure changes what the hold can accomplish.

Round the cementite into spheroidite

Holding pearlite or bainite just below A1, around 700 °C, for many hours allows carbon to diffuse and cementite to change shape. Roughly spherical particles in a continuous ferrite matrix form spheroidite. A typical treatment takes about 15–25 h.

Spheres reduce ferrite–cementite boundary area and therefore lower interface energy. The widely spaced particles leave long paths through soft ferrite for dislocation motion. Among the ferrite–cementite structures, spheroidite is the softest and most ductile, making it useful before machining or cold forming high-carbon bearing and tool steels. The part can be austenitized and hardened after shaping.

A high-carbon bar with a brittle grain-boundary cementite network benefits from a treatment that breaks up that arrangement. Holding above A1 for the entire cycle instead creates austenite; a long subcritical hold promotes spheroidization. Some spheroidizing cycles briefly cross A1, but their soft final structure is still ferrite with rounded cementite particles.

Key Takeaways

  • Bainite has ferrite and carbide particles, not alternating lamellae.
  • Upper and lower bainite differ in where their carbides form.
  • A bainite hold transforms available austenite, not previously formed pearlite.
  • Spheroidizing lowers interface area and makes high-carbon steel easier to shape.

2.3 Martensite traps carbon during a rapid change

Quenching can carry austenite past the pearlite and bainite regions before they have time to form. Below Ms, the martensite start temperature, austenite can change by coordinated atom shifts instead of long-range diffusion.

A diffusionless change

Atoms move together over distances smaller than an interatomic spacing. Carbon remains trapped at the concentration present in the parent austenite. The FCC lattice changes into a carbon-supersaturated, body-centered tetragonal (BCT) lattice, stretched along one cell direction. More carbon increases this distortion.

Martensite is metastable and does not appear as an equilibrium phase on the iron–iron carbide diagram. On reheating below A1, carbon can diffuse out and carbides can form: this is the basis of tempering. The original martensite is hard because trapped carbon, lattice strain, a fine substructure, and a high dislocation density all impede dislocation motion.

Temperature controls the amount

The usual steel martensite transformation is athermal. Individual laths or plates form almost immediately, and further conversion follows a further drop in temperature. Waiting at a fixed temperature between Ms and Mf does not progressively complete the martensite transformation.

A diagram may mark Ms, M50, M90, and Mf, meaning start, 50%, 90%, and finish. If Ms is 220 °C and M50 is 150 °C, stopping at 180 °C produces less than half martensite. A longer hold there does not make it 50%. Cooling farther produces more.

High-carbon steels can have Mf below room temperature. A quench then leaves retained austenite, which can reduce hardness and later change dimensions if it transforms. Sub-zero treatment or suitable tempering reduces this retained fraction.

Estimate Ms from composition

For low-alloy steels within its fitted range, up to about 0.6 wt% C, the empirical Andrews relation is

Ms=539−423C−30.4Mn−17.7Ni−12.1Cr−7.5Mo.

The result is in °C and each element content is in wt%. For 0.45 wt% C and 0.75 wt% Mn, with the other terms zero,

Ms=539−423(0.45)−30.4(0.75)≈326 ∘C.

Carbon and most alloy additions lower Ms. Do not enter 45 for 0.45 wt% C or use this low-alloy fit as a universal alloy equation.

Separate carbon hardness from hardening depth

Low- and medium-carbon steels usually form lath martensite; above about 1 wt% C, plates predominate. Intermediate compositions can contain both. Representative fully martensitic hardnesses are about 44 HRC at 0.2 wt% C, 56 HRC at 0.4 wt% C, and 64–65 HRC around 0.6–0.8 wt% C.

Alloy additions mainly make it easier to form martensite throughout a section; carbon mainly sets the maximum as-quenched hardness. The transformation also expands the steel by a few percent. Surface and center transform at different times, creating large internal stresses and possible cracks. As-quenched steel is therefore normally tempered before service.

Key Takeaways

  • Martensite forms without long-range diffusion and retains its parent composition.
  • Steel martensite is carbon-supersaturated and commonly BCT.
  • Cooling farther below Ms increases martensite; waiting alone does not.
  • Carbon largely sets maximum hardness; alloying largely controls hardening depth.
  • Retained austenite remains when cooling stops before transformation is complete.
  • Quench stresses and brittleness make tempering necessary for most uses.

2.4 Match a microstructure to the property needed

Two pieces of steel with the same composition can behave very differently after different heat treatments. Their microstructures control how dislocations move and how cracks start and spread.

Compare structures at equal carbon content

A typical hardness and strength ranking is martensite, tempered martensite, bainite, fine pearlite, coarse pearlite, and spheroidite. Tempered martensite moves within this ranking as its tempering temperature changes. Ductility generally increases toward the softer end; toughness also depends on particle shape and crack paths.

StructureMain obstacle to deformationUseful property
MartensiteTrapped carbon, strained lattice, fine substructureVery high hardness
Tempered martensiteFine carbides in ferriteStrength with toughness
BainiteFine ferrite and carbide arrangementStrength with useful ductility
Fine pearliteClosely spaced lamellar boundariesGreater strength than coarse pearlite
SpheroiditeWidely spaced rounded carbidesEasy machining and forming

Fine pearlite has more interface area than coarse pearlite, so a moving dislocation meets obstacles more often. Bainite contains a finer particle arrangement. Spheroidite has relatively little interface area and a continuous soft ferrite matrix. These observations connect a microscope image to a property prediction.

Carbon and heat treatment act together

Carbon changes both the amount and the nature of strengthening. In hypoeutectoid steels, more carbon gives more pearlite on slow cooling. In bainite and spheroidite, it increases the cementite fraction. The cementite fraction inside eutectoid pearlite itself stays about 11 wt%.

Carbon also raises martensite hardness. A fully martensitic 0.2 wt% C steel can be about 20 HRC softer than a fully martensitic 0.8 wt% C steel. A claim that one named structure is harder than another therefore needs a fair comparison of composition and treatment.

Choose for service

A cutting edge needs wear resistance, so hard martensite with a low-temperature temper is useful. A heavily loaded shaft or bolt must also tolerate stress concentrations and shocks; quenching and a higher-temperature temper provide a better strength–toughness balance. A high-carbon bar waiting to be machined benefits from spheroidite. A general structural part with moderate demands can use normalized ferrite–pearlite.

At equal hardness, tempered martensite is usually tougher than pearlite. Its fine, rounded carbides in ferrite interrupt crack paths more effectively than continuous cementite layers. Hardness alone therefore cannot determine whether two conditions are interchangeable.

Estimate tensile strength from Brinell hardness

For many steels, a useful approximate relation is

TS (MPa)≈3.45HB.

A 300 HB part gives 3.45(300)=1035 MPa, while 170 HB gives about 590 MPa. This is an estimate based on Brinell hardness, not a formula into which HRC can be inserted. It also does not supply yield strength, toughness, or a complete service rating.

Key Takeaways

  • Compare hardness rankings at the same carbon content.
  • Fine interfaces and small particle spacing impede dislocations.
  • Tempered martensite often gives better toughness than pearlite at equal hardness.
  • Select adequate hardness together with the toughness the service needs.
3

Microstructures with ttt and cct diagrams

Transformation diagrams turn a thermal history into a microstructure prediction. Read start, half, and finish curves on logarithmic time axes, then follow the austenite through single and multiple holds. Switch to a continuous cooling diagram when temperature keeps changing. Comparing paths through the surface and center of a part shows why a single quench can give different structures at different depths.

3.1 Read the curves on a TTT diagram

A phase diagram tells you which phases are favored at equilibrium. A TTT diagram adds the time needed for austenite to transform during a constant-temperature hold. It belongs to one composition and one austenitizing condition.

Read temperature and logarithmic time

Temperature is on the vertical axis and time on the horizontal axis. Equal horizontal distances usually represent tenfold time increases: 1, 10, 100, and 1000 s. Halfway between 10 and 100 s on this axis is about 32 s, not 55 s.

To obtain the diagram experimentally, austenitized samples are rapidly cooled to chosen temperatures and held. Fraction-transformed measurements supply a start time, often at about 1%, and a finish time, often at about 99%. A middle curve may mark 50%.

At a chosen temperature, the region before the start curve is still austenite. Between start and finish, austenite coexists with the product. Past finish, the diffusion-dependent transformation is practically complete. Below A1, austenite before the start curve is present because kinetics have delayed its decomposition, not because it is the equilibrium structure.

Identify the product and the nose

For a plain eutectoid steel, the upper part of the C-curve gives pearlite. Higher transformation temperatures give coarser layers. Below the nose, the product is bainite. The nose, around 540 °C in this example, has the shortest start time. A rapid quench must pass this vulnerable region before the reaction starts.

Horizontal Ms and M50 lines have a different meaning from the C-curves. Martensite forms as temperature falls below these thresholds; its fraction does not grow simply because the path extends farther right.

Practice with one example data set

These rounded example times describe holds after rapid transfer:

TemperatureStart50%FinishProduct
700 °C10 s30 s100 sPearlite
650 °C2 s6 s20 sPearlite
540 °C1 s—6 sNose region
400 °C4 s20 s80 sBainite
300 °C60 s300 s1000 sBainite

Take Ms as 220 °C and M50 as 150 °C. A 20 s hold at 400 °C reaches the 50% curve, leaving half austenite and half bainite before further cooling. A 20 s hold at 300 °C has not yet reached the start curve. Equal hold durations can therefore give very different structures.

Check what changed before reusing a diagram

Hypoeutectoid and hypereutectoid steels add proeutectoid ferrite or cementite curves. Cr, Mo, Ni, and Mn commonly delay diffusional transformations, moving the curves right. Many alloy steels have separate pearlite and bainite noses. Coarser austenite grains also delay transformation because fewer boundaries provide nucleation sites.

A continuous cooling path needs a CCT diagram. Drawing that path on a TTT diagram neglects the changing-temperature history and generally predicts transformation too early and too hot.

Key Takeaways

  • Read each hold at a constant temperature on a logarithmic time axis.
  • Start, half, and finish curves track how much austenite has transformed.
  • The shortest start time lies at the nose.
  • Composition and austenitizing conditions determine which diagram applies.
  • Ms and fraction lines describe cooling-controlled martensite formation.

3.2 Keep track of austenite through each hold

A multistep path is a material balance. At every stage, record how much austenite remains and what has already formed. A later quench acts on that remaining austenite.

Trace a path in order
  1. Begin in the fully austenitic field.
  2. Follow each rapid transfer downward. In an idealized TTT problem, no transformation occurs during this transfer.
  3. Follow each hold horizontally and compare its duration with the start, half, and finish curves at that temperature.
  4. Record the new product and the austenite left.
  5. Follow the final quench. Cooling below Mf converts the remaining austenite to martensite; stopping between Ms and Mf leaves some austenite.

Count an isothermal hold from arrival at its temperature. Different holds have different kinetics; their durations cannot simply be added and compared with a finish time at one temperature.

Finish one transformation

Use the rounded example data: at 650 °C, pearlite starts at 2 s, is half formed at 6 s, and finishes at 20 s. A rapid transfer to 650 °C followed by 30 s gives complete pearlite. The final quench produces no martensite because no austenite remains available.

At 400 °C, bainite finishes at 80 s. A 200 s hold therefore gives complete upper bainite. At 300 °C, bainite does not start until 60 s, so a 10 s hold leaves all the austenite for the final quench. Cooling sufficiently low then gives martensite, with any retained austenite determined by the final temperature.

Make two products deliberately

Hold at 650 °C for 6 s, reaching 50% pearlite. The state immediately before quenching is 50% pearlite and 50% austenite. A final quench below Mf changes the second half into martensite:

0.50P+0.50A→0.50P+0.50M.

Pearlite is already ferrite and cementite. Cooling it faster does not convert it into martensite.

Now change the second stage: after that same 6 s pearlite hold, transfer rapidly to 400 °C and hold long enough to complete the transformation of the remaining austenite. In this example, 200 s is beyond the 80 s finish time. The final balance is 50% pearlite and 50% bainite. There is no austenite left for the final quench to harden.

If an exercise gives the fraction of remaining austenite transformed during a later stage, multiply it by the fraction that remains. For example, 50% of a remaining 50% is 25% of the original specimen. Keep each fraction's denominator explicit.

Stop inside the martensite range

With Ms at 220 °C and M50 at 150 °C, a direct quench to 180 °C makes less than half martensite. Extending the hold does not increase that fraction: martensite is athermal. Cooling farther increases it. Exact fractions require a martensite-fraction relation or marked lines; two temperature labels alone do not justify linear interpolation between them.

A useful final check is that all product fractions and retained austenite add to one. Also check that every product had parent austenite available at the stage where it formed.

Key Takeaways

  • Only austenite still present can form martensite on the final quench.
  • A finished pearlite or bainite product persists during later cooling.
  • Track fractions relative to the whole specimen and to remaining austenite separately.
  • A fixed-temperature martensite hold does not progressively complete the reaction.

3.3 Predict products during continuous cooling

Most parts cool through a range of temperatures. A continuous cooling transformation (CCT) diagram accounts for this changing thermal history and is the appropriate diagram for furnace cooling, air cooling, and quenching.

Follow the cooling curve

Start at the austenitizing temperature and follow the curve downward. Mark the crossing of each transformation-start and transformation-finish boundary. At high temperatures, pearlite can form; an alloy steel may also form bainite at intermediate temperatures. Austenite that survives to Ms begins forming martensite.

For the same steel, CCT transformation boundaries generally occur at longer times and lower temperatures than the isothermal boundaries. During cooling, the specimen does not spend its whole elapsed time at its current temperature. A TTT start time therefore cannot be treated as a universal countdown during a continuous quench.

In the introductory plain-carbon eutectoid CCT diagram, the products are pearlite, martensite, or a mixture. Pearlite formation stops before bainite develops during continuous cooling. Many alloy steels, including Ni–Cr–Mo steels, have a bainite region accessible on continuous cooling. Read the actual steel's diagram before predicting bainite.

Use the critical cooling rate

The critical cooling rate is the slowest cooling rate that avoids the diffusion-dependent start curves and allows a fully martensitic result on sufficiently deep cooling. Its path just misses the controlling nose.

For the textbook plain-eutectoid example, the critical rate is about 140 °C/s. Below about 35 °C/s the result is pearlitic; between these values it is pearlite plus martensite. These numbers describe that example diagram, not all carbon steels.

Example cooling ratePredicted product
1 °C/sCoarse pearlite
20 °C/sFine pearlite
60 °C/sFine pearlite plus martensite
200 °C/sMartensite on sufficiently deep cooling

An alloy such as 4340 has a much lower example critical rate, about 8 °C/s. Its delayed pearlite and bainite reactions permit hardening with a less severe quench or in a thicker section.

Compare the surface with the center

Heat leaves a part through its surface. The surface normally cools faster than the center, and a thick part cools more slowly than a thin one. Each position therefore has its own path on the CCT diagram.

A plain-carbon bar can develop a martensitic surface while the center becomes pearlitic. The surface hardness alone cannot prove that the center hardened. Increasing hardenability moves diffusion-controlled transformation curves right and makes through-hardening possible at the slower center rate.

Real quench curves are not straight constant-rate paths. Cooling slows as the part approaches the medium temperature, and boiling or agitation changes heat transfer. A quoted cooling rate refers to a defined temperature or interval. Choose a quench that achieves the necessary structure at the required depth; excessive severity raises thermal stresses, distortion, and cracking.

Key Takeaways

  • Use CCT diagrams for continuous cooling.
  • The critical cooling rate just avoids diffusion-dependent transformations.
  • One part has different cooling paths at its surface and center.
  • Alloy steels can through-harden at lower cooling rates.
  • Example critical rates belong to the named diagram, not every steel.
  • A faster quench also increases distortion and cracking risk.
4

Heat treatments for steels

A useful steel treatment starts with the needed properties and the structure already present. Choose between softening cold-worked metal, relieving stress, refining grains, and forming martensite. Compare cooling media and Jominy data to judge hardening depth, then select a temper that provides the required hardness and toughness. Interrupted quenches offer ways to reduce distortion while controlling the final transformation.

4.1 Choose the anneal for the starting condition

An anneal heats, holds, and cools a metal to soften it, restore ductility, relieve stress, or establish a useful structure. The treatment depends on what needs to change: cold-work effects, residual stress, or the phases and their arrangement.

Locate the critical temperatures

A1 is the eutectoid temperature, 727 °C. A3 is the upper boundary for hypoeutectoid steel; Acm is the upper boundary for hypereutectoid steel. Above the relevant upper boundary, the equilibrium structure is fully austenitic. The subscript c denotes measured heating temperatures, as in Ac3; r denotes cooling temperatures, as in Ar3. Heating values tend to lie above equilibrium boundaries and cooling values below them.

A simplified Andrews estimate is

Ac3 (∘C)≈910−203C+44.7Si,

using wt% carbon and silicon. At 0.45 C and 0.25 Si, the carbon term is about 136.2 and the silicon term about 11.2, giving 785 °C. The equilibrium diagram gives about 770–780 °C. An empirical heating estimate and an equilibrium boundary need not coincide.

Separate four treatments
TreatmentThermal routeMain purpose
Process annealBelow A1, commonly 550–650 °C for steelRestore cold-worked metal's ductility
Stress reliefModerate subcritical heat, then slow coolingRelax residual stress
Full annealAustenitize as appropriate, then furnace coolProduce a soft coarse structure
SpheroidizeLong hold near but below A1, or a suitable cycleRound carbides for machining high-carbon steel

Process annealing allows recovery and recrystallization in cold-drawn wire or sheet between forming steps. It does not need an austenite transformation. Stress relief targets stresses from machining, welding, or uneven cooling while keeping the microstructure essentially unchanged.

For full annealing, heat hypoeutectoid steel typically about 30–50 °C above A3. Slow furnace cooling forms coarse pearlite and proeutectoid ferrite. Hypereutectoid steel is normally heated about 30–50 °C above A1, leaving some cementite. Heating above Acm followed by slow cooling promotes an undesirable grain-boundary cementite network.

Spheroidizing commonly holds steel around 700 °C for 15–25 h. Other routes cycle around A1 or briefly heat above it before a slow subcritical stage. Rounded cementite particles in ferrite give high-carbon steels their most machinable condition.

Work from the processing need

Cold-drawn 0.10 wt% C wire that cracks during further drawing needs a process anneal to restore ductility. A welded frame that distorts during machining needs stress relief. A 0.45 wt% C forging with A3 near 780 °C can be fully annealed around 810–830 °C and furnace cooled. A 1.0 wt% C bearing-steel bar awaiting machining benefits from spheroidizing.

Soaking must let the intended change occur throughout the section. Excessive temperature or time causes grain growth, scaling, and decarburization—the loss of surface carbon. Cooling in still air changes the route to normalizing; it does not reproduce the slow-cooling full-anneal structure.

Key Takeaways

  • Process annealing restores ductility below A1.
  • Stress relief targets residual stress with little structural change.
  • Full annealing uses slow furnace cooling.
  • For hypereutectoid full annealing, heat above A1 but avoid full dissolution above Acm.
  • Spheroidizing prepares high-carbon steel for machining.

4.2 Refine grains by normalizing

Casting and hot working can leave coarse, uneven grains. Normalizing uses an austenite transformation followed by still-air cooling to create a finer, more uniform structure.

Heat above the upper critical boundary

A typical normalizing temperature is about 55–85 °C above A3 for hypoeutectoid steel or above Acm for hypereutectoid steel. Hold until the required austenitic condition is uniform, then remove the part from the furnace and cool it in still air.

On heating, many austenite grains nucleate within the previous structure. During cooling, their boundaries provide sites for ferrite and pearlite to form. The two transformations replace a coarse starting arrangement with finer grains and a more even distribution of products. This is refinement by phase transformation; it is different from recrystallizing a cold-worked metal below A1.

Compare air cooling with furnace cooling
FeatureFull annealingNormalizing
CoolingSlow, inside the furnaceFaster, in still air
PearliteCoarser layersFiner layers
Typical hardness and strengthLowerHigher
Furnace useOccupied during slow coolingAvailable after the hold

Faster cooling lowers the transformation temperature, shortens carbon diffusion distances, and produces finer pearlite. It can also reduce the amount of proeutectoid ferrite compared with slow equilibrium cooling. Normalized plain-carbon steel retains useful ductility while gaining strength. Refining an initially coarse grain structure can also improve toughness.

These comparisons refer to the same steel. They do not imply that every normalized alloy has the same structure. Highly alloyed air-hardening steels can form bainite or martensite in air and need a subsequent temper.

Follow an example forging

A 0.45 wt% C forging has A3 near 780 °C and an uneven coarse structure. Heating to roughly 840–860 °C puts it above A3 by a typical normalizing margin. Hold until the section is uniformly hot and suitably austenitized, then cool in still air. The resulting ferrite–pearlite structure is finer and generally harder than after a full anneal.

A common textbook soaking estimate is about one hour per 25 mm of section thickness. Its purpose is to allow the interior to reach the intended condition. Actual soaking depends on the alloy, furnace, starting structure, and section; extending a hold unnecessarily promotes grain growth.

Consider carbon-rich steels and section size

In a hypereutectoid steel, normalizing above Acm dissolves a cementite network. The faster air cool helps limit its re-formation. Spheroidizing or hardening can follow when the next operation requires a different condition.

A thin section loses heat more quickly than a thick one in the same air. It can develop finer pearlite and higher hardness. The center of a large forging can therefore differ from the surface even after one normalizing cycle. A uniform furnace temperature does not make every later cooling curve identical.

Key Takeaways

  • Normalizing uses austenitizing followed by still-air cooling.
  • New austenite and product grains refine a coarse starting structure.
  • Normalized pearlite is finer and harder than fully annealed pearlite.
  • Air cooling and section thickness jointly determine the final structure.

4.3 Harden to the required depth

Quench hardening requires both an austenitic starting structure and cooling fast enough to avoid unwanted decomposition. The design question is how much of the section must become martensitic.

Austenitize and quench

Hypoeutectoid steel is typically heated about 30–50 °C above A3. Hypereutectoid steel is typically heated about 30–50 °C above A1, leaving some wear-resistant cementite undissolved. Hold long enough to establish the intended austenite and carbon distribution, then quench to exceed the critical rate at the depth that must harden.

Hardness is resistance to indentation. Hardenability is the ability to form martensite through a depth under a specified quench. Carbon mainly sets the maximum martensite hardness; alloying elements and austenite grain size strongly affect hardenability. Two steels with equal carbon can have similar surface hardness but very different center hardness.

Read a Jominy curve

The Jominy end-quench test austenitizes a bar about 25 mm in diameter and 100 mm long, then water-quenches one end. Cooling rate decreases with distance from that end. Hardness is measured on ground flats, commonly at about 1.6 mm intervals in the ASTM method. A hardness curve that stays high farther from the quenched end indicates greater hardenability.

To predict a component's hardness, first find its equivalent Jominy distance from a chart for its diameter, location, and quench medium. Then read that distance on the steel's curve. The distance is a cooling-history equivalent, not the depth of a hardened layer.

Suppose a chart maps the center of a 50 mm oil-quenched bar to 14 mm on a Jominy specimen. Given hardnesses at 14 mm are 25 HRC for a plain 0.40 wt% C steel and 48 HRC for a 0.40 wt% C Cr–Mo steel. Only the Cr–Mo steel exceeds a 40 HRC center requirement, despite similar maximum hardness at the quenched ends.

Balance cooling severity with stress

A typical severity order is agitated brine, water, adjustable polymer solution, oil, molten salt, and still air. Agitation removes insulating vapor and increases heat transfer. Polymer concentration changes severity, so a particular solution is judged by its actual cooling behavior.

Cr, Mo, Ni, Mn, and small effective boron additions delay diffusional reactions. This allows an adequately hardenable steel to use oil or even air instead of a severe water quench. Increasing severity helps depth of hardening but also raises thermal and transformation stresses.

The surface cools and hardens before the center. Later core transformation and expansion can put the hard outer region in tension. Sharp corners, holes, and sudden thickness changes concentrate stress. Rounded transitions, even sections, an adequate alloy, a less severe quench, martempering, and prompt tempering reduce cracking and distortion.

Harden a surface when the core must stay tough

Induction or flame hardening heats the surface of a medium-carbon steel before quenching. Carburizing first adds carbon to the surface of a low-carbon steel, followed by quenching and tempering. These routes target a wear-resistant case while preserving a tougher core.

Key Takeaways

  • Hardness measures indentation resistance; hardenability measures depth response.
  • Read component hardness through its equivalent Jominy distance.
  • A flatter Jominy hardness curve indicates greater hardenability.
  • Choose enough quench severity without unnecessary thermal stress.
  • Surface hardening combines a hard case with a tough core.
  • Alloying delays diffusion-controlled transformations.

4.4 Temper steel and control interrupted quenches

As-quenched martensite has high hardness, low ductility, and large internal stresses. Tempering reheats it below A1 so carbon can redistribute and a more useful balance of strength and toughness develops.

Choose temperature and time together

A typical temper uses about 150–650 °C for one to a few hours. Fine carbides form in a ferrite matrix, producing tempered martensite and relieving quench stresses. Increasing time or temperature generally coarsens the carbides, lowers hardness and strength, and raises ductility and toughness. Very long treatment just below A1 approaches spheroidite.

Low-temperature tempering around 150–250 °C preserves much of the hardness needed for bearings, cutting edges, and carburized cases. Higher tempering around 500–650 °C provides toughness for shafts, axles, bolts, and gears. Some high-alloy tool steels show secondary hardening around 500–600 °C as alloy carbides form; the simple softening trend has this important exception.

Select from example hardness data

A 0.40 wt% C Cr–Mo steel has the following given hardness after a one-hour temper:

Temperature200 °C400 °C500 °C600 °C
Hardness52 HRC44 HRC38 HRC30 HRC

For a 36–40 HRC target, interpolate between adjacent points. The 40 HRC boundary is 400+100(44−40)/(44−38)≈467 °C. The 36 HRC boundary is 500+100(38−36)/(38−30)=525 °C. A typical working choice falls around 470–525 °C for these example data, with the alloy's embrittlement behavior also considered.

Separate two toughness problems

Tempered martensite embrittlement can reduce toughness around 250–400 °C. Avoid this tempering range for a part that needs high toughness; rapid cooling after the same temper does not provide the usual remedy.

Temper embrittlement involves impurity segregation at prior austenite boundaries in susceptible alloy steels, roughly within 375–575 °C. Low impurity levels, suitable molybdenum additions, and fast cooling through the range reduce it. Reheating above about 600 °C and cooling quickly can reverse it. The example tempering window overlaps this second range, so cooling after tempering matters as well as the chosen hardness.

Distinguish interrupted-quench routes

Martempering quenches to just above Ms and holds only long enough to equalize surface and core temperatures, before bainite starts. Cooling through the martensite range then reduces transformation-time differences across the part. The product is martensite and still needs tempering.

Austempering holds above Ms in the bainite range until transformation finishes. The steel's final structure is bainite and normally needs no separate temper. The pearlite nose must be bypassed, which limits suitable steels and section sizes. A similar cycle in ductile iron produces ausferrite—acicular ferrite and carbon-enriched austenite—with graphite nodules retained.

Tempering above A1 instead creates austenite and changes the treatment. Temper promptly after a martensitic quench to reduce the chance of delayed cracking.

Key Takeaways

  • Tempering below A1 generally trades hardness for toughness.
  • Temperature and duration both control carbide coarsening.
  • Use hardness data and embrittlement behavior together.
  • Tempered martensite embrittlement differs from impurity-driven temper embrittlement.
  • Martempering equalizes temperature before martensite forms.
  • Austempering completes a bainite transformation during the hold.
  • Martempered steel still needs tempering.
5

Strengthening alloys by precipitation hardening

Fine precipitates can strengthen an alloy even when quenching alone leaves it relatively soft. Check the solubility change on a phase diagram, then follow solution treatment, quenching, and aging. Connect the evolving particles with the rising and falling parts of an aging curve. The choice of temperature and time affects both production speed and service properties, including the consequences of later heating.

5.1 Solution treat, quench, and age an alloy

Precipitation hardening creates fine particles inside a metal matrix to obstruct dislocations. It requires an alloy whose solute can first dissolve at high temperature and then become supersaturated after rapid cooling.

Check the phase diagram

The solute must have appreciable high-temperature solubility, and that solubility must fall strongly on cooling. A sloping solvus separates the single-phase solid solution from the two-solid-phase field. Choose a composition that can enter the single-phase field without melting.

In Al–Cu, the maximum copper solubility is about 5.65 wt% at 548 °C, compared with only about 0.2 wt% at 250 °C. An alloy below the maximum can dissolve its copper-rich second phase at a suitable solution temperature. An alloy above the maximum cannot dissolve all that phase by the same route.

Follow three distinct steps
  1. Solution heat treatment: heat above the solvus but below the solidus, then hold until the hardening solute is dissolved. In Al–Cu, this means dissolving the copper-rich θ phase, CuAl₂, into the aluminum matrix.
  2. Quench: cool rapidly to suppress precipitation during cooling. The result is a supersaturated solid solution, relatively soft and ductile compared with the later aged condition.
  3. Age: hold below the solvus where diffusion allows a fine dispersion of precipitates to form. This step raises hardness and strength.

Overheating can melt low-melting regions at grain boundaries. Such incipient melting damages the part and cannot be repaired by a later aging cycle. A slow transfer before quenching also causes trouble: premature precipitation consumes solute that should have supplied fine hardening particles later.

Natural and artificial aging

Natural aging takes place at room temperature, often over days. Artificial aging uses an elevated temperature for hours. In aluminum, the unstable solution-treated condition is designated W; it changes as natural aging proceeds.

A typical 6061 route solution treats near 530 °C, water quenches, and artificially ages around 160–180 °C for 8–18 h to reach T6. A typical 2024 route solution treats near 495 °C and water quenches before natural aging to T4; inserting cold work gives the T3 route. These temperatures and times illustrate alloy-specific schedules, not one universal aluminum recipe.

Some 2017 and 2024 rivets are refrigerated after solution treatment and quenching. Cold storage slows natural aging, keeping them soft for installation. They gain strength through aging after the joint is assembled.

Identify alloys that can use the route

The main wrought aluminum heat-treatable series are 2xxx, 6xxx, and 7xxx. Common 1xxx, 3xxx, and 5xxx alloys use solid-solution strengthening and cold work instead. Precipitation hardening also strengthens copper–beryllium, nickel superalloys, some titanium and magnesium alloys, precipitation-hardening stainless steels, and maraging steels.

A steel martensitic quench hardens immediately. A precipitation-hardening quench preserves solute for a later strengthening step. Confusing these outcomes can lead to choosing an unaged aluminum part for a load that needs the final aged strength.

Key Takeaways

  • A falling solubility with cooling makes precipitation hardening possible.
  • Solution treatment dissolves the hardening phase without melting the alloy.
  • Quenching retains a supersaturated solid solution.
  • Aging creates the fine particles that raise strength.
  • Natural aging occurs at room temperature; artificial aging uses elevated temperature.

5.2 Find the peak on an aging curve

Aging does not keep increasing strength forever. The size, spacing, and interface structure of the particles change with time, so a hardness–time curve rises to a peak and then falls.

Follow the Al–Cu precipitation sequence

After quenching, the supersaturated solution forms Guinier–Preston (GP) zones, copper-rich disks only a few atomic layers thick. Transition precipitates θ″ and θ′ follow, and the equilibrium θ phase, CuAl₂, eventually becomes dominant.

Early structures have coherent or semicoherent interfaces: their atomic arrangement fits the matrix relatively well. This fit lowers their nucleation barrier, so they can form before the equilibrium phase. Their strain fields and fine spacing strongly obstruct dislocations, which must cut through the small coherent particles. Peak-aged precipitates are too small for an optical microscope; an electron microscope is needed to resolve them.

Explain underaging, the peak, and overaging

Before the peak, the developing fine dispersion increases resistance to dislocation motion. At the peak-aged condition, obstacle size and spacing give the greatest strength for that aging temperature.

With further exposure, particles coarsen, become fewer, and move farther apart. They also lose coherency as the structure moves toward equilibrium θ. Dislocations can bow between widely spaced particles more readily. This overaging lowers hardness and strength; ductility generally moves in the opposite direction.

The presence of a second phase alone does not establish maximum strength. A coarse equilibrium particle population can be much less effective than a fine metastable dispersion containing the same overall solute.

Choose time and temperature together

An aging curve normally plots hardness or strength against logarithmic time at one fixed temperature. Different temperatures give different curves. Higher aging temperature generally brings an earlier, lower peak; lower temperature can provide a higher peak after a longer wait.

Given example data for an Al–Cu alloy show a peak after about 50 h at 150 °C and about 2 h at 200 °C, with the lower-temperature peak higher. Maximum-strength production favors the first route. A shorter production cycle may justify the second if its lower strength still meets the requirement. Extending the 200 °C hold toward 50 h would put the alloy well beyond its own peak.

Account for service and deliberate overaging

An overaged condition can be useful. T7 tempers of some 7xxx aluminum alloys accept lower strength to improve stress-corrosion resistance and dimensional stability. The design aim is a suitable property combination, not always the largest hardness value.

Service heating can continue the aging process. Allowable temperature and exposure depend on alloy and temper. Welding can locally overage or dissolve precipitates, reducing strength near the joint even when the base metal retains its temper away from the weld.

Both aging and steel tempering form particles in a matrix. Their starting states explain their usual opposite property changes: aging hardens a relatively soft supersaturated solution; tempering softens a highly strained, hard martensitic starting structure.

Key Takeaways

  • Fine, closely spaced precipitates obstruct dislocations strongly.
  • Peak strength precedes the coarse equilibrium particle condition.
  • Overaging coarsens particles and reduces strength.
  • Higher aging temperature usually reaches a lower peak sooner.
  • Controlled overaging can improve other service properties.
  • Service heating and welding can change the precipitate population.
6

Metal families and alloy designations

An alloy designation is useful only when its composition and condition are read correctly. Compare steel, cast-iron, and nonferrous families by the properties their structures support. Decode AISI/SAE, UNS, and EN steel names, then separate an aluminum series from its temper code. This lets you distinguish a composition label, a specified property, and a processing condition when assessing a material choice.

6.1 Choose among steel and cast-iron families

Ferrous alloys are based on iron. Their low raw-material cost and wide response to alloying and heat treatment make them widely used, although their density, about 7.8–7.9 g/cm³ for steels, is high and most grades need corrosion protection.

Match carbon and alloy content to the need

Steels contain up to about 2.14 wt% C; most contain less than 1 wt%. Plain-carbon steels include controlled manganese and silicon as well as carbon and residual elements. Alloy-steel classification depends on specified composition limits, not simply on whether an element was deliberately added.

Steel classTypical composition featureCommon use
Low carbonBelow about 0.25 wt% CSheet, drawn panels, structural shapes
Medium carbonAbout 0.25–0.60 wt% CQuenched-and-tempered shafts and gears
High carbonAbout 0.60–1.4 wt% CSprings, cutting edges, wear-resistant wire
HSLALow C with small strengthening additionsBridges, pipelines, vehicle frames
Low alloyCr, Ni, Mo, or Mn additionsThrough-hardened loaded components
Tool steelMedium or high C, often carbide-forming additionsDies, molds, cutting tools

Low-carbon steel is ductile, weldable, and readily formed. Its lower carbon content limits martensitic hardness compared with medium- and high-carbon steel; it does not make martensite formation impossible. High-carbon steel provides greater wear resistance but less ductility. HSLA additions such as V and Nb raise strength while retaining useful weldability. Tool steels can contain Cr, V, W, or Mo carbides and are not all high-carbon grades.

Distinguish stainless families

Stainless steels contain at least about 10.5 wt% Cr, supporting a protective oxide film. Austenitic grades such as 304 and 316 are FCC, nonmagnetic when annealed, and do not harden by a martensitic quench. Ferritic grades such as 430 are BCC and magnetic. Martensitic grades such as 410, 420, and 440C can be quenched and tempered. Precipitation-hardening grades such as 17-4 PH gain strength by aging. Duplex steels combine ferrite and austenite.

A corrosion-resistant knife needs a hardenable stainless family, while a ductile formed container can use austenitic stainless steel. Magnetism alone does not establish corrosion resistance. Stainless steel can still pit or crack in environments such as chloride-containing solutions.

Use graphite shape to distinguish cast irons

Cast irons contain more than 2.14 wt% C, typically 3.0–4.5 wt% C and 1–3 wt% Si. Their relatively low melting range, roughly 1150–1300 °C, helps casting. Silicon and slow cooling favor graphite over metastable cementite.

Gray iron has graphite flakes. Flake tips concentrate stress, reducing tensile ductility, while the structure provides useful damping, compression resistance, and machinability. Machine bases, brake discs, and engine blocks are common uses.

Ductile iron has graphite nodules produced with small Mg or Ce additions. Rounded graphite reduces stress concentration and improves strength and ductility. White iron retains carbon mainly as cementite after conditions such as low silicon and fast cooling; it is hard, brittle, and wear resistant. Long heating of white iron around 800–900 °C produces graphite clusters and malleable iron. Compacted graphite iron has worm-shaped graphite and properties between gray and ductile iron.

For a vibration-damping machine bed, gray iron is useful. A pressure-carrying valve body benefits from ductile iron's nodule structure. Wear liners can use hard white iron. The graphite or carbide arrangement matters as much as the shared name “cast iron.”

Key Takeaways

  • Carbon content guides steel strength, ductility, and hardening response.
  • HSLA and alloy steels add strength or hardenability through controlled additions.
  • Stainless families differ in crystal structure and hardening route.
  • Graphite flakes concentrate stress; nodules reduce that concentration.
  • White iron is carbide rich; malleable iron forms by heat treating white iron.

6.2 Read grade names without confusing them with treatment

A grade name can identify composition, a property class, or a delivery condition. First identify the naming system, then decode its parts. Similar grades from different systems still need a specification comparison before substitution.

AISI/SAE and UNS

For carbon and low-alloy steels, the first two AISI/SAE digits identify the family and the final two give nominal carbon in hundredths of wt%. Thus 1045 is plain-carbon steel near 0.45 wt% C, while 4140 is Cr–Mo steel near 0.40 wt% C. Five-digit 52100 is a chromium bearing steel near 1.00 wt% C.

Common prefixes include 10 for plain carbon, 11 and 12 for free-machining grades, 15 for higher-Mn carbon steels, 13 for Mn, 40 for Mo, 41 for Cr–Mo, 43 and 86 for Ni–Cr–Mo, and 51 for Cr. B marks boron, L can mark lead, and H at the end denotes a hardenability band.

UNS uses one letter and five digits. Examples include G10450 and G41400 for carbon/alloy steels; S30400 and S31603 for stainless steels; A96061 for aluminum; C17200 for copper alloy; N07718 for nickel alloy; R56400 for titanium alloy; and F-prefix cast irons. The full UNS number identifies a composition, not a heat-treatment schedule.

AISI stainless grades use three digits: 2xx and 3xx are austenitic; 4xx includes both ferritic and martensitic grades. L in a stainless designation such as 316L means low carbon, commonly at most 0.03 wt%, reducing welding-related grain-boundary carbide formation. This is a different use of L from lead-bearing free-machining steel.

EN composition-based names

C45 is a non-alloy steel near 0.45 wt% C. For low-alloy names, the leading number is also 100 times the carbon content. Element-content numbers use factors:

Multiply nominal content byElements
4Cr, Co, Mn, Ni, Si, W
10Al, Be, Cu, Mo, Nb, Pb, Ta, Ti, V, Zr
100Ce, N, P, S
1000B

In 42CrMo4, 42 means about 0.42 wt% C and 4 gives about 1 wt% Cr after division by four. Mo is present but its amount is not stated by that final 4. In 13CrMo4-5, the nominal values are 0.13 wt% C, 1 wt% Cr, and 0.5 wt% Mo. Likewise, 34CrNiMo6 gives about 0.34 wt% C and 1.5 wt% Cr.

High-alloy names begin with X. X5CrNi18-10 means approximately 0.05 wt% C, 18 wt% Cr, and 10 wt% Ni. Alloy-content factors are not applied after X. X2CrNiMo17-12-2 similarly gives about 0.02 C, 17 Cr, 12 Ni, and 2 Mo.

EN property names and material numbers

S355JR identifies structural steel with a specified minimum yield strength of 355 MPa in thin sections. JR means 27 J impact energy at 20 °C; J0 and J2 use 0 °C and −20 °C. The number 355 is not carbon content.

EN material numbers identify grades: C45 is 1.0503; 42CrMo4 is 1.7225; X5CrNi18-10 is 1.4301; and X2CrNiMo17-12-2 is 1.4404. A suffix can identify delivery condition: +A is soft annealed, +N normalized, and +QT quenched and tempered.

1045 and C45, 4140 and 42CrMo4, or 304 and X5CrNi18-10 are similar grades. Composition ranges and product requirements still need comparison before substitution. A composition name alone does not establish the final microstructure or hardness.

Key Takeaways

  • In AISI/SAE carbon and low-alloy grades, the final digits give nominal carbon.
  • UNS combines a family letter with a five-digit identity.
  • EN low-alloy numbers use element-specific factors.
  • EN X names state nominal alloy contents without those factors.
  • S355JR is property based, while C45 is composition based.
  • Delivery suffixes such as +QT describe condition.
  • Similar cross-system grades still have different specification limits.

6.3 Read aluminum alloy and temper codes

Nonferrous alloys provide combinations of low mass, conductivity, corrosion resistance, and high-temperature performance that steels may not offer. The alloy identity and its processing condition are separate parts of a complete designation.

Recognize the aluminum series

Aluminum has density about 2.7 g/cm³, good electrical and thermal conductivity, and useful corrosion resistance. Its FCC structure retains ductility at low temperature; its melting point is only about 660 °C.

Wrought seriesMain composition feature
1xxxAt least 99.00% aluminum
2xxxCopper
3xxxManganese
4xxxSilicon
5xxxMagnesium
6xxxMagnesium and silicon
7xxxZinc, often with Mg and Cu
8xxxOther additions, including lithium

The main precipitation-hardenable wrought series are 2xxx, 6xxx, and 7xxx, with some 8xxx alloys also heat treatable. The 1xxx, 3xxx, and 5xxx series principally use solid solution and cold work. Casting designations have three digits and a decimal, such as A356.0 for an Al–Si–Mg casting alloy.

Read the condition after the hyphen

F means as fabricated; O means annealed; H means strain hardened; W means solution heat-treated and unstable during natural aging; T means thermally treated to a stable condition. In H1x, the metal is strain hardened only; H2x adds partial annealing; H3x adds stabilization. The final digit gives the degree: 2 quarter hard, 4 half hard, and 8 full hard.

TemperMain processing meaning
T3Solution treated, cold worked, naturally aged
T4Solution treated, naturally aged
T5Cooled from hot shaping, artificially aged
T6Solution treated, artificially aged
T7Solution treated, overaged or stabilized
T8Solution treated, cold worked, artificially aged

Thus 3003-H14 is Al–Mn sheet strain hardened only to half hard. 6061-T6 is Al–Mg–Si in a solution-treated and artificially aged condition. 2024-T3 includes cold work and natural aging. In 7075-T651, the added 51 identifies stress relief by stretching after solution treatment and before artificial aging. H18 is cold-worked full hard, not a precipitation-hardening schedule.

EN AW-6061 names a wrought alloy, while EN AC- denotes cast aluminum. Temper codes still carry the condition. Heat from welding can overage or dissolve strengthening precipitates near a joint, so a parent's T6 strength does not describe the whole welded region.

Compare other nonferrous families

Copper alloys favor conductivity and formability. Brass is Cu–Zn, such as C26000 with about 30 wt% Zn; bronzes include Cu–Sn, Cu–Al, and Cu–Si families. Copper–beryllium C17200, around 2 wt% Be, can be precipitation hardened for strong springs and non-sparking tools.

Titanium, around 4.5 g/cm³, combines specific strength with corrosion resistance; Ti-6Al-4V is common in aircraft and implants. Magnesium alloys, around 1.7–1.8 g/cm³, are very light, but HCP structure limits cold formability; AZ91 has about 9 wt% Al and 1 wt% Zn. Nickel superalloys such as 718 retain strength at high temperature through precipitation strengthening. Refractory metals such as Mo, W, Ta, and Nb offer very high melting points.

Key Takeaways

  • Read the aluminum alloy number and temper as separate information.
  • 2xxx, 6xxx, and 7xxx are the main heat-treatable wrought families.
  • H describes strain hardening; T describes a stable thermal treatment.
  • T6 is solution treated and artificially aged; 51 adds stretching stress relief.
  • Choose nonferrous families by the property needed, not density alone.
  • Welding can reduce the strength of a precipitation-hardened region.

Heat Treatment of Metals examples

6 Walkthroughs

1

From a nucleus to a transformation curve

13 steps
Connect nucleation energy, atom mobility, and fraction-transformed calculations.
  1. 1
    IntroductionWhy crossing a temperature is not enough

    A furnace changes temperature, but the structure still needs a route to change. New regions must survive an energy barrier, then enlarge by moving atoms. Those two stages are nucleation and growth, and together they set how fast a structure transforms.

    Follow these two stages and use a measured transformation fraction to predict a later time with the Avrami equation. The same reasoning explains why a fast quench can preserve a nonequilibrium starting state.

  2. 2
    ExplanationBalance surface and volume energy

    A tiny new-phase cluster creates interface, which costs energy. Below the equilibrium transformation temperature, its volume change lowers free energy.

    For a sphere, ΔG=(4/3)πr3ΔGv+4πr2γ. The positive surface term dominates at first. Beyond the peak, the negative volume term wins and further growth is favorable.

  3. 3
    ExampleCalculate the critical size

    Suppose γ=0.15 J/m² and ΔGv=−3.0×108 J/m³. The critical radius is r∗=−2γ/ΔGv=1.0×10−9 m.

    That is 1.0 nm. A smaller embryo tends to dissolve; a larger nucleus can lower its energy by growing. The negative sign of the driving force produces a positive radius.

  4. 4
    ChallengeChange the undercooling

    The undercooling doubles. In the linear driving-force model, interface energy stays fixed. What happens to the critical radius and nucleation barrier?

    ---reveal---

    The driving-force magnitude doubles. The critical radius halves because it varies inversely with that magnitude, while the barrier falls to one quarter because it varies inversely with its square.

  5. 5
    ConnectionUse an existing boundary

    A grain boundary can replace part of the costly new interface. This lowers the heterogeneous nucleation barrier, while the spherical-cap model leaves the critical radius unchanged.

    That makes boundaries useful starting sites for ferrite and pearlite. It also explains why grain-refining additions in a casting can produce many small grains without requiring homogeneous nucleation throughout the melt.

  6. 6
    Key InsightExplain the nose

    Cooling raises the driving force for austenite decomposition but reduces diffusion. Near equilibrium, nucleation is difficult; far below it, atom transport is slow.

    The combined transformation is fastest at an intermediate temperature. This competition creates a nose on the transformation diagram. More driving force alone cannot establish the fastest treatment.

  7. 7
    ExplanationTrack a fraction with Avrami

    At a fixed temperature, use y=1−exp⁡(−ktn). The transformed fraction rises slowly, then rapidly, then levels off as particles meet and parent material runs out.

    Use a fraction such as 0.30 for 30%. The constants belong to the specified reaction and temperature. If time is in seconds and n=2, then k has units s⁻².

  8. 8
    ExampleFind the rate constant first

    A reaction with n=2 is 50% complete after 80 s. Substitute y=0.50 and rearrange: k=ln⁡2/802≈1.08×10−4 s−2.

    This establishes the fitted curve at that temperature. The half-time also directly gives the conventional rate: r=1/80=0.0125 s−1.

  9. 9
    ExamplePredict a later fraction

    Keep the same reaction and double the time to 160 s. The exponent magnitude becomes four times larger because time is squared.

    Using the half-time form, 1−y=exp⁡[−4ln⁡2]=(1/2)4=1/16. Thus y=15/16=0.9375, or 93.75%. A doubled time did not produce a doubled percentage.

  10. 10
    ChallengeCheck a rate comparison

    One specimen reaches half transformation in 80 s and another in 40 s. How do their conventional rates compare, and does this tell you their instantaneous slopes at every time?

    ---reveal---

    The second rate is twice the first because rate is reciprocal half-time. It does not establish the full curve or every slope; those depend on the fitted reaction behavior.

  11. 11
    TipPrepare an Arrhenius comparison

    For a diffusion-controlled rate comparison, convert each temperature to kelvin before using reciprocal temperatures. If half-time falls tenfold, the rate rises tenfold.

    Keep the rate ratio in the same direction as the temperature labels in ln⁡(r2/r1)=(Q/R)(1/T1−1/T2). A hotter, faster reaction should give a positive activation energy.

  12. 12
    ChallengeExplain a cold but slow reaction

    A cooled specimen has a larger driving force but transforms more slowly than a warmer one. Does this conflict with a measured Avrami curve at the warmer temperature?

    ---reveal---

    No. Low atom mobility can limit the colder reaction, and the warmer curve's constants apply at its own temperature. Driving force and diffusion jointly determine the behavior; one curve is not a universal temperature law.

  13. 13
    RecapChoose the right kinetic question

    Ask first whether a viable nucleus can form, then whether atoms can move rapidly enough for growth. For a specified isothermal reaction, use fraction and time data to establish the Avrami curve.

    Use reciprocal half-time for the conventional rate and absolute temperature for Arrhenius comparisons. A phase diagram alone cannot supply the elapsed time needed to reach its equilibrium state.

2

Read a steel structure and predict its behavior

15 steps
Distinguish phases, product fractions, and the structures that control hardness and toughness.

Save this lesson to follow every Walkthrough step by step.

  1. 1
    IntroductionOne composition, several useful structures
  2. 2
    ExplanationIdentify the layered product
  3. 3
    ExampleFind pearlite in a low-carbon steel
  4. 4
    ExampleNow count total cementite
  5. 5
    ChallengeChoose the quantity before the tie line
  6. 6
    ExplanationLocate the carbide particles
  7. 7
    ConnectionMake a soft structure from the same phases
  8. 8
    ChallengeChoose a hold for machining
  9. 9
    ExplanationTrap carbon in the lattice
  10. 10
    ExampleRead a martensite temperature stop
  11. 11
    ChallengeCompare waiting and cooling
  12. 12
    Key InsightSeparate hardness from toughness
  13. 13
    ExampleEstimate strength with the right test scale
  14. 14
    ChallengeChoose the final structure for a shaft
  15. 15
    RecapConnect the structure to the job
3

Follow austenite through a thermal path

15 steps
Read TTT holds, keep a product balance, and compare continuous cooling at different depths.

Save this lesson to follow every Walkthrough step by step.

  1. 1
    IntroductionMake the path a material balance
  2. 2
    ExplanationRead one horizontal slice
  3. 3
    ExampleUse the example hold data
  4. 4
    ChallengeRead equal spacing correctly
  5. 5
    ExplanationCarry forward the remaining parent
  6. 6
    ExampleComplete the first stage
  7. 7
    ExampleChange the second stage
  8. 8
    ChallengeMultiply a fraction of the remainder
  9. 9
    TipCheck the final temperature
  10. 10
    ExplanationSwitch diagrams when the temperature changes continuously
  11. 11
    ExampleUse a diagram-specific cooling range
  12. 12
    ChallengeExplain the two depths
  13. 13
    ConnectionMake a thicker part hardenable
  14. 14
    ChallengeChoose the diagram and the alloy response
  15. 15
    RecapFinish with a balance and a path check
4

Choose a steel treatment from the requirement

18 steps
Work from the processing problem to a thermal route, hardening-depth check, and temper.

Save this lesson to follow every Walkthrough step by step.

  1. 1
    IntroductionStart with the needed change
  2. 2
    ExplanationSeparate cold-work effects from residual stress
  3. 3
    ExampleChoose a full-anneal temperature
  4. 4
    ChallengeAvoid a cementite network
  5. 5
    ConnectionPrepare a high-carbon bar for cutting
  6. 6
    ExplanationRefine the forging with air cooling
  7. 7
    ChallengeCompare two normalized sections
  8. 8
    ExplanationDistinguish depth from local hardness
  9. 9
    ExampleMap a component to a test position
  10. 10
    ChallengeChoose a less severe quench
  11. 11
    TipReduce quench stress at the source
  12. 12
    ExplanationTurn hard martensite into a useful condition
  13. 13
    ExampleInterpolate a hardness target
  14. 14
    Key InsightCooling after tempering also matters
  15. 15
    ExplanationUse two different interrupted holds
  16. 16
    ChallengeDiagnose an interrupted-quench claim
  17. 17
    ChallengeCombine depth and final properties
  18. 18
    RecapEvaluate the whole route
5

Choose and stop an aging treatment

12 steps
Use solubility and particle evolution to explain when precipitation hardening works.

Save this lesson to follow every Walkthrough step by step.

  1. 1
    IntroductionMake particles when they are most useful
  2. 2
    ExplanationLook for falling solubility
  3. 3
    ExampleDissolve the particles first
  4. 4
    ExampleQuench before precipitation consumes the solute
  5. 5
    ChallengeChoose the strengthening stage
  6. 6
    ConnectionControl the delay before shaping
  7. 7
    ExplanationFollow the particles toward equilibrium
  8. 8
    Key InsightExplain the falling side of the curve
  9. 9
    ExampleCompare two given aging curves
  10. 10
    ChallengeReject the mixed schedule
  11. 11
    ChallengeExplain a softened welded region
  12. 12
    RecapTie the phase diagram to the aging curve
6

Decode a grade and connect it to a treatment

15 steps
Use family, composition, property, and condition information without mixing their meanings.

Save this lesson to follow every Walkthrough step by step.

  1. 1
    IntroductionRead the label in parts
  2. 2
    ExplanationChoose a steel family by its response
  3. 3
    ConnectionUse graphite shape as a design clue
  4. 4
    ChallengeChoose a casting for the load
  5. 5
    ExplanationDecode the SAE digits first
  6. 6
    ExampleRead a low-alloy EN name
  7. 7
    ExampleSwitch rules after X
  8. 8
    Key InsightSeparate properties from composition
  9. 9
    ChallengeCorrect a proposed steel reading
  10. 10
    ExplanationSeparate aluminum family from condition
  11. 11
    ExampleRead a stretching suffix
  12. 12
    ChallengeChoose the right strengthening route
  13. 13
    ConnectionChoose another nonferrous family
  14. 14
    ChallengeExplain a lost temper after heating
  15. 15
    RecapDecode only what each part actually says

Heat Treatment of Metals practice questions

60 Practice Questions in 6 sets

Set 1: Nucleation and transformation kinetics10 Practice Questions

Question 1 of 10

The driving-force magnitude triples while interface energy stays fixed. How does the critical radius change?
  1. It becomes one third as large.
  2. It becomes three times as large.
  3. It becomes one ninth as large.
  4. It becomes nine times as large.
Show answerHide answer
Answer: A
The critical radius is inversely proportional to the driving-force magnitude, so tripling that magnitude divides the radius by three. The one-ninth result belongs to the nucleation barrier, which depends on the inverse square. It does not describe the radius.

Question 2 of 10

A new spherical particle has a radius below the critical radius. What change is energetically favored?
  1. Continued stable growth
  2. Growth at constant free energy
  3. Dissolution of the embryo
  4. Immediate complete transformation
Show answerHide answer
Answer: C
Below the critical radius, the interface-energy cost dominates the benefit of forming the new phase. Shrinking the embryo lowers its free energy, so it tends to dissolve. A favorable bulk driving force alone does not make every tiny cluster stable.

Question 3 of 10

Why can an inclusion allow a new phase to nucleate more easily than the same phase forming inside a uniform grain?
  1. It increases the equilibrium solute concentration.
  2. It removes the need for a volume driving force.
  3. It increases the critical radius at fixed driving force.
  4. It lowers the required interface-energy barrier.
Show answerHide answer
Answer: D
An existing surface can replace part of the interface that a new particle would otherwise have to create. This lowers the heterogeneous nucleation barrier. It does not remove the need for a thermodynamically favorable new phase, and the cap model does not increase the critical radius.

Question 4 of 10

A colder isothermal hold gives a larger driving force but a longer transformation time. What mechanism explains this result?
  1. The larger driving force prevents atom attachment.
  2. Slower diffusion limits the growth process.
  3. The critical radius must have become larger.
  4. More time is needed because the hold is isothermal.
Show answerHide answer
Answer: B
Lower temperature reduces atom mobility exponentially, so diffusion-dependent growth can slow even when the driving force increases. The stronger driving force tends to reduce the critical radius, not enlarge it. Both the energy barrier and atom transport are needed to judge the overall reaction speed.

Question 5 of 10

A transformation has a half-time of 25 s. What is its conventional rate?
  1. 25 s⁻¹
  2. 0.040 s⁻¹
  3. 0.020 s⁻¹
  4. 0.40 s⁻¹
Show answerHide answer
Answer: B
The conventional rate is the reciprocal half-time, so dividing one by 25 s gives 0.040 s⁻¹. Using 25 s⁻¹ would treat a time as a rate and reverse the physical relationship. A shorter half-time should correspond to a larger rate, not a smaller one.

Question 6 of 10

For an Avrami reaction, the exponent is 2 and the half-time is 40 s. What fraction is transformed after 80 s?
  1. 0.7500
  2. 0.8750
  3. 1.0000
  4. 0.9375
Show answerHide answer
Answer: D
Doubling time multiplies the exponent magnitude by four when the Avrami exponent is two. The untransformed fraction becomes one half raised to the fourth power, or 0.0625, leaving 0.9375 transformed. A value of 0.75 would follow doubling time with an exponent of one.

Question 7 of 10

What temperature should replace 175 °C in an Arrhenius rate calculation?
  1. 448.15 K
  2. 175.00 K
  3. 98.15 K
  4. 548.15 K
Show answerHide answer
Answer: A
Add 273.15 to the Celsius temperature to obtain 448.15 K. The Arrhenius expression uses absolute temperature through thermal energy and reciprocal temperature. Entering 175 directly keeps the Celsius zero and gives the wrong exponential dependence, even if the rest of the arithmetic is correct.

Question 8 of 10

An Avrami plot of ln⁡[−ln⁡(1−y)] against ln⁡t has slope 3 and intercept −8. What are the fitted constants?
  1. n=exp⁡(3)andk=−8
  2. n=−8andk=exp⁡(3)
  3. n=3andk=exp⁡(−8)
  4. n=3andk=−8
Show answerHide answer
Answer: C
The linearized equation has slope n and intercept ln⁡k, so the constants are n=3 and k=exp⁡(−8). Taking the intercept itself as k would give a negative rate constant. Exponentiating the intercept is essential because the plotted vertical relation contains its natural logarithm.

Question 9 of 10

A melt has critical radius 2 nm and barrier E. Its undercooling doubles, and a substrate gives a heterogeneous barrier factor of 0.20. What radius and barrier follow in the cap model, with interface energy unchanged?
  1. 1 nm and 0.20E
  2. 0.4 nm and 0.05E
  3. 4 nm and 0.80E
  4. 1 nm and 0.05E
Show answerHide answer
Answer: D
Doubling undercooling halves the critical radius and reduces the homogeneous barrier to one quarter. The substrate then multiplies that barrier by 0.20, leaving 0.05E. Its geometric factor changes the barrier, not the critical radius; using 0.20E overlooks the undercooling effect.

Question 10 of 10

A recrystallization half-time falls from 72 min to 18 min as temperature rises. What rate ratio belongs in the Arrhenius comparison, hotter over colder?
  1. 4
  2. 0.25
  3. 54
  4. 90
Show answerHide answer
Answer: A
Rate is reciprocal half-time, so the hotter-to-colder ratio is (1/18)/(1/72)=4. The ratio 0.25 compares the times in the same order instead of the rates. Subtracting the durations gives a time difference, which cannot replace the dimensionless rate ratio in a logarithm.
Set 2: Steel products and mechanical properties10 Practice Questions

Save this lesson to see every answer and practice every set.

Question 1 of 10

What proeutectoid phase forms when a 1.10 wt% C steel cools slowly from austenite?
  1. Ferrite
  2. Cementite
  3. Martensite
  4. Bainite
Show answerHide answer

Save this lesson to see this answer.

Question 2 of 10

A 0.25 wt% C steel cools slowly to just below 727 °C. Using 0.022 and 0.76 wt% C as the ferrite and eutectoid compositions, what is its pearlite fraction?
  1. About 69%
  2. About 3.4%
  3. About 11%
  4. About 31%
Show answerHide answer

Save this lesson to see this answer.

Question 3 of 10

A slowly cooled 0.55 wt% C steel is examined just below A1. Use 0.022, 0.76, and 6.70 wt% C for ferrite, eutectoid austenite, and cementite. What pair gives pearlite fraction and total cementite fraction?
  1. About 71.5% and 7.9%
  2. About 71.5% and 11.1%
  3. About 28.5% and 7.9%
  4. About 7.9% and 71.5%
Show answerHide answer

Save this lesson to see this answer.

Question 4 of 10

A micrograph shows rounded cementite particles dispersed in continuous ferrite after a long subcritical hold. What structure is present?
  1. Fine pearlite
  2. Upper bainite
  3. Spheroidite
  4. Plate martensite
Show answerHide answer

Save this lesson to see this answer.

Question 5 of 10

Pearlite has completely formed in a steel before it is cooled to 380 °C and held there. Why does that hold not produce bainite by austenite decomposition?
  1. The hold is below every steel’s Ms.
  2. Pearlite and bainite are the same layered structure.
  3. No parent austenite remains for the reaction.
  4. Bainite requires a hold above the eutectoid temperature.
Show answerHide answer

Save this lesson to see this answer.

Question 6 of 10

A steel has Ms = 290 °C and M50 = 210 °C. It is quenched directly to 240 °C. What can be said about its initial martensite fraction?
  1. It is above zero but below 50%.
  2. It is exactly 50%.
  3. It is zero until another hold is completed.
  4. It is complete because Ms has been crossed.
Show answerHide answer

Save this lesson to see this answer.

Question 7 of 10

Two steels with 0.40 wt% C are fully martensitic after quenching. One contains more Cr and Mo. What main difference should those additions usually provide?
  1. A much higher carbon-limited maximum hardness
  2. A greater martensite fraction after full transformation
  3. A change from martensite to equilibrium pearlite
  4. Greater ability to harden through a thick section
Show answerHide answer

Save this lesson to see this answer.

Question 8 of 10

A low-alloy steel contains 0.30 wt% C, 1.00 wt% Mn, 1.00 wt% Ni, 0.80 wt% Cr, and 0.20 wt% Mo. Use Ms=539−423C−30.4Mn−17.7Ni−12.1Cr−7.5Mo. It is then cooled to 280 °C without diffusional transformation, but Mf is unknown. What conclusion is justified?
  1. Ms is about 353 °C; martensite must be complete at 280 °C.
  2. Ms is about 353 °C; martensite has begun, but completion is unknown.
  3. Ms is about 480 °C; martensite has not begun at 280 °C.
  4. Ms is about 353 °C; waiting at 280 °C must complete martensite.
Show answerHide answer

Save this lesson to see this answer.

Question 9 of 10

A steel component measures 260 HB. What approximate tensile strength follows from the steel correlation?
  1. 897 MPa
  2. 75 MPa
  3. 754 MPa
  4. 260 MPa
Show answerHide answer

Save this lesson to see this answer.

Question 10 of 10

A notched shaft can be supplied as pearlite or tempered martensite at the same hardness. Why is tempered martensite usually preferred when impact toughness matters?
  1. Its carbon content must be higher at equal hardness.
  2. Its hardness guarantees a greater elastic modulus.
  3. Its carbide arrangement gives better resistance to crack growth.
  4. Its carbide plates are more continuous across the matrix.
Show answerHide answer

Save this lesson to see this answer.

Set 3: Transformation diagrams and product balances10 Practice Questions

Save this lesson to see every answer and practice every set.

Question 1 of 10

A TTT path at a fixed temperature ends between the transformation-start and transformation-finish curves. What is present immediately before further cooling?
  1. Only the final product named in that region
  2. Only austenite because finish has not been crossed
  3. Martensite and no other parent or product
  4. Austenite and the product forming during the hold
Show answerHide answer

Save this lesson to see this answer.

Question 2 of 10

Two TTT diagrams use the same composition but different austenite grain sizes. Why can the coarser-grained condition show later pearlite start?
  1. It has more grain-boundary area for nucleation.
  2. It has less grain-boundary area for nucleation.
  3. It must have a larger equilibrium cementite fraction.
  4. It changes logarithmic seconds into linear seconds.
Show answerHide answer

Save this lesson to see this answer.

Question 3 of 10

For a fully austenitic steel, example pearlite start and finish times at 625 °C are 3 s and 28 s. After rapid transfer, it is held 35 s and quenched below Mf. What is the idealized result?
  1. Pearlite plus martensite
  2. Essentially 100% martensite
  3. Essentially 100% pearlite
  4. Pearlite and retained austenite
Show answerHide answer

Save this lesson to see this answer.

Question 4 of 10

An idealized path converts 35% of austenite to pearlite, then quenches the specimen below Mf without further diffusional change. What final fractions result?
  1. 35% pearlite and 65% martensite
  2. 65% pearlite and 35% martensite
  3. 35% pearlite and 65% retained austenite
  4. 35% bainite and 65% martensite
Show answerHide answer

Save this lesson to see this answer.

Question 5 of 10

A first hold converts 20% of the original austenite to pearlite. A second stage converts 75% of the remaining austenite to bainite. A final quench reaches below Mf. What is the final structure?
  1. 20% pearlite, 75% bainite, 5% martensite
  2. 20% pearlite, 20% bainite, 60% martensite
  3. 20% pearlite, 60% bainite, 20% martensite
  4. 0% pearlite, 60% bainite, 40% martensite
Show answerHide answer

Save this lesson to see this answer.

Question 6 of 10

A steel is rapidly cooled to a bainitic temperature where the given start time is 90 s. It stays 25 s, then reaches below Mf before any other transformation. What forms?
  1. Essentially all bainite
  2. Bainite plus pearlite
  3. Pearlite plus retained austenite
  4. Essentially all martensite
Show answerHide answer

Save this lesson to see this answer.

Question 7 of 10

A steel part cools steadily from its austenitizing temperature without an isothermal hold. What diagram should be used to predict the transformation path?
  1. Its TTT diagram
  2. Its CCT diagram
  3. Its equilibrium tie line alone
  4. Its fixed-temperature aging curve
Show answerHide answer

Save this lesson to see this answer.

Question 8 of 10

A given plain-eutectoid CCT diagram shows complete pearlite below 32 °C/s and a martensitic critical rate of 150 °C/s. A specimen cools at 75 °C/s through the controlling range and then below Mf. What result is expected?
  1. Pearlite plus martensite
  2. Only coarse pearlite
  3. Only martensite
  4. Bainite plus retained austenite
Show answerHide answer

Save this lesson to see this answer.

Question 9 of 10

Two equal-carbon steels have critical rates of 110 and 12 °C/s. A component’s surface cools at 160 °C/s and its center at 30 °C/s through the controlling range. Both reach below Mf. Which steel can avoid diffusional products at both locations?
  1. Only the steel with the 110 °C/s critical rate
  2. Only the steel with the 12 °C/s critical rate
  3. Both steels because the surface rate is 160 °C/s
  4. Neither steel because the center is slower than the surface
Show answerHide answer

Save this lesson to see this answer.

Question 10 of 10

A first hold forms 45% pearlite. A second stage converts 40% of the remaining austenite to bainite. Final cooling reaches the diagram’s M50 line. What fractions result in this idealized path?
  1. 45% pearlite, 40% bainite, 7.5% martensite, 7.5% austenite
  2. 45% pearlite, 22% bainite, 33% martensite, 0% austenite
  3. 45% pearlite, 11% bainite, 22% martensite, 22% austenite
  4. 45% pearlite, 22% bainite, 16.5% martensite, 16.5% austenite
Show answerHide answer

Save this lesson to see this answer.

Set 4: Steel heat-treatment decisions10 Practice Questions

Save this lesson to see every answer and practice every set.

Question 1 of 10

A cold-rolled 0.08 wt% C strip has lost ductility between rolling passes. What treatment is designed to remove the cold-work effects without austenitizing?
  1. Process annealing below A1
  2. Normalizing above A3
  3. Quenching from the austenite field
  4. Tempering an as-quenched structure
Show answerHide answer

Save this lesson to see this answer.

Question 2 of 10

A coarse hypoeutectoid forging has A3 = 800 °C. What typical normalizing route fits this condition?
  1. Heat to about 830–850 °C, then furnace cool
  2. Heat to about 650–700 °C, then still-air cool
  3. Heat to about 855–885 °C, then still-air cool
  4. Heat to about 855–885 °C, then furnace cool
Show answerHide answer

Save this lesson to see this answer.

Question 3 of 10

A normalized plain-carbon-steel part is harder than the same steel after full annealing. What structural difference explains this?
  1. Wider lamellae from slower air cooling
  2. Finer pearlite from the faster air cool
  3. A fully martensitic structure throughout
  4. Higher bulk carbon content after normalizing
Show answerHide answer

Save this lesson to see this answer.

Question 4 of 10

Two Jominy curves start at 55 HRC. At 20 mm from the quenched end, one reads 27 HRC and the other 45 HRC. Which has greater hardenability?
  1. The steel reading 27 HRC at 20 mm
  2. Both have equal hardenability because the end values match.
  3. The curves cannot show hardenability without carbon percentages.
  4. The steel reading 45 HRC at 20 mm
Show answerHide answer

Save this lesson to see this answer.

Question 5 of 10

A chart maps a gear’s critical section to 18 mm Jominy distance. Given hardness there is 34 HRC for steel R and 47 HRC for steel S. The minimum is 44 HRC. What selection follows?
  1. Steel S meets the hardness requirement; steel R does not.
  2. Steel R meets the hardness requirement; steel S does not.
  3. Both meet the requirement if their quenched ends exceed 44 HRC.
  4. Neither can be assessed because 18 mm is not the actual case depth.
Show answerHide answer

Save this lesson to see this answer.

Question 6 of 10

A shaft needs at least 43 HRC at its center. Given chart-and-curve data predict 45 HRC for steel U in water, 35 HRC for U in oil, and 46 HRC for steel V in oil. Surface hardness is adequate in all cases. What choice meets the center need while reducing quench severity?
  1. Steel U with an oil quench
  2. Steel V with an oil quench
  3. Steel U with a water quench
  4. Either steel in oil because surface hardness is adequate
Show answerHide answer

Save this lesson to see this answer.

Question 7 of 10

One-hour tempering data give 48 HRC at 420 °C and 40 HRC at 520 °C. What temperature gives a linear estimate of 44 HRC?
  1. 445 °C
  2. 495 °C
  3. 500 °C
  4. 470 °C
Show answerHide answer

Save this lesson to see this answer.

Question 8 of 10

An interrupted quench equalizes a steel part’s temperature just above Ms before air cooling through the martensite range. What follow-up treatment is normally needed?
  1. A long bainite hold
  2. An anneal above Acm
  3. A temper below A1
  4. No further treatment
Show answerHide answer

Save this lesson to see this answer.

Question 9 of 10

A steel must finish between 39 and 43 HRC after a one-hour temper. Given data are 47 HRC at 400 °C, 41 HRC at 500 °C, and 33 HRC at 600 °C. It is susceptible to impurity-driven temper embrittlement. What approximate route fits both hardness and that risk?
  1. Temper at 467–525 °C and cool quickly through the susceptible range.
  2. Temper at 467–525 °C and cool slowly through the susceptible range.
  3. Temper at 425–467 °C and cool quickly through the susceptible range.
  4. Temper at 525–567 °C and cool slowly through the susceptible range.
Show answerHide answer

Save this lesson to see this answer.

Question 10 of 10

A steel has Ms = 270 °C and needs 45 s in a bath to equalize its section temperature. Bainite starts after 30 s at 280 °C and after 90 s at 310 °C. All transfers bypass earlier transformations. What bath-and-hold plan preserves the intended martempering route before final cooling and tempering?
  1. 250 °C for 45 s
  2. 310 °C for 45 s
  3. 280 °C for 45 s
  4. 310 °C for 100 s
Show answerHide answer

Save this lesson to see this answer.

Set 5: Precipitation hardening and aluminum conditions10 Practice Questions

Save this lesson to see every answer and practice every set.

Question 1 of 10

An alloy has almost the same solute solubility at its solution temperature and at room temperature. Why is it a poor candidate for ordinary precipitation hardening?
  1. Cooling must always produce a fully martensitic structure.
  2. A single solid phase can never dissolve alloying elements.
  3. Cooling creates little supersaturation to drive later precipitation.
  4. The absence of a solubility drop guarantees incipient melting.
Show answerHide answer

Save this lesson to see this answer.

Question 2 of 10

A chosen alloy’s single-phase solution-treatment window lies above 485 °C and below a solidus of 545 °C. What proposed temperature is inside that window?
  1. 470 °C
  2. 550 °C
  3. 455 °C
  4. 515 °C
Show answerHide answer

Save this lesson to see this answer.

Question 3 of 10

An alloy has 3.2 wt% solute. Equilibrium solubility is 4.0 wt% at 500 °C and 0.7 wt% at 350 °C; its solidus is 550 °C. It is held at 500 °C, left at 350 °C long enough for appreciable precipitation, then quenched and aged. What best explains its low final strength?
  1. The first hold exceeds the solidus and necessarily melts the alloy.
  2. The first hold can dissolve the solute, but the later delay consumes supersaturation.
  3. The composition is above the 500 °C solubility, so full dissolution is impossible.
  4. The 350 °C delay increases dissolved solute and prevents all precipitation.
Show answerHide answer

Save this lesson to see this answer.

Question 4 of 10

Hardness rises during aging and later falls while particles become larger and farther apart. What explains the fall?
  1. Dislocations can bypass the coarser dispersion more easily.
  2. The number of closely spaced coherent obstacles keeps increasing.
  3. The alloy is returning to its hardest as-quenched martensite.
  4. The larger equilibrium particles must be the strongest barriers.
Show answerHide answer

Save this lesson to see this answer.

Question 5 of 10

Given aging data for one alloy: at 145 °C, 140 HB after 4 h and 165 HB after 16 h; at 190 °C, 158 HB after 3 h and 146 HB after 8 h. A part needs at least 155 HB within 5 h. What demonstrated route meets both constraints?
  1. 145 °C for 4 h
  2. 145 °C for 16 h
  3. 190 °C for 8 h
  4. 190 °C for 3 h
Show answerHide answer

Save this lesson to see this answer.

Question 6 of 10

Two aging schedules give the required strength initially. Schedule A is peak aged; schedule B is deliberately overaged and has demonstrated better stress-corrosion resistance. A component’s governing concern is stress-corrosion cracking, and both remain above its strength minimum. What choice follows?
  1. Choose A for its higher peak strength.
  2. Choose A since overaging removes precipitates.
  3. Choose B for the stated service priority.
  4. Reject both as identical aging states.
Show answerHide answer

Save this lesson to see this answer.

Question 7 of 10

What condition does the H18 suffix identify on aluminum sheet?
  1. Strain hardened only to full hard
  2. Solution treated and naturally aged
  3. Solution treated and artificially aged
  4. Strain hardened and partly annealed
Show answerHide answer

Save this lesson to see this answer.

Question 8 of 10

An aluminum extrusion is labeled 6063-T5. What process distinction separates T5 from T6?
  1. T5 naturally ages; T6 has no aging stage.
  2. T5 ages after cooling from hot shaping; T6 includes solution heat treatment.
  3. T5 is strain hardened; T6 is fully annealed.
  4. T5 and T6 differ only in the alloy’s magnesium percentage.
Show answerHide answer

Save this lesson to see this answer.

Question 9 of 10

A drawing requires an Al–Mg–Si plate supplied solution treated, stress relieved by stretching, and artificially aged. What designation matches the full requirement?
  1. 6061-T6
  2. 3003-H14
  3. 6061-T651
  4. 2024-T3
Show answerHide answer

Save this lesson to see this answer.

Question 10 of 10

A designer needs a lightweight alloy but expects prolonged hot service that would substantially overage the proposed aluminum temper. Why should the family choice be reconsidered?
  1. Aluminum becomes denser than steel during aging.
  2. Every aluminum alloy melts at its artificial-aging temperature.
  3. All lightweight alloys have the same hot-strength behavior.
  4. The original precipitate strength may not survive the exposure.
Show answerHide answer

Save this lesson to see this answer.

Set 6: Combine alloy labels, structures, and treatment choices10 Practice Questions

Save this lesson to see every answer and practice every set.

Question 1 of 10

What nominal carbon content does SAE 1050 indicate?
  1. About 5.0 wt% C
  2. About 0.50 wt% C
  3. About 0.10 wt% C
  4. About 1.05 wt% C
Show answerHide answer

Save this lesson to see this answer.

Question 2 of 10

What approximate carbon, chromium, and molybdenum contents are encoded by EN 13CrMo4-5?
  1. 0.13 wt% C, 1 wt% Cr, 0.5 wt% Mo
  2. 0.13 wt% C, 4 wt% Cr, 5 wt% Mo
  3. 1.3 wt% C, 1 wt% Cr, 0.5 wt% Mo
  4. 0.13 wt% C, 0.4 wt% Cr, 0.05 wt% Mo
Show answerHide answer

Save this lesson to see this answer.

Question 3 of 10

A drawing specifies S355J2+N in a thin-section product. A proposal calls it “0.355 wt% carbon steel supplied quenched and tempered.” What is the corrected interpretation?
  1. Carbon 0.355 wt%, 27 J at −20 °C, normalized
  2. Structural yield class 355 MPa, 27 J at 20 °C, quenched and tempered
  3. Structural yield class 355 MPa, 27 J at 0 °C, soft annealed
  4. Structural yield class 355 MPa, 27 J at −20 °C, normalized
Show answerHide answer

Save this lesson to see this answer.

Question 4 of 10

A nominal-composition screen requires at most 0.03 wt% C, at least 16 wt% Cr, and at least 2 wt% Mo. Compare X5CrNi18-10 with X2CrNiMo17-12-2. Which name passes that screen, and does the composition name alone establish its supplied heat-treatment condition?
  1. X5CrNi18-10 passes; the condition still needs specification.
  2. X2CrNiMo17-12-2 passes; it must be supplied quenched and tempered.
  3. X2CrNiMo17-12-2 passes; the condition still needs specification.
  4. Both names pass; each must be supplied fully annealed.
Show answerHide answer

Save this lesson to see this answer.

Question 5 of 10

A corrosion-resistant valve stem must gain wear resistance by quenching and tempering. What stainless family is a suitable candidate?
  1. Austenitic stainless steel
  2. Martensitic stainless steel
  3. Ferritic stainless steel
  4. Annealed duplex stainless steel
Show answerHide answer

Save this lesson to see this answer.

Question 6 of 10

A brittle cast-iron part has carbon mainly in cementite. It must gain ductility through a solid-state treatment that converts carbide carbon to graphite without recasting. What treatment and final graphite form fit this requirement?
  1. A brief quench from above A1; graphite nodules in ductile iron
  2. Prolonged heating around 800–900 °C; graphite flakes in gray iron
  3. Prolonged heating around 800–900 °C; graphite clusters in malleable iron
  4. A short normalizing cycle; graphite nodules in ductile iron
Show answerHide answer

Save this lesson to see this answer.

Question 7 of 10

A formed aerospace panel requires an Al–Cu alloy supplied solution treated, cold worked, and naturally aged. What alloy-temper combination matches that description?
  1. 2014-T3
  2. 6061-T6
  3. 3003-H14
  4. 7075-T651
Show answerHide answer

Save this lesson to see this answer.

Question 8 of 10

A Jominy-based chart predicts 52 HRC at a shaft center after quenching. Given one-hour temper losses are 9 HRC at 500 °C and 17 HRC at 600 °C. The center must retain at least 40 HRC, and the steel is susceptible to impurity-driven temper embrittlement. With linear interpolation, what is the highest tempering temperature and suitable cooling choice?
  1. About 600 °C, followed by fast cooling
  2. About 538 °C, followed by slow cooling
  3. About 500 °C, followed by slow cooling
  4. About 538 °C, followed by fast cooling
Show answerHide answer

Save this lesson to see this answer.

Question 9 of 10

A reaction has n=2 and is 20% transformed after 30 s at one temperature. A production hold must reach at least 90% in no more than 80 s at that same temperature. Does the fitted Avrami relation support the plan?
  1. Yes; 90% requires about 64 s.
  2. No; 90% requires about 96 s.
  3. Yes; 90% requires about 45 s.
  4. No; 90% requires about 135 s.
Show answerHide answer

Save this lesson to see this answer.

Question 10 of 10

A two-stage path leaves 25% pearlite and 45% bainite before a final cooling step. A marked martensite-fraction relation shows that the final temperature converts 80% of the then-remaining austenite. What final fractions follow?
  1. 25% pearlite, 45% bainite, 24% martensite, 6% austenite
  2. 25% pearlite, 45% bainite, 30% martensite, 0% austenite
  3. 25% pearlite, 45% bainite, 6% martensite, 24% austenite
  4. 0% pearlite, 45% bainite, 44% martensite, 11% austenite
Show answerHide answer

Save this lesson to see this answer.

Stuck on your own question? Homework Help

Key Terms

94 Key Terms, each with its definition

A

A1
A1 is the equilibrium eutectoid critical temperature, taken as 727 °C for the iron–iron carbide data used in this material.
A process anneal stays below A1, while full annealing includes an appropriate austenitizing stage.
A3
A3 is the equilibrium upper critical boundary above which a hypoeutectoid steel becomes fully austenitic at its composition.
A 0.45 wt% carbon forging with A3 near 780 °C needs a higher temperature for full austenitizing.
Acm
Acm is the equilibrium boundary between austenite plus cementite and fully austenitic hypereutectoid steel.
Normalizing above Acm can dissolve a grain-boundary cementite network before faster air cooling.
Activation energy
An activation energy is the energy barrier that controls the temperature sensitivity of a thermally activated process such as diffusion.
Two recrystallization rates at different absolute temperatures can be used to estimate activation energy.
Aging curve
An aging curve plots hardness or strength against aging time at one temperature, showing development of a peak and later overaging.
Comparing two aging curves helps choose between maximum strength and a shorter production cycle.
AISI/SAE designation
An AISI/SAE designation identifies a steel family and, for common carbon and low-alloy steels, a nominal carbon level in its final digits.
The 41 family identifies Cr–Mo steel, while 40 in 4140 indicates about 0.40 wt% carbon.
Aluminum temper
An aluminum temper is a letter-and-number designation describing processing condition after the alloy number, rather than a different chemistry.
6061-O and 6061-T6 share an alloy identity but represent very different supplied conditions.
Artificial aging
Artificial aging is controlled elevated-temperature holding that accelerates precipitation and develops a chosen strength condition.
A 6061 component can be artificially aged after quenching to establish its T6 thermal condition.
Athermal transformation
An athermal transformation is one whose extent follows the temperature reached instead of increasing through a hold at that temperature.
Waiting at 180 °C does not increase martensite fraction when the steel follows athermal behavior.
Austempering
Austempering is quenching to a bainitic hold above Ms and waiting until the austenite-to-bainite transformation has completed.
A suitable thin steel spring can be austempered to gain strength and toughness with limited distortion.
Austenite
Austenite is the FCC iron-based solid solution that dissolves carbon and serves as the parent structure for many steel heat treatments.
A fully austenitized specimen can become pearlite, bainite, or martensite depending on its cooling path.
Austenitizing
Austenitizing is heating and holding steel to establish the austenite condition needed for its subsequent transformation treatment.
Excessive austenitizing temperature can coarsen grains even when the later quench is fast enough.
Avrami equation
The Avrami equation is a relation between transformed fraction and time for a reaction described by fixed nucleation-and-growth constants.
A measured 40% conversion at 60 s can help determine an Avrami constant when the exponent is known.

B

Bainite
Bainite is a nonlamellar steel microstructure of ferrite and fine carbides formed from austenite below the pearlite temperature range.
An isothermal hold at 400 °C can form upper bainite when the steel's TTT diagram supports that path.
Body-centered tetragonal lattice
A body-centered tetragonal lattice has a central atom and unequal cell lengths, as in carbon-distorted steel martensite.
Trapped interstitial carbon stretches the martensite cell along one direction after a rapid quench.
Brass
A brass is a copper–zinc alloy family that combines useful corrosion resistance and formability with properties set by composition.
Cartridge brass containing about 30 wt% zinc is useful where sheet or tube must be formed.

C

Carburizing
Carburizing is diffusion of carbon into a low-carbon steel surface before hardening to obtain a wear-resistant case over a tougher core.
A carburized gear can combine high tooth-surface hardness with a core that better tolerates impact.
CCT diagram
A CCT diagram shows transformation boundaries and products for continuously cooled steel rather than constant-temperature holds.
A furnace-cooling curve should be followed on a CCT diagram when predicting the final pearlite structure.
Cementite
Cementite is the hard iron carbide Fe₃C containing 6.70 wt% carbon, present as layers, particles, or boundary networks in steels.
Cementite layers reinforce pearlite, while a continuous boundary network can make steel brittle.
Coherent precipitate
A coherent precipitate has an interface whose atomic lattice fits continuously with the surrounding matrix, creating local strain.
Fine coherent particles can strengthen an alloy through strain fields and resistance to dislocation cutting.
Cooling curve
A cooling curve records temperature against time for a location in a part, defining the transformation history experienced there.
The surface and center of a quenched cylinder follow different cooling curves on the same CCT diagram.
Critical cooling rate
The critical cooling rate is the slowest rate that avoids diffusional products and permits fully martensitic steel after deep enough cooling.
A steel with a lower critical cooling rate can harden in thicker sections under the same quench.
Critical radius
The critical radius is the particle size at the top of the nucleation energy barrier, above which further growth lowers free energy.
Increasing undercooling reduces the critical radius when the interface energy remains unchanged.

D

Delivery condition
A delivery condition describes the supplied processing state of a metal, which can be specified separately from its alloy grade.
The +QT suffix requests a quenched-and-tempered condition instead of merely identifying composition.
Ductile iron
Ductile iron is cast iron with mainly rounded graphite nodules that reduce stress concentration and improve strength and ductility.
A valve body can use ductile iron when graphite-flake iron would provide too little tensile ductility.
Ductility
Ductility is the capacity for plastic deformation before fracture, commonly measured by elongation or reduction in area.
Spheroidized high-carbon steel has useful ductility for forming before a later hardening treatment.

E

EN steel name
An EN steel name encodes a steel's composition or its use and specified properties according to the applicable naming rules.
C45 conveys carbon content, while S355JR conveys a structural strength and impact-test class.
Equivalent Jominy distance
An equivalent Jominy distance is a test-bar position representing the cooling behavior of a specified location in a quenched component.
A chart can map the center of an oil-quenched bar to a test-bar position, such as 14 mm, used to read a hardness curve.
Eutectoid reaction
A eutectoid reaction is a solid-state transformation in which one solid phase forms two different solid phases at a specific condition.
At 727 °C, eutectoid austenite containing 0.76 wt% carbon forms ferrite and cementite.

F

Ferrite
Ferrite is the BCC iron-based solid solution with low carbon solubility that forms the soft matrix in many ordinary steel microstructures.
A slowly cooled low-carbon sheet contains much ferrite, helping it deform during a drawing operation.
Full annealing
Full annealing is suitable austenitizing followed by slow furnace cooling to develop a relatively soft, coarse steel structure.
A medium-carbon forging may be fully annealed before a machining operation that needs a softer condition.

G

GP zone
A GP zone is an early solute-rich cluster, such as a thin copper-rich disk in Al–Cu, that fits coherently within the matrix.
GP zones precede later transition precipitates during decomposition of a quenched Al–Cu solution.
Grain refinement
Grain refinement is a decrease in characteristic grain size, achieved in normalizing through new grains formed during phase changes.
New austenite grains and later ferrite–pearlite nucleation refine the original coarse structure.
Gray iron
Gray iron is a cast iron with graphite flakes in a ferritic or pearlitic matrix, giving strong damping but limited tensile ductility.
A machine-tool bed benefits from gray iron's damping when vibration would reduce machining accuracy.
Growth
Growth is the enlargement of a viable new-phase region as its interface advances and consumes material from the parent phase.
Carbon transport helps control growth when austenite decomposes into ferrite and cementite.

H

Half-transformation time
The half-transformation time is the duration needed for a reaction at a specified temperature to reach a transformed fraction of one half.
A reduction in half-transformation time from 100 s to 25 s means the conventional rate quadruples.
Hardenability
Hardenability is the ability of steel to form martensite to a useful depth under a specified cooling or quenching condition.
Two 0.40 wt% carbon steels may reach similar end hardness but show different Jominy curve shapes.
Hardness
Hardness is resistance to local plastic indentation, measured by a specified test such as Rockwell C or Brinell hardness.
A hardness reading helps compare two heat-treated conditions but does not directly measure their toughness.
Heterogeneous nucleation
Heterogeneous nucleation is the formation of a new phase on an existing surface or defect that reduces the nucleation energy barrier.
Grain refiners provide sites for heterogeneous nucleation and help create a finer cast structure.
HSLA steel
An HSLA steel is a high-strength low-alloy steel with low carbon and small alloy additions that preserve useful forming and welding behavior.
An HSLA grade can supply a pipeline with more strength than an ordinary low-carbon steel.

I

Induction hardening
Induction hardening uses induced electrical heating to austenitize a surface layer before quenching, without first adding carbon.
A medium-carbon shaft can be induction hardened locally where its surface needs greater wear resistance.
Interface energy
Interface energy is the excess energy per unit area associated with the boundary separating two phases or differently oriented regions.
A new spherical nucleus must supply enough volume-energy reduction to offset its interface-energy cost.
Isothermal hold
An isothermal hold is a period at an approximately constant temperature during which a time-dependent transformation can progress.
For a steel that forms bainite fully within 200 s at 400 °C, a rapid transfer followed by a 200 s hold there can complete the reaction.

J

Jominy end-quench test
The Jominy end-quench test measures steel hardenability by recording hardness with distance from one water-quenched end of a standard bar.
Hardness remaining high far from the quenched end indicates a strong response at slower cooling rates.

L

Logarithmic time axis
A logarithmic time axis spaces equal time ratios equally, allowing very short and very long transformation times on the same diagram.
The intervals from 1 to 10 s and from 10 to 100 s occupy equal widths on a logarithmic axis.
Lower bainite
Lower bainite is a bainitic structure containing very fine carbide particles within ferrite plates, formed closer to Ms.
A suitable lower-bainite treatment can combine high strength with better toughness than upper bainite.

M

Malleable iron
Malleable iron is produced by prolonged heat treatment of white iron to decompose cementite into graphite clusters and improve ductility.
A casting can gain a more deformable condition when its white-iron starting structure is made malleable.
Martempering
Martempering is interrupted quenching with a short hold just above Ms to equalize temperature before cooling through martensite formation.
A martempered component still needs a temper after its more uniform martensitic transformation.
Martensite
Martensite is a metastable steel phase formed by a rapid diffusionless lattice change that traps carbon from the parent austenite.
Austenite surviving a fast quench begins forming martensite after the temperature drops below Ms.
Martensite finish temperature
The martensite finish temperature, Mf, is the cooling temperature associated with practical completion of martensite formation.
A final quench specified below Mf lets an idealized path convert all remaining austenite to martensite.
Martensite start temperature
The martensite start temperature, Ms, is the temperature below which austenite begins transforming into martensite during cooling.
Alloy composition can lower Ms even while increasing the steel's ability to harden through a thick section.
Material number
An EN material number is a numerical grade identifier such as 1.4301, distinct from a chemical-content formula or delivery-condition suffix.
A drawing may identify X5CrNi18-10 by its material number 1.4301 while listing the required product standard.
Metastable state
A metastable state is a structure that persists despite not having the lowest available free energy because change is kinetically hindered.
A quenched supersaturated solid solution can persist until aging supplies enough mobility for precipitation.
Microconstituent
A microconstituent is a recognizable region or arrangement in a microstructure that can contain one phase or several phases.
Pearlite is one microconstituent even though its layers belong to two distinct phases.
Multistep thermal path
A multistep thermal path is a sequence of temperature changes and holds whose successive transformations determine the final structure.
A pearlite hold followed by a complete bainite hold can leave two products without final martensite.

N

Natural aging
Natural aging is strengthening-related precipitation that develops at room temperature after solution treatment and quenching.
Refrigerating certain quenched aluminum rivets slows natural aging until the rivets can be installed.
Nickel superalloy
A nickel superalloy is a nickel-based alloy designed to retain useful mechanical strength at high temperature, often through precipitation.
Alloy 718 is used in turbine-related components exposed to temperatures that soften many other alloys.
Normalizing
Normalizing is heating above the appropriate upper critical boundary, holding for austenitization, and cooling steel in still air.
A coarse forging can be normalized before a later hardening cycle to improve structural uniformity.
Nose
The nose is the region of a transformation-start curve with the shortest start time and greatest vulnerability to early transformation.
Alloying that shifts the nose to longer times makes a practical quench more likely to avoid it.
Nucleation
Nucleation is the formation of small regions of a new phase that can survive and begin growing within a parent material.
Ferrite often begins by nucleation at the boundaries of austenite grains during slow steel cooling.

O

Overaging
Overaging is aging beyond peak strength as particles coarsen, become more widely spaced, and lose strengthening effectiveness.
A long hold after the hardness maximum can soften an alloy even though precipitation has continued.

P

Peak-aged condition
The peak-aged condition is the time-dependent precipitate state that gives maximum strength or hardness at a specified aging temperature.
A hotter aging curve may reach its peak sooner while never reaching the colder curve's maximum hardness.
Pearlite
Pearlite is a two-phase eutectoid microconstituent made of alternating ferrite and cementite layers that grow together from austenite.
Lower transformation temperature within the pearlite range produces finer layers and higher hardness.
Precipitation hardening
Precipitation hardening is strengthening by a fine dispersion of second-phase particles created through solution treatment, quenching, and aging.
A heat-treatable aluminum bracket reaches its stronger condition when aging develops fine precipitates.
Process annealing
Process annealing is a subcritical treatment that restores cold-worked metal's ductility through recovery and recrystallization.
Cold-drawn wire can be process annealed between drawing passes when its remaining ductility is low.
Proeutectoid phase
A proeutectoid phase is ferrite or cementite that forms from austenite before the remaining austenite undergoes the eutectoid reaction.
A hypoeutectoid steel forms proeutectoid ferrite, whereas a hypereutectoid steel forms proeutectoid cementite.

Q

Quench severity
Quench severity describes the cooling intensity produced by a medium and its conditions, including agitation and temperature.
A more severe quench may harden deeper but increase the chance of distortion around a sharp corner.

R

Refractory metal
A refractory metal is a very-high-melting metal, such as tungsten or molybdenum, used where high-temperature resistance is important.
A high-temperature application may call for a refractory metal when aluminum's low melting point is limiting.
Retained austenite
Retained austenite is parent austenite left in a steel after cooling has formed martensite without completing the transformation.
A high-carbon steel with Mf below room temperature can retain austenite after an ordinary quench.

S

Secondary hardening
Secondary hardening is an increase in hardness during tempering of some high-alloy steels as fine alloy-carbide precipitates develop.
A tool steel can resist the ordinary softening trend when Mo, V, or W carbides form during tempering.
Solution heat treatment
Solution heat treatment heats an alloy into the suitable solid-solution field and holds it to dissolve the hardening second phase.
Copper-rich particles dissolve during a suitable Al–Cu solution treatment, supplying solute for later aging.
Solvus
A solvus is a phase-diagram boundary separating a single solid solution from a region containing that solid solution and another solid phase.
Solution treatment moves the selected alloy above its solvus without crossing into a melting region.
Spheroidite
Spheroidite is a soft steel microstructure with rounded cementite particles dispersed through a continuous ferrite matrix.
A long hold just below A1 prepares a high-carbon bar for machining by promoting spheroidite.
Spheroidizing
Spheroidizing is a heat treatment that rounds cementite particles in ferrite to soften medium- and high-carbon steels for shaping.
Holding a bearing-steel bar near 700 °C for many hours promotes a machinable spheroidized condition.
Stainless steel
A stainless steel is an iron-based alloy with at least about 10.5 wt% chromium that can form a protective chromium-rich oxide film.
A martensitic stainless grade can provide a corrosion-resistant knife with a hardenable cutting edge.
Strain hardening
Strain hardening is strengthening through plastic deformation that increases resistance to further deformation without requiring precipitation.
An H14 aluminum sheet gains its half-hard condition through controlled cold work.
Stress-relief annealing
Stress-relief annealing is controlled heating and cooling that relaxes residual stresses while aiming to preserve the main microstructure.
A machined frame can receive stress relief to reduce later distortion during precision finishing.
Supersaturated solid solution
A supersaturated solid solution contains more dissolved solute than its equilibrium solubility at the current temperature permits.
Rapid cooling preserves excess copper in aluminum until diffusion during aging enables precipitation.

T

T6 temper
The T6 temper is an aluminum condition produced by solution heat treatment followed by artificial aging to a stable condition.
A structural 6061-T6 extrusion relies on its precipitate structure for much of its strength.
Temper embrittlement
Temper embrittlement is a toughness loss caused by impurity segregation to prior austenite grain boundaries in susceptible steels.
Fast cooling after an appropriate temper can reduce impurity segregation while preserving the chosen hardness.
Tempered martensite
Tempered martensite is the ferrite-and-fine-carbide structure produced when quenched steel is reheated below its austenite range.
A quenched-and-tempered bolt combines substantial strength with better toughness than its as-quenched state.
Tempered martensite embrittlement
Tempered martensite embrittlement is a toughness loss associated with tempering quenched steels in an intermediate low-temperature range.
A part needing high toughness avoids the approximate 250–400 °C range when its steel is susceptible.
Tempering
Tempering is reheating quenched steel below A1 to alter its carbide structure, relieve stress, and adjust hardness and toughness.
A high-temperature temper is useful for a loaded axle that needs toughness as well as strength.
Through-hardening
Through-hardening is development of the required hardened structure across a component's section, including its slower-cooling interior.
An alloy steel may through-harden in oil when a plain-carbon steel of equal carbon remains soft at its center.
Toughness
Toughness is the ability of a material to absorb energy before fracture, depending on its structure and the conditions of loading.
A loaded shaft may need a higher temper to improve toughness even though its hardness decreases.
Transformation rate
The conventional transformation rate is the reciprocal half-transformation time, used to compare the characteristic speed of reactions.
A half-time of 80 s corresponds to a transformation rate of 0.0125 s⁻¹ at that temperature.
Transformation-finish curve
A transformation-finish curve joins the times when a reaction is practically complete, often defined as about 99% transformed.
A hold beyond the finish curve leaves little parent austenite for the later quench to transform.
Transformation-start curve
A transformation-start curve joins the times at which a small defined fraction of the parent phase has transformed at each temperature.
A quench must pass to the left of the relevant start curve to prevent that product from forming.
TTT diagram
A TTT diagram maps transformation times and products during constant-temperature holds for a specified steel and starting condition.
On a steel's TTT diagram, a hold at 650 °C that reaches the 50% curve leaves half pearlite and half austenite.

U

Undercooling
Undercooling is the temperature drop below an equilibrium transformation temperature that increases the driving force for a new phase.
Large undercooling can favor nucleation even while low atom mobility limits the overall transformation.
UNS designation
A UNS designation is a unified material identifier consisting of a family letter and five digits, used across several metal families.
S30400 identifies a stainless grade, while G41400 identifies a carbon-and-alloy-steel grade.
Untransformed austenite
Untransformed austenite is the portion of the parent structure still available to form later products during a thermal path.
After 30% pearlite forms, the remaining 70% austenite supplies any later bainite or martensite.
Upper bainite
Upper bainite is a bainitic structure with cementite mainly between ferrite laths, formed in the warmer part of the bainite range.
A feathery optical appearance can suggest upper bainite, but fine carbide details need higher resolution.

W

White iron
White iron is a hard, brittle cast iron in which much of the carbon is retained as cementite instead of free graphite.
A wear-resistant liner may use white iron where hardness matters more than easy machining.

About this lesson

By StudeliReport a mistake

Make your own Study Materials

Turn your notes, slides and documents into Study Guides, Practice Questions, Flashcards and 6 more tools.

Get Started