Ceramics, Polymers and Composites

Learn how the structure of ceramics, polymers and composites explains the way they behave. Predict ceramic crystal structures and explain why ceramics are hard but brittle, and see how glass is shaped and tempered and how cement hardens into concrete. Describe polymer chains, their molecular weight and crystallinity, compare thermoplastics, thermosets and elastomers, and interpret how polymers respond to temperature, load and time. Finally, use the rule of mixtures and the critical fiber length to explain how fibers and matrices share the load in composites, from short-fiber moldings to laminates and sandwich panels.

BeginnerLesson 8 of 9 in Materials Science and Engineering Course

What you will learn

  1. Explain how bonding, ion sizes and charge balance set the crystal structures of ceramics, how silicate and carbon structures are built, and why ceramics are hard, stiff and brittle.
    • Predict the crystal structures and densities of ionic ceramics
      Use charge neutrality and the cation–anion radius ratio to predict coordination and crystal structure, and calculate the theoretical density of a ceramic.
    • Describe silicate and carbon structures
      Build silicate structures from linked SiO₄ tetrahedra, check their charge balance, and compare diamond, graphite, graphene, nanotubes and fullerenes.
    • Explain the mechanical behavior of ceramics
      Explain why ceramics fracture in a brittle way, calculate flexural strength from a bend test, and describe how porosity and flaws lower stiffness and strength.
  2. Describe how glass behaves as it cools and how it is shaped and strengthened, how clay and powder products are formed and fired, and how cement hardens to bind concrete.
    • Explain glass behavior, forming and tempering
      Use the specific volume and viscosity of glass to explain how it is formed, annealed and tempered, and describe how glass-ceramics are made.
    • Describe clay products, refractories and advanced ceramics
      Explain how clay and powder ceramics are shaped, dried, fired and sintered, and match refractories, abrasives and advanced ceramics to their uses.
    • Explain how cement hardens and how concrete behaves
      Describe how portland cement is made and how hydration hardens it, use the water–cement ratio, and explain why concrete is reinforced or prestressed.
  3. Describe polymers as long chains of repeat units, calculate their average molecular weights, classify their molecular structures and configurations, and explain how far and why they crystallize.
    • Describe polymer chains and calculate molecular weight
      Identify monomers and repeat units, distinguish how chains form, and calculate number-average and weight-average molecular weight and degree of polymerization.
    • Classify molecular structures, configurations and copolymers
      Distinguish linear, branched, crosslinked and network polymers, tacticity and cis–trans forms, and the main types of copolymer, and relate each to properties.
    • Explain polymer crystallinity and calculate it from density
      Describe chain-folded lamellae and spherulites, predict which polymers crystallize, calculate percent crystallinity from densities, and relate crystallinity to properties.
  4. Use the glass transition and melting temperatures, the classes of thermoplastics, thermosets and elastomers, stress–strain curves and viscoelastic behavior to explain and predict how polymers perform.
    • Interpret melting and the glass transition in polymers
      Distinguish melting from the glass transition, read specific volume curves, and explain how chain structure shifts both temperatures and what they mean for service temperature.
    • Compare thermoplastics, thermosets and elastomers
      Explain how each class responds to heat in terms of chain structure, how rubber elasticity and vulcanization work, and choose a class for a simple application.
    • Interpret polymer stress–strain behavior
      Read the three types of polymer stress–strain curve, calculate modulus, yield and tensile strength from test data, and explain how temperature, strain rate and structure change the response.
    • Describe viscoelastic behavior and creep in polymers
      Distinguish elastic, viscous and viscoelastic responses, calculate a relaxation modulus, interpret its change with temperature, and explain creep under constant load.
  5. Classify composites, estimate their properties with the rule of mixtures, explain how fibers, matrix and interface share the load, and analyze aligned, short-fiber, laminated and sandwich composites.
    • Classify composites and estimate particle-composite properties
      Define a composite and its phases, compare the main classes and matrix types, and bound the modulus of a particle-reinforced composite with the rule of mixtures.
    • Explain the roles of fibers, matrix and interface
      Describe what fibers and matrices each contribute, compare common fiber and matrix materials, and use the critical fiber length to judge when fibers reinforce effectively.
    • Apply the rule of mixtures to continuous aligned fibers
      Derive and use the longitudinal and transverse moduli, the fiber load fraction and the longitudinal strength of a continuous aligned fiber composite.
    • Analyze short-fiber, random-fiber and structural composites
      Estimate the strength of discontinuous aligned composites and the modulus of randomly oriented ones, and explain how laminates, sandwich panels and hybrids are designed, using specific stiffness to compare materials.

Ceramics, Polymers and Composites study guide

5 chapters

1

Ceramic structure and brittle behavior

An oxide insulator, a glass pane and a diamond tool are all ceramics, yet their properties differ sharply. Start with the atoms: their charges, sizes and bonds decide which arrangements can form. Then connect those arrangements to density, hardness and the movement of cracks. Calculations with unit cells and bend tests turn these structural ideas into properties that can be measured and compared.

1.1 Ion packing, defects and theoretical density

Ceramics are inorganic, nonmetallic solids. Most are compounds such as oxides, nitrides and carbides; glasses and several forms of carbon also belong to this class. Bonding ranges from largely ionic in MgO to largely covalent in silicon carbide. For ionic crystals, composition and packing have to work together.

Balance charge, then examine size

A crystal must be electrically neutral. A calcium ion has charge +2 and a fluoride ion has charge −1, so calcium fluoride has two fluoride ions per calcium ion: CaF₂. This formula fixes the ratio of ions, but it does not by itself specify their positions.

The coordination number is the number of nearest anions around a cation. Divide the cation radius by the anion radius to estimate the coordination favored by ionic packing:

Radius ratioTypical coordinationArrangement
Below 0.1552Linear
0.155–0.2253Triangle
0.225–0.4144Tetrahedron
0.414–0.7326Octahedron
0.732–1.08Cube

These geometric ranges guide predictions for mostly ionic compounds. Directional covalent bonds can favor another arrangement. The lower octahedral limit, 2−1≈0.414, comes from the geometry at which surrounding anions touch both one another and the central cation.

Recognize the main structures

For NaCl, 0.102/0.181=0.564, predicting sixfold coordination. In rock salt, chloride ions occupy face-centered cubic positions and sodium ions fill every octahedral hole. The conventional cell contains four NaCl formula units. MgO and FeO share this structure.

CsCl has a ratio of about 0.94 and eightfold coordination. One ion species occupies the corners and the other the center. This is a simple cubic lattice with a two-ion basis, not a BCC Bravais lattice: a corner and the center are chemically different sites.

In zinc blende, anions occupy FCC positions and cations fill half the tetrahedral holes; ZnS has fourfold coordination and substantial covalent bonding. SiC can adopt this structure. In fluorite, CaF₂, calcium has eight fluoride neighbors. The different ion ratio changes which sites are occupied. In cubic perovskite, BaTiO₃, barium occupies corners, oxygen face centers and titanium the center. Below about 120 °C a small displacement of ions creates electric polarization and a response between electric fields and strain, useful in capacitors and sensors.

Calculate mass per cell volume

The theoretical density is

ρ=n′Ma3NA.

Here n′ counts formula units, M is the molar mass of one formula unit, a is the cubic cell edge and NA=6.022×1023 mol⁻¹. For NaCl, contact occurs along an edge:

a=2(0.102+0.181)=0.566 nm.

Use M=0.05844 kg/mol and convert the edge to 0.566×10−9 m before cubing:

ρ=4(0.05844)(0.566×10−9)3(6.022×1023)≈2140 kg/m3.

Counting eight ions as eight formula units would double the answer. Taking an edge from a metallic packing formula would also give the wrong volume.

Keep defects electrically neutral

A Frenkel defect moves a cation from its normal site to an interstitial site, leaving a vacancy. A Schottky defect in an MX crystal removes one cation and one anion. Both preserve neutrality. Replacing Na⁺ with Ca²⁺ in NaCl requires one sodium vacancy per calcium substitution. In nonstoichiometric Fe₁₋ₓO, every two Fe³⁺ ions replacing Fe²⁺ are balanced by one vacant iron site.

Key Takeaways

  • Charge balance fixes ion ratios; radius ratio guides coordination in mostly ionic crystals.
  • Rock salt has sixfold coordination and four formula units per conventional cell.
  • CsCl is a simple cubic lattice with a two-ion basis.
  • Theoretical density is cell mass divided by cell volume; convert length before cubing.
  • Ionic defects and substitutions must preserve overall charge neutrality.
  • Fluorite, zinc blende and perovskite have different site occupancies and coordinations.

1.2 Silicate networks and forms of carbon

The same building unit can produce very different solids. Silicates use tetrahedra joined in different patterns; carbon uses different bonding arrangements of the same element. In each case, the connections between units explain properties that composition alone cannot.

Count shared oxygen atoms

A silicate tetrahedron, SiO₄⁴⁻, contains silicon bonded to four corner oxygens. The silicon contributes +4 and the oxygens contribute −8, leaving charge −4. Neighboring tetrahedra can share corner oxygen atoms.

In silica, every corner is shared by two tetrahedra. Four half-oxygens per silicon give the formula SiO₂ and a neutral three-dimensional network. Quartz, cristobalite and tridymite are crystalline forms of this composition. Quartz has a relatively open structure and a density near 2650 kg/m³; silica melts near 1710 °C.

With no shared corners, forsterite contains isolated SiO₄⁴⁻ units. Two Mg²⁺ ions balance each one, giving Mg₂SiO₄. Sharing two corners per tetrahedron makes chains; sharing three makes sheets with the repeat composition (Si₂O₅)²⁻. Do not count a shared oxygen twice when finding the formula.

Kaolinite has composition Al₂(Si₂O₅)(OH)₄. Check its charge in parts:

2(+3)+[2(+4)+5(−2)]+4(−1)=6−2−4=0.

Its layered structure produces plate-shaped particles. Water films between particles let the plates slide, making wet clay easy to shape. Mica also has a layered silicate structure and splits into thin sheets.

Compare a crystal with a glass

Fused silica contains corner-linked tetrahedra like crystalline silica, but lacks long-range order. The crystal melts at a definite temperature; the glass softens through a range as its resistance to flow falls.

Network modifiers, including Na₂O and CaO, introduce nonbridging oxygens that interrupt Si–O–Si links. This lowers the softening temperature. Typical soda-lime glass contains roughly 70 wt% silica, 15 wt% sodium oxide and 10 wt% calcium oxide, with other ingredients making up the balance. Intermediate oxides such as Al₂O₃ can join the network. Composition controls how connected the network is and how easily the glass can be formed.

Follow the bonds in carbon
FormAtomic arrangementMain property and use
DiamondEach atom bonded to four neighbors in a 3D networkExtremely hard; cutting tools and abrasives
GraphiteStrong hexagonal sheets, weak attraction between sheetsSoft, electrically conducting along sheets; lubricant and electrodes
GrapheneOne hexagonal sheetVery high in-plane stiffness and electrical conductivity
Carbon nanotubeA sheet wrapped into a cylinderHigh axial stiffness and strength; reinforcement
FullereneA closed molecular cage, such as C₆₀Nanoscale carbon molecule

Diamond also conducts heat well while electrically insulating. Its extended covalent network resists deformation. Graphite's softness comes from layers sliding across one another, not from weak carbon bonds within each sheet. Those in-plane bonds remain strong.

A nanotube is only a few nanometers across and can have an axial modulus near 1 TPa. That property belongs to the nanotube's structure and direction; turning nanotubes into a bulk composite also requires effective dispersion and load transfer.

Key Takeaways

  • Silicate structures differ in shared tetrahedron corners and charge-balancing cations.
  • Quartz and fused silica have the same composition but different long-range order.
  • Network modifiers interrupt silica-network links and lower the softening temperature.
  • Diamond resists deformation through a three-dimensional covalent network.
  • Graphite has strong bonds within sheets and weak attraction between sheets.

1.3 Flaws, bend tests and porosity

A ceramic can be stiff and hard yet break suddenly. Stiffness describes elastic resistance to deformation; hardness describes resistance to indentation. Neither tells you how much energy the material can absorb before a crack causes failure.

Why cracks dominate strength

At room temperature, most ceramics deform elastically and then fracture with little plastic strain. Ionic slip can bring like charges together, and covalent bonds resist changes in direction. Dislocations therefore move with difficulty. Glass lacks crystal slip planes; at high temperatures it can deform permanently by viscous flow.

Pores, scratches and microcracks concentrate tensile stress. The most severe flaw starts fracture, so measured strength is far below the strength implied by ideal bonds. Nominally identical specimens can fail at different stresses. Larger parts are more likely to contain a severe flaw, and damaged surfaces are especially important because bending puts one surface in tension.

Compression closes cracks while tension opens them. Ceramic compressive strength is often roughly ten times tensile strength. This explains the use of compression in masonry arches, prestressed concrete and strengthened glass. Strong bonds give a high modulus, but limited crack-tip plasticity gives low toughness.

Find flexural strength

Gripping a brittle specimen in a tensile test can cause premature failure. A bend test supports a bar and loads it until its tensile face fractures. For a rectangular bar in three-point bending,

σfs=3FfL2bd2.

The fracture load is Ff, support span is L, width is b, and depth parallel to the loading direction is d. This flexural strength is also called the modulus of rupture. For a circular bar of radius R, use σfs=FfL/(πR3). Four-point bending places a larger region under the maximum bending stress.

For an alumina bar, take a 40 mm span, 4.0 mm width, 3.0 mm depth and 250 N fracture load:

3FfL=3(250)(40)=30 000, 2bd2=2(4)(32)=72, σfs=30 000/72=417 MPa.

Using newtons and millimeters gives N/mm², equal to MPa. Depth is squared, so swapping width and depth changes the result. A modulus of rupture is a strength, not an elastic modulus. The elastic modulus instead comes from the elastic load–deflection slope together with specimen geometry.

Account for pores

Dense alumina has an elastic modulus near 380 GPa, compared with about 70 GPa for soda-lime glass. Porosity removes load-bearing material and adds stress concentrations. A common empirical relation is

E=E0(1−1.9P+0.9P2),

where P is pore volume fraction and E0 is the pore-free modulus. With 5% pores, use 0.05:

E=380[1−1.9(0.05)+0.9(0.05)2]≈345 GPa.

Flexural strength often falls approximately as σfs=σ0exp⁡(−nP), with n fitted experimentally. A density measurement can reveal pores, but porosity alone does not capture the size and position of the worst flaw.

Diamond, cubic boron nitride, silicon carbide and alumina serve as abrasives because they are hard. Small Knoop or Vickers indentations measure ceramic hardness while limiting specimen damage. A hard cutting surface still needs protection against impact and tensile cracking.

Key Takeaways

  • Flaws concentrate tensile stress and produce scatter in ceramic strength.
  • Compression closes flaws; tension opens them.
  • Flexural strength is the tensile-face stress at fracture in a bend test.
  • Use the depth parallel to the load, squared, in the rectangular-bar formula.
  • Porosity lowers stiffness and strength.
  • High hardness or strength can coexist with low toughness.
2

Glass, fired ceramics and cement

Ceramic products reach their final form by several routes: glass flows while hot, powder particles bond during firing, and cement reacts with water. Each route leaves a different structure behind. Follow the change in viscosity, porosity or chemical bonding to explain the finished product, including why a glass surface can be strengthened and why freshly placed concrete must retain moisture.

2.1 Glass viscosity, shaping and strengthening

Glass is a noncrystalline solid. Cooling a melt fast enough to avoid crystallization preserves a disordered structure, but the material becomes rigid as atomic rearrangement slows. Heating reverses this gradual change in flow behavior.

Read temperature through viscosity

A crystal's specific volume drops abruptly when it freezes. Glass instead shows a continuous volume curve with a change of slope at the glass transition temperature, Tg. Above the transition it is a supercooled liquid; below it the structure is effectively frozen on the observation time scale. Faster cooling gives a somewhat higher measured transition temperature.

Viscosity measures resistance to flow. The conventional glassmaking points specify viscosities, not a universal temperature:

PointApproximate viscosity, Pa·sMeaning
Melting10Fluid melt
Working10³Easy shaping
Softening4 × 10⁶Shape starts to change noticeably
Annealing10¹²Stresses relax in about 15 minutes
Strain3 × 10¹³Stress relaxation is too slow for ordinary cooling

Forming usually occurs between the working and softening points. One poise equals 0.1 Pa·s, so 10³ Pa·s is 10⁴ poise. The same named viscosity point occurs at different temperatures for different glass compositions.

Fused silica softens near 1600 °C and has very low expansion. Soda-lime glass softens near 700 °C and is convenient for bottles and windows. Borosilicate glass, containing about 13 wt% boron oxide, expands little and tolerates temperature changes well.

Shape, then control cooling

Pressing makes plates and dishes; blowing makes hollow bottles and jars. Drawing pulls tubes, rods or fibers from a melt. In the float process, molten glass spreads on molten tin, producing smooth parallel surfaces for sheet glass.

Uneven cooling can trap residual stresses. Annealing holds glass near the annealing point and cools it slowly through the strain point so stresses can relax. Thermal tempering deliberately creates a useful stress pattern: heat the glass above its transition but below softening, then cool its surfaces rapidly with air jets. The surfaces stiffen first. As the hot interior later contracts, it leaves the surfaces compressed and the interior in tension.

Surface cracks must overcome this compression before they can open. With 100 MPa of surface compression and 80 MPa of bending tension, the net stress is

−100+80=−20 MPa,

still compressive. Fully tempered flat glass commonly has about 70–150 MPa surface compression and breaks into many small pieces. Cut and finish it before tempering; cutting afterward disrupts the stress system. Chemical strengthening also compresses the surface by replacing smaller sodium ions with larger potassium ions.

Crystallize glass deliberately

A glass-ceramic is shaped as glass, then heat treated to nucleate and grow fine crystals, often with a nucleating agent such as TiO₂. Tailored cooktop and ovenware compositions have very low thermal expansion. Unwanted crystallization in ordinary glass is called devitrification and can cause cloudiness and reduced strength.

Glass panes are not thicker at the bottom because they have flowed over centuries. Flow at room temperature is negligible; old pane thickness reflects manufacture and installation.

Key Takeaways

  • Glass softens through a range; its transition changes the slope of the specific-volume curve.
  • Viscosity points describe flow and stress relaxation; composition sets their temperatures.
  • Annealing relaxes residual stress, while tempering creates surface compression.
  • Glass-ceramics use controlled crystallization and tailored compositions.

2.2 From clay or powder to a ceramic product

A ceramic powder does not have to be melted into a liquid to become a solid part. Shape the particles first, then use drying and heating to develop a bonded structure. The starting mixture and the heat treatment determine the remaining pores, shrinkage and final properties.

Shape and dry clay

Water films let clay's plate-shaped particles slide. This hydroplastic mixture can be molded or pushed through a die to make bricks and pipes. In slip casting, a clay suspension enters a porous plaster mold. The mold removes water, leaving a layer against its walls. Draining the remaining slip produces a hollow body.

Drying removes water before firing. Particles approach one another and the body shrinks. If the surface dries well before the interior, unequal shrinkage can crack or warp the piece. Thick sections therefore need slow, controlled drying. Structural clay products include bricks, tiles and pipes; whitewares include porcelain, pottery and sanitary ware.

Understand firing and sintering

Traditional whiteware combines clay, quartz filler and feldspar flux. During firing, commonly around 900–1400 °C, the flux helps form a glassy liquid. It fills some pores and bonds surviving crystal particles on cooling. This vitrification lowers porosity and generally increases strength and shrinkage as firing proceeds.

Advanced ceramics such as alumina, zirconia and silicon nitride start from fine powders. Uniaxial pressing compresses them in a die. Isostatic pressing applies fluid pressure around a flexible mold; hot pressing combines pressure and heat. Tape casting spreads a slurry into a thin sheet for products such as electronic substrates.

In sintering, particles bond during heating below the bulk melting temperature. Atoms diffuse around contact regions, forming growing necks. Densifying sintering reduces pore volume and shrinks the body. The driving force is lower total surface energy as particle surfaces disappear. Do not picture the whole part becoming a pool of liquid: its high melting temperature is precisely why powder routes are useful.

Allow for shrinkage

Suppose a fired component must be 100 mm long and loses 15% of its initial length. The final length is 85% of the initial length:

100=0.85L0, L0=100/0.85=117.6 mm.

Adding 15% to the final dimension gives 115 mm, which shrinks to 97.75 mm. Shrinkage is measured relative to the initial size, so finding that size requires division.

Match structure to the job

Refractories line kilns, furnaces and glass tanks. They must resist heat and chemical attack from their surroundings. Fireclay, silica, magnesia and special alumina or zirconia refractories serve different environments. More porosity can improve insulation and resistance to rapid temperature change, but lowers strength and allows slag to enter more easily.

Abrasives need high hardness and enough toughness to survive useful cutting. Diamond, silicon carbide, tungsten carbide and alumina are used in grinding wheels, coated paper and polishing compounds.

Advanced ceramics exploit selected properties: silicon nitride for light bearing balls, alumina for electrical insulators, toughened zirconia for blades or dental crowns, and piezoelectric ceramics for sensors and ultrasound transducers. Dense, well-controlled microstructures help prevent critical flaws in these parts.

Key Takeaways

  • Water films make wet clay shapeable; uneven drying causes uneven shrinkage.
  • Vitrification forms a glassy bonding phase during firing.
  • Sintering grows bonds between particles without bulk melting.
  • Reverse a fractional shrinkage by dividing the required final size by the retained fraction.
  • Refractory porosity trades insulation against strength and resistance to penetration.

2.3 Hydration, water content and concrete reinforcement

Cement and concrete are different materials. Cement is the binder; concrete combines cement paste with fine and coarse aggregates. The paste hardens through a chemical reaction, and the aggregates provide most of the volume of the finished composite.

Make a hydraulic binder

Portland cement is a hydraulic cement: it reacts with water and can harden under water. Air-lime mortar instead hardens mainly by reacting with carbon dioxide from the air. Hardening cement is not simply drying a wet powder.

Manufacture starts with limestone mixed with clay or shale. A rotary kiln heats the mixture to about 1400–1500 °C. Limestone decomposes into lime and carbon dioxide, and the lime reacts with other oxides to produce nodules called clinker. Grinding clinker with a few percent gypsum produces cement powder; gypsum controls the early reaction so setting does not happen too fast. Both limestone decomposition and kiln fuel contribute to cement production's substantial carbon emissions.

Cement shorthand uses C for CaO, S for SiO₂, A for Al₂O₃ and F for Fe₂O₃. The main clinker compounds are tricalcium silicate, C₃S; dicalcium silicate, C₂S; tricalcium aluminate, C₃A; and tetracalcium aluminoferrite, C₄AF. These letters represent oxides, not individual elements.

Supply water for strength development

Hydrating calcium silicates form calcium silicate hydrate, C–S–H, plus calcium hydroxide. The fine C–S–H structure supplies most of the strength. C₃S reacts relatively quickly and gives early strength and heat; C₂S reacts more slowly and supports later strength gain.

Setting occurs over hours, but strength develops over weeks and months. A 28-day strength value is a common reference age, not an end to hydration. The reactions release heat, which can create temperature differences and cracking in large pours.

Curing maintains moisture and a suitable temperature so hydration continues. Early drying restricts the reaction and leaves a weaker surface. Prevent freezing during early strength development. Chemically bound water is only about one quarter of cement mass; additional water also occupies gel pores and gives a workable fresh mix.

The water–cement ratio is a mass ratio:

w/c=mwatermcement.

For 350 kg cement per cubic meter at a ratio of 0.45,

mwater=0.45(350)=157.5 kg.

Increasing the ratio to 0.60 uses 210 kg of water. The mix flows more easily, but excess water leaves capillary pores, lowering strength and durability. Ratio comparisons assume comparable materials, compaction and curing.

Place tensile resistance where it is needed

Concrete usually contains 60–80% aggregate by volume. Mortar contains paste and sand; concrete also contains gravel or crushed stone. Ordinary structural concrete often reaches 20–50 MPa in compression, but only about one tenth as much in tension.

Steel reinforcement placed in tensile regions carries tension after concrete cracks. Bond transfers load between steel and concrete; similar thermal expansion helps them remain compatible. The alkaline paste protects embedded steel while that protection remains intact.

Prestressing compresses concrete before service loads arrive. Tendons are tensioned before casting in pretensioning, or after hardening in post-tensioning. A face with 6 MPa precompression and 4 MPa service tension remains at −6+4=−2 MPa. Keeping the concrete compressed delays tensile cracking, using the same broad principle as surface compression in tempered glass.

Key Takeaways

  • Portland cement hardens by hydration, and curing supplies conditions for that reaction.
  • C–S–H supplies most strength; C₃S reacts earlier than C₂S.
  • The water–cement ratio uses masses; excess water increases capillary porosity.
  • Concrete contains paste, sand and coarse aggregate; cement is its binder.
  • Rebar carries tension, while prestressing introduces compression before service loading.
  • Concrete strength continues developing beyond the common 28-day reference age.
3

Polymer chains and crystalline regions

A polymer sample contains many chains, with different lengths, shapes and packing arrangements. These differences explain why two materials with the same repeat unit can feel very different. Learn to describe the chains, calculate useful molecular-weight averages and connect regular packing to crystallinity. Keep track of whether a fraction counts molecules, mass or volume: each answers a different question.

3.1 Repeat units and molecular-weight averages

A polymer is a macromolecule made of many linked repeat units. Strong covalent bonds hold the backbone together. Weaker attractions between chains, together with entanglements, strongly influence whether a bulk sample flows, stretches or stays rigid.

Identify what repeats

Monomers are the small starting molecules; repeat units are the structural patterns in the finished chain. Ethylene contains a carbon–carbon double bond. When it forms polyethylene, the atoms become the –CH₂–CH₂– repeat pattern with single backbone bonds. Monomer and repeat unit contain the same atoms in this case, but their bonding differs.

Replacing one hydrogen in the polyethylene pattern with chlorine gives the PVC pattern; a methyl group gives polypropylene; a phenyl ring gives polystyrene. Replacing all hydrogens with fluorine gives PTFE. A homopolymer contains one type of repeat unit.

In the introductory synthesis classification, addition or chain-growth polymerization adds monomers at active chain ends, as in PE, PP, PVC and PS. Condensation or step-growth reactions join molecules through reactive end groups and commonly release a small molecule; nylon 6,6 is a familiar condensation example. The reaction mechanism itself is separate from identifying a finished repeat unit.

Average a distribution correctly

A sample contains chains of different lengths. The number-average molecular weight weights each size class by its fraction of all chains:

Mˉn=∑ixiMi.

The weight-average molecular weight weights each size class by its mass fraction:

Mˉw=∑iwiMi.

A long chain counts as one molecule in the first average but contributes more mass in the second. Therefore Mˉw≥Mˉn. The ratio Mˉw/Mˉn is dispersity; it equals 1 when every chain has the same molecular weight.

For a PE sample with number fractions 0.20, 0.50 and 0.30 at 10 000, 30 000 and 50 000 g/mol:

Mˉn=2000+15 000+15 000=32 000 g/mol.

To obtain mass fractions, multiply each number fraction by its molecular weight and divide by the number average:

wi=xiMiMˉn.

The fractions are 0.0625, 0.46875 and 0.46875. They sum to 1. Then

Mˉw=625+14 062.5+23 437.5=38 125 g/mol.

Dispersity is about 1.19. Using the number fractions again in the weight-average formula would merely repeat the first average.

Relate molecular weight to chain length

The number-average degree of polymerization is

DP=Mˉnm,

where m is repeat-unit molar mass. PE has a repeat mass near 28.05 g/mol, so the sample has DP=32 000/28.05≈1140 units per chain. Keep both molar masses in the same units.

Single bonds can rotate, producing kinked random coils whose end-to-end distance is much shorter than their full contour length. Neighboring coils entangle. Longer chains usually increase entanglement, toughness and resistance to flow, while also raising melt viscosity. Very short chains can behave like waxes or liquids; ultrahigh-molecular-weight PE reaches several million g/mol and is used for wear-resistant joint components.

Key Takeaways

  • Monomers are starting molecules; repeat units describe the finished chain.
  • Number-average molecular weight uses number fractions, and weight-average uses mass fractions.
  • Dispersity is at least 1.
  • Degree of polymerization divides number-average molecular weight by repeat-unit molar mass.
  • Long chains form coils and entanglements that affect strength and flow.

3.2 Chain architecture, configuration and copolymers

A chemical repeat unit does not completely specify a polymer. Chains can have branches, links, different side-group arrangements or different sequences of units. These structural differences control how readily chains pack and whether they can move past one another.

Distinguish a branch from a crosslink
ArchitectureConnection patternTypical example
LinearLong separate chainsHDPE, PVC, nylon
BranchedSide chains attached to a backboneLDPE
CrosslinkedCovalent links between separate chainsVulcanized rubber
NetworkDense three-dimensional covalent connectivityCured epoxy

A branch is part of a molecule; a crosslink joins chains. Branched thermoplastics can soften and flow. A permanent crosslinked network prevents unrestricted chain sliding.

HDPE and LDPE have the same repeat unit. HDPE's nearly linear chains pack readily, giving typical densities of 940–970 kg/m³. More branching in LDPE disrupts packing, giving about 910–930 kg/m³. Greater crystallinity makes HDPE stiffer and gives it a higher melting range. This explains the different feel of a rigid container and a flexible PE film without requiring a different repeat unit.

Keep configuration separate from conformation

Conformation is the chain shape produced by rotations about single bonds. A coil can change shape without changing which atoms are bonded. Configuration fixes arrangements that require bond breaking and re-forming to change.

For a chain with pendant groups, tacticity describes their relative arrangement:

  • Isotactic chains have groups on the same side in the usual chain representation.
  • Syndiotactic chains have groups on alternating sides.
  • Atactic chains have an irregular arrangement.

Regular isotactic and syndiotactic structures can pack into crystals. Atactic arrangements generally hinder packing. Commercial isotactic polypropylene is semicrystalline and rigid; atactic polypropylene is soft and tacky. Stretching an atactic chain can change its conformation, but cannot make its configuration isotactic.

Cis and trans arrangements occur around double bonds that restrict rotation. Natural rubber is cis-polyisoprene, while trans-polyisoprene forms harder gutta-percha at room temperature. Their atom counts agree; their geometric configurations differ.

Read copolymer sequences

A copolymer contains at least two kinds of repeat unit. With A and B standing for those units, the sequence can be random, alternating, block or graft:

TypeArrangement
RandomIrregular A/B sequence
AlternatingABABAB…
BlockLong runs such as AAAA…BBBB…
GraftA backbone carrying branches made from B units

Styrene–butadiene rubber is a common random copolymer. Styrene–butadiene–styrene uses blocks whose different properties create rubbery behavior with heat-reversible physical junctions.

Architecture, configuration and sequence are separate descriptions. A graft copolymer is branched, but a branch containing a different repeat unit tells you more than the word "branched" alone. Linear and branched structures commonly make thermoplastics; dense permanent networks make thermosets. Regularity promotes crystallization, while irregularity interferes with it.

Key Takeaways

  • A branch extends one molecule; a crosslink covalently joins chains.
  • Linear HDPE packs more readily than branched LDPE.
  • Conformation changes by bond rotation; configuration requires bond changes.
  • Tacticity and cis–trans geometry affect packing and properties.
  • Copolymers can be random, alternating, block or graft.

3.3 Crystallinity, lamellae and density

Polymer chains are long and tangled, so complete ordering is difficult. Most polymers that crystallize contain ordered regions mixed with disordered material. The fraction that becomes crystalline affects density, stiffness, transparency and thermal behavior.

Build crystals from chain segments

In a crystalline region, chain segments pack into a regular repeating arrangement. Chains fold into thin plates called lamellae, often about 10 nm thick. Growing lamellae can radiate from a center into spherulites. Amorphous material remains between lamellae, and tie molecules connect neighboring ordered regions through that material. Under polarized light, spherulites show a characteristic dark cross.

A semicrystalline polymer is therefore not a collection of separate fully crystalline molecules mixed with fully amorphous molecules. Parts of a single chain can pass through both regions. Crystallinity can range from nearly zero to about 95%, depending on structure and thermal history.

Predict which chains pack

Linear, regular chains pack most easily. Small side groups, isotactic or syndiotactic configurations and regular alternating copolymer sequences support order. Branches, bulky irregular groups, random sequences and crosslinks hinder it. Slow cooling gives chains more time to arrange; fast cooling can trap a less ordered state.

Atactic polystyrene, PMMA and polycarbonate are essentially amorphous. Polyethylene commonly crystallizes strongly. PET can be clear when rapidly cooled into a largely amorphous state, or become opaque as crystalline structures develop during slower cooling.

More crystalline material is generally denser, stiffer, stronger and more resistant to solvents. Crystals continue to support a semicrystalline polymer above the glass transition of its amorphous regions. They disappear only on melting. Light scattering by crystalline structures often makes semicrystalline polymers translucent or opaque; an amorphous polymer can be clear.

Calculate a mass percentage

The fully crystalline density is higher than the fully amorphous density. If their values and the sample density are known, crystallinity by mass is

Xc=ρc(ρs−ρa)ρs(ρc−ρa),

where subscripts c, s and a denote fully crystalline, sample and fully amorphous material. Multiply by 100 to report a percentage. All densities must use the same units.

For PE, take crystalline density 1000 kg/m³, amorphous density 860 kg/m³ and sample density 950 kg/m³:

Xc=1000(950−860)950(1000−860)=90 000133 000=0.677.

The crystallinity is 67.7% by mass. Check the endpoints: inserting the amorphous density gives zero, and inserting the crystalline density gives one.

The simple density interval fraction,

(ρs−ρa)/(ρc−ρa)=90/140=0.643,

is the crystalline volume fraction, 64.3%. It is smaller because the crystalline region carries more mass per unit volume. Confusing these fractions changes the meaning of the result even when the arithmetic is sound.

Drawing can align chains and raise strength and crystallinity along the drawing direction. That alignment creates direction-dependent properties; a strengthened film or fiber need not gain the same strength across its width.

Key Takeaways

  • Semicrystalline polymers contain both ordered lamellae and amorphous regions.
  • Tie molecules connect lamellae; spherulites are larger radial clusters.
  • Regular chains and slower cooling generally promote crystallization.
  • The density formula for mass crystallinity includes the factor of crystalline density divided by sample density.
4

Polymers under heat and load

A polymer that seems rigid in a quick room-temperature test may creep under a lasting load or become brittle in the cold. Its response depends on chain motion as well as structure. Connect glass transition, crystallinity and crosslinks to stress–strain curves, elastic recovery and time-dependent deformation. Use the loading conditions to decide which measured property answers the engineering question.

4.1 Glass transition and melting

Heating a polymer can activate chain motion without destroying all of its solid structure. Separate the response of amorphous regions from that of crystalline regions to understand the temperatures that matter.

Identify the moving structure

At the glass transition, Tg, amorphous chain segments gain enough mobility to respond much more readily. Below it they are glassy and rigid; above it they become rubbery or leathery. This transition does not mean that crystals melt.

At the melting range, Tm, ordered crystalline regions lose their order. Polymer lamellae differ in thickness and perfection, so melting occurs over a range. A semicrystalline thermoplastic has both transitions. An amorphous polymer, such as ordinary atactic polystyrene, has a glass transition but no crystalline melting point. A heavily crosslinked thermoset does not melt into a reshaping liquid; sufficiently strong heating decomposes it.

On a specific-volume plot, an amorphous polymer changes slope at the glass transition. A semicrystalline polymer shows that slope change and a large volume rise through melting. A fully crystalline idealization would show only a melting jump.

Connect structure to transition temperature

Stiff backbone groups, bulky or polar side groups and strong attractions such as hydrogen bonds restrict segment motion and tend to raise the glass transition. Crosslinking also raises it. Molecular weight raises transition temperatures toward limiting values; branching often lowers the melting temperature by disrupting crystal packing. Melting comparisons require a polymer that can crystallize in the first place.

Useful approximate values are:

PolymerGlass transition, °CMelting range or value, °C
PEAbout −100 or lowerAbout 115 for LDPE to 135 for HDPE
PPAbout −20 to −10165–175
Ordinary PSAbout 100No crystalline melting point
PVCAbout 80–90—
PETAbout 70250–265
Nylon 6,6About 50–60About 265
PolycarbonateAbout 150No crystalline melting point
PTFE—About 327
Natural rubberAbout −70—

Values depend on grade and measurement conditions.

Judge the operating temperature

At 20 °C, polystyrene is below its glass transition and is stiff and often brittle. Natural rubber is well above its glass transition and can deform easily. PE is also above its glass transition, but its crystals keep it solid and provide stiffness.

An elastomer with a glass transition at −20 °C becomes glassy in a −30 °C environment. A second elastomer with a transition at −45 °C retains much greater chain mobility there. The relevant comparison is the lowest operating temperature against the transition, not simply whether the material is called rubber.

For many polymers, Tg/Tm is roughly 0.5–0.8 when temperatures are in kelvin. PET at 70 °C and 265 °C gives

Tg/Tm=343/538≈0.64.

Using Celsius gives 0.26 because its zero is arbitrary. Always use an absolute temperature scale for a temperature ratio. Service stiffness also depends on loading time: remaining below a melting point alone does not ensure that a part will resist creep.

Key Takeaways

  • The glass transition changes amorphous chain mobility; melting destroys crystalline order.
  • Semicrystalline polymers have both transitions; amorphous polymers have no crystalline melting point.
  • Crosslinked thermosets decompose instead of melting into a reshaping liquid.
  • Compare operating temperature with the transitions to interpret stiffness.
  • Use kelvin for temperature ratios.

4.2 Thermoplastics, thermosets and rubber elasticity

Heating, reshaping and elastic recovery depend on what holds polymer chains together. Some junctions release with heat; others are permanent covalent bonds. The number of junctions also matters: a sparse network can stretch greatly, while a dense one is rigid.

Compare thermal response
ClassStructure and responseExamples
ThermoplasticSeparate linear or branched chains; softens repeatedly with heatPE, PP, PVC, PET, nylon, PMMA
ThermosetPermanent covalent network after curing; cannot be remeltedEpoxy, phenolic, unsaturated polyester
ElastomerMobile coiled chains with enough junctions to recoverNatural rubber, SBR, nitrile, silicone

Thermoplastic chains slide as heat weakens the effect of secondary attractions and entanglements. The material can be melted and reshaped, although overheating degrades chains. This thermal reversibility enables remelting routes for recycling.

A thermoset's curing reaction builds a permanent network, often with heat or a hardener. Heating cannot release that network into independent chains; severe heating chars or decomposes it. Thermosets generally resist creep and retain dimensions better than ordinary thermoplastics, but properties vary widely between grades. A class name is not a universal ranking of strength.

Explain large rubber recovery

An elastomer needs amorphous, coiled chains, a temperature above its glass transition and junctions that stop permanent sliding. Stretching straightens the coils and makes their arrangements more ordered. On unloading, the chains tend to return to the many more possible coiled arrangements. This entropic elasticity explains large recoverable strains without requiring the covalent backbone bonds to stretch by hundreds of percent.

A rubber strip held at a fixed extension can pull harder when warmed. A rapid stretch can also warm rubber slightly. These observations follow from the importance of chain configurations and temperature in the restoring force.

Vulcanization makes permanent crosslinks, classically sulfur bridges, between rubber chains. A modest crosslink density improves recovery, modulus and strength and prevents sticky permanent flow. Too many links greatly restrict motion; high-sulfur rubber can become hard ebonite. Vulcanized rubber is soft yet permanently crosslinked, so "thermoset" does not mean "rigid" in every case.

Distinguish physical from permanent junctions

A thermoplastic elastomer behaves like rubber at its operating temperature but can flow when heated. In styrene–butadiene–styrene, hard polystyrene domains anchor the rubbery middle blocks. These physical junctions soften with heat and form again on cooling. Covalent sulfur crosslinks in vulcanized rubber do not release this way.

For a remeltable storage container, a thermoplastic such as PP fits the thermal requirement. A hot electrical fitting may use a phenolic network to resist softening. A recovering seal needs an elastomer with a glass transition below its coldest service condition. Oil-resistant seals often use nitrile rubber; silicone rubbers serve broad temperature ranges. Match heat response and recovery requirements before comparing detailed grade data.

Key Takeaways

  • Thermoplastics soften reversibly because separate chains can move past one another.
  • Thermoset curing makes a permanent covalent network.
  • Rubber recovery requires mobile coiled chains and junctions that prevent permanent sliding.
  • Vulcanization adds permanent crosslinks; sparse crosslinks preserve stretch.
  • Thermoplastic elastomers use heat-reversible physical junctions.
  • Thermal class and stiffness describe different aspects of a polymer.

4.3 Reading polymer tensile curves

A polymer tensile curve records more than a fracture load. Its shape reveals whether chains remain locked, slide permanently or uncoil and recover. Temperature and test speed can move the same polymer between quite different responses.

Recognize three responses

A brittle polymer breaks near the end of its elastic region with little plastic deformation. A plastic response has an elastic region, a yield maximum and substantial permanent strain. An elastomer has a curved response with large recoverable strain at relatively low stress.

The initial elastic slope gives the modulus. For a polymer with a clear yield maximum, its stress gives the yield strength. In the introductory fracture-stress convention used here, tensile strength is the engineering stress at fracture; it can be below the yield maximum. A metal-style 0.2% offset construction is unnecessary when the polymer has a clearly identifiable yield peak.

Calculate from original dimensions

A bar starts with a 10 mm by 4 mm cross-section and a 50 mm gauge length. Its original area is 40 mm². At 1000 N and 0.50 mm extension in the linear region,

σ=1000/40=25 MPa, ε=0.50/50=0.010, E=25/0.010=2500 MPa=2.5 GPa.

A yield load of 2400 N gives 60 MPa. Fracture at 2200 N gives 55 MPa by the fracture-stress convention. If the gauge length at fracture is 150 mm, the extension is 100 mm and the elongation is

100(150−50)/50=200%.

Engineering values use the original area and gauge length, even after a neck forms. Dividing by the final gauge length would understate elongation.

Follow the neck

In many semicrystalline polymers, yielding produces a neck. Tie chains stretch, lamellae rotate and fragment, and chain segments align along the load. The oriented region becomes stronger, so the neck can spread along the specimen instead of immediately ending in fracture. This is drawing, or cold drawing when done near room temperature.

Drawing increases strength along the alignment direction and creates unequal properties across directions. Higher molecular weight, crystallinity and crosslinking also tend to increase strength and stiffness. Annealing an undrawn semicrystalline sample can raise crystallinity, modulus and yield strength while reducing ductility. Annealing a drawn sample can relax its orientation.

Account for temperature and speed

Heating usually lowers modulus and strength and increases ductility. Faster straining gives chains less time to rearrange, acting much like cooling: the response becomes stiffer and less ductile. A slow room-temperature test can therefore misrepresent an impact in a cold environment.

Soft elastomers have moduli of only a few MPa; rigid bulk plastics are often around a few GPa. Bulk plastic strengths are commonly below 100 MPa, though highly oriented polymer fibers reach several GPa. Low density and large extensibility are separate advantages, not signs of metal-like stiffness.

Glassy polymers can form crazes: localized zones with voids crossed by stretched fibrils. These zones can whiten and absorb energy before developing into cracks. A craze still contains load-bearing bridges; it is not yet a fully open crack.

Key Takeaways

  • Tensile curves can show brittle, plastic or highly elastic behavior.
  • Engineering stress and strain use the original specimen dimensions.
  • A polymer neck can spread as drawing aligns and strengthens chains.
  • Heating and slower loading generally allow more chain rearrangement.
  • Crazes contain voids bridged by fibrils and can develop into cracks.

4.4 Stress relaxation, creep and loading time

Some polymer deformation occurs immediately, while some grows as chains rearrange. A brief test can miss this delayed response. Identify the quantity held constant before deciding whether you are observing creep or stress relaxation.

Separate ideal responses

An ideal linear elastic solid deforms immediately in proportion to stress and recovers fully when unloaded. An ideal viscous material keeps flowing under sustained stress and does not recover its deformation. A viscoelastic material combines elastic and time-dependent response. Silicone putty can bounce during a quick impact yet flow slowly when left under its own weight.

Temperature controls how rapidly chain arrangements can change. An amorphous thermoplastic is glassy far below its glass transition, becomes leathery through the transition, then reaches a rubbery regime and eventually flows at higher temperatures. Sparse permanent crosslinks prevent the final flow even when chains are mobile.

Hold strain: observe stress relaxation

Stretch a specimen rapidly to a small fixed strain and hold its length. The stress needed to maintain that length falls as chains rearrange. The relaxation modulus is

Er(t)=σ(t)ε0.

For a strip held at 0.5% strain, convert the percentage first: ε0=0.005. If stress is 6 MPa at 10 s and 4.5 MPa at 100 s,

Er(10 s)=6/0.005=1200 MPa, Er(100 s)=4.5/0.005=900 MPa.

The same fixed extension now requires less force. Dividing by 0.5 instead of 0.005 makes the modulus 100 times too small. A time label belongs with the modulus because the value changes during the test.

A fixed-time plot of log relaxation modulus against temperature shows a high glassy region, a steep fall near the glass transition, a rubbery plateau and eventual flow. The transition drop can span roughly three orders of magnitude. Crystals reduce that drop in a semicrystalline polymer and support it until melting. Light crosslinks extend the rubbery plateau without a flow region before decomposition.

Hold stress: observe creep

Under constant applied stress, a polymer's strain can increase slowly. This is creep, with a time-dependent modulus

Ec(t)=σ0ε(t).

As strain grows, creep modulus falls. A plastic shelf that sags over months illustrates creep; a clamp held at fixed displacement that loses force illustrates relaxation. The two tests hold different quantities constant, even though both reflect chain rearrangement.

Many polymers show important time dependence near room temperature. Long-term design therefore uses data for the intended temperature and load duration, not only a rapid tensile modulus. Warming and waiting often have similar effects because both allow more molecular motion. Conversely, a rapid impact can produce a much more glassy response. Faster tests can also place the apparent glass transition at a somewhat higher temperature.

Key Takeaways

  • Viscoelastic response depends on both loading time and temperature.
  • Stress relaxation holds strain constant and measures decreasing stress.
  • Creep holds stress constant and measures increasing strain.
  • Convert percent strain to a decimal before calculating a modulus.
5

How composite constituents share load

A composite combines phases whose geometry matters as much as their individual properties. Particles, fibers and bonded layers distribute load in different ways. Start by identifying the matrix and reinforcement, then use volume fractions, loading direction and interface behavior to choose a model. Extend the same reasoning from a single aligned ply to short fibers, laminates and light sandwich panels.

5.1 Composite phases and mixture bounds

A composite deliberately combines chemically or structurally distinct phases separated by interfaces. The aim is a useful property combination: a light matrix with stiff fibers, or hard particles supported by a tougher binder. Natural composites include wood and bone.

Identify the continuous phase

The matrix is the continuous phase surrounding a dispersed phase. Reinforcement performance depends on its concentration, size, shape, distribution and orientation, as well as its own properties. A conventional alloy whose phases form during processing, such as pearlitic steel, is not usually classified as a deliberately assembled composite in this sense.

Composites can be particle-reinforced, fiber-reinforced or structural. Fibers may be continuous and aligned, short and aligned, or short and random. Laminates and sandwich panels are structural composites. Classification by matrix gives polymer-, metal- or ceramic-matrix composites; carbon–carbon uses carbon in both structurally distinct phases.

Distinguish particle mechanisms

Large particles share load with the matrix and constrain its deformation. Examples include aggregate in cement paste, hard carbide particles in a cobalt or nickel binder, and carbon black in tire rubber. Small, evenly distributed particles reduce local weak regions. A cermet combines ceramic particles with a metal matrix, providing hardness with support from a tougher binder.

In dispersion strengthening, much finer stable particles, typically 10–100 nm, obstruct dislocation motion in a metal. Stable oxides can retain their strengthening effect at high temperatures. Examples include alumina in aluminum and thoria in nickel. This mechanism differs from the direct load sharing emphasized for large particles.

Bound the elastic modulus

For an ideal pore-free two-phase composite, the volume fractions sum to one. The equal-strain upper bound is

Eu=EmVm+EpVp.

The equal-stress lower bound is

El=1Vm/Em+Vp/Ep.

The actual modulus of a large-particle material lies between these ideal bounds. Subscripts m and p denote matrix and particles. These models use volume fraction, not mass fraction.

For 40 vol% tungsten particles at 400 GPa in copper at 110 GPa, the matrix fraction is 0.60. Then

Eu=110(0.60)+400(0.40)=226 GPa, El=10.60/110+0.40/400=155 GPa.

The stiff phase increases both bounds, but their difference shows that concentration alone does not fix the response.

Convert fractions before mixing

A dense phase contributes more mass than its volume fraction suggests. Convert a constituent mass fraction using

Vi=wi/ρi∑jwj/ρj.

Equal masses of tungsten and copper give a tungsten volume fraction

0.5/19 3000.5/19 300+0.5/8960=0.317.

It occupies about 32% of the volume, not 50%. Use densities in consistent units; their common scale cancels in the fraction.

For a pore-free composite, density adds by volume:

ρc=ρmVm+ρpVp.

The 40 vol% tungsten mixture has density 0.60(8960)+0.40(19 300)≈13 100 kg/m³.

Key Takeaways

  • The matrix is continuous, while reinforcement geometry helps control the response.
  • Large particles share load; fine dispersions obstruct dislocations.
  • Equal-strain and equal-stress models give upper and lower modulus bounds.
  • Mixture equations use volume fractions, so mass fractions must be converted.
  • Pore-free composite density is a volume-weighted average.

5.2 Fiber load transfer and critical length

A strong fiber cannot help a composite unless load reaches it. The matrix and interface provide that route, and the distance needed for transfer explains why fiber length affects performance.

Give each constituent a role

Fibers provide most of the longitudinal stiffness and strength in a high-performance fiber composite. The matrix binds them together, protects their surfaces, keeps them separated and supports them against compression buckling. It transfers load by shear near the fiber–matrix interface. A ductile matrix can also make failure less abrupt.

Thin fibers contain fewer severe flaws than large pieces, allowing strength closer to the capacity of their bonds. Whiskers are very thin single crystals with high strength but high cost. Common fibers include glass, carbon, aramid, silicon carbide and alumina; metal wires include the steel cords used in tires.

FiberTypical modulusTypical densityUseful feature
E-glass72 GPa2580 kg/m³Low cost
Standard carbon230 GPa1800 kg/m³High stiffness at low mass
Aramid130 GPa1440 kg/m³High toughness and impact resistance

Typical fiber tensile strengths are several GPa, but values vary by grade and damage. Aramid performs poorly in compression compared with its tensile behavior.

Polyesters and vinyl esters serve inexpensive polymer matrices; epoxies provide good bonding for demanding parts. High-temperature thermoplastics such as PEEK extend service temperatures. Metal matrices allow hotter service. Ceramic matrices use fibers mainly to improve toughness. Carbon–carbon composites tolerate temperatures above 2000 °C when protected from oxidation.

Follow shear transfer from the ends

Fiber axial stress starts near zero at a free end and rises as interface shear transfers load inward. The critical fiber length is

lc=σf∗d2τc,

where σf∗ is fiber tensile strength, d is diameter, and τc is the smaller of interface shear capacity and matrix shear yield strength.

A fiber exactly this long reaches full tensile strength only at its midpoint. Longer fibers reach that stress over more of their length. At roughly 15 critical lengths or more, end effects are small enough to treat the fiber as continuous in this introductory model.

For a 15 µm glass fiber, convert the diameter to 0.015 mm. With 2500 MPa tensile strength and 30 MPa shear capacity,

lc=2500(0.015)2(30)=0.625 mm.

A continuous-like length is about 15(0.625)=9.4 mm. Using the radius instead of the diameter halves the result incorrectly. A stronger interface shortens the required transfer length.

Match the interface to the purpose

Sizing and coupling agents improve bonding, such as silanes on glass. A fiber shorter than its critical length cannot reach full tensile strength before transfer is limited, but can still carry substantial load. It is less efficient, not useless.

For ceramic-matrix toughness, a deliberately controlled weaker interface lets cracks deflect and fibers pull out, absorbing energy. Maximum bond strength is therefore not the best objective for every composite. Aligned continuous fibers maximize one-direction performance; short random fibers trade some of that performance for a more uniform response across directions.

Key Takeaways

  • The matrix protects and supports fibers and transfers load through interface shear.
  • Fiber stress builds inward from the ends.
  • Critical length increases with diameter or fiber strength and decreases with shear-transfer capacity.
  • Subcritical fibers still reinforce, but cannot reach their full tensile strength.
  • An interface chosen for crack deflection can improve ceramic-matrix toughness.
  • Fiber alignment and length must match the intended loads.

5.3 Aligned fibers: stiffness, load and strength

A unidirectional composite responds very differently along and across its fibers. Begin with continuous parallel fibers, good bonding and elastic constituent behavior. The direction of load decides how their stresses and strains combine.

Add forces under equal strain

Along the fibers, the matrix and fibers extend together:

εc=εm=εf.

The forces add. With phase areas proportional to volume fractions, the average stress is σc=σmVm+σfVf. Dividing by the common strain gives

EL=EmVm+EfVf.

For carbon–epoxy with 60 vol% fibers, fiber modulus 230 GPa and matrix modulus 3 GPa,

EL=3(0.40)+230(0.60)=139.2 GPa.

Equal strain does not mean equal stress. The stiff fiber carries much more stress at the same extension. Its load ratio relative to the matrix is

FfFm=EfVfEmVm=138/1.2=115.

The fiber fraction of total load is 115/(115+1)≈99.1%.

Recover constituent stresses

A 100 mm² bar carrying 20 kN has composite stress 200 MPa. Convert the composite modulus to 139 200 MPa:

εc=200/139 200≈0.001437.

The fiber stress is 230 000(0.001437)=330.5 MPa and the matrix stress is 3000(0.001437)=4.31 MPa. Multiplying by phase areas of 60 and 40 mm² gives forces that sum to 20 kN.

Across the fibers, the introductory equal-stress model adds the constituent strains:

1ET=VmEm+VfEf.

It gives ET=1/(0.40/3+0.60/230)=7.36 GPa, much lower than the longitudinal value. This is an idealized transverse estimate; actual local stresses are not uniform. The compliant matrix strongly controls the across-fiber response.

Evaluate strength at a common failure strain

If fibers fail first, the longitudinal strength estimate is

σL∗=σm′(1−Vf)+σf∗Vf.

The prime marks matrix stress at the strain where the fibers break, not the matrix's independent ultimate strength. With fiber strength 3500 MPa,

εf∗=3500/230 000≈0.01522.

If the matrix remains elastic, its stress then is 3000(0.01522)=45.7 MPa. Thus

σL∗=45.7(0.40)+3500(0.60)≈2120 MPa.

Transverse strength is much lower and often controlled by matrix or interface failure. If the matrix yields before fiber failure, the composite curve develops a lower slope, roughly the fiber contribution EfVf, while the fibers continue carrying increasing load.

Solve for a required fraction

To reach a longitudinal modulus of 100 GPa with these constituents,

100=3(1−Vf)+230Vf, Vf=(100−3)/(230−3)=0.427.

The estimate requires about 43 vol% fiber.

Key Takeaways

  • Longitudinal loading gives equal strain and a volume-weighted modulus.
  • The fiber-to-matrix load ratio differs from the fiber fraction of total load.
  • The equal-stress transverse model gives a much lower modulus.
  • Longitudinal strength uses matrix stress at fiber failure strain.
  • A required longitudinal modulus can be used to solve for fiber volume fraction.

5.4 Short fibers, laminates and sandwich panels

Not every part is loaded in one direction, and not every reinforcement is continuous. End effects reduce short-fiber performance, orientation spreads it across directions, and layered structures place reinforcement where it is useful.

Choose the correct fiber-length regime

For aligned fibers longer than the critical length,

σd∗=σf∗Vf(1−lc2l)+σm′(1−Vf).

The factor in parentheses accounts for lower stress near the ends. If l<lc, load transfer limits the fiber stress before fiber tensile failure:

σd∗=lτcdVf+σm′(1−Vf).

Here σm′ is matrix stress at composite failure. For glass with strength 2500 MPa, diameter 0.015 mm and critical length 0.625 mm at 30 vol%, assume matrix stress 30 MPa at composite failure. At a fiber length of 5 mm, the fiber factor is 1−0.625/(2×5)=0.9375. The strength is 2500(0.30)(0.9375)+30(0.70)=724 MPa. At 0.4 mm, use the subcritical formula: [0.4(30)/0.015](0.30)+21=261 MPa. The shorter fibers still carry load.

Include orientation in a stiffness estimate

A simple estimate for random short fibers is

E=KEfVf+EmVm.

The orientation factor is 1 for parallel fibers, 0 for perpendicular fibers, 3/8 for random in-plane fibers and 1/5 for random three-dimensional fibers. This efficiency expression is not a replacement for the transverse equal-stress model; its zero factor omits the direct fiber contribution in this simplified model.

With 30 vol% glass at 72 GPa in a 3 GPa matrix, in-plane random fibers give E=(3/8)(72)(0.30)+3(0.70)=10.2 GPa. Parallel alignment gives 23.7 GPa. Random orientation sacrifices peak stiffness but makes it more uniform across equivalent directions.

Stack plies for several load directions

A laminate bonds plies with chosen fiber directions. Unidirectional stacks favor a single axis, cross-ply uses 0°/90°, angle-ply uses opposing angles, and quasi-isotropic layouts commonly combine 0°, ±45° and 90° plies. Mid-plane symmetry prevents direct coupling of in-plane loads to bending or twisting and helps limit warping during uniform cooling. It does not prevent bending under general loads.

An equal-thickness 0°/90° stack of the carbon–epoxy example has a rough equal-strain modulus [139.2+7.36]/2≈73 GPa along either axis. This first estimate ignores Poisson coupling. It trades the highest axial value for a balanced pair of directions. Hybrid composites combine fiber types, such as carbon and glass, to balance stiffness, cost and failure behavior.

Separate faces to resist bending

A sandwich panel bonds thin stiff faces to a thick light core. During bending, faces carry tension and compression; the core keeps them apart, carries shear and resists crushing. For thin faces, stiffness grows roughly with the square of face separation, so doubling that separation gives about four times the bending stiffness.

Specific modulus, E/ρ, compares stiffness per density. Carbon–epoxy at 60 vol% fiber has density 0.60(1780)+0.40(1200)=1548 kg/m³. Its longitudinal ratio is 139.2×109/1548≈90×106 m²/s², versus about 26 × 10⁶ for steel or aluminum. Across the fibers it is about 4.8 × 10⁶ m²/s². Always attach a direction to that comparison.

Key Takeaways

  • Choose the short-fiber strength equation by comparing fiber length with critical length.
  • Random orientation lowers peak stiffness but distributes reinforcement across directions.
  • Ply angles match reinforcement to several load directions.
  • Mid-plane symmetry removes direct in-plane-to-bending coupling, not all bending.
  • Sandwich faces carry bending tension and compression; the core carries shear and separates the faces.
  • Specific modulus compares stiffness per density and remains direction-dependent.
  • Hybrid composites combine fiber types to balance properties and cost.

Ceramics, Polymers and Composites examples

5 Walkthroughs

1

From ion packing to fracture

14 steps
Use structure to predict coordination and density, then connect ceramic flaws to bend-test failure.
  1. 1
    IntroductionStart at two different scales

    A ceramic’s density depends on the mass and arrangement of its atoms. Its measured fracture strength often depends on a much larger defect: a scratch, pore or microcrack. We will move from ionic packing to silicate and carbon networks, then test a bar in bending. Keep those scales separate: a strong atomic network does not remove the stress concentration at a crack tip.

  2. 2
    ExplanationBalance charge before arranging ions

    An ionic structure must satisfy charge balance. For an MX₂ formula, each +2 cation can balance two −1 anions. The formula tells you how many ions are needed, but their radii help determine how they fit together. The cation-to-anion radius ratio guides coordination: roughly 0.225–0.414 favors four neighbors, 0.414–0.732 favors six, and 0.732–1.0 favors eight in mostly ionic packing.

  3. 3
    ExampleFind the edge of a rock-salt cell

    For NaCl, the radius ratio is 0.102/0.181=0.564, consistent with sixfold coordination. Neighboring unlike ions touch along the cube edge. Two cation–anion contact distances fit along that edge, so a=2(0.102+0.181)=0.566 nm. The conventional cell holds four NaCl formula units. These two results supply the volume and mass needed for density.

  4. 4
    ExampleDivide cell mass by cell volume

    Use NaCl molar mass 0.05844 kg/mol and convert the edge to meters before cubing. Cell mass is 4(0.05844)/(6.022×1023) kg. Cell volume is (0.566×10−9)3 m³. Dividing gives about 2140 kg/m³. Four formula units contain eight individual ions; using eight as the formula-unit count would double the calculated density.

  5. 5
    ChallengeCompensate a substitution

    A NaCl crystal contains seven Ca²⁺ ions on sodium sites, with sodium vacancies providing all charge compensation. How many vacancies are required?

    ---reveal---

    Seven. Each substitution replaces +1 with +2 and therefore adds one positive charge relative to the original lattice. One missing Na⁺ removes that extra unit. Balance the charge change created by substitution, not the full charge of the incoming calcium ion.

  6. 6
    ExplanationShare oxygen corners

    A SiO₄ tetrahedron has charge −4 when isolated. Sharing corners changes both composition and the charge left to balance. If every corner oxygen belongs to two tetrahedra, four half-oxygens give two oxygens per silicon: SiO₂. Sharing two corners makes chains; sharing three makes sheets. When counting composition, a shared oxygen contributes only its appropriate share to each tetrahedron.

  7. 7
    ExampleCheck a layered silicate’s charge

    Kaolinite has formula Al₂(Si₂O₅)(OH)₄. Split its charge into three contributions. Two Al³⁺ ions give +6; the silicate part gives 2(+4)+5(−2)=−2; four hydroxide ions give −4. The total is zero. Its layered structure produces plate-shaped particles, and water films between those particles help wet clay deform. Charge balance and particle shape explain different features of the same material.

  8. 8
    ChallengeExplain graphite without weakening its sheets

    Graphite and diamond contain carbon, but graphite can lubricate a sliding contact. Where does the easy movement occur, and why does composition alone miss the difference?

    ---reveal---

    Graphite sheets slide across weakly bonded interfaces; bonds within each sheet remain strong. Diamond links carbon atoms into a three-dimensional covalent network. Equal elemental composition leaves these very different connection patterns unspecified.

  9. 9
    Key InsightStrong bonds can coexist with sudden failure

    Most ceramics cannot move dislocations easily at room temperature. A crack therefore receives little plastic blunting before it grows. Tensile stress opens flaws and concentrates at their tips, while compression tends to close them. This explains both brittle failure and the advantage of compressive loading. It also explains why hardness, strength and toughness cannot be used as interchangeable descriptions.

  10. 10
    ExampleSet up a bend-test calculation

    An alumina bar is 4.0 mm wide and 3.0 mm deep, with a 40 mm support span. It fractures at 250 N. For three-point bending, σfs=3FfL/(2bd2). The 3.0 mm dimension is parallel to the load, so it is the depth and must be squared. Use newtons and millimeters throughout; the result will be N/mm², equal to MPa.

  11. 11
    ExampleEvaluate the fracture stress

    The bend-test numerator is 3(250)(40)=30 000. The denominator is 2(4)(32)=72. Their ratio gives σfs=417 MPa. This is the tensile-face stress at fracture, called flexural strength or modulus of rupture. It is not the elastic modulus: that quantity describes the elastic slope, not the stress at which a flaw causes the specimen to break.

  12. 12
    ChallengeTurn the same rectangular bar

    A rectangular bar is tested again with its width and depth exchanged. Its dimensions were 6 mm wide and 3 mm deep. For the same span and fracture stress, how does the predicted fracture load change?

    ---reveal---

    It doubles. The geometric factor bd² changes from 6 × 3² = 54 to 3 × 6² = 108. At fixed strength and span, fracture load follows that factor. Treating width and depth symmetrically misses the squared dependence on depth.

  13. 13
    ChallengeConnect density and reliability

    Two ceramic parts have the same measured density, but one has a fresh surface scratch. Must they have the same bending strength?

    ---reveal---

    No. A small scratch can strongly concentrate tensile stress while changing overall mass and volume negligibly. Density is sensitive to composition and bulk porosity; strength can be controlled by one severe surface flaw. Equal density therefore leaves a crucial part of the fracture problem unresolved.

  14. 14
    RecapChoose the structural scale that answers the question

    For ionic packing, combine neutrality with the radius-ratio guide. For density, count formula units and divide cell mass by cell volume. For silicates and carbon, inspect how strong units connect. For brittle strength, locate the flaws and ask whether loading opens or closes them. A bend-test result becomes meaningful only with the specimen geometry, surface condition and loading arrangement attached.

2

Control flow, firing and hydration

14 steps
Follow the routes that turn glass, clay powders and cement into useful solid products.

Save this lesson to follow every Walkthrough step by step.

  1. 1
    IntroductionThree ways to develop a useful solid
  2. 2
    ExplanationRead glass behavior through viscosity
  3. 3
    ExplanationCreate compression at the surface
  4. 4
    ChallengeAdd applied and residual stress
  5. 5
    ExplanationRemove water without uneven shrinkage
  6. 6
    ConnectionDistinguish two bonding routes
  7. 7
    ExampleWork backward from the finished dimension
  8. 8
    ChallengeChoose porosity for a furnace lining
  9. 9
    ExplanationLet cement react with water
  10. 10
    ExampleFind the mixing-water mass
  11. 11
    ChallengeDiagnose early drying
  12. 12
    ExampleOffset bending tension with prestress
  13. 13
    ChallengeLink concrete and tempered glass
  14. 14
    RecapTrack the change that creates performance
3

Build a polymer description from the chain upward

15 steps
Calculate chain-size averages, distinguish architecture from configuration, and interpret crystallinity.

Save this lesson to follow every Walkthrough step by step.

  1. 1
    IntroductionDescribe more than the polymer name
  2. 2
    ExplanationSeparate monomer from repeat unit
  3. 3
    ExampleFind the number-weighted average
  4. 4
    ExampleConvert to mass weighting
  5. 5
    ExampleCount repeat units per chain
  6. 6
    ChallengeCheck an impossible average
  7. 7
    AnalogyDistinguish a side branch from a bridge
  8. 8
    ExplanationKeep shape and configuration separate
  9. 9
    ChallengeRead a copolymer arrangement
  10. 10
    ExplanationBuild order inside a tangled chain material
  11. 11
    Key InsightGive regular chains time to pack
  12. 12
    ExampleEstimate crystallinity from density
  13. 13
    ChallengeDecide what a midpoint density means
  14. 14
    ChallengeExplain two polyethylene grades
  15. 15
    RecapChoose the description that fits the evidence
4

Predict polymer response from motion and time

17 steps
Interpret transitions, recovery and tensile data, then distinguish creep from stress relaxation.

Save this lesson to follow every Walkthrough step by step.

  1. 1
    IntroductionAsk how freely the chains can move
  2. 2
    ExplanationSeparate amorphous motion from crystal melting
  3. 3
    ChallengeChoose a seal for a cold environment
  4. 4
    TipUse an absolute scale for a ratio
  5. 5
    ExplanationFollow permanent and reversible junctions
  6. 6
    AnalogyUncoil without stretching every bond
  7. 7
    ChallengePredict the effect of too many crosslinks
  8. 8
    ExampleTurn test data into stress and strain
  9. 9
    ExampleRead modulus and yield separately
  10. 10
    Key InsightA polymer neck can keep spreading
  11. 11
    ChallengeChange the test speed
  12. 12
    ExplanationHold strain to observe relaxation
  13. 13
    ExampleCalculate a time-labeled modulus
  14. 14
    ConnectionHold stress to observe creep
  15. 15
    ChallengeIdentify the right long-term test
  16. 16
    ChallengeConnect structure with the warm response
  17. 17
    RecapState both the material and the conditions
5

Design a path for composite load

20 steps
Use phase fractions, fiber length and direction to estimate stiffness and strength, then arrange plies and sandwich faces.

Save this lesson to follow every Walkthrough step by step.

  1. 1
    IntroductionStart with a load path
  2. 2
    ExplanationIdentify phases and reinforcement shape
  3. 3
    ChallengeConvert equal masses into volumes
  4. 4
    ExamplePlace a particle modulus between bounds
  5. 5
    ExplanationTransfer fiber load through shear
  6. 6
    ExampleCalculate the critical length
  7. 7
    ChallengeImprove the actual weak link
  8. 8
    ExplanationUse equal strain along continuous fibers
  9. 9
    ExampleCalculate longitudinal stiffness
  10. 10
    ExampleFind the load share
  11. 11
    ConnectionChange the loading direction
  12. 12
    ExampleEvaluate strength at one shared strain
  13. 13
    ChallengeSolve a stiffness requirement backward
  14. 14
    ExplanationChoose the short-fiber regime
  15. 15
    ExampleCalculate a subcritical contribution
  16. 16
    ChallengeCompare two random orientations
  17. 17
    Key InsightUse ply angles to match several loads
  18. 18
    AnalogySeparate faces like an I-beam
  19. 19
    ChallengeCheck a claimed mass advantage
  20. 20
    RecapCarry the model conditions with the result

Ceramics, Polymers and Composites practice questions

50 Practice Questions in 5 sets

Set 1: Ceramic packing, networks and brittle failure10 Practice Questions

Question 1 of 10

A rectangular ceramic bar breaks at 180 N in three-point bending. The support span is 30 mm, width 6 mm and depth parallel to the load 3 mm. What is its flexural strength?
  1. 100 MPa
  2. 225 MPa
  3. 450 MPa
  4. 150 MPa
Show answerHide answer
Answer: D
Use σfs=3FfL/(2bd2), giving 3(180)(30)/[2(6)(32)]=150 MPa. Newtons and millimeters give N/mm², equal to MPa. Omitting the square on the 3 mm depth gives 450 MPa and misrepresents how bending stress depends on section geometry.

Question 2 of 10

An ionic ceramic contains Al³⁺ and O²⁻. What is its electrically neutral formula?
  1. AlO
  2. Al₂O₃
  3. Al₃O₂
  4. AlO₃
Show answerHide answer
Answer: B
Two aluminum ions contribute +6 and three oxide ions contribute −6, giving Al₂O₃. Al₃O₂ reverses the required ratio: its charges total +5 instead of zero. Choose the smallest whole-number ion counts that balance the total positive and negative charge.

Question 3 of 10

A mostly ionic MX crystal has cation radius 0.084 nm and anion radius 0.150 nm. What coordination number does the radius-ratio guide predict?
  1. 4
  2. 8
  3. 3
  4. 6
Show answerHide answer
Answer: D
The cation-to-anion radius ratio is 0.084/0.150=0.56, inside the sixfold interval 0.414–0.732. Fourfold coordination would require a smaller ratio. Reversing the division gives a value above one and loses the intended comparison of the smaller cation with the larger anion.

Question 4 of 10

A cubic rock-salt ceramic has cation radius 0.080 nm, anion radius 0.160 nm and formula molar mass 0.0600 kg/mol. What theoretical density follows from this structure? Use NA=6.022×1023 mol⁻¹.
  1. About 900 kg/m³
  2. About 7200 kg/m³
  3. About 3600 kg/m³
  4. About 1800 kg/m³
Show answerHide answer
Answer: C
Rock salt contains four formula units per conventional cell, and its edge is twice the radius sum: 0.480 nm. Thus ρ=4(0.0600)/[(0.480×10−9)3NA]≈3600 kg/m³. Counting eight ions as eight formula units doubles the mass and gives the tempting 7200 kg/m³ result.

Question 5 of 10

A NaCl crystal contains 12 Ca²⁺ ions substituted on sodium sites. With sodium vacancies as the only compensating defects, how many sodium vacancies are needed?
  1. 12
  2. 6
  3. 24
  4. 0
Show answerHide answer
Answer: A
Each Ca²⁺ replacing Na⁺ adds one unit of positive charge relative to the original lattice. One sodium vacancy removes one unit, so 12 substitutions require 12 vacancies. Six vacancies would compensate only half the extra charge; the calcium charge itself is not the charge difference created by substitution.

Question 6 of 10

Why can graphite act as a dry lubricant while diamond resists scratching?
  1. Graphite has weak bonds inside each carbon sheet.
  2. Diamond is held together mainly by weak surface forces.
  3. Graphite contains fewer covalent bonds per unit mass.
  4. Graphite sheets slide across weakly bonded interfaces.
Show answerHide answer
Answer: D
Graphite has strong covalent bonds within each sheet and much weaker attraction between sheets, allowing sliding. Diamond connects its atoms through a three-dimensional covalent network. Attributing graphite softness to weak in-plane bonds confuses the strong sheets with the interfaces that allow their relative motion.

Question 7 of 10

A silicate sheet has repeat composition (Si₂O₅)²⁻. How many Mg²⁺ ions balance three such sheet units?
  1. 3
  2. 2
  3. 6
  4. 1
Show answerHide answer
Answer: A
Three sheet units carry a total charge of −6. Three Mg²⁺ ions contribute +6 and make the combination neutral. Six magnesium ions would double the required positive charge; the number of oxygen atoms is not the number of charge-balancing cations needed.

Question 8 of 10

Two samples are pure SiO₂. One has long-range order and the other does not. How should their thermal behavior differ?
  1. Both melt sharply because their compositions match.
  2. The ordered sample softens gradually; the other melts sharply.
  3. The ordered sample melts; the other softens through a range.
  4. Both have identical transitions because their bonds match.
Show answerHide answer
Answer: C
The ordered SiO₂ crystal has a crystalline melting transition, while the disordered glass softens as its viscosity falls through a temperature range. Equal chemical composition does not impose equal long-range structure. Bond identity alone therefore cannot make their thermal responses identical.

Question 9 of 10

Why does a ceramic usually withstand more compressive stress than tensile stress?
  1. Compression removes all pores permanently.
  2. Compression closes flaws that tension would open.
  3. Compression lets dislocations move without resistance.
  4. Compression increases the strength of every atomic bond.
Show answerHide answer
Answer: B
Compression tends to close cracks, while tension opens them and concentrates stress at their tips. This makes brittle ceramics much more resistant to compression. The difference does not require pores to disappear: a compressed flaw can remain present even while its faces are pushed together.

Question 10 of 10

Two alumina batches have equal porosity and elastic modulus. Batch B has deeper surface scratches and a larger stressed surface area than batch A. What failure behavior is most defensible?
  1. B should have higher strength because scratches reduce constraint.
  2. B should be less strong on average, with brittle strength scatter.
  3. Both should have identical strength because their moduli agree.
  4. Both should become more ductile because their pores are equal.
Show answerHide answer
Answer: B
Deeper scratches create more severe stress concentrations, and a larger stressed area increases the chance of a critical flaw. Batch B should therefore have lower average brittle strength, with specimen-to-specimen scatter. Equal modulus and porosity do not specify the size or location of the worst surface flaw.
Set 2: Glass treatment, ceramic firing and cement hydration10 Practice Questions

Save this lesson to see every answer and practice every set.

Question 1 of 10

What residual stress pattern strengthens thermally tempered glass?
  1. Surface compression and interior tension
  2. Surface tension and interior compression
  3. Compression throughout its full thickness
  4. Tension throughout its full thickness
Show answerHide answer

Save this lesson to see this answer.

Question 2 of 10

A glass surface has 85 MPa residual compression. A bending load adds 110 MPa tension there. What is the net surface stress?
  1. 195 MPa tension
  2. 25 MPa compression
  3. 25 MPa tension
  4. 195 MPa compression
Show answerHide answer

Save this lesson to see this answer.

Question 3 of 10

A glass part needs a machined opening and high resistance to tensile opening of surface flaws. A proposed sequence tempers the part, then machines the opening, then anneals it. What sequence and explanation best meet the need?
  1. Machine, anneal, temper; retain surface compression afterward.
  2. Anneal, temper, machine; leave the surface tension unchanged.
  3. Temper, machine, anneal; restore compression by slow cooling.
  4. Machine, temper, anneal; preserve compression during relaxation.
Show answerHide answer

Save this lesson to see this answer.

Question 4 of 10

What process bonds a pressed ceramic powder below its bulk melting temperature?
  1. Slip casting
  2. Vitrification
  3. Annealing
  4. Sintering
Show answerHide answer

Save this lesson to see this answer.

Question 5 of 10

A ceramic tube must be 88 mm long after 12% linear firing shrinkage. What length should it have before firing?
  1. 98.6 mm
  2. 100.0 mm
  3. 77.4 mm
  4. 105.6 mm
Show answerHide answer

Save this lesson to see this answer.

Question 6 of 10

A furnace backup lining carries little load and is protected from molten slag by a separate dense hot-face layer. Why could a more porous backup refractory be useful, and what change would make that choice less attractive?
  1. It improves stiffness; direct slag contact preserves its strength.
  2. It improves abrasion resistance; direct slag contact seals pores.
  3. It improves insulation; direct slag contact could penetrate pores.
  4. It improves tensile strength; direct slag contact removes flaws.
Show answerHide answer

Save this lesson to see this answer.

Question 7 of 10

Why is fresh concrete kept moist during curing?
  1. Water maintains the hydration reactions that develop strength.
  2. Water prevents all thermal expansion throughout its life.
  3. Water makes the paste harden by evaporating more rapidly.
  4. Water dissolves aggregate to increase its bonding surface.
Show answerHide answer

Save this lesson to see this answer.

Question 8 of 10

A concrete batch contains 420 kg cement and 189 kg water. Another batch uses the same cement but 231 kg water. How do their water–cement ratios compare?
  1. 0.55 then 0.45; the second has less excess water.
  2. 0.45 then 0.55; the second tends to leave more pores.
  3. 0.45 then 0.55; the second must develop more strength.
  4. 0.55 then 0.45; the second must hydrate more slowly.
Show answerHide answer

Save this lesson to see this answer.

Question 9 of 10

A prestressed beam face begins at 9 MPa compression and later receives 12 MPa tensile stress from bending. What is its final stress there?
  1. 21 MPa tension
  2. 3 MPa compression
  3. 21 MPa compression
  4. 3 MPa tension
Show answerHide answer

Save this lesson to see this answer.

Question 10 of 10

A thick concrete pour develops strength early but its surface dries rapidly while its interior remains hot. What combined response best addresses the two risks?
  1. Add water after setting and remove all temperature control.
  2. Stop curing after setting and rely on aggregate stiffness.
  3. Retain moisture and manage temperature differences during curing.
  4. Dry the surface faster and maximize the initial heat release.
Show answerHide answer

Save this lesson to see this answer.

Set 3: Chain length, architecture and crystalline order10 Practice Questions

Save this lesson to see every answer and practice every set.

Question 1 of 10

What changes when ethylene becomes the repeat units of a polyethylene chain?
  1. The atoms stay the same and backbone double bonds remain.
  2. Each unit loses two hydrogens and forms single backbone bonds.
  3. The atoms stay the same but single backbone bonds form.
  4. Each unit gains two hydrogens and forms single backbone bonds.
Show answerHide answer

Save this lesson to see this answer.

Question 2 of 10

A polymer has 25% of its chains at 20 000 g/mol and 75% at 40 000 g/mol. What is its number-average molecular weight?
  1. 35 000 g/mol
  2. 30 000 g/mol
  3. 37 100 g/mol
  4. 60 000 g/mol
Show answerHide answer

Save this lesson to see this answer.

Question 3 of 10

A polymer contains equal numbers of chains at 12 000 and 36 000 g/mol. Its repeat unit has molar mass 120 g/mol. What are its dispersity and number-average degree of polymerization?
  1. 1.00 and 200
  2. 1.25 and 250
  3. 1.50 and 200
  4. 1.25 and 200
Show answerHide answer

Save this lesson to see this answer.

Question 4 of 10

A polymer chain changes from a tight coil to an extended shape by rotating single bonds. What structural description changes?
  1. Tacticity
  2. Conformation
  3. Repeat-unit identity
  4. Covalent connectivity
Show answerHide answer

Save this lesson to see this answer.

Question 5 of 10

Two polyethylene grades have identical repeat units. Grade A is nearly linear; grade B has many side branches. Under comparable cooling, which grade should pack more densely, and why?
  1. A, because regular chains pack more readily.
  2. B, because branches fill every gap between chains.
  3. A, because it has a different repeat-unit mass.
  4. B, because branches create permanent crosslinks.
Show answerHide answer

Save this lesson to see this answer.

Question 6 of 10

A copolymer has a backbone made mostly of A units with attached side chains made of B units. What arrangement is this?
  1. Alternating
  2. Block
  3. Graft
  4. Random
Show answerHide answer

Save this lesson to see this answer.

Question 7 of 10

What connects neighboring crystalline lamellae through the amorphous regions of a semicrystalline polymer?
  1. Free chain ends
  2. Tie molecules
  3. Chain folds
  4. Lamella cores
Show answerHide answer

Save this lesson to see this answer.

Question 8 of 10

A polymer has fully crystalline density 1200 kg/m³, fully amorphous density 1000 kg/m³ and sample density 1100 kg/m³. What is its crystallinity by mass?
  1. 45.5%
  2. 60.0%
  3. 50.0%
  4. 54.5%
Show answerHide answer

Save this lesson to see this answer.

Question 9 of 10

A clear PET sample and an opaque PET sample have the same chemical composition. The opaque sample is denser. What cooling history and structural explanation best fit these observations?
  1. Faster cooling allowed more crystals and increased density.
  2. Slower cooling broke chains and removed all ordered regions.
  3. Slower cooling allowed more crystals that scatter light.
  4. Faster cooling created larger amorphous voids that scatter light.
Show answerHide answer

Save this lesson to see this answer.

Question 10 of 10

A polypropylene sample is atactic and weakly crystalline. A proposal claims that stretching it will make it isotactic and therefore highly crystalline. What is the central error?
  1. Stretching changes conformation, but not the fixed tacticity.
  2. Stretching changes tacticity, but cannot change chain orientation.
  3. Atactic chains already have regularly alternating side groups.
  4. Isotactic chains have the same irregularity as atactic chains.
Show answerHide answer

Save this lesson to see this answer.

Set 4: Thermal transitions, tensile tests and time-dependent response10 Practice Questions

Save this lesson to see every answer and practice every set.

Question 1 of 10

What structural change occurs when an amorphous polymer passes upward through its glass transition?
  1. Crystalline chain segments lose their ordered packing.
  2. Amorphous segments arrange into new crystalline regions.
  3. Separate chains become a permanent covalent network.
  4. Long chain segments become substantially more mobile.
Show answerHide answer

Save this lesson to see this answer.

Question 2 of 10

A semicrystalline polymer has a glass transition at −40 °C and a melting range near 150 °C. Why can it remain a solid at 25 °C?
  1. Its amorphous regions remain below their glass transition.
  2. Its crystalline regions still support the mobile amorphous regions.
  3. Its crystals have melted into a permanent covalent network.
  4. Its glass transition is the temperature of complete melting.
Show answerHide answer

Save this lesson to see this answer.

Question 3 of 10

Why can a cured epoxy component not be remelted into a new shape like polyethylene?
  1. It contains permanent covalent network links.
  2. Its crystals have an unusually high melting range.
  3. Its secondary attractions exceed all thermoplastic bonds.
  4. Its chains have an unusually high molecular weight.
Show answerHide answer

Save this lesson to see this answer.

Question 4 of 10

Two flexible seals recover after stretching at 20 °C. Seal A flows on heating and recovers its rubbery response after cooling; seal B decomposes without remelting. What junction structures explain both results?
  1. A has sulfur crosslinks; B has heat-reversible hard domains.
  2. Both have permanent networks that reversibly melt on heating.
  3. A has physical junctions; B has permanent covalent crosslinks.
  4. Both lack junctions and recover through unrestricted chain sliding.
Show answerHide answer

Save this lesson to see this answer.

Question 5 of 10

A polymer bar has original area 24 mm² and gauge length 60 mm. In its linear region, 720 N causes 0.60 mm extension. What is its elastic modulus?
  1. 0.30 GPa
  2. 3.0 GPa
  3. 30 GPa
  4. 1.2 GPa
Show answerHide answer

Save this lesson to see this answer.

Question 6 of 10

A semicrystalline polymer develops a neck during tension. The force remains roughly steady while the neck spreads along the gauge. What molecular explanation fits, and what directional property should the drawn region develop?
  1. Bonds all break in the neck; strength becomes equal in all directions.
  2. Chains become random; transverse strength must exceed axial strength.
  3. Crystals fully melt; the specimen becomes a liquid under constant force.
  4. Chains align in the neck; strength increases along the drawing direction.
Show answerHide answer

Save this lesson to see this answer.

Question 7 of 10

A polymer strip is kept at a fixed extension while the measured force slowly decreases. What behavior is being measured?
  1. Stress relaxation
  2. Creep under fixed stress
  3. Thermal crystallization
  4. Permanent melting
Show answerHide answer

Save this lesson to see this answer.

Question 8 of 10

A strip is held at 0.8% strain. Its stress after 40 s is 4 MPa. What is its relaxation modulus at that time?
  1. 5 MPa
  2. 50 MPa
  3. 500 MPa
  4. 5000 MPa
Show answerHide answer

Save this lesson to see this answer.

Question 9 of 10

A polymer clip passes a fast room-temperature pull test but loses grip during months at a warmer fixed opening. What test most directly represents the loss of grip, and why?
  1. A fast impact test, because high rate reproduces long waiting.
  2. A constant-strain relaxation test at the warmer temperature.
  3. A constant-stress test that prevents any change in extension.
  4. A melting test, because grip loss requires complete melting.
Show answerHide answer

Save this lesson to see this answer.

Question 10 of 10

An amorphous thermoplastic with a glass transition of 90 °C must hold a lasting load at 110 °C. A designer approves it because a comparison polymer melts at 180 °C. What two mistakes undermine that approval?
  1. The operating temperatures require kelvin comparisons, and the test temperature must exceed both transitions.
  2. The two polymers must have equal molecular weight, and crystalline regions cannot support a warm material.
  3. The amorphous polymer must crystallize on heating, and long loading prevents segment rearrangement.
  4. The amorphous polymer has no crystal melting point, and warm long-term loading allows rearrangement.
Show answerHide answer

Save this lesson to see this answer.

Set 5: Load sharing and composite design decisions10 Practice Questions

Save this lesson to see every answer and practice every set.

Question 1 of 10

In a glass-fiber polymer composite, which phase is the matrix?
  1. The continuous polymer surrounding the glass fibers
  2. The dispersed glass fibers within the polymer
  3. The thin interfacial coating around each fiber
  4. The combined polymer and fiber population
Show answerHide answer

Save this lesson to see this answer.

Question 2 of 10

A pore-free two-phase material contains equal masses of particles and matrix. Particle density is 6000 kg/m³ and modulus 180 GPa; matrix density is 2000 kg/m³ and modulus 20 GPa. What is its equal-strain upper modulus?
  1. 100 GPa
  2. 140 GPa
  3. 60 GPa
  4. 45 GPa
Show answerHide answer

Save this lesson to see this answer.

Question 3 of 10

A fiber has tensile strength 1800 MPa, diameter 0.020 mm and limiting shear strength 25 MPa. What is its critical length?
  1. 0.36 mm
  2. 1.44 mm
  3. 0.90 mm
  4. 0.72 mm
Show answerHide answer

Save this lesson to see this answer.

Question 4 of 10

A 1.0 mm fiber has strength 2400 MPa and diameter 0.020 mm. Its matrix limits shear transfer to 20 MPa. A surface treatment raises interface capacity from 30 to 60 MPa. How does the treatment change whether the fiber reaches full tensile strength?
  1. It halves critical length to 0.4 mm, so full strength is reached.
  2. It leaves critical length at 1.2 mm, so full strength is not reached.
  3. It leaves critical length at 0.8 mm, so full strength is reached.
  4. It doubles critical length to 2.4 mm, so full strength is not reached.
Show answerHide answer

Save this lesson to see this answer.

Question 5 of 10

Continuous aligned fibers have modulus 150 GPa and occupy 40% of a well-bonded elastic composite. The matrix modulus is 5 GPa. What is its longitudinal modulus?
  1. 57 GPa
  2. 65 GPa
  3. 63 GPa
  4. 12 GPa
Show answerHide answer

Save this lesson to see this answer.

Question 6 of 10

A continuous aligned composite has 50 vol% fibers with modulus 100 GPa and strength 2000 MPa. The matrix has modulus 4 GPa and independent tensile strength 120 MPa. The fibers fail first and the matrix stays elastic until then. What longitudinal strength is predicted?
  1. 1040 MPa
  2. 1000 MPa
  3. 1060 MPa
  4. 2040 MPa
Show answerHide answer

Save this lesson to see this answer.

Question 7 of 10

A continuous aligned elastic composite uses 200 GPa fibers and a 4 GPa matrix. It needs a longitudinal modulus of 82.4 GPa. At the required fiber fraction, what fraction of total longitudinal load do the fibers carry?
  1. 40.0%
  2. 96.0%
  3. 99.0%
  4. 97.1%
Show answerHide answer

Save this lesson to see this answer.

Question 8 of 10

A short-glass composite has 25 vol% fibers with modulus 80 GPa in a 4 GPa matrix. What modulus does the orientation-factor model predict for fibers randomly oriented in a plane?
  1. 23.0 GPa
  2. 10.5 GPa
  3. 7.0 GPa
  4. 8.6 GPa
Show answerHide answer

Save this lesson to see this answer.

Question 9 of 10

Aligned short fibers have strength 1600 MPa, diameter 0.010 mm and limiting shear strength 20 MPa. They occupy 20 vol% and are 0.20 mm long. Matrix stress at composite failure is 15 MPa. What strength does the appropriate short-fiber model predict?
  1. 172 MPa
  2. 252 MPa
  3. 332 MPa
  4. 92 MPa
Show answerHide answer

Save this lesson to see this answer.

Question 10 of 10

A thin-faced sandwich panel keeps the same face sheets and doubles their separation using a light core. In the simple face-dominated bending model, how does its bending stiffness change?
  1. It stays approximately unchanged.
  2. It becomes about twice as large.
  3. It becomes about four times as large.
  4. It becomes about eight times as large.
Show answerHide answer

Save this lesson to see this answer.

Stuck on your own question? Homework Help

Key Terms

97 Key Terms, each with its definition

A

Abrasive
An abrasive is a hard material used to remove another material by cutting or wear, as in grinding, sanding and polishing.
Alumina abrasive grains bonded into a grinding wheel remove material from a workpiece.
Anisotropy
Anisotropy is dependence of a material property on measurement direction, common when fibers or polymer chains are strongly aligned.
A unidirectional carbon composite shows anisotropy because its along-fiber and across-fiber moduli differ.
Annealing point
The annealing point is the glass temperature corresponding to a viscosity near 10¹² Pa·s, where internal stresses relax in minutes.
A shaped glass part is held near its annealing point before slow cooling through the stress-relaxation range.

B

Branch
A branch is a polymer side chain attached to a main chain, affecting molecular shape and often interfering with regular packing.
Many branches in LDPE reduce its ability to crystallize compared with nearly linear HDPE.
Brittle fracture
Brittle fracture is rapid crack-driven failure with little plastic deformation, so a material absorbs limited energy before breaking.
A scratched ceramic plate can fail by brittle fracture while its overall elastic deformation remains small.

C

Calcium silicate hydrate
Calcium silicate hydrate, or C–S–H, is the fine binding product of calcium-silicate hydration that supplies most cement-paste strength.
C–S–H develops as the silicate compounds in portland cement react with the available water.
Ceramic
A ceramic is an inorganic, nonmetallic solid, commonly an oxide, nitride or carbide, with mainly ionic or covalent bonding.
Alumina is a ceramic used as an electrical insulator and a wear-resistant engineering material.
Cermet
A cermet is a composite combining hard ceramic particles with a metal binder that supports them and provides a tougher continuous phase.
Tungsten carbide particles in cobalt make a cermet used for demanding cutting-tool applications.
Clinker
Clinker is the nodular material formed by high-temperature reactions of cement raw materials and later ground with gypsum into cement.
A rotary kiln produces clinker from limestone mixed with clay or shale at roughly 1400–1500 °C.
Composite
A composite is a deliberate combination of chemically or structurally distinct phases with interfaces, chosen for a useful set of properties.
Concrete is a composite whose aggregate particles are held together by hardened cement paste.
Configuration
Configuration is a fixed arrangement of atoms in a polymer that requires breaking and re-forming bonds to change.
Polypropylene tacticity is a configuration that ordinary stretching cannot turn from atactic to isotactic.
Conformation
Conformation is the shape of a polymer chain produced by rotations about single bonds without changing the chain’s covalent connectivity.
A chain can change conformation from a compact coil toward an extended shape during stretching.
Coordination number
The coordination number is the number of nearest neighboring ions around a chosen ion, usually anions around a cation in ionic packing.
The coordination number of sodium in rock-salt NaCl is six because six chloride ions surround it.
Copolymer
A copolymer is a polymer containing more than one repeat-unit type, with the units arranged in random, alternating, block or graft patterns.
Styrene–butadiene rubber is a copolymer whose different units occur in a largely random sequence.
Craze
A craze is a localized voided zone in a glassy polymer with stretched fibrils bridging the voids and still transmitting some load.
A whitened craze can absorb energy before its fibrils fail and it develops into an open crack.
Creep
Creep is a gradual increase in strain under sustained applied stress, often important in polymers at ordinary operating temperatures.
A polymer shelf that sags over months under an unchanged load is showing creep.
Critical fiber length
The critical fiber length is the length needed for an embedded fiber to reach its tensile strength at its midpoint through shear transfer.
Increasing the effective interface shear strength reduces critical fiber length for the same fiber diameter and strength.
Crosslink
A crosslink is a covalent connection between polymer chains that restricts their relative movement and can prevent permanent flow.
Sulfur bridges form crosslinks between rubber chains during conventional vulcanization.
Curing
Curing is maintaining moisture and suitable temperature in fresh concrete so hydration can develop the intended strength and durability.
Keeping a young concrete surface moist during curing prevents early drying from restricting hydration.

D

Degree of polymerization
The degree of polymerization is the average number of repeat units per chain, found from compatible chain and repeat-unit molar masses.
A number-average chain mass of 28 050 g/mol gives polyethylene a degree of polymerization near 1000.
Devitrification
Devitrification is crystallization within a glass; when unwanted, it can create cloudiness and reduce the quality of a glass product.
Uncontrolled devitrification can spoil a clear glass article during an unsuitable heat treatment.
Dispersed phase
The dispersed phase is the constituent embedded within a continuous matrix, with shape, distribution and orientation affecting properties.
Glass fibers form the dispersed phase in a glass-filled polymer molding.
Dispersity
Dispersity is weight-average divided by number-average molecular weight, with a value of one for a single chain molecular weight.
A dispersity above one shows that the polymer sample contains a distribution of chain molecular weights.
Drawing
Drawing is plastic extension that aligns polymer chains and reorganizes crystalline regions, increasing strength especially along the stretch direction.
A spreading neck during drawing leaves an oriented, stronger region behind it along the polymer gauge length.

E

Elastomer
An elastomer is a polymer that undergoes large recoverable strains through mobile coiled chains held by a suitable density of junctions.
An elastomer seal must remain above its glass transition to show its usual flexible recovery.
Engineering strain
Engineering strain is extension divided by original gauge length, expressed as a dimensionless fraction or as percent elongation.
A 2 mm extension over a 100 mm original gauge length gives engineering strain 0.02, or 2%.
Engineering stress
Engineering stress is the applied force divided by the specimen’s original cross-sectional area, even after the area changes during deformation.
A 600 N force on an original 20 mm² section gives an engineering stress of 30 MPa.
Entropic elasticity
Entropic elasticity is a restoring response driven mainly by chains returning from stretched, ordered shapes to more numerous coiled arrangements.
Entropic elasticity explains why stretching rubber can produce large reversible extension without huge bond stretch.

F

Fiber pullout
Fiber pullout is sliding of a fiber from a surrounding matrix after interface separation, consuming energy during composite fracture.
Controlled fiber pullout can increase toughness when a crack meets fibers in a ceramic-matrix composite.
Fiber–matrix interface
The fiber–matrix interface is the boundary across which shear transfers load between a fiber and its surrounding matrix.
A coupling agent improves bonding at the fiber–matrix interface of a glass-reinforced polymer.
Flexural strength
Flexural strength is the maximum tensile-face stress at fracture in a bend test and is also called the modulus of rupture.
An alumina bar’s flexural strength is calculated from its fracture load, support span and dimensions.
Float process
The float process forms flat glass by spreading molten glass over molten tin, producing smooth, nearly parallel surfaces.
Window sheet made by the float process needs no mold wall to define its broad upper surface.
Formula unit
A formula unit is the smallest composition unit expressing a compound’s ion ratio, such as one sodium and one chloride in NaCl.
Density calculations count four formula units in a rock-salt cell, although that cell contains eight ions.
Frenkel defect
A Frenkel defect is a vacancy–interstitial pair formed when a cation leaves its normal lattice site for an interstitial position.
An ionic crystal retains overall charge neutrality when a cation forms a Frenkel defect.
Fullerene
A fullerene is a molecule made of carbon atoms connected into a closed hollow cage, such as the sixty-atom molecule C₆₀.
The fullerene C₆₀ is a closed carbon cage, unlike the extended flat sheet of graphene.

G

Glass transition temperature
The glass transition temperature marks a time-dependent change in amorphous segment mobility between rigid glassy and more rubbery response.
A seal operating below its glass transition temperature can become stiff and vulnerable to cracking.
Glass-ceramic
A glass-ceramic is a material shaped as glass and then heat treated to grow a controlled population of fine crystals within it.
A cooktop glass-ceramic uses a tailored composition to keep thermal expansion very low.
Glassy state
The glassy state is a rigid amorphous state in which large-scale segment rearrangement is slow relative to the observation time.
Ordinary polystyrene is in a glassy state at room temperature because its glass transition is much higher.
Graphene
Graphene is a single atom-thick hexagonal carbon sheet with strong in-plane bonding and high stiffness and electrical conductivity.
A carbon nanotube can be pictured as a graphene sheet wrapped into a narrow cylinder.
Graphite
Graphite is a crystalline carbon form with strong hexagonal sheets held together by weak attractions, allowing interlayer sliding.
Graphite works as a dry lubricant because its carbon sheets can slide across one another.

H

Hybrid composite
A hybrid composite combines two or more reinforcement types in one matrix to balance properties such as stiffness, toughness and cost.
A carbon-and-glass hybrid composite can reduce cost while retaining much of carbon’s stiffness benefit.
Hydration
Hydration is the chemical reaction of cement compounds with water that creates the products responsible for setting and strength gain.
Moist curing supports hydration after concrete has set and can no longer be placed or reshaped.
Hydraulic cement
A hydraulic cement is an inorganic binder that hardens by reaction with water and can continue hardening while under water.
Portland cement is a hydraulic cement, so its hardening does not depend on exposure to dry air.
Hydroplasticity
Hydroplasticity is the ability of a clay–water mixture to deform and retain a new shape as water films let plate-shaped particles slide.
Hydroplasticity allows wet clay to pass through a die and retain a brick or pipe cross-section.

I

Isostrain condition
An isostrain condition gives constituents the same axial strain, as in ideal longitudinal loading of well-bonded continuous aligned fibers.
Under the isostrain condition, a stiff fiber carries greater stress than the softer surrounding matrix.
Isostress condition
An isostress condition gives constituents equal stress and is used for the ideal lower-bound transverse mixture model.
The isostress condition adds the constituent strain contributions to estimate a transverse modulus.

L

Lamella
A lamella is a thin polymer crystal plate made of closely packed chain segments, commonly with chains folded back and forth.
Growing lamellae can spread outward from a center as a polymer crystallizes from its melt.
Laminate
A laminate is a bonded stack of layers whose material and orientation are selected to provide useful properties in chosen directions.
A cross-ply laminate alternates fiber directions so it can carry substantial loads along two axes.
Longitudinal modulus
The longitudinal modulus is the elastic stiffness measured along aligned fibers, estimated by a volume-weighted average under equal strain.
A carbon–epoxy ply can have a longitudinal modulus far above its across-fiber stiffness.

M

Mass crystallinity
Mass crystallinity is the fraction of a polymer sample’s mass in crystalline regions, calculated with densities or other suitable measurements.
Mass crystallinity exceeds the crystalline volume fraction when crystalline material is denser than amorphous material.
Matrix
The matrix is the continuous phase of a composite that surrounds the dispersed phase and binds it into a useful material.
Epoxy is the matrix in a carbon–epoxy composite, while carbon fibers provide much of its axial stiffness.
Melting temperature
The melting temperature describes loss of crystalline order on heating; polymers usually melt over a range because their crystals vary.
Polyethylene remains supported by crystals until it approaches its melting temperature range.
Monomer
A monomer is a small starting molecule that can react with other molecules to form the repeating structure of a polymer chain.
Ethylene is the monomer used to form the long carbon-backbone chains of polyethylene.

N

Network modifier
A network modifier is an oxide that interrupts glass-network links by introducing nonbridging oxygens, making flow easier.
Sodium oxide acts as a network modifier that lowers the softening temperature of silica-based glass.
Number-average molecular weight
Number-average molecular weight is the mean chain molecular weight calculated by weighting each size class by its fraction of all chains.
Two equally populated chain classes contribute equally to the number-average molecular weight calculation.

O

Orientation factor
An orientation factor reduces a fiber contribution in a simplified stiffness estimate to account for its direction relative to the load.
An orientation factor of 3/8 represents fibers distributed randomly in a plane in the introductory estimate.

P

Ply
A ply is one layer of a laminate, commonly containing aligned fibers with a specified direction relative to a reference axis.
A 90° ply reinforces a direction perpendicular to the fibers in a neighboring 0° ply.
Polymorph
A polymorph is one of several crystalline structures with the same chemical composition but different atomic arrangements.
Quartz and cristobalite are silica polymorphs built from differently arranged tetrahedra.
Porosity
Porosity is the fraction of a material’s volume occupied by pores, which reduce load-bearing material and create stress concentrations.
Five percent porosity is entered as 0.05 when estimating the elastic modulus of an alumina body.
Prestressing
Prestressing is introducing compression into concrete before service loading, usually by the action of tensioned steel tendons.
Prestressing can keep a beam’s lower face compressed even when its service load adds bending tension.

Q

Quasi-isotropic laminate
A quasi-isotropic laminate uses selected ply angles to give approximately equal in-plane elastic stiffness in different directions.
A quasi-isotropic laminate may combine 0°, +45°, −45° and 90° plies in a suitable balanced arrangement.

R

Radius ratio
The radius ratio is the cation radius divided by the anion radius, used as a geometric guide to stable ionic coordination.
A radius ratio near 0.56 falls within the usual sixfold-coordination interval for ionic packing.
Refractory
A refractory is a material designed to withstand high temperatures and the chemical environment inside furnaces, kilns or similar equipment.
A magnesia-rich refractory may be chosen when a furnace lining must resist a compatible basic slag.
Relaxation modulus
The relaxation modulus is the time-dependent stress divided by the fixed strain during a small-strain stress-relaxation test.
Reporting relaxation modulus at 10 s distinguishes it from the value after a much longer hold.
Repeat unit
A repeat unit is the recurring bonded atomic pattern in a polymer chain, which can differ in bonding from the starting monomer.
Polyethylene’s repeat unit contains two carbon atoms and four hydrogen atoms joined into its chain pattern.
Rock-salt structure
The rock-salt structure has one ion species on FCC positions and the other in all octahedral holes, giving sixfold coordination.
MgO adopts the rock-salt structure, with four MgO formula units in the conventional cubic cell.
Rubbery plateau
The rubbery plateau is a temperature region of relatively low, slowly changing modulus after the glass-transition drop.
Permanent crosslinks extend a rubbery plateau while preventing the unrestricted flow of separate chains.
Rule of mixtures
The rule of mixtures estimates composite properties from constituent properties and volume fractions under specified load-sharing conditions.
The equal-strain rule of mixtures gives an upper elastic-modulus bound for a two-phase particle composite.

S

Sandwich panel
A sandwich panel bonds two thin stiff faces to a thick light core, separating the faces to increase bending stiffness efficiently.
A foam-core sandwich panel uses its faces for bending tension and compression while the core carries shear.
Schottky defect
A Schottky defect is a charge-balanced set of vacant ion sites; in an MX compound, it consists of one vacancy of each ion type.
One missing sodium and one missing chloride form a Schottky defect in a NaCl crystal.
Semicrystalline polymer
A semicrystalline polymer contains both ordered crystalline regions and disordered amorphous regions, sometimes within the same chains.
Polyethylene is a semicrystalline polymer whose crystals support it above its amorphous glass transition.
Silicate tetrahedron
A silicate tetrahedron is a SiO₄ unit with silicon at its center and oxygen at four corners; an isolated unit has charge −4.
Two magnesium ions balance each isolated silicate tetrahedron in the mineral forsterite.
Sintering
Sintering is heat-driven bonding of powder particles below bulk melting, driven by reduced surface energy and often accompanied by densification.
During sintering, necks grow between neighboring alumina particles and the compact can shrink.
Sizing
Sizing is a surface treatment applied to fibers to protect them during handling and help provide suitable bonding with a matrix.
Glass-fiber sizing can include a silane coupling agent that improves compatibility with the polymer matrix.
Slip casting
Slip casting is shaping a ceramic suspension in a porous mold that removes liquid and builds a solid particle layer at its wall.
A hollow vase forms by slip casting when the liquid center is drained after a wall layer develops.
Specific modulus
Specific modulus is elastic modulus divided by density, comparing stiffness per unit density in a stated loading direction.
A high longitudinal specific modulus does not establish high across-fiber stiffness for the same composite.
Specific volume
Specific volume is volume per unit mass, the reciprocal of density, used to show changes in packing and thermal expansion.
A specific-volume curve changes slope through a glass transition and rises sharply through crystalline melting.
Spherulite
A spherulite is a roughly spherical cluster of radiating polymer lamellae, with amorphous material remaining between the crystalline plates.
A spherulite can show a dark cross pattern when examined using a polarizing microscope.
Stress concentration
A stress concentration is a local increase in stress around a feature such as a pore, notch or sharp crack tip.
A deep surface scratch creates a stress concentration that can start fracture during bending.
Stress relaxation
Stress relaxation is a fall in stress over time while a specimen is held at constant strain and temperature.
A plastic clip held at a fixed opening can lose gripping force through stress relaxation.

T

Tacticity
Tacticity is the pattern of pendant-group placement along a polymer chain, described as isotactic, syndiotactic or atactic.
Regular tacticity helps polypropylene chains pack into ordered regions more readily than an irregular pattern.
Thermal tempering
Thermal tempering is rapid surface cooling of hot glass that leaves the surface compressed and the interior in tension.
Thermal tempering raises a finished glass panel’s resistance to tensile opening of surface flaws.
Thermoplastic
A thermoplastic is a polymer with separate chains that softens on heating and hardens on cooling, allowing repeated thermal reshaping.
A polypropylene container is thermoplastic and can be reshaped by remelting under suitable conditions.
Thermoplastic elastomer
A thermoplastic elastomer is a rubberlike polymer whose physical junctions release on heating, allowing flow and thermal reshaping.
A styrene–butadiene–styrene thermoplastic elastomer uses hard end-block domains as reversible anchors.
Thermoset
A thermoset is a polymer cured into a permanent covalent network that cannot be remelted into a liquid for ordinary reshaping.
Cured epoxy is a thermoset that eventually degrades when heated strongly instead of becoming a remoldable melt.
Tie molecule
A tie molecule is a polymer chain that passes through amorphous material and connects neighboring crystalline lamellae.
Tie molecules help transfer stress between ordered regions in a semicrystalline polymer.
Toughness
Toughness is the energy a material can absorb per unit volume before fracture, combining resistance to load with deformation capacity.
High hardness does not give a ceramic high toughness when cracks propagate with little plastic strain.
Transverse modulus
The transverse modulus is elastic stiffness across the fiber direction, strongly influenced by matrix compliance and constituent arrangement.
The ideal transverse modulus of a unidirectional composite is much lower than its longitudinal modulus.

V

Viscoelasticity
Viscoelasticity is a combination of elastic and time-dependent response, making deformation or force depend on load duration and temperature.
Viscoelasticity lets silicone putty respond firmly to a quick impact yet flow slowly under sustained loading.
Viscosity
Viscosity is a material’s resistance to flow, measured in Pa·s; glass becomes easier to shape as its viscosity falls during heating.
Glassblowing uses a temperature range where viscosity is low enough for shaping but high enough for control.
Vitrification
Vitrification is the formation of a glassy phase during ceramic firing that fills some pores and bonds remaining particles on cooling.
Feldspar promotes vitrification in a whiteware body by helping form a glassy liquid during firing.
Volume fraction
A volume fraction is the volume occupied by a constituent divided by total material volume, distinct from its share of mass.
A dense particle phase can have a much smaller volume fraction than its mass fraction suggests.
Vulcanization
Vulcanization is the creation of permanent crosslinks in rubber, classically sulfur bridges, improving recovery and resistance to flow.
Light vulcanization keeps natural rubber flexible while stopping chains from sliding permanently apart.

W

Water–cement ratio
The water–cement ratio is the mass of mixing water divided by cement mass, influencing workability and hardened capillary porosity.
A water–cement ratio of 0.50 means 150 kg of water for 300 kg of cement, before any separate adjustments.
Weight-average molecular weight
Weight-average molecular weight is the mean chain molecular weight weighted by each class’s mass fraction, emphasizing longer chains.
Long chains contribute disproportionately to weight-average molecular weight because each carries more mass.
Whisker
A whisker is a very thin single-crystal reinforcement with high strength due to its small size and low population of severe flaws.
A whisker can be extremely strong but difficult and expensive to incorporate into a uniform composite.

Y

Yield strength
Yield strength is the stress at the clear maximum after the elastic region of a plastic polymer’s tensile curve.
A polymer specimen with an obvious yield maximum does not need a metal-style offset construction to locate that yield strength.

About this lesson

By StudeliReport a mistake

Make your own Study Materials

Turn your notes, slides and documents into Study Guides, Practice Questions, Flashcards and 6 more tools.

Get Started